Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato


Biological detoxification processes - A check list for assessments
1998 - IRG/WP 98-50120
The number of scientific publications on the biological purification of preservative treated wood implies that the biological treatment of wood wastes becomes more and more important. But an information about a successful industrial application is almost missing in all cases. Therefore the applicability of the proposed purification processes is often uncertain. The feasability of such a biological...
H Leithoff, R-D Peek


A prototypical needle-incisor for refractory timber
1995 - IRG/WP 95-40041
A needle-incisor was manufactured for trial. This machine has an incising mechanism that a set of needles held by a rotary plate incises timber which is moved toward the front simultaneously, and then another set of needles incises a new part of the timber. Timber is incised by recycling the process. Timber incised of 4400 incisons/m² with the depth of 56 mm by 2.8 mm-diameter needles on all the ...
A Yakuwa, H Endoh, M Mori, S Doi


Electrodialytic remediation of CCA-treated wood in larger scale
2005 - IRG/WP 05-50224-20
A pilot plant for the electrodialytic remediation of CCA-treated waste wood has been developed and tested at the Technical University of Denmark. Results from two experiments with different amount of wood chips are presented here. Prior to the electrodialytic remediation the wood was soaked in oxalic acid and phosphoric acid. The main purpose of soaking is to remove the most available fraction fir...
I V Christensen, L M Ottosen, A J Pedersen


Marine exposure assessment of the natural resistance of a number of lesser known species of tropical hardwoods to teredinid and limnoriid borers
2004 - IRG/WP 04-10520
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, candidate timber species were selected for testing in the sea on the basi...
J R Williams, S M Cragg, L M S Borges, J D Icely


Application of roller-pressing method to the novel liquid impregnation treatment of green timber
2001 - IRG/WP 01-40198
A transverse compression technique enabled us to impregnate liquid into green timber through replacement of the free water in the timber with a treatment liquid without any critical physical damage to the timber by the roller-pressing method. The roller-pressing is supposed to remove free water the cell cavities and to concurrently introduce the treatment solution into green timber in the treatmen...
M Inoue, K Adachi, K Tsunoda, Y Imamura, S Kawai


The influence of copper (II) chemicals on the weathering of treated wood. Part 1: ACQ treatment of wood on its weathering
1994 - IRG/WP 94-30040
Wood weathering can be accelerated by alkylammonium compound (AAC) treatment, and slowed by ammoniacal copper quat (ACQ) treatment. This study aims at investigating the influence of ACQ treatment of wood, especially the present of copper (II), on its weathering. ACQ, CCA and DDAC treated microtomed sections of southern yellow pine earlywood were prepared and naturally weathered for five periods, t...
Ruiying Liu, J N R Ruddick, L Jin


Determination of total fluoride and boron in preservative-treated wood fluoride by ion selective electrode without steam distillation, and boron colorimetrically using azornethine-h
1998 - IRG/WP 98-20135
An analytical method was developed to determine total fluoride and boron in wood treated with aqueous or solid diffusing fluoride or borate-fluoride formulations. Ground wood was mixed with 30% sodium hydroxide solution and oven-dried for 2 hours before furnacing at 600° C for 1 hour. The cool fused product was dissolved in hot water, transferred to a plastic beaker and neutralised. Fluoride was ...
P A Collins, M J Kennedy


Introduction of plank-built catamarans along the north coast of Andhra Pradesh, India – A development of recent origin
2003 - IRG/WP 03-10483
Hitherto, the most versatile fishing craft of the poor traditional Indian fishermen - the catamaran is made of solid timber logs of a few selected species of broad-leaved softwoods. Of late, the fishermen find it difficult to get these conventional varieties of timber chiefly because of three reasons, a) scarcity of commodity, b) prohibitive costs and c) competition from match and veneer industri...
M V Rao, K S Rao, M Balaji, V Kuppusamy


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 1: Treatment of reference samples
1977 - IRG/WP 426
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying samples of the reference timbers treated w...
R Cockcroft, T B Dearling, W O Schulz, H V Borck


Will political initiatives stop the use of preservative-treated wood in Sweden?
1990 - IRG/WP 3578
The Swedish government has initiated several investigations on how to reduce the use of different chemicals. Among these chemicals are creosote, arsenic, chromium and organotin. A special investigation was carried out concerning wood preservatives resulting in different proposals on how to reduce the use of preservatives and preservative treated wood. The most important proposals were an "environm...
J Jermer, M-L Edlund


In situ timber treatments by spraying. Distribution of preservative in wood
1991 - IRG/WP 3678
This study was carried out in order to make the Pest Control Operators able to achieve correct treatments and enhance their efficacy. It was carried out in two steps: 1) in laboratory, to learn the influence of various parameters like spraying pressure, use of repeated applications, distance from nozzle to wood; 2) in situ on roof timber of five buildings. In this case, the applications of the pre...
C Defoin, G Dupont, M Lamour, H Sageot, M-M Serment


Bending & tensile properties of vapor boron-treated composites
2002 - IRG/WP 02-40228
North American composites including laminated veneer lumber, oriented strandboard, and medium density fiberboard were treated by vapor boron technology and subsequently tested in static bending. Tensile properties were also determined for the two composite boards. The study was designed as 3 x 2 factorial with three treatment levels and two mill locations for each composite type. In general, mil...
H M Barnes, R J Murphy, B K Via


