Validation by micro-computed tomography of an assessment method to measure the residual strength of anobiids infested timber
2019 - IRG/WP 19-20650
In this article a quantitative correlation study of pine timber structural elements, which have been subject to attack by anobiids, is presented. The main objective of the study was to establish a valid empirical correlation between the lost material percentage (consumed by beetles) and original/residual apparent density. Since the beetles’ attack produces a diffuse damage with a set of tunnels ...
J L Parracha, M F Pereira, A Maurício, P Faria, L Nunes


Visual assessment of longitudinal wheel timbers and assessing the feasibility of extending wheel timber service life in the UK railway network
2019 - IRG/WP 19-20651
Timber has been a versatile building material for centuries and during the start of the Railway Age in the nineteenth century it was in considerable demand for use in the railway network, particularly bridge building. Timber is still in service and widely used throughout the UK railway network. The resilience