Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus


Use of Variable Pressure Scanning Electron Microscopy for in situ Observation of Degradation of Wood Surfaces during Artificial Weathering
2012 - IRG/WP 12-20489
Variable pressure scanning electron microscopy (VPSEM) is capable of observing electrically non-conductive materials like wood without the need to render the surface conductive by applying a coating of gold, platinum or carbon. Hence, there is the possibility that VPSEM could be used to non-destructively follow the structural changes occurring at wood surfaces during weathering, because specimens ...
F Hatae, Y Kataoka, M Kiguchi, H Matsunaga, J Matsumura


Evaluation of Five Novel Organotin(IV) Complexes as Wood Preservatives
2012 - IRG/WP 12-30590
Three selected non durable tropical wood species namely Alstonia scholaris (pulai), Macaranga triloba (mahang) and Hevea brasiliensis (rubber) were chemically impregnated with five novel organotin(IV) complexes using vacuum-pressure treatment method. The objectives of this study were to determine the treatability and efficacy of novel organotin(IV) complexes against white and brown rot decay fungi...
M M Rahman, I Jusoh, M A Affan, A Husaini


Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin


Comparison of exterior performance of two coating systems based polyurethane applied Pinus sylvestris L. and Picea orientalis L. wood
2012 - IRG/WP 12-40588
Some surface changes in sapwood and heartwood of two species before applying clear-coating were characterized after accelerated weathering time. Wood specimens covered with two types polyurethane (PU) films were also observed in accelerated weathering exposure. In this study, changes on the wood surface were compared of between wood specimens covered with two types polyurethane (PU) films after ir...
Ö Özgenç, Û Cafer Yıldız


Effects Of Wood Preservative On Mechanical Properties Of Glulam Manufactured From Lower Density Malaysian Tropical Timber
2012 - IRG/WP 12-40590
This study is to investigate the effect of wood preservative on the mechanical properties of glulam timbers made from low density Malaysian hardwood timbers. Utilization of lower density Malaysian tropical timber for structural applications have not exploited extensively due to their inferior strength. By converting into treated glued laminated (glulam) timbers it could offer the possibility of th...
L Francis, Z Ahmad


Improvement of the biological performance and dimensional stability of two tropical woods by thermal modification
2012 - IRG/WP 12-40605
Pink cedar wood and rubberwood were thermally modified at 230°C in air for 4 h or for 8 h, and then subjected to bending, compression and hardness tests to evaluate the effect of the treatment on these mechanical properties. The biological performance of the modified wood was also determined, according to EN113, and the dimensional stability measured by means of the anti-swelling efficiency. The ...
M M González-Peña


Biodegration of treated wood waste by native fungal communities of tropical soil in French Guiana
2012 - IRG/WP 12-50285
Woods have been protected with fungicides for a long time, and the effects of these fungicides on soil after being leached into the ground have turned out to be a true environmental issue. It is in this perspective that we are proposing to study fungal communities of these contaminated woods in a purpose of bioremediation. Most of precedent studies have focused on ability of some Basidiomycetes an...
A Zaremski, L Gastonguay, C Zaremski, F Chaffannel, J Beauchêne, G LeFloch


Fixation and leaching characteristics of Malaysian tropical hardwoods treated with CCA-C
2012 - IRG/WP 12-50289
The fixation and leaching characteristics of 8 Malaysian tropical hardwood (MTH) species treated with chromated copper arsenate (CCA-C) wood preservative were examined. The species evaluated were Acacia (Acacia mangium), Bintangor (Calophyllum sp.), Geronggang (Cratoxylon arborescens), Medang (Litsea sp.), Meranti rambai daun (Shorea acuminata), Putat (Planchonia sp.), Ramin (Gonystylus sp.) and S...
S Salim, S Shahomlail, Z Ashaari, Yong-Seok Choi, Gyu-Hyeok Kim


Classifying white rot decay resistance of some hardwoods from Sarawak and Peninsular Malaysia and correlations with their tropical in-ground durability
2012 - IRG/WP 12-10788
White rot wood decay under Malaysian (humid tropical) terrestrial conditions pose more serious threats to the in-ground service life of hardwoods than other common fungal decay types. A study is made on decay resistance variation for a total combined list of 30 Peninsular Malaysian and Sarawak timber species (plus 6 exotic reference temperate commercial woods for comparison) using the laboratory s...
A H H Wong, J M E Jem, Lai Jiew Kok


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Study of UV resistance and natural weathering of coatings on chemically modified wood
2013 - IRG/WP 13-40629
In this study, UV resistance and weathering performance of rubberwood (Hevea brasiliensis) and radiata pine (Pinus radiata) modified with benzoyl chloride and acetic anhydride was studied. Performance of polyurethane based wood coatings on modified wood was also evaluated. Unmodified and chemically modified specimens were exposed to accelerated and natural weathering. Modified and unmodified woo...
K K Pandey, K Srinivas


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Molecular characterization and biodiversity of wood-decaying fungi in French Guiana
2014 - IRG/WP 14-10825
Fungi from tropical regions are currently under-represented in the classification system. Indeed, difficult access to tropical forests and irregular occurrence carpophores make it complicated to study fungus species in such environments, unlike in European zones where fungal diversity and taxonomy are better known. The purpose of this work was to enhance classification by integrating new data that...
A Zaremski, L Gastonguay, C Zaremski, J Beauchene


Unexpected natural decay resistance strategies of durable tropical woods Bocoa prouacencis, Vouacapoua americana, Inga alba and relationship with specific gravity and wood extractives
2014 - IRG/WP 14-10832
The study of decay resistance in wood is of interest for wood end-users but also for the global carbon balance since wood biodegradation is a key driver of forest ecosystem functioning through its impacts on carbon and nutrient cycling. We studied the specific gravity and wood extractive contents in order to understand decay resistance against soil microflora after 90 days exposure of sapwood and ...
N Amusant, M Migg, B Thibaut, J Beauchene


Effect of polyurea coatings on performance of Douglas-fir in tropical above ground exposures
2014 - IRG/WP 14-40665
The potential for using polyurea barriers to limit fungal and termite attack was investigated on Douglas-fir lumber and timbers. Termites were capable of penetrating the barrier to attack non-treated wood as well as wood dip-treated with disodium octaborate. The coatings were also exposed above ground for 48 months in Hilo Hawaii. Samples were dissected to detect internal decay. Coated non-trea...
S Uysal, J J Morrell


Study of weathering Characteristics in Profiled and Treated Deck Boards
2014 - IRG/WP 14-40680
Wood exposed outdoors to repeated wetting and drying develops surface checks. Excessive checking of wooden deck boards has been a major source of dissatisfaction to consumers. In this study, Southern pine (Pinus sp.) deck boards were machined to flat (control) and ribbed surface profiles. The specimens were treated with aqueous formulations of 4,5-dichloro-2-N-octyl-4-isothiazolin-3-one (EL2) and ...
M Akhtari, D Nicholas, L Sites


Laboratory Study of Relative Leachability of Chromated Copper Arsenate Preservative from Treated Woods among Soil Types of Sarawak
2014 - IRG/WP 14-50307
Wood and soils are important natural resources from the environment and serves mankind well respectively as structural materials and natural platform erecting such materials. With shortfalls of naturally durable timber species for protected in-ground uses under Malaysian environments, Chromated Copper Arsenate (CCA) treated woods are widely used instead, incurring serious potential threats of pres...
A H H Wong, P K F Chong


Effects of UV Radiation on Melanization and Growth of Fungi Isolated from Weathered Wood Surfaces
2015 - IRG/WP 15-10842
This research tests the hypothesis that fungi isolated from weathered wood will respond to elevated levels of UV radiation by increasing their melanin production. To test this hypothesis, we measured the melanin production and mycelial color of Aureobasidium pullulans and Cladosporium cladosporioides, before and after the fungi were grown under artificial UV, visible light and complete darkness. T...
V A Hernández, P D Evans


Influence of artificial and natural weathering on water exclusion efficacy of wood
2015 - IRG/WP 15-20559
Water exclusion efficacy (WEE) is one of the most important properties of wood that contributes to the overall performance of naturally durable wood species in outdoor above ground applications. WEE is in strong correlation with moisture dynamics of wood, its hydrophobicity and can indicates susceptibility against wood decay fungi. Despite of the importance of this parameter, WEE is not completely...
M Žlahtič, M Humar


Above ground field testing: results of experiments in Brazil after one year
2015 - IRG/WP 15-30660
After the development of new products they need to be field-tested to assess their efficacy under diverse conditions of climate, comparing them with a preservative with proven efficacy. In some testing sites, decay occurs very slowly. The solution would be to bring these tests to locations that are conducive to biodeterioration, like tropical climates. Tropical sites provide higher temperature and...
M F Natale, J M Vidal


Application of nanoparticles of silver and nanoparticles of titanium dioxide in reinforcement of wood and coating for wood in Costa Rica
2015 - IRG/WP 15-40698
Wood is one of the most widely used materials in last 20 years by society in many applications, with a considerable proportion of this material coming from forest plantations. Plantations usually produce timber with reduced strength properties and low natural durability. On the other hand, nanotechnology applications have the potential to increase wood properties. Likewise, nanotechnology cannot o...
A Berrocal Jiménez, R Moya Roque, A Lucrecia Rodríguez, J R Vega Baudrit


How to Increase the Lifespan of Exterior Wood Coatings
2015 - IRG/WP 15-40700
In addition to aesthetic appeal, coatings are designed to protect the wood from weathering degradation in outdoor conditions. This paper gives an overview of the effects of main components of coating, coating properties, and wood treatments on coating performance. Understanding how different type of resins (alkyd, acrylic or polyurethane), amount of pigments, type of solvents (organic or water), a...
M Nejad


Durability of reaction to fire performance of FRT wood products in different end use applications – Methods and results
2015 - IRG/WP 15-40705
Fire retardant treatments (FRT) may considerably improve the reaction to fire properties of wood-based products and the highest fire classifications for combustible products can be reached, but the maintained reaction to fire performance e. g. in exterior applications needs to be addressed in order to form a basis for new and reliable wood products with improved fire performance. A European Techn...