Performance of untreated French Guianan piling in marine exposure
1992 - IRG/WP 92-4173
Round piling of seven French Guianan species, greenheart, and preservativ-treated Southern Pine were installed as fender piling in Key West, FL. After 12½ years, none of the tropical hardwoods performed as well as dual-treated Southern Pine. Of the hardwoods, kouata patou and maho noir were the most resistant to decay and marine borers....
B R Johnson


Elimination of alternative explanations for the effect of iron on treated wood
1993 - IRG/WP 93-30006
Amounts of iron which had previously been found in stakes removed from ground contact reduced decay of untreated wood by four brown-rot fungi. This suggested that the effect of iron may be on the preservative. Analysis of the leachates from CCA- and ACA-treated wood blocks first exposed to rusting iron, then to a brown-rot fungus, showed that the increased decay found in the laboratory for wood ex...
P I Morris, J K Ingram, D L Gent


Fire resistance of Alder wood treated with some chemicals. Part II. Effect of Other Chemicals on the Combustion Properties
2002 - IRG/WP 02-40235
Samples from alder wood (Alnus glutinosa (L.) Gaertn. subsp. barbata (C.A.Mey) Yalt.) were impregnated according to ASTM D 1413-88 with boron compounds (boric acid, borax, sodium perborate), vinyl monomers (styrene, methyl methacrylate), Tanalith-CBC, Phosphoric acid, Vacsol, Immersol, Polyethylene glycole (PEG-400) and their mixed solutions of chemicals in order to determine their combustion pro...
A Temiz, Ü C Yildiz


Performance of surface-treated hardwoods and softwoods out of ground contact
1990 - IRG/WP 3592
A number of fungicides were tested as brush treatments for protection of southern pine, Douglas-fir, maple, and red oak against decay above ground. Cross-brace and L-joint test units were treated just before assembly and exposed from 3-10 years. Untreated Douglas-fir cross-brace units were not decayed at either the Mississippi or Madison, WI, site. Untreated red oak cross-brace units were not deca...
T L Highley


Preservative-treated wood as a component in the recovered wood stream in Europe – A quantitative and qualitative review
2004 - IRG/WP 04-50218
Wood preservatives have been used for the protection of timber products in the European market in appreciable quantities for about 100 years. Between the 1960s up to the present day this usage has been particularly noticeable. The aim of this paper is to present quantitative and qualitative data on the volumes of preservative treated wood placed on the market in the UK and Sweden and to evaluate t...
R J Murphy, P Mc Quillan, J Jermer, R-D Peek


Proposed test procedure to determine the effect of timber substrate on the effectiveness of a copper/chrome/arsenic preservative in seawater
1975 - IRG/WP 411
R A Eaton


A short note on fungal decay in K33-treated poles
1982 - IRG/WP 1169
Soft rot cavities and erosion of the lumen have been found in K33-treated Pinus sylvestris poles from the years 1956-66 by microscopic studies. Poor treatment quality has been proved for some of these poles. The microscopy showed an unusual pattern of attack, and pre-treatment decay is suspected but not yet proved. Sounding the poles and using the Pilodyn indicated decay, but poking did not. Quant...
H Friis-Hansen


Current and future options for managing used preservative-treated wood
1995 - IRG/WP 95-50042
The amount of preservative-treated wood available for disposal will continue to increase exponentially in the next several decades as landfill availability declines. At the same time, recent legal ruling on competitiveness among utilities and disposal of ash has clouded the economic outlook for combustion of treated wood for energy recovery. This report identifies current and future options for ma...
R C De Groot, C Felton


nvestigation of anomalous fixation and leaching of CCA-treated red maple
2004 - IRG/WP 04-30341
The fixation of CCA-C preservative was investigated in red maple sawdust (Acer rubrum L.) at target retentions of 4.0, 6.4, 9.6 and 30.0 kg/m3. The effect of water-soluble extractives on the course of fixation was evaluated comparing the non-extracted with pre-extracted samples treated to 6.4 and 30 kg/m3. Leaching of the CCA components was monitored after complete fixation for all retentions. Fix...
S Radivojevic, P A Cooper


Ultrastructural and TEM-EDAX studies on the degradation of CCA treated radiata pine by tunnelling bacteria
1985 - IRG/WP 1260
An ultrastructural study was carried out on bacterial attacked Pinus radiata stakes treated with a high level (24.7 kg/m³) of Tanalith NCA preservative. The purpose of the investigation was to determine whether the organism possessed intracellular and/or extracellular detoxification mechanisms in order to overcome the high levels of copper, chrome and arsenic present within the wood fibre walls. ...
G F Daniel, T Nilsson


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1983 - IRG/WP 3269
G C Johnson, J D Thornton


Biological control of decay in standing creosote-treated poles
1976 - IRG/WP 156
Internal decay caused by basidiomycetes in standing creosoted poles can be controlled biologically, it seems, by artificial inoculation near the ground line. For such inoculation IC-type facultative mycoparasites, Scytalidium sp FY strain or Trichoderma spp for example, may be used. Apparent residual action can be explained by the release of non water soluble chemically stable antibiotics from the...
J Ricard


