Improvement of short rotation teak wood properties through thermal modification
2018 - IRG/WP 18-40842
Teak (Tectona grandis L.f) is one of the most popular tropical timber species. Nowadays, the source of long rotation teak is limited in the availability. Many wood processing industries use short rotation teak, which has lower quality especially in durability and dimensional stability. Heat treatment is an eco-friendly method improving dimensional stability and durability of wood. The objectives o...
L A Pratiwi, I W Darmawan, B George, A Merlin, C Gérardin, S Dumarçay, T Priadi, P Gérardin


Determining the natural durability on xylarium samples: mini-block test, wood powder and chemical profiling
2019 - IRG/WP 19-10944
Xylaria, or wood collections, can be considered sleeping beauties in terms of wood technological and biological output. In this study we focus on determining the natural durability of xylarium specimens from the Federal Xylarium in the Royal Museum for Central Africa. The Federal Xylarium contains over 80,000 specimens, covering more than 13,000 species, mainly from Central Africa. These specimens...
V Deklerck, L De Ligne, J Van den Bulcke, E Espinoza, H Beeckman, J Van Acker


Durability by design – a case study of the performance of wooden decks after 9.5 years of natural weathering
2019 - IRG/WP 19-20648
The service life expected for wood decking manufactured with poorly durable wood species, left untreated and exposed to severe environmental conditions such as high humidity and active biological agents, is usually assumed to be short (less than 10 years). The current classification of wood’s natural durability is based on EN standardised tests which do not fully reflect the real end-use conditi...
M Kutnik, M Montibus


Gloss and hardness variations as early indicators of wood coating failure during weathering tests
2019 - IRG/WP 19-40866
The objective was to track early changes which ultimately will lead to coating failure when exposed to artificial weathering. Two different coatings (one waterborne acrylic paint and one solventborne alkyd stain) were exposed to artificial weathering for 2016 hours according to EN 927-6. Every 168 hours, samples were removed from the artificial weathering device for assessment (general appearance,...
L Podgorski


Potential Use of the Pigment from Scytalidium cuboideum and Chlorociboria aeruginosa as an UV-light Protection Additive in Oil Finishes
2019 - IRG/WP 19-40868
UV-light degradation of wood is one of the top reasons for consumer replacement of outdoor wooden structures. This type of degradation is seldom mechanical, and is instead often motivated by loss of aesthetics (graying). There are numerous commercial products available on the market that deal with this loss of color, many of which contain added pigments to ‘rejuvenate’ or ‘revitalize’ grey...
S M Vega Gutierrez, D W Stone, R He3, P T Vega Gutierrez, Z M Walsh, S C Robinson


The anti-weathering mechanism of extractives in thermally modified Scots pine
2019 - IRG/WP 19-40880
Results from the electron spin-resonance spectroscopy (ESR) analysis indicated that thermally modification of wood can inhibit the generation of phenoxyl radicals during UV irradiation and consequently lead to the increase of the color stability of wood. In order to clarify the evolution and role of extractives in thermally modified wood during the process of weathering, the compositions of aceton...
H Shen, J Cao


Effect of pretreatment of wood surfaces with a copper monoethanolamine solution on the natural weathering performance of semitransparent stains
2019 - IRG/WP 19-40881
Semitransparent stains for wood products are favored for outdoor applications in Japan because these finishes do not hide the wood grain. However, the photoprotective effects of wood surfaces are low, therefor there is a need to improve the weathering performance. We examined the natural weathering performance of semitransparent stains on wood pretreated with a copper monoethanolamine solution (Cu...
S Isaji, H Shibui, Y Hirabayashi


Wood protection techniques and natural weathering: their effect on aesthetics and preference of people
2019 - IRG/WP 19-50351
Current research successfully contributes to improving wood protection techniques. However, the vast majority of research on preventing degradation of wood ignores a critical aspect of making successful products and processes – user selection of materials, which may largely depend on the aesthetical qualities. Wood treatments change the tactile and visual properties of wood substantially and the...
D Lipovac, M D Burnard, A Sandak, J Sandak


