An appraisal of the vertical distribution of attack of untreated and treated wood by warm water sphaeromatids at some tropical sites - A discussion paper
1986 - IRG/WP 4124
Examples of the vertical distribution of burrows of warm water sphaeromatids relative to tide levels and mud line from sites in India, Papua New Guinea and tropical Australia are discussed in detail. These data show clearly that these animals concentrate their attack of resistant natural wood or resistant treated wood in the tidal zone, particularly around Mean Sea Level. Supportive evidence from ...
J E Barnacle, L J Cookson, C N McEvoy


Properties-enhanced albizzia particleboards by incorporating fungicide and insecticide in the glue
1994 - IRG/WP 94-30060
Preservative-treated particleboards were prepared by using tropical fast-growing albizzia and adding fungicides and insecticides to the adhesive-glue. the physical and biological properties of these boards were evaluated. No significant reduction in bending or internal-bond strength due to incorporation of the chemicals was detected. Treated particleboards effectively resisted attack by Coptoterme...
B Subiyanto, S Yusuf, Y Imamura, S Fushiki, T Saito, T Katuzawa


Performance of Two Imidacloprid-Treated Malaysian Hardwoods in an Accelerated Aboveground Termite Test
2005 - IRG/WP 05-30389
The performance of the chloronicotinyl insecticide imidacloprid as a wood protecting termiticide, under a simulated Malaysian biological hazard class H2 (exposure aboveground indoors against termites and wood borers), was evaluated by a novel termite field test protocol. Replicate end-grain sealed air dried test blocks (20 x 20 x 20 mm) of two Malaysian hardwoods, Kembang Semangkok (Scaphium spp.)...
A H H Wong


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


The need for realism in wood preservation research. A key address
1983 - IRG/WP 3254
The approval of a chemical for use as a timber preservative and the design of in service retention requirements represents an act linking fundamental research and commercial timber preservation. How difficult is it to translate figures generated through controlled experimentation into working specifications and how confident can we be in the methods used to provide such figures? The chairman of Wo...
L E Leightley


Evaluation of teak sawdayst Tectona grandis L Fil as a potential source to obtain a natural wood preservative in Colombia
2004 - IRG/WP 04-30356
Plantation Teak (Tectona grandis L. Fil) has been tested as a possible source of natural wood preservatives due to the known excellent durability of old-growth teak wood. Field tests (ground proximity termite and above ground simulated decking exposures) were established in Colombia in April 2003 at two different test sites with different climates (Tropical Dry and Rain forest). Teak heartwood ex...
A Castillo, Y Cabrera, A F Preston, R Morris


Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles
1996 - IRG/WP 96-40075
The Eucalyptus camaldulensis and Acacia mangium round timbers kiln-dried at EMC and full cell pressure treated with CCA-C ensured requisite penetration and adequate dry retention (30 kg/m³ or 4% w/w). The sufficient inherent strength, seasoning property, treatability of sapwood and heartwood equivalent to 44% of radius, natural durability of heartwood, and field investigation on service performan...
A K Lahiry


Assessing the importance of degradation mechanisms on the loss of effectiveness of wood preservatives
2000 - IRG/WP 00-20193
Accelerated ageing systems developed for application to samples in the laboratory prior to biological tests, should reflect those natural deterioration processes that are likely to occur in the hazard classes defined in EN 335-1. Losses through evaporation or the effects of leaching have been recognised, however their importance, relative to other mechanisms has not been quantified. Degradation me...
E D Suttie, R J Orsler, T Dearling


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


Depth of foraging of subterranean termites in tropical Australia
1996 - IRG/WP 96-10141
Stakes of radiata pine (Pinus radiata D.Don) of varying lengths to 800 mm were inserted vertically in the soil with all but their lower 100 mm sheathed in a capped UPVC tube representing a physical barrier to termites. In one series of trials, termites were encouraged to aggregate at the upper ends of the tubes, in order to determine whether they would descend to the lower end of the barrier. In a...
L R Miller, M Hoschke, M Neal


Artificial weathering as an aid to assessing the effectiveness of chemicals for preventing blue stain in service - a co-operative study
1984 - IRG/WP 2215
The paper reports co-operative studies carried out within Working Group II of the International Research Group on Wood Preservation to assess the effects of different artificial weathering systems on the performance of fungicides to control blue-stain in service. It has been shown that Atlas, Xenotest and Marr equipments operated according to particular standard schedules can give essentially the ...
A F Bravery, D J Dickinson


Artificial weathering exposure as an alternative for standard ageing according to EN 84 (leaching) and EN 73 (evaporation)
2002 - IRG/WP 02-20254
In order to verify potential weaknesses of wood preservatives fungal tests are carried out after ageing of wood preservative treated test blocks. The European standard EN 599 as a framework for efficacy assessment of wood preservatives includes the use of two ageing methods prior to fungal testing, namely a leaching method (EN 84) and an evaporation method (EN 73). The European research project "F...
J Van Acker, M Grinda, D J Dickinson


Termite resistance of twenty-eight Indonesian timbers
1982 - IRG/WP 1150
A comparative study of termite resistance of 28 Indonesian wood species has been conducted using small samples measuring 5 x 10 x 20 mm³. The drywood termite Cryptotermes cynocephallus (Kalotermitidae) and the subterranean termite Coptotermes curvignathus (Rhinotermitidae) were used in the study. A resistance classification was derived on the basis of cluster analysis. The result reveals that Alb...
Nana Supriana, P E Howse


Evaluation of tropical wood by-products as a potential source for termite control products
2001 - IRG/WP 01-10408
Termites damaging in houses represent an ever growing threat in Europe, where the phenomenon has accelerated during the last ten years, as well as in the tropics, where infestations are permanent. To fight against this plague, the current methods used, through injection of organochloric or organophosphorized products into the timber structures and walls, are belonging to the past due to the toxici...
A Zaremski, S Robert, J-L Clement, D Fouquet


