Partial seasoning and preservative treatment systems for pine roundwood
1982 - IRG/WP 3187
Experimental trials at FRI, Rotorua showed that the steaming schedule normally used for steaming and venting is also suitable for steaming and vacuum seasoning. Applying vacuum of up to -84 kPa immediately after steaming did not increase the initial loss of wood moisture significantly in comparison to steam/venting. The main improvement to wood condition by using steam/vacuum appeared to be to dis...
A J Bergervoet


Survey of practical methods for conditioning of forest products before preservative treatment
1971 - IRG/WP 39
The seasoning of forest products is undertaken for a wide range of end uses and is becoming increasingly required for applications and building construction and secondary manufacturing industries. A wide range of applications of new technology and specifically required seasoning schedules is being actively developed for such requirements, but less attention has been given to the means by which woo...
J Rak, T S McKnight


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


Effect of juglone from Juglans mandshurica bark activity of wood decay fungi
2009 - IRG/WP 09-30502
Juglone was extracted from Juglans mandshurica bark via vacuum-assisted steam stripping. The extract was characterized by Fourier Transform Infrared Spectroscopy (FTIR), 1H Nuclear Magnetic Resonance (NMR) and Gas chromatography/mass spectrometry (GC-MS). The extraction process was easy to perform and produced excellent yields (0.22 g juglone/100 g of bark) of a high purity extract (96.42% juglone...
Dongmei Yang, Shuangyue Li, Shujun Li, Wenqiang Su, Yan Jin, Molong Sun


Drying Rates and Mold Growth on Various Building Materials under Different Environmental Conditions
2010 - IRG/WP 10-20454
Mold growth on building materials is a major problem for homeowners. The most suitable method to control mold growth on building materials is to utilize design features, construction tools and practices that prevent moisture accumulation, and keep the wood as dry as possible. In order to achieve this, engineers and homebuilders have to know the effects of various temperature and moisture conditi...
Dian-Qing Yang


Influence of Copper Preservative Type on Earlywood and Latewood Distribution of Copper in Treated Wood
2010 - IRG/WP 10-40507
Some of the new water based copper containing wood preservative systems use particulate “micronized” copper as the primary biocide instead of the more traditional soluble amine copper based systems. Studies were conducted to investigate how this difference in the type of copper system might impact both initial and post drying distribution of the preservatives in wood. Of specific interest wa...
A Zahora


Chapter 11 - Preservation of talla bamboo
2007 - IRG/WP 07-10635-11
Researches revealed that the talla bamboo (Bambusa tulda Roxb.)) in Bangladesh could be full-cell pressure treated with CCA in green and dry conditions. The dry bamboo gives higher loading absorptions than green one when impregnated at same treating conditions. Also higher absorptions are obtained at nodes rather than internodes. Adequate penetration and retention results for ground and wate...
A K Lahiry


Chapter 12 - Treatment Groups of Bamboo
2007 - IRG/WP 07-10635-12
Study on distribution of CCA in three major bamboo species in Bangladesh, full-cell pressure treated at green and dry conditions revealed two treatment groups and some treating principles. Higher adequate treatment for ground and water contact use is only possible by treating problematic bamboo species pre-kiln dried up to half of its FSP and non-problematic species pre-dried up to FSP (20% ...
A K Lahiry


Chapter 14 - Accelerated fixation of CCA-treated bamboo
2007 - IRG/WP 07-10635-14
Chromated copper arsenate type C (CCA-C) fixation study on impregnated (with adequate w/v 6% CCA solution) then boiled, oven-dried, normal, air-dried and steamed bamboo slices of airdried borakbamboo (Bambusa balcooa Roxb.) of Bangladesh, revealed almost complete fixation in steamed (accelerated fixation) and air-dried (3 weeks, slow fixation) bamboo slices compared to moderate to low fixati...
A K Lahiry