An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley


Use of biossay to determine CCF and CCB preservative retentions in treated Pinus sylvestris
1984 - IRG/WP 2216
The retention of each a copper/chromium/boron and copper/chromium/fluoride preservative in pressure treated pinepoles was tested by bioassay using Aspergillus niger as test fungus. Small samples of 5 mm³ were taken from various depth of the poles and placed on potato-dextrose agar plates. The inhibition of fungal growth depends on the preservative retention in the cubes and corresponds closely to...
J C Moreschi, H Willeitner


Evaluation of wood treated with copper-based preservatives for Cu loss during exposure to heat and copper-tolerant Bacillus licheniformis
1999 - IRG/WP 99-20155
Copper-based wood preservatives need to be effective against exposure to all types of microorganisms. Wood treated with six copper-based preservatives was exposed to 121°C and 20 psi pressure for 15 minutes under standard autoclave conditions and the copper-tolerant bacterium, Bacillus licheniformis CC01, for 10 d at 28°C and 150 rpm. Sixteen to 37 percent of the copper was released from the woo...
D M Crawford, C A Clausen


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


The collaborative developement of soil acceptance criteria for timber treatment chemicals in New Zealand
1995 - IRG/WP 95-50040-34
In New Zealand, the issue of potential contamination on timber treatment sites arose in the late 80's due to the long history of use of PCP by the industry. One of the recommendations from the task group set up to investigate the issue was the development of a set of acceptance criteria to define trigger levels for remediation. A technical group from the government, industry and regional ...
H C Boyd


Biological agents of timber degradation in Portugal. Marine borers
1991 - IRG/WP 4171
A brief report of the studies carried out in Portugal on marine borers is presented. The marine borers found in the portuguese coast are refered as well as the wood species where those organisms were identified. Emphasis is given to a study carried out from 1960 to 1975 at the Tagus estuary in Lisbon with the purpose, among others, of establishing the natural durability of different timbers....
J S Machado, L Nunes


Wood preservation in East European countries
1989 - IRG/WP 3527
The paper discusses the main problems of wood preservation in Bulgaria, Czechoslovakia, German DR, Hungary, Poland, Rumania and the USSR. The main types of wood preservatives produced have been presented, as well as the state of standarization to test their properties. There have been considered methods of wood treatment in use and application range of treated wood....
J Wazny


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests
1980 - IRG/WP 2135
With the exception of acid-copper-chromate, zinc-chrome-arsenate, and sodium pentachlorophenoxide, the relative performance of preservatives in the fungus cellar was similar to that in the field....
M E Hedley


An investigation to assess the feasibility of developing an accelerated laboratory test to determine the abrasion resistance of lesser-used timber species for use in marine constructio
2005 - IRG/WP 05-20317
The paper describes the evaluation of a laboratory-accelerated test to compare the shingle abrasion resistance of current and potential timbers for use in marine construction. Useful results were achieved in 47.5 hours, but identified a number of issues to be resolved for the test to be refined and the subsequent results to be interpreted correctly....
G S Sawyer, J R Williams


Chemical investigation of 23-year-old CDDC treated southern yellow pine
1997 - IRG/WP 97-30141
The effect of 23 years exterior exposure on CDDC treated southern yellow pine was evaluated by the application of solid state analytical instrumentation. Analytical methods including environmental scanning electron microscopy (ESEM),energy dispersive X-ray analysis (EDXA), X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD), inductively coupled plasma (ICP) and atomic absorption spectr...
D P Kamdem, C R McIntyre


Ultrastructure of the attack of a naturally durable timber by tunnelling bacteria
1990 - IRG/WP 1462
The attack of the wood of Eusideroxylon zwageri, a naturally durable species, by tunnelling bacteria (TB) was examined by light microscopy and transmission electron microscopy. Observations were made primarily on fibres. Parenchyma were included in some cases. Both fibres and parenchyma are rich in extractives. In fibres, extractives are primarily present in the lumen. The amber colouration of fib...
A P Singh, T Nilsson, G F Daniel


Sequential exposure of borate treated Douglas-fir to multiple Formosan subterranean termite colonies in a 40-week field test
1993 - IRG/WP 93-10006
Douglas-fir boards (ca. 74.5 g) pressure-treated with disodium octaborate tetrahydrate (DOT) retentions of 0 (controls), 0.88, 1.23, 1.60, or 2.10% (weight/weight) DOT were sequentially exposed to four active field colonies of Formosan subterranean termites, Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae), in an above-ground field test. Samples were placed in contact with each colony fo...
J K Grace, R T Yamamoto


An investigation into the stability of TBTO in LOSP-treated radiata pine
1987 - IRG/WP 3459
Nuclear magnetic resonance (NMR) spectroscopy and reverse phase paper chromatography were used to characterise the organotin compounds found in radiata pine treated with bis (tri-n-butyl) tin oxide (TBTO). Preliminary results indicate that the preservative is remarkably unstable in wood after light organic solvent preservative (LOSP) treatment. Significant decomposition of TBTO occurs in a matter ...
K J Archer, R Meder