Screening of modified linseed oils on their applicability in wood protection
2004 - IRG/WP 04-30346
In this study modified linseed oils, rape oil and three waxes were screened on their efficacy as wood protecting agents. By testing all products when impregnated with high retentions in Scots Pine sapwood on water repellence qualities, additionally an accelerated weathering test, drying quality, accelerated brown rot and blue stain test, an indication is formed of the capability of these products ...
A Treu, J Lückers, H Militz


Weathering of copper-amine treated wood
2000 - IRG/WP 00-40155
Copper ethanolamine (Cu-EA) treated southern pine (SP) were artificially weathered with a QUV Weathering Tester. The weathering regime was composed of a continuous UV-light irradiation for 2 hours followed by a water spray for 18 minutes for a total time of 1200 hours. The changes on the surface of the weathered samples were characterized by Fourier transform infrared spectroscopy (FTIR) analysis,...
J Zhang, D P Kamdem


Natural Durability studies and Changes in wood chemistry of some Ghanaian hardwoods during decay by white- and brown-rot fungi
2004 - IRG/WP 04-10542
The natural decay resistance of Esa (Celtis mildbraedii), Wawabima (Sterculia rhinopetela) and Dahoma (Piptadeniastrum africanum) obtained from Ghana was determined according to BS EN 113 (1997). Esa was found not durable to the white-rot, but very durable to the brown-rot; Wawabima was very durable to both white- and brown-rots; and Dahoma was durable to the white-rot, and very durable to the bro...
Zeen Huang, K Maher, S A Amartey


Termite resistance classification of some tropical and temperate species based on the laboratory choice test results against formosan termite, Coptotermes formosanu
2004 - IRG/WP 04-20291
The results of classification of termite durability were varied. We carried out laboratory evaluation of the classification of termite durability on various species by the choice test against formosan termite, Coptotermes formosanus. We classified five grades (very sensitive to very resistant). According to our results, azobe, ipe, keruing, intsia, kapur, yellow meranti, jarraah, malas, cypres...
K Suzuki


Suitability of propiconazole (R 49362) as a new-generation fungicide
1989 - IRG/WP 3529
Propiconazole (R 49362), an anti-fungal triazole-compound of Janssen Pharmaceutica, has been extensively tested to determine its potential use as a wood preserving fungicide. Various tests in both private laboratories and official institutes indicate a good activity against Basidiomycetes (brown and white rot) and Ascomycetes (blue stain-in-service). The active ingredient seems very resistant to w...
A R Valcke


Decay evaluation of the effectiveness of a LOSP envelope treatment in eucalypt and meranti heartwoods for window joinery
1996 - IRG/WP 96-30099
The effectiveness and penetration in heartwood boards of an LOSP formulation containing TBTN was examined by determining decay resistance to the white-rot fungus Perenniporia tephropora. Boards, one metre long, of Eucalyptus regnans, Eucalyptus delegatensis, Eucalyptus obliqua and Eucalyptus sieberi were treated, along with boards of 'light' and 'dark' meranti. ...
L J Cookson, A Trajstman


Accelerated weathering test for the evaluation of wood preservative efficacy
2003 - IRG/WP 03-20262
Wood samples treated with ammonium copper quat (ACQ-1900 and ACQ-2200), Chromated copper arsenate (CCA), Tanalith E 3491 and Wolmanit CX-8 have been studied in accelerated weathering experiments. The weathering experiment was performed by cycles of 2 hours UV-light irradiation followed by water spray for 18 minutes. The changes on the surface of the weathered samples were characterized by FTIR Sp...
A Temiz, M Eikenes, Ü C Yildiz, F G Evans, B Jacobsen


Weathering trials on natural wood finishes in New Zealand
1986 - IRG/WP 3383
The weathering properties of various transparent and semi-transparent exterior finishes for New Zealand-grown radiata pine are currently being examined. After 12 to 16 months' weathering, unpigmented water repellents have failed to provide satisfactory protection from weathering under field test conditions. With the exception of two formulations, penetrating oil-based stains are already s...
D V Plackett, C M Chittenden


Biological and physical properties of phenolic-resin treated wood before and after natural weathering
1999 - IRG/WP 99-40132
Biological and physical properties of phenolic resin-treated particleboards, which were made from fast growing tress and agrowaste as raw materials, were evaluated before and after natural weathering in tropical climate. The particles were sprayed with a mixture of a low molecular weight phenol-formaldehyde resin (5.0, 7.5 and 10% loading) and the adhesive phenol resin (8% loading). Results with l...
S Yusuf, Y Sudiyani, H Kajita, Y Imamura, M Takahashi


Development of software to automate the quantification of checking occurring in preservative treated wood exposed to weathering
2001 - IRG/WP 01-20228
Surface checking often disfigures the appearance of wood treated with water-borne preservatives and treatments designed to reduce such checking have been receiving increasing attention. Progress in this area has however been slowed by the lack of a method of rapidly and accurately quantifying checking at treated wood surfaces. A software package has therefore been developed which identifies, measu...
A G Christy, P D Evans


Field study: Wood degradation pattern in buildings and utility poles in tropical climates of Nigeria
1992 - IRG/WP 92-1521
The paper is the result of five years field study of wood degradation patterns in three ecological forest zones (Guinea Savannah, Tropical rain forest and mangrove forest zones, respectively). It involved 800 residential buildings and 700 electric overhead transmission poles. The methodology used was a modified Eslyn (6) test. A high rate of Ascomycetes and Basidiomycetes attack especially on the ...