Multilayer hot-press drying and chemical modifying of poplar wood with urea-formaldehyde prepolymer
2011 - IRG/WP 10-40539
The objective of this study was to determine the technology of chemical modifying and multilayer hot-press drying on poplar wood. The chemicals were impregnated into cell lumen space by pulse-dipping machine to improve the dimension stability and mechanical property of timber. The timbers were compressed and dried by the multilayer hot-press drying to increase the density of timber. Results indica...
Guofeng Wu, Yifei Jiang, Sheng Yao, Junwen


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani


Limited variability in biological durability of thermally modified timber using vacuum based technology
2011 - IRG/WP 11-40567
The SmartHeat® thermal timber treatment is a new technology based on the process parameters being steered very precisely mainly due to the vacuum applied and heating system involved. Timber treated with this technology shows a potential for less variability of biological durability in one batch. Several batch treatments were sampled and assessed on statistical variability of decay resistance agai...
J Van Acker, S Michon, J Van den Bulcke, I De Windt, B Van Swaay, M Stevens


Characterizing long term leaching behaviour of copper from preservative treated wood in a practical exposure scenario
2011 - IRG/WP 11-50278
To investigate the prediction of the long term emission of copper from preservative treated wood in a Use Class Class 3 scenario, treated boards were exposed vertically above ground to natural weather conditions. The study included two products; an amine copper ACQ-type formulation, air-dried after treatment to a 22 kg/m3 retention, and the same formulation which was hot oil vacuum dried after tre...
T Mark Venås, M Klamer


The activity of a wood-decaying fungus during drying and rewetting cycles measured by isothermal calorimetry
2013 - IRG/WP 13-20526
Wood decaying fungi are an essential part of any ecosystems as they are the main decomposers of cellulose and lignin-containing materials. But as wood is a common building material the risk for decay fungi growth and subsequent degradation of our construction material is a concern. There are important physiological aspects of the growth and activity of decay fungi that are unknown today, and witho...
S Johansson, L Wadsö, A Pilgård, G Alfredsen


Effect of the nature of the inert atmosphere used during thermal treatment on chemical composition, decay durability and mechanical properties of wood
2013 - IRG/WP 13-40625
Wood heat treatment is an attractive alternative to improve decay resistance of low natural durability wood species. Nowadays, several types of thermal treatments of wood exist. These treatments differ mainly by the nature of the inert atmosphere used to avoid wood combustion which may correspond to: nitrogen, vacuum, steam or oil. Decay resistances as well as mechanical properties are strongly co...
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Comparison of moisture loss and its increment during the rehearsal process based on natural drying and water soaking application with or without sealing the trial discs of Common black poplar (Populus nigra L.)
2013 - IRG/WP 13-40639
This study was subjected to be set up to prove the pattern of moisture loss and moisture increment within the same wood samples prepared as the discs (30x23±3 cm diameter) with or without the bark intact during drying and in the duration of the water soaking application. In this concept, wood was exemplified by Common black poplar (Populus nigra L.) of the five 12 year old trees that are grown in...
I Usta


A screening of factors that might influence the result of laboratory decay tests
2014 - IRG/WP 14-20548
Laboratory fungal decay tests provide important tools for performance testing of wood materials. But they are also hampered with some uncertainties regarding reproducibility. In addition to variation between fungal species and strains the test conditions are also believed to have some influence. The aim of this study was to screen the effect of a selection of test parameters that might influence t...
E Larnøy, G Alfredsen, A Treu, S Kolstad


Functional silicones used as a potential tool for the development of non-biocidal wood treatments
2015 - IRG/WP 15-30665
The increase of wood resistance against biological agents for outdoor use is conventionally performed by deep impregnation with preservatives. However, some of the traditional wood preservatives, used for decades for wood protection and regarded as the most effective, are currently subjected to severe restrictions because of their toxicity. In fact, new preservation technologies are constantly ent...
F Lhumeau, C Delaite, F Marchal, F Pochon, M Kutnik


