Comparison of laboratory and natural exposure leaching of copper from wood treated with three wood preservatives
2008 - IRG/WP 08-50258
Standard and non-standard laboratory and field leaching tests were used to compare copper leaching from wood treated to above ground and ground contact specified retentions for three wood preservative systems, CCA-C, ACQ-D and a micronized copper formulation with quat DDAC as co-biocide. Copper leaching was highest for the ACQ formulation. Percent leaching was lowest for the micronized copper sy...
P A Cooper, Y T Ung


Categorization of 300 timber, bamboo and cane grown in Bangladesh based on their families, origins, growths, physical and mechanical properties
2009 - IRG/WP 09-10684
In this study the 300 timber, bamboo and cane plants grown in Bangladesh have been classified into various categories based on their taxonomic families, origin of species, rate of growth, color of wood, texture of wood, shrinkage of wood, equilibrium moisture content (EMC) of wood, flammability of wood, cutting and sawing properties of timber, finishing and polishing qualities of wood, machining p...
A K Lahiry


Durability and fungal colonisation patterns in wood samples after six years in soil contact evaluated with qPCR, microscopy, TGA, chitin- and ergosterol assays
2009 - IRG/WP 09-20402
There is a need to establish new objective and sensitive methods for early detection and quantification of decay fungi in wood materials. Molecular methods have proven to be a useful tool within wood protection issues, however, this field is still poorly explored and so far relatively few have used these methods within the field of wood deterioration. Among the techniques used in the indirect quan...
A Pilgård, G Alfredsen, I Børja, C Björdal


Wart Morphology can Distinguish White Cypress Pine from the Less Durable Species, Black Cypress Pine
2009 - IRG/WP 09-20406
White cypress pine (Callitris glaucophylla) wood is durable enough to be used outdoors, but occasionally there are reports of its premature failure in ground contact, which may be due to its substitution by the less durable species, black cypress pine (C. endlicheri). It has been difficult to prove this, however, because the woods of both species are very similar in structure and cannot be separat...
R Heady, R Cunningham, P Evans


The Promotion of Timber and Timber Product uses in China - Government's Role in Regulation and Standardization
2009 - IRG/WP 09-20424
Chinese Government always pays special attention to resource and environmental issues, therefore, resource saving and environmental protection are part of the basic state policies. This paper provides a brief summary of the key policies which guide the practices in promoting timber conservation and efficient utilization in order to meeting social demands of the wood uses. In the paper, the develop...
Liu Nengwen


Copper to quat ratio in alkaline copper quat (ACQ) wood preservative - Effects on fixation and leaching of preservative components in red pine
2009 - IRG/WP 09-30496
This study investigates the effect of the relative proportion of copper oxide (CuO) to didecy dimethyl ammonium carbonate (DDACb) in an alkaline copper quat (ACQ) formulation on the rate of copper fixation or stabilization and the resistance of treated wood to leaching of copper and quat (DDACb). Red pine samples were treated with ACQ, having CuO to DDACb ratios of 2:1 (the normal ratio for ACQ-D...
S Pankras, P A Cooper, T Ung, L Awoyemi


Re-Distribution of Copper in the Cell Walls of Wood Treated with Micronized Copper Quat
2009 - IRG/WP 09-30506
Wood treated with copper-based preservatives to be used in ground contact may fail to inhibit soft rot fungi if penetration of copper into the cell wall is insufficient. Preservatives containing soluble copper are known to penetrate the cell wall; however, it is not known whether preservatives containing particulate copper will also migrate into the cell wall in sufficient quantities to control so...
R Stirling, J Drummond


Colour change monitoring of photodegradation in Scots pine (Pinus sylvestris) – a short term focus
2009 - IRG/WP 09-40442
Colour change monitoring of photodegradation is a quick and easy method for monitoring rates of photodegradation in timber. A study was undertaken to compare this technique to other monitoring methods, including microtensile strength changes and weight loss. Colour changes due to accelerated sunlight exposure were monitored using a Datacolor check spectrophotometer and compared with a set of contr...
V Sharratt, C A S Hill, D P R Kint


Effectiveness of a superficial treatment of bifenthrin to protect softwood framing from damage by subterranean and drywood termites in Indonesia
2009 - IRG/WP 09-40443
Various experimental testing procedures were undertaken in Indonesia to determine the effectiveness of a superficial (envelope) treatment of bifenthrin to protect softwood framing from damage by two species of subterranean termite (Macrotermes gilvus and Coptotermes curvignathus) and one species of drywood termite (Cryptotermes cynocephalus). Lengths of framing (Pinus radiata sapwood) were commerc...
P Sukartana, J W Creffield, A Ismanto, N E Lelana


Component leaching from CCA, ACQ and a micronized copper quat (MCQ) system as affected by leaching protocol
2009 - IRG/WP 09-50261
Leaching results for Cu, Cr and As (CCA) and Cu (ACQ and MCQ) from southern pine are compared for laboratory tests (AWPA E11, and draft OECD methods I and II) and natural weathering of horizontally and vertically oriented lumber samples over two seasons. This paper expands on results and comparison of results presented at the IRG regional meeting in Costa Rica in Dec 2008 (Cooper and Ung 2008) a...
P A Cooper, Y T Ung


Rapid Microwave-Assisted Acid Extraction of Metals from Chromated Copper Arsenate (CCA)-Treated Southern Pine Wood
2009 - IRG/WP 09-50262
The effects of acid concentration, reaction time, and temperature in a microwave reactor on recovery of CCA-treated wood were evaluated. Extraction of copper, chromium, and arsenic metals from chromated copper arsenate (CCA)-treated southern pine wood samples with three different acids (i.e., acetic acid, oxalic acid, and phosphoric acid) was investigated using in microwave reactor. Oxalic acid wa...
Bin Yu, Chung Y Hse, T F Shupe


Life Cycle Assessment of treated timber: methodological aspects and first results
2009 - IRG/WP 09-50264
Environmental information on products is more and more required as a key to the market, and the building sector in Europe is certainly advanced in that direction. In France, Environmental Product Declarations are becoming very common for construction products. Therefore, the CTB P+ and CTB B+ certification comity as commissioned FCBA to perform the Life Cycle Analysis of treated timber in order to...
E Vial, M Bertrand, C Cornillier, G Deroubaix


Microwave Surface Modification of Radiata Pine Peeler Cores for Preservative Treatment
2009 - IRG/WP 09-40453
Radiata pine peeler cores are classified as a by-product derived from the cores of logs left over after the veneer peeling process. The core can be potentially developed for value added solid wood products as it is abundantly available and has a constant diameter. However, the core needs to be preservative treated because of low durability in ground contact. An additional problem is that the wood ...
K Sugiyanto, G Torgovnikov, P Vinden


Barefoot-heat-impact of oil-heat-treated wood: An important thermal property of decking boards
2009 - IRG/WP 09-40458
In this study the phenomenon of sensual heat impression was examined, when walking with bare feet on sun exposed wood based decking boards. A suitable method for measuring the heat flux from decking boards into an artificial foot was developed. The method and measuring device is described as well as results from measuring three different decking board materials: Oil-heat-treated spruce (OHT), untr...
A O Rapp, C R Welzbacher, C Brischke


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp


Hydrofluoroalkanes as carrier solvents for timber preservation
2009 - IRG/WP 09-40463
Hydrofluoroalkanes are a specific category of hydrofluorocarbon (HFC) commonly used in refrigeration applications. Some HFCs hold potential for use as carrier fluids for preservatives used to protect timber above ground. They do not share the most significant disadvantages of currently used carriers for these applications. At ‘conventional’ operating pressures, they are capable of rapid, full ...
M J Kennedy, B Walker, C Erskine


Wood properties influencing the penetration of Scots pine (Pinus sylvestris) sapwood with the wood modification agent furfuryl alcohol
2009 - IRG/WP 09-40470
The European standard EN 350-2 classifies Scots pine sapwood as class 1 (easy to treat). However large variations in sapwood penetration exist which affect a homogenous distribution of preservatives. Hence individual penetration schemes have to be developed and adjusted to the material most difficult to treat in order to provide adequate sapwood penetration. To ensure better economic process con...
K Zimmer, E Larnøy, G Koch


Assessment of the marine borer resistance and abrasion resistance of lesser known hardwood timber species for use in marine construction
2010 - IRG/WP 10-10711
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, candidate timber species were selected for testing both in the laboratory...
J R Williams, G S Sawyer, G Malyon, S M Cragg, J D Icely, J Simm, M Meaden


Control of Reticulitermes grassei as a pest in Spain: Termite distribution in an urban area
2010 - IRG/WP 10-10719
The European subterranean termite Reticulitermes grassei Clément, 1978, has been an important pest in Palenciana, a locality in the southern province of Cordoba (Spain) for a long time. The different stages of the pest elimination process have been studied and are presented here. Firstly, a through inspection of all town dwellings was conducted in order to determine a theoretical affected area of...
E Alcaide, R Molero, J Diz, M Gaju


Frequency of fungal decay in softwood windows in Germany
2010 - IRG/WP 10-10725
Knowing how often fungal decay occurs is a fundamental basis for general recommendations of preservative measures. To optimize the German recommendations for chemical wood preservation of windows made out of pine or spruce more than 2000 windows have been inspected. All windows had an opaque coating and were between 2 and 17 years old. The selection of the inspected windows was kept as randomly as...
D Lukowsky, O Moarcas, A Luette


Estimating the age of subterranean termite attack and damage in buildings
2010 - IRG/WP 10-10727
This paper describes physical and experimental methods and a mathematical model (Rotramel 2003) to assist in estimating the age of subterranean termite attack and damage to building structures. Timber, building and termite management industries have to develop new strategies to assess and estimate termite attack and damage in the current climate of global warming. A case study will be used as an e...
J R J French, B M Ahmed Shiday, J Thorpe


Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas


Onset of mould growth – the effect of climate variability and different geographic locations
2010 - IRG/WP 10-20446
This paper presents a study on how climate conditions at numerous locations in Sweden affect the risk of onset of mould on wood sheltered outdoors. The results indicate that the risk is clearly higher in the south compared to the north of Sweden. These differences are mainly explained by colder and dryer winter periods in the north which is unfavorable for development of mould. The results also sh...
M Häglund, T Isaksson, S Thelandersson


Adsorption of ionic liquids by Scots pine wood (Pinus sylvestris L.) and beech (Fagus sylvatica L.): equilibrium and kinetic modeling
2010 - IRG/WP 10-20447
In this paper methods for the adsorption study of quaternary ammonium-based ionic liquids on Scots pine (Pinus sylvestris L.) and beech (Fagus sylvatica L) are presented. Kinetic and equilibrium adsorption of compounds were evaluated. The equilibrium data fitted very well to the Langmuir adsorption models. The highest correlation coefficients determined from the pseudo-second order kinetic model ...
J Zabielska-Matejuk, A Stangierska, M Kot


Non-destructive evaluation of termite and decay damaged to timber-in- service
2010 - IRG/WP 10-20451
A leading joint research project was financed by the ARC, engaging some of the leading Universities in Australia, to look at field techniques to determine if timber-in-service is infested with termites and decay fungi after which microwave technology will be employed to eliminate the termites and/or decay in-situ. The next step will be to quantify the damage caused on the sectional dimensions of t...
C Adam, B M Ahmed Shiday, G Brodie


Previous Page | Next Page