IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 643 documents. Displaying 25 entries per page.


Water repellency and dimensional stabilIty of wodd treated with waterborne resin acids/TOR
2007 - IRG/WP 07-40364
Wood used in above ground applications such as decking undergoes undesired dimensional changes leading to the lumber warping, cupping, splitting, etc. This is a major concern to consumers but it can be reduced by treating lumber with a water repellent. The ability of resin acids, hydrophobic compounds naturally present in southern yellow pines, was examined as a possible water repellent. A wate...
T P Schultz, D D Nicholas, J Shi


Multivariate analysis of infrared spectra for the prediction of the mechanical performance and dimensional stability of thermally modified wood
2007 - IRG/WP 07-40367
The use of calibrated mid-infrared Fourier transform (FTIR) spectroscopy for predicting the main bending strength parameters of thermally modified wood is described for the first time. The analysis is based on the handling of OSC-filtered FTIR data from control and treated wood samples, using partial least squares (PLS) regression. Sets of Norway spruce, Scots pine and Beech wood samples were th...
M M González-Peña, M D C Hale


Evaluating the Process of ACQ-Treated Woods with TGAand CEM Analysis
2007 - IRG/WP 07-20374
To provide an understanding of the fundamental thermal behaviour and the disposal-end products of ACQ-treated woods, this study is comprised of two categories of examination. The first is related to the use of TGA under different thermal decomposition conditions (nitrogen or air, and 5 or 40 oC/min), and the use of EDX to examine certain residual elements of the char. The second applies the CEM ...
Han Chien Lin, Tsang-Chyi Shiah, Jung Ting Tsai


Characterization of protein patterns from decayed wood of loblolly pine (Pinus taeda L.) by proteomic analysis
2008 - IRG/WP 08-10654
The primary biotic decomposers of wood belong to the basidiomycetes. The members of this group can attack and biodegrade both wood in the forest and in service. By the time wood decay is visible, there has already been a significant loss of strength. The identification of basidiomycetes and other organisms on wood only tell us what is present, not what is actively decaying the wood. When organisms...
Young-Min Kang, L Prewitt, S Diehl


Water Absorption of Various Building Materials and Mold Growth
2008 - IRG/WP 08-10657
Mold growth is a major problem for house owners, as it often occurs on the surface of building materials in damp houses. The principal method to control mold growth on building materials is to prevent water penetration into the materials. A study was recently conducted to determine water absorption rates of different wood species and panel materials used as building materials, when water intrusi...
Dian-Qing Yang


Hydrophobic characteristics of pyrolysis oil
2008 - IRG/WP 08-30458
Hydrophobic behavior of pyrolysis oils obtained by pyrolysis of Scots pine wood (Pinus sylvestris L.) by using extruder type pyrolyzer at 450, 550 and 600 ºC was the objective of the study. Sapwood specimens (15×25×50 mm along the grain) were impregnated with the obtained pyrolysis oils by full- and empty cell treatment. The results indicated that wood impregnated with the studied pyrolysis o...
A Temiz, M Hakki Alma, N Terziev


Microbial Community Analysis Using Terminal Restriction Fragment Length Polymorphism (T-RFLP) Analysis: Field Study Results
2008 - IRG/WP 08-20377
The effects of chlorothalonil (CTN) and butylated hydroxytoluene (BHT) on the fungal community in southern yellow pine (SYP) were assessed using terminal restriction fragment length polymorphism (T-RFLP) analysis. Field stakes treated with 0.25% and 0.37% ammoniacal copper quat (ACQ-C), 0.1 and 0.25% CTN, and 0.1 and 0.25% CTN combined with 2% BHT were installed with untreated controls in field s...
G T Kirker, S V Diehl, M L Prewitt, W J Diehl


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


A preliminary note on the role of moisture absorption rate in durability assessment
2008 - IRG/WP 08-20383
The rate of moisture uptake was studied in 15 wood species using vermiculite at varying moisture levels as the exposure medium. As might be expected, moisture uptake varied widely among the species studied. While some of the more durable wood species were also resistant to moisture uptake, this was not always true. The results are discussed in relation to performance in under varying environmenta...
J J Morrell, L P Francis


Wood preservation by a mixed anhydride treatment: Using simple models of polymeric wood compounds
2008 - IRG/WP 08-30457
Treatment of wood by a mixed aceto/oleic (or other fatty acid residue) anhydride promoted as a safe and environment friendly wood preservation system has been examined quantitatively by liquid phase 13C NMR and solid phase MAS-DEC (proton decoupling) 13C NMR through all its different stages to determine which reactions occur with simple model compounds of the polymeric constituents of wood. The p...
F Lyon, M-F Thevenon, A Pizzi, G Tondi, A Despres, J Gril, S Rigolet


The effect of gamma radiation on selected wood properties
2008 - IRG/WP 08-40394
As an easy, fast, and effective sterilisation method, gamma irradiation changes molecular structures not only in pest’s living cells, but also in wooden cell walls. Radiation-induced depolymerisation causes significant changes in some properties of wood crucial for restoration and for laboratory testing of wood-preservative effectiveness. The influence of gamma radiation concerning total amount ...
R Despot, M Hasan, A O Rapp, C Brischke, C R Welzbacher


Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III


The Effect of Heat Treatment on Water Absorption and Dimensional Stability of Anatolian Chestnut (Castanea sativa Mill.) wood
2008 - IRG/WP 08-40407
The heat treatment of wood is an environment-friendly method for wood preservation. This process improves wood’s resistance to decay and its dimensional stability. However, mechanical properties decrease in different ration because of density loss as a result of heat treatment. In this study, the effect of heat treatment on water absorption and dimensional stability at different relative humidit...
G Gunduz, D Aydemir


Termites y otros insectos xiliofagos en bienes arquitectonicos monumentos nacionalos de Colombia
2009 - IRG/WP 08-10679
The incidence of termites and other wood destroying insects was surveyed in ten historical buildings in Colombia. The most common insects were termites (Kalotermes, Cryptotermes, Heterotermes), although numerous decay organisms were also detected, including beetles (Anobium, Lyctus, Cerambycids) and various wood decaying fungi. Structural wood elements were classified according to the degree of a...
M G Ramírez


Chemical Analysis in Production Quality Control at Wood Treatment Plants
2008 - IRG/WP 08-20396
Analysis methods for quality control analysis in wood treatment plants have evolved with the changes in treatment preservative chemistries and analytical instrument technology. The basic hydrometer specific gravity measurements used for solution strength and classic wet chemistry methods for wood have given way to instrumental techniques such as X-ray fluorescence, automatic titrator, and HPLC. No...
P Walcheski, L Jin


Mold fungi - Major impediments to cleaning/repairing flood and rain-damaged homes
2008 - IRG/WP 08-40427
Damage to homes by hurricanes that make landfall in the south and southeastern United States, or sub-tropical and tropical regions, during the hot, humid summer months is compounded by the growth of mold fungi on wetted building materials. Most homeowners are better equipped to deal with construction problems associated with storm damage than to control the growth of mold fungi. Following hurrican...
T L Amburgey


Moisture adsorption isotherms of wood studies using a dynamic vapour sorption apparatus
2009 - IRG/WP 09-20398
Five types of wood including two Malaysian hardwoods acacia mangium (Acacia mangium) and sesenduk (Endospermum malaccense), two temperate softwoods, Sitka spruce (Picea sitchensis), radiata pine (Pinus radiata) and Accoya (commercially modified wood) were studied to determine their moisture sorption behaviour using a Dynamic Vapour Sorption (DVS) apparatus. The isotherm plot for each species teste...
J Zaihan, C A S Hill, S Curling


Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston


Assessment of mould growth on coated wood - methods and application
2009 - IRG/WP 09-20423
Discolouring fungi reduce the service life of coated wooden claddings in façades and increase the total cost of ownership due to shorter maintenance intervals. The project “Enhanced service life on coated wooden facades” has as its main objective to develop new methods for early prediction of durability and longer aesthetic service life of coated wooden cladding related to consumer needs and ...
L Ross Gobakken, C M Whist, O Høibø, P J Hovde, E Larnøy


Analysis on dynamics of basidiomycetes in decayed wood by a method using non-specific amplification of DNA
2009 - IRG/WP 09-20426
A combination of non-specific amplification of DNA by Phi29 DNA polymerase and specific amplification of the internal transcribed spacer (ITS) region of ribosomal DNA (rDNA) by polymerase chain reaction (PCR) was applied to elucidate the ratio of basidiomycete species inhabiting decayed wood from an outdoor bench. After more than 8 hours incubation with Phi29 DNA polymerase, concentration of DNA ...
T Wada, K Igarashi, M Samejima


Thermal behavior of zinc borate-treated wood
2009 - IRG/WP 09-30511
The objective of this study was to investigate the thermal behavior of zinc borate (ZnB)-treated solid wood by thermal analysis (TA). Thermogravimetry (TG) and differential thermogravimetry (DTG) curves obtained from TA showed that ZnB-treated wood specimens had higher char yields and lower maximum thermal decomposition temperature than untreated wood specimens. Reducing thermal decomposition temp...
E Terzi, H Sutcu, S N Kartal


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Environmental Emission of Wood Preservatives: Interpretation of Data Relevant to BPD Risk Assessments
2009 - IRG/WP 09-50259
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. The leaching rates can be derived from laboratory testing and from field testing. The relationship between laboratory and f...
D G Cantrell


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Life Cycle Assessment of treated timber: methodological aspects and first results
2009 - IRG/WP 09-50264
Environmental information on products is more and more required as a key to the market, and the building sector in Europe is certainly advanced in that direction. In France, Environmental Product Declarations are becoming very common for construction products. Therefore, the CTB P+ and CTB B+ certification comity as commissioned FCBA to perform the Life Cycle Analysis of treated timber in order to...
E Vial, M Bertrand, C Cornillier, G Deroubaix


Previous Page | Next Page