Performance of kiln-dried and air-dried anti-sapstain treated pallet timber under use scenarios against wood discolouring fungi
2015 - IRG/WP 30669
During their lifespan there is a high probability that wooden pallets and packaging material will be exposed to rainfall or rewetting conditions, increasing the risk of growth of discolouring fungi. Kiln-drying of wooden pallets and packaging material without anti-sapstain treatment does not give efficient protection against wood discolouring fungi during rewetting periods. However additional temp...
A Steitz, E Stoyanova, N Pfabigan, R Gründlinger


Chemical, physical-mechanical characterization and durability of thermally modified beech and ash wood by thermo-vacuum process (Termovuoto)
2016 - IRG/WP 16-40758
The paper illustrates part of the results from the CIP Eco-innovation project “Thermo-vacuum: new process for new generation of thermally modified wood”. The project is part of the 7th Framework Programme for European Research and Technological Development, and thermo-vacuum modified wood is already on the European market. The project was selected by the European Commission, EASME Agency, as "...
M Jebrane, I Cuccui, O Allegretti, N Terziev


Three-Dimensional Digital Image Correlation of Strains in Profiled Wood Decking Exposed to Wetting & Drying
2017 - IRG/WP 17-20611
We use three dimensional digital image correlation to measure the strains that develop at the surface of profiled radiata pine (Pinus radiata D. Don) deck boards subjected to a wetting and drying cycle. We hypothesise that surface profiling will change the pattern of strain distribution at the surface of deck boards by concentrating stresses at the base of profile grooves. Five groups of three deck board samples were produced from five different pieces of machine stress-graded radiata pine wood. Two wavy profiles, ribble or ripple, were tested. Flat unprofiled boards acted a control. Each board was fixed to a rigid frame and subjected to a wetting and drying cycle. Full field surface strain data was collected using 3D digital image correlation. Strains varied across the surface of both flat and profiled boards. Profiling changed surface strain patterns; strain maxima and minima developed in the profile ridges and grooves during wetting, respectively, but this pattern of strains reversed during drying. Such a pronounced reversal of strains was not observed when flat boards were exposed to wetting and drying, although there was a shift towards negative strains when flat boards were dried. We conclude that profiling changes surface strain distribution in deck boards exposed to wetting and drying, and causes high strains to develop in the grooves of profiled boards. These findings help explain why checks in profiled deck boards are mainly confined to profile grooves where they are difficult to see, and the success of profiling at reducing the negative effects of checking on the appearance of wood decking.
J Mallet, S Kalyanasundaram, P D Evansa


Treatability of beechwood railway sleepers with potential creosote substitutes
2017 - IRG/WP 17-40790
Maintenance of an efficient railway infrastructure still requires the use of wooden railway sleepers, particularly because wooden sleepers have more favourable properties for intensified vibrations than concrete or steel sleepers. Creosote, used for decades for the impregnation of railway sleepers, will possibly no longer be available for this application due to European legislation. This reveals ...
N Pfabigan, E Habla, R Gründlinger


Charring of Norway spruce wood surface – an alternative surface modification technique?
2019 - IRG/WP 19-40870
Charring is an old wood surface treatment technique, mainly performed on wooden façade elements with the aesthetical aims, but also with the purpose of protection. This flame treatment method can be grouped into heat treatment processes. Below the top charred layer of damaged wood there is a layer which is during flame treatment exposed to high temperatures in anoxic or semi-anoxic conditions. Th...
M Petric, M Pavlic, J Zigon


Promoting Commercially Available Epoxy Resins for Non-biocidal Wood Preservation
2019 - IRG/WP 19-40877
Commercially available epoxy and polyamine resins were evaluated with the aim of developing new non-biocidal wood preservation treatments. A simple method allowing the impregnation of wood by vacuum double impregnation followed by a curing process was developed for two reference species, beech Fagus sylvatica and Scots pine Pinus sylvestris. The tested products were evaluated for their ability to ...
P Poveda, M Mubarok, S Dumarcay, M Montibus, I Le Bayon, M Kutnik, P Gerardin, F Simon