Durability of tropical species from Peru according to European Standards
2020 - IRG/WP 20-10964
Natural durability is defined as the intrinsic resistance of wood against the attack of destructive organisms. There are standardized methods to estimate a durability value. In Europe, the standard EN-350 is responsible for establishing the basic guidelines, as well as the necessary tests to determine this value, which is essential to know the degree of protection needed for the tested wood to ext...
J Valdivia, P Gómez, M T Troya, L Robertson, J A Martín, A Loayza


Monitoring of wood preservatives exposed to weathering: Extraction and analysis methods of organic biocides from treated wood and collected rain runoff
2020 - IRG/WP 20-30753
Weathering is the cause of numerous damages for outdoor joineries. Protection of wood using a preservative treatment covered with a coating is a process widely used to limit these damages. However, biocides from preservative treated wood are prone to degradation and leaching, having a direct influence on the joinery service life. This document deals with extraction and analytical methods for bioci...
O Ouali, K Le Ménach, E Raphalen, L Podgorski, S Legay, H Budzinski


Influence of weathering on surface roughness of thermally modified wood
2021 - IRG/WP 21-40915
Thermally modified wood is exposed to weathering similarly as other wood-based building materials. It has been reported that if thermally modified wood is exposed to weathering, its moisture performance might decrease fairly fast. The aim of this study was to determine whether this phenomenon is associated with crack formations or roughness. Norway spruce, thermally modified spruce, wax-treated th...
E Kerzic, B Lesar, M Humar


Dynamics of fungi colonization on the surface of Scots pine wood during natural weathering in different European climate zones
2022 - IRG/WP 22-10984
Wood The presence of fungi leads to biomaterial decay and/or changes in aesthetical appeal. The start of fungi colonization as well as the following growth on wood are primarily influenced by four factors: ambient temperature, moisture history of the object, access to oxygen, and intrinsic properties of the exposed wood, considered here as a source of nutrients for microorganisms. A prevalence of ...
F Poohphajai, O Myronycheva, O Karlsson, L Rautkari, J Sandak, A Sandak


Natural durability and moisture dynamics of commercially important European wood species after weathering
2022 - IRG/WP 22-10992
Wood is a frequently used material. Timbers’ mechanical properties, particularly its favourable strength-to-mass ratio, make them suitable for many uses. Current environmental awareness has led to its renewed importance as a building material. However, wood is susceptible to decay that severely affect its outdoor performance. This study investigated how weathering affects the natural durability ...
E Keržič, M Humar


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Field tests of different tropical wood species in sea water
2022 - IRG/WP 22-30773
A number of tropical timbers have been tested according to EN 275 at Kristineberg Marine Research Station in Sweden since 1999. Most of these tests have started during the last 5-8 years. Wood species included have been Lophira alata (Azobé/Ekki), Minquartia guianensis (Manwood/Acaria), Chlorocardium rodiei (Greenheart), Cyclodiscus gabonensis (Okan/Denya), Shorea spp. (Bankirai), Dicorynia guia...
M Westin, P Larsson Brelid


Effect of furfurylation treatment on the performance of three Canadian wood species
2022 - IRG/WP 22-40925
The demand for exterior wood siding is stagnating in North America, partly due to the perception of consumers, architects and contractors regarding their durability and maintenance. Improving attributes such as the dimensional stability of wood is therefore necessary to make it more attractive to consumers. This project aims to assess the performance of Canadian species; white spruce (Picea glauca...
G Boivin, D Schorr


A novel wood preservation technology improving durability and water-related properties
2022 - IRG/WP 22-40926
A newly developed silicone oil (Archroma Management GmbH, Switzerland) was tested for wood modification purposes. Scots pine sapwood was treated with aqueous solutions of this silicone oil and showed a penetration of the modification agent into the wood cell wall. Both, biological durability and moisture-related properties, experienced significant improvements by the modification. Besides, the mod...
L Emmerich, H Militz, M Vila