Long-term efficacy of wood dip-treated with multicomponent biocides
2005 - IRG/WP 05-30379
Biocides designed for prevention of indoor mold growth on wood-based materials need to provide long-term protection under conditions of high humidity. Specimens of kiln-dried southern pine and unseasoned southern pine, aspen, and Douglas-fir were dip-treated with borate-dimethylcocoamine (DMCA) supplemented with voriconazole, thiabendazole, or thujaplicin and evaluated at 4-week intervals for inhi...
C A Clausen, V W Yang


The environment and the timber preservation in the Benelux countries
1990 - IRG/WP 3580
The environment has become a major issue in all industries. To focus on the timber preservation industry an analysis is made of the production chain. Suggestions are made for diminishing or excluding emissions of agents of pollution. After a review of the legislation in Holland, some important statements are made on the production process, the products involved and the waste materials. Finally raw...
C De Mey, R Leegwater


Chemical evaluation of borate treated pine sapwood attacked by the subterranean termite Coptotermes acinaciformis
1993 - IRG/WP 93-20003
Sapwood of hoop (Araucaria cunninghamii Ait. ex D. Don) and slash (Pinus elliottii Englem.) pines were treated by Vacuum Pressure Impregnation (VPI) to provide test specimens. The concentration of boron was defined by chemical analyses of the timber, in the zone of primary attack by the termite being bioassayed. A common method of definition of preservative retention, weight uptake of preservative...
A R Moffat, B C Peters


Treatment details for the field experiment to determine the performance of preservative treated hardwoods with particlar reference to soft rot
1977 - IRG/WP 384
These notes are compiled to complement and supplement Document No: IRG/WP/367 which described the plan for the treatment of the stakes, using a CCA preservative, for the field experiment. This document gives extra details of the treatment characteristics of the different timber species and as such may give IRG members useful information on the sapwood permeability of a range of hardwoods. The repo...
F W Brooks, M R Gayles


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper/chrome/arsenic preservative
1981 - IRG/WP 3180
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. The growth characteristics of spruces (Picea spp) make them attractive candidates for forestry schemes. In 1975 the UK Forestry Commission had about 400 000 hectares, about 20% of total UK forest area, planted with Sitka spruce (Picea sitchensis)...
C R Coggins


Effects of fixation conditions and seawater on leaching of wood treated with marine retention CCA
1997 - IRG/WP 97-50088
The effect of post-treatment conditioning temperature and humidity on leaching of chromated copper arsenate (CCA) was compared in seawater and deionized water. Southern pine cubes treated to 40 kg/m3 CCA were stored at 2° C and 82% relative humidity (RH), 24° C and 65% RH, or 32° C and 30% RH for 3, 10, or 17 days. Cubes were then leached in deionized water or artificial seawater. The rate of l...
S T Lebow


The use of the Shigometer® and Pilodyn® as non-destructive test methods for detecting decay in CCA treated eucalypt poles
1981 - IRG/WP 2153
The groundline condition of sixty C.C.A. treated eucalypt poles comprising six different species was examined using the Pilodyn® and Shigometer®. Although sensitive to the presence of soft-rot decay, the Shigometer® would seem to offer little practical advantage in the eucalypt soft-rot decay situation, since a comparable visual examination could reveal the presence and extent of decay. Initial...
L E Leightley


Leaching characteristics, decay and termite resistance of treated wood with boron compounds, N'-N-(1,8-Naphthalyl) hydroxylamine (NHA-Na), and hydroxynaphthalimide (NHA-H)
2003 - IRG/WP 03-30307
Despite many advantages of boron wood preservatives, boron itself does not adequately protect wood in ground contact and exterior applications because its natural diffusibility and susceptibility to leaching. As a result of previous studies to limit or decrease boron leaching, several fixation systems have been developed. In this study, we evaluated the effects of N'-N-(1, 8-Naphthalyl) h...
S N Kartal, Y Imamura


A light and electron microscopic study of decayed CCA-treated radiata pine (Pinus radiata) wood from a cooling tower
1994 - IRG/WP 94-10056
An inspection of an industrial cooling tower in New Zealand showed surface decay of 12 year old Pinus radiata wood panels treated with CCA preservative to a retention of around 15 kg/m³ of salt. Wood decay micromorphology typical of that caused by soft rot fungi, white rot fungi, 'stripy' and 'v-shaped' erosion bacteria and cavitation bacteria were all commonly...
A P Singh, R N Wakeling, D R Page


Observations on the activities of Sphaeroma in Australia
1994 - IRG/WP 94-10059
Polyurethane coated timber specimens are being attacked at Townsville by Sphaeroma terebrans in the tidal zone. To understand this marine borer better, the results from several other marine tests at Townsville are briefly described, and information about Sphaeroma spp. from elsewhere in Australia is presented. At Townsville, Sphaeroma seems to prefer the shady side of timber fender piles. Also, it...
L J Cookson


Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


The residual effects of remedial timber treatments on bats
1986 - IRG/WP 1281
By means of controlled laboratory experiments it was established that timber treatment fluids containing g-HCH and pentachlorophenol (PCP) and used according to manufacturers recommendations rapidly cause the death of pipistrelle bats roosting in contact with timber treated between six weeks and 14 months previously. The chemicals responsible are presumably ingested when the bats groom their fur a...
P A Racey, S M Swift