Your search resulted in 3425 documents. Displaying 25 entries per page.


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Influence of wood swelling agents on penetration and copper leaching of copper-ethanolamine based wood preservatives
2011 - IRG/WP 11-30556
Copper ethanolamine based preservatives are currently the most important solutions for impregnation of wood in ground contact in Europe. One of the issues related to those and similar water based solutions is insufficient penetration to refractory wood species like Norway spruce. In order to elucidate this issue, commercial copper ethanolamine based solution was supplemented with five different wo...
M Humar, N Thaler, B Lesar


Characterisation and evaluation of various chitosan oligomers, and decay resistance
2011 - IRG/WP 11-30562
Chitosan, a polymer of D-glucosamine, is known for its antimicrobial activity. However, the physicochemical properties of chitosan depend upon three principal factors, i.e. source of raw material, molecular weight and degree of deacetylation. Here, we report synthesis and characterization of chitosan oligomers prepared by deaminative depolymerization of chitosan (s) obtained from Sigma Aldrich and...
I Hussain, C Chittenden, T Singh


Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa


Tannin resin-boron for outdoor wood protection and fire retardancy
2011 - IRG/WP 11-30567
Boron in the form of boric acid is well known for its efficacy against wood destroying organisms, as well as for its high leachability from treated wood when in outside exposure. Moreover, due to the European directive 2008/58/EC, boric acid is only authorized at low levels. In order to keep considering boric acid as an interesting active ingredient for wood protection, the issue is now to fix it ...
M-F Thévenon, G Tondi, N Leménager, S Wieland, A Pizzi


ISPM No. 15 and the Incidence of Wood Pests: Recent Findings, Policy Changes, and Current Knowledge Gaps
2011 - IRG/WP 11-30568
Largely as a result of international trade, hundreds of species of bark- and wood-infesting insects have become established in countries outside their native range. Many of these exotic insects have caused severe economic and environmental impact to urban and forest trees in the receiving countries. Most bark- and wood-infesting insects have been transported to new countries by means of the wood...
R A Haack, E G Brockerhoff


The potential for using CuO nanoparticles as a wood preservative
2011 - IRG/WP 11-30569
The potential for using nano-copper particles for wood protection was investigated using mini-agar slant and wood block tests with Gloeophyllum trabeum or Trametes versicolor. Nano-copper was more effective against G. trabeum than T. versicolor, although neither of these fungi would be considered copper tolerant. Nano-copper solutions were stable over a 17 week storage period, but precipitated w...
I S Weitz, K Knani, M Maoz, C Freitag, J J Morrell


Termite resistance of timber envelope treated with imidacloprid then modified by typical building site operations
2011 - IRG/WP 11-30570
Imidacloprid is a new envelope insecticide approved by Australian regulatory authorities for framing timber. It is a non repellent insecticide. Results are reported for timber envelope treated with imidacloprid and altered post treatment with typical building site operations to expose untreated surfaces. These modifications included, cutting, notching and drilling. Pinus radiata timber samples w...
K Day, A Siraa, P Lobb


The study of fungicidal values und sorption processes of ionic liquids- potential wood preservatives on soils
2011 - IRG/WP 11-30572
In the paper, the fungicidal activity of new ionic liquids structures, N,N-dimethylalkylamines derivatives, containing a spacer built of 7 or 10 methylene groups with nitrate(V) and tetrafluoroborate anions, didecyldimethylammonium and benzalkonium nitrate(V) were presented. The research was also conducted on the sorption of cations of ammonium ionic liquids on five types of podzolic, humic alluvi...
W Przybylska, J Zabielska-Matejuk, A Stangierska, A Skrzypczak


Design, synthesis, characterisation and effectiveness of ‘Locked-in-Boron’ chemicals for H3.2 level of wood protection
2011 - IRG/WP 11-30577
Boratrane molecules with five-membered and six-membered molecular ring systems, and with various ring substituents were synthesised, characterised and formulated for wood treatment for accelerated laboratory bioassays using wood decay fungi as test organisms. Six-membered ring boratranes showed lower efficacy in laboratory assays than five-membered ring boratranes. One alkyl-substituted boratran...
R Franich, H Kroese, S Gallagher, S Hill, B Kelly, G Billett, R Meder, W Rae


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


Biological and mechanical performances of particleboard panels made from maritime pine (Pinus pinaster) and glued with cornstarch-mimosa tannin-urea formaldehyde adhesive
2011 - IRG/WP 11-40542
The objective of this work was to demonstrate the utility of cornstarch-mimosa tannin-based resins designed for application as an adhesive in the particleboard production. Bond qualities of cornstarch-mimosa tannin- urea formaldehyde (UF) (10:4:86, weight ratios) resins and commercial UF resin were assessed by using an automatic bonding evaluation system, prior to production of particleboard panel...
A Moubarik, F Charrier, A Pizzi, A Allal, B Charrier


Acetylation Properties of Southern Pine and Radiata Pine
2011 - IRG/WP 11-40543
The chemical modification of wood via acetylation with acetic anhydride has been a well investigated technology and is of current commercial interest due to improved properties such as dimensional stability as well as resistance to termites and resistance to rot and decay fungi. Despite this, the acetylation of a board substrate requires further investigation in order to assess board properties a...
J Allen, T Guinn, J Dickerson


A Critical Review and Survey of the US Wooden Pallet Industry: Focusing on Market Segmentation & N. American Trends
2011 - IRG/WP 11-40545
This paper reviews the history and current and predicted future use values in N. America. Included in this work is historical data on rationality and wood species used to manufacture wooden pallets in the USA and an ongoing current market survey sent to the 1000 largest manufacturers and re-manufacturers in the USA based on SIC Code 2448(Standard Industrial Code Classification). Although CHEP, the...
M H Freeman


The resistance to Basidiomycetes fungi of chipboard 35 years after their industrial preservation with wood preservative on fluoroborate basis
2011 - IRG/WP 11-40546
The research on wood-based panels’ (WBP) behaviour towards fungi impact demonstrated rather low resistance of wood-based materials to wood rotting fungi. However, these materials are used in construction under conditions favourable to fungi growth. In such conditions WBP treated with wood preservatives should be used. Preservation durability is of great importance in such cases. The resistance o...
A Fojutowski, A Kropacz


Study of the durability of the Maderon® against wood decay fungi and insects
2011 - IRG/WP 11-40548
Many industries produce residues that are not easily degradable. One of these is nut husks which, due to their high level of resistance to biological and environmental degradation, have become an ecological problem. Maderón® is a material invented and patented in Spain employed as an ecological substitute and a modern alternative to certain uses of wood. At present, Maderón® is commercialized ...
M T Troya, F Llinares, P Jiménez, J I Fernández-Golfín, M Conde, R Díaz


Physical properties of Pinus radiata veneers modified with hexamethoxymethyl melamine prepolymers
2011 - IRG/WP 11-40551
Prepolymers containing hexamethoxymethyl melamine and either sucrose (Suc-HMMM) or polyvinyl alcohol (PVA-HMMM) were prepared by acid catalysis under reaction conditions optimised with respect to stiffening effect when introduced into Pinus radiata veneers by vacuum impregnation and cured by hot pressing at 150C. Maximum increases in MOE were 20% for Suc-HMMM (50% WPG), 22% for PVA-HMMM (...
C Molloy, W Rae, S Connor, T Henderson, A Siraa


Biological properties of Pinus radiata veneers modified with hexamethoxymethyl melamine
2011 - IRG/WP 11-40552
An investigation of the effects on decay and termite resistance of a wood modification process involving prepolymers of hexamethoxymethyl melamine (HMMM) was conducted using LVL as a model engineered wood product. Dry Pinus radiata veneers were vacuum-impregnated with a wood modification formulation containing a mixture (P-H:S-H) of two separate prepolymerisation reactions containing polyvinyl al...
A Siraa, S Millward, C Molloy


Challenges and new developments in testing electro osmotic pulsing technology (PLEOT) by means of conventional laboratory methods
2011 - IRG/WP 11-40555
A new wood protection system, electro-osmotic pulsing technology, called PLEOT, is tested in lab trials using different test setup. The technology is tested on Scots pine sapwood and beech wood samples exposed to brown- and white rot fungi. Mass loss and moisture content is calculated after testing and a chitin analysis are performed on the sample powder. Two different electrodes are used in ord...
A Treu, E Larnøy


Effects of Heat-Treatment in Hot Water and Steam Mediums on Gas Permeability of Beech Wood
2011 - IRG/WP 11-40557
Heat-treatment, as a major method of wood modification, improving dimensional stability, and natural durability, has been studied greatly from different aspects. The effect of heat-treatment on gas permeability, as an important physical property of wood, in two different mediums of hot water and steam, as well as in two buffers of 7 and 8, is the main topic of the present study. Hydrothermal treat...
H Reza Taghiyari, A Talaei, A Karimi


Utilization of thermodesorption coupled to GC-MS to study kinetics of thermodegradation of different wood species
2011 - IRG/WP 11-40559
Thermdesorption coupled to Gas Chromatography coupled to Mass Spectroscopy (TD-GC-MS) has been investigated to identify volatile degradation products generated during wood heat treatment by mild pyrolysis. For this purpose, wood samples of different softwood and hardwood species have been heat treated under nitrogen for different temperatures comprised between 180 and 230°C during 15 min. in the ...
K Candelier, M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Study of properties and application of Paulownia in wood industries
2011 - IRG/WP 11-40560
Important of required raw material supply regarding constraint in harvesting, increasingly population, change in consumption pattern and increasingly focus on wood products and per capita in consumption is obvious for anyone. Paulownia is a marvelous tree species with its characteristics of fast-growing, good Wood quality, multiple uses, wide-ranged distribution, easy propagation, deep root system...
M Akhtari


Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller


Durability of modified wood in UC3 and UC4. Results from lab tests and 5 years testing in 3 fields
2011 - IRG/WP 11-40562
In 2005 an extensive test program including field tests was set up in order to obtain more data on the durability and long term performance of modified wood and semi-durable wood species. One of the main challenges for modified wood is to predict accurate service life time in UC3 (use class 3, above ground) and UC4 (use class 4, in soil or fresh water contact). So far, data from in-service condi...
M Westin, G Alfredsen


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani