Termite resistance of treated wood in an above-ground field test
1985 - IRG/WP 2241
A field test method has been developed for evaluating the susceptibility of wood products to termites in protected situations above ground. In this method fungal attack on the wood products is minimal, though decay has been observed in conjunction with termite attack in some specimens. Preliminary results from exposure of replicate wood samples treated with preservatives in Florida to Reticuliterm...
A F Preston, P A McKaig, P J Walcheski


FTIR studies on the weathering of didecyldimethylammonium compound (DDAC) treated wood
1993 - IRG/WP 93-30013
Wood treated with alkylammonium compounds (AACs), such as DDAC, weathered more rapidly than untreated wood. In order to examine the influence of DDAC treatment of wood on its weathering, treated and untreated microtomed sections of southern yellow pine earlywood of various thicknesses, were prepared and weathered for approximately one month. The changes in these samples were monitored using FTIR. ...
R Liu, J N R Ruddick


Durability of Sugi (Cryptomeria japonica D.DoN ) wood treated in high temperature liquid paraffin
2002 - IRG/WP 02-40221
Sugi(Cryptomeria japonica D.DoN )wood was subject to a heat treatment in high-temperature liquid paraffin for the purpose of improving the resistance against fungi and termites without chemicals. The bath of paraffin liquid, which can provide a uniform heat transfer (±2?), was used at temperatures of 90?,120?and 150?.?ecay resistance according to JIS K 15711) was evaluated using a brown rot fungu...
Y Matsuoka, W Ohmura, S Fujiwara, Y Kanagawa


An analysis of the effects of some factors on the natural durability of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.)
1986 - IRG/WP 1279
The effects of some factors on the natural resistance of pine and spruce sapwood against fungal decay and against attack of house-longhorn beetle larvae have been studied in laboratory tests and the results are evaluated by analysis of variance and regression analysis. Following conclusions were reached: Wood from summer-felled trees did not have a lower inherent natural durability against fungal ...
J B Boutelje, T Nilsson, S Rasmussen


Recycling of CCA treated wood in the US
1998 - IRG/WP 98-50101-08
The production of CCA treated wood has increased dramatically in recent years. Previous estimates of the volume of treated wood to be removed were based on the assumed service life of the material, generally 20 to 25 years. This study based on a survey of contractors installing treated decks, determined that the actual service life of these decks is much shorter than their assumed functional servi...
J McQueen, J Stevens, D P Kamdem


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Durability of some alternatives to preservative treated wood
2004 - IRG/WP 04-30353
The environmental discussion in Sweden has lead to an increasing use of naturally durable domestic wood species and wood treated according to alternative methods for use above ground. A number of these alternatives have been tested according to field- and laboratory tests and compared to wood treated with preservatives for above ground use. Seven untreated wood species, four alternative wood treat...
M-L Edlund


Termite resistance of treated wood in an above-ground field test
1986 - IRG/WP 1300
This paper provides an update on the results from an above ground field test evaluating the effectiveness of wood preservatives against subterranean termites. Results for the one and two year inspections of treated southern pine sapwood exposed in Hawaii to Coptotermes formosanus are presented. Chromated copper arsenate is providing excellent protection as is the pyrethroid deltamethrin. Borate an...
A F Preston, P A McKaig, P J Walcheski


Fluoride and chromium concentrations in soil adjacent to remedially treated distribution poles
1996 - IRG/WP 96-50066
Soils adjacent to Rentex treated 'on-line' distribution poles were analysed for total fluoride and chromium content for comparison with background values of these elements. Soil samples 6 cm and 25 cm downslope of selected poles were recovered at 1 week, 1 month, 6 and 12 months after treatment. Background soil samples were taken 50 m from the poles at sampling times. Fourteen po...
D C R Sinclair, G M Smith, A Bruce, H J Staines, P Durrant


Examination of preservative-treated Pinus sylvestris using electron paramagnetic resonance
1992 - IRG/WP 92-3710
EPR is currently being used to help elucidate the nature and extent of the chemical reactions occurring between wood and copper based timber preservatives. In the work reported here treated Scots pine samples were examined at room temperature and in the frozen state. Plots of the electronic parameters A|| vs. g|| were found to be a useful index of the electronic properties of the various formulati...
A S Hughes, R J Murphy, J F Gibson, A J Cornfield


An audit of copper chrome arsenic timber treatment plants throughout Queensland
1995 - IRG/WP 95-50047
Thirty seven copper chrome arsenic (CCA) timber treatment plants in Queensland were assessed according to the operational criteria specified in Australian Standard 2843.2 - 1985, Timber Preservation Safety Code - Plant Operation. The criteria have been designed to provide information on the design and operational activities of a CCA plant. Design aspects that have an effect on the environment are ...
J Norton


Application of oscillating pressure to improve treatability of refractory species
1987 - IRG/WP 3449
Under practical conditions a minimum moisture content of 80% demande by the German quality standard RAL-RG 411 can not be guaranteed throughout the year. Storage of logs with bark prolonges the drying process; a storage without bark must be avoided. A sufficient penetration according the standard can be achieved at least with a moisture content of 60%, optimal conditions may prevail between 100% a...
R-D Peek


The influence of timber species and preservative treatment on spore germination of some wood-destroying Basidiomycetes
1988 - IRG/WP 2300
Basidiospores from six wood decay fungi exhibited varying germination rates on untreated softwood and hardwood blocks. Germination inhibition of all test fungi was recorded on pine sapwood. No preference for a certain timber species by a particular fungus was evident. Whereas almost complete inhibition of germination occurred on wood treated with a quarternary-ammonium based wood preservative, mos...
B M Hegarty, G Buchwald


Life Cycle Assessment of borate treated wood
2005 - IRG/WP 05-50224-12
Life Cycle Assessment (LCA) is being used increasingly around the world by decision-makers to help incorporate the environmental component of sustainability into their activities. U.S. Borax regularly assesses how its products contribute to sustainable development. Using data gleaned from LCA of its products, the company recently completed its first ISO 14040 compliant cradle-to-grave LCA of lum...
M J Manning


The microbial ecology of treated birch stakes in a soil-bed
1983 - IRG/WP 1209
The microbial ecology of small birch stakes exposed in soil beds in two Fungus Cellars was investigated. Patterns of fungal colonisation and decay initiation are described in untreated birch and copper fluosilicate-treated stakes. Results are based on fungal isolation onto selective media and direct light microscopical observations of decay features. In untreated stakes there was a rapid build-up ...
C P Clubbe


PCP in aquatic environments arising from historic contamination at wood processing and preservation sites
1995 - IRG/WP 95-50040-14
Three different studies are reported that assess the impacts of Pentachlorophenol (PCP) in aquatic environments arising from its historic use at sawmilling and wood preservation sites. These studies involved New Zealand wood processing facilities, and collectively they aimed to measure the transport of PCP from sawmill sites into the aquatic environment, determine the background environmental conc...
J S Gifford, P N McFarlane, M C Judd, S M Anderson


Present status of using treated wood and private house owner’s expectations in Bangladesh
2004 - IRG/WP 04-30329
In a developing country like Bangladesh more than 80 % of the total population lives in rural areas where building materials are mainly comprised of wood, bamboo, thatch grass, golpata, etc. All these materials, being cellulosic, are easily infected by deteriorating agencies like fungi, termites, beetles etc., as climatic condition of the country is ideal for their thrive. This is a great wastage ...
M A Islam, A K M A Bosunia, S C Ghosh, M O Hannan, A K Lahiry


Quantification of creosote migration down wooden poles and the prevention of its depletion during flood irrigation
1994 - IRG/WP 94-50032
Polyethylene field liners heat-shrunk onto soil-contact surfaces prevented decay of creosote-treated Eucalyptus grandis vineyard poles under flood-irrigation. The present work quantified losses of creosote from these poles after six and 24 months' service. After six months' service the mean creosote retention of unlined poles above the ground line was 12.62% (m/m dry wood), with ...
M Behr, A A W Baecker


The effect of moisture content on the electrical resistance of timber as detected by a pulsed current reistance meter (Shigometer)
1984 - IRG/WP 2212
The literature concerning the use of the Shigometer® for detecting decay in standing trees and wood poles is reviewed and the differences of opinion over the effect of timber moisture content on electrical resistance are highlighted. A simple experiment designed to test this effect is described and the implications of the results for testing poles in service are discussed. There was a large diffe...
P I Morris, D J Dickinson


Limnoria quadripunctata Holthuis - a threat to copper-treated wood
1983 - IRG/WP 4100
This paper presents the first reported attack by the crustacean marine wood-borer Limnoria quadripunctata Holthuis of CCA treated eucalypt piles. The attack occurred after 12 years service of the piles in the River Derwent at Hobart, Tasmania. Attack by both this borer and Limnoria tripunctata Menzies is also reported in CCA treated softwoods and hardwoods over periods ranging from 5 to 22.9 years...
J E Barnacle, L J Cookson, C N McEvoy


Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston


Leaching of Copper from ACQ treated wood exposed above ground
2004 - IRG/WP 04-50219
The leaching of chemicals of ACQ Type C treated wood exposed above ground for 16 months was studied. Commercially treated Hem-fir boards (Tsuga heterophylla Raf. and Amabilis fir Forb) of 37.5 mm by 87.5 mm were used. The amounts of chemical leached monthly by the rainfall were determined and the leachate was collected and analyzed. Also, the environmental factors influencing the leaching were ...
P A Chung, J N R Ruddick


The use of low cost X-ray fluorescence instruments in the determination of copper chromium and arsenic in preservative treated wood
1987 - IRG/WP 2278
Internal quality control in timber treatment plants can be pursued by analysis of preservative treatment solutions and treated timber. Treaters must proceed with costly and lengthy analyses through analytical laboratories. An alternative approach for the timber treater, is to use low cost analysers (L.C.A.'s) based upon x-ray fluorescence. Detailed comparisons have been made between stand...
J Norton, L E Leightley


A study on insect pests and preservation of fire-damaged timbers in Da Xing An Ling forest region
1991 - IRG/WP 1499
Investigated insect pest of timbers of Da Xing An Ling forest region by means of sampling inspection. Meanwhile we had researched insects pest situation, regularity occurred and biological nature for fire damaged timbers attacked in the log yard. The results showed that the mainly insect species are small black-marmorated longicorn (Monochamus sutor L). We had eagaged in various small tests of tim...
Lu Wenda, Li Jian, Shao Jing Wen, Liu Yixing, Cui Yongzhi


The study of blue stain found in coniferous timber in SR Slovenia (Yugoslavia)
1983 - IRG/WP 1177
The report concerns the problems connected with blue stain in coniferous timbers stored in warehouses at wood-processing plants in SR Slovenia (Yugoslavia). The amounts of spruce-wood (Picea abies Karst.) found to have been infected with blue stain have been measured and some of the fungi causing the stain have been identified and their biology studied. It was found that the percentage of spruce-w...
R Benko