Optimized composition of alkyd emulsion with nanoparticles of iron oxide for enhancing protection of thermally modified wood
2022 - IRG/WP 22-40940
Thermal treatment is acknowledged as an environmentally friendly method to improve durability of wood and some of its properties, such as biological resistance, dimensional stability, reduced hygroscopy. Despite these improvements, when used outdoors, also thermally treated wood is subjected to the action of environmental factors, like solar radiation, moisture, precipitations, temperature, etc., ...
E Sansonetti, D Cīrule, I Andersone, B Andersons, E Kuka


Influence of weathering on the mechanical properties and performance of exterior wood coatings
2022 - IRG/WP 22-40951
Three commercial coatings were exposed to artificial (EN 927-6) and natural weathering (EN 927-3) on wood samples. Cracking was visually assessed as well as Persoz hardness. Free films of the same coatings were also exposed to the same weathering tests before their tensile properties were measured. Results show that artificial and natural weathering modified the overall mechanical properties of wo...
L Podgorski, J-D Lanvin


Unlocking the potential of tropical fast-growing hardwood species
2023 - IRG/WP 23-11010
Social forestry or community managed forestry practices have been promoted as an inclusive way to mitigate climate change through the framework of the UNFCCC scheme of the Reduce Emission Deforestation and forest Degradation (REDD+) programme. Fast growing wood species are one of the least tapped social forestry commodities in Southeast Asia, and they have the potential to be upscaled to meet the ...
S Fauziyyah, R Wimmer, C Brischke


Natural durability of tropical plantation woods case in teak
2023 - IRG/WP 23-11011
Teak (T. grandis) is one of the most popular tropical timber species when it comes to the natural durability. High value of teak timber is attracting the attention to expand fast growing teak plantations, and the natural durability of plantation teak wood has been examined in various provenances of tropics. Natural durability of plantation and natural teak wood using three disks was examined throu...
K Yamamoto


Natural durability of 9 tropical species suitable for round wood timber building: fungi and termites laboratory screening tests
2023 - IRG/WP 23-11013
In numerous tropical forest species, wood properties are poorly described and wood is under-valorized. Especially very few is known about small diameter trees although they may be used, directly as round wood, in construction timber building. A selection of abundant species was done and characterization tests were performed to assess their usability as building material. The aim of this work was t...
M Leroy, K Candelier, J Damay, J Bossu, R Lehnebach, M-F Thevenon, J Beauchene, B Clair


Long-term Performance of Treated Timbers in a Sub-tropical Marine Exposure
2023 - IRG/WP 23-11015
The long-term performance of preservative-treated and modified wood in marine exposures was assessed in Brisbane, Queensland, Australia. This report describes the final destructive assessment of the surviving Australian panels after 11 years of exposure. This site presents the potential for attack by shipworms (likely Bankia spp.), pholads (Martesia striata), Limnoria and Sphaeroma terebrans. Mos...
E L Galore, J Norton, A Zahora


Optimisation of accelerated weathering procedure as an alternative to natural weathering
2023 - IRG/WP 23-20693
Comprehensive tests need to be performed to obtain the most accurate data possible on the durability of wood. The most reliable performance tests are field tests. However, since this is very time-consuming, we frequently rely on laboratory tests. To increase the reliability of the laboratory tests, samples are preconditioned with natural or artificially accelerated weathering methods that simulate...
E Keržič, M Humar, V Vek


Accelerated surface mould testing for exterior wood treatment in Temperate, Tropical and Laboratory environments
2023 - IRG/WP 23-20699
Mould attack is a very common cause of discoloration on wooden surfaces and can subsequently promote development of wood decay by other organisms. Prevention of mould growth is relevant for both pigmented wood paints as well as more transparent systems with a high or low amount of binder. The use of commercial biocides has led to effective microbiological inhibition in many contexts, but the incre...
A Nazeri, J Stenbaek, T R Laursen, A H H Wong, B M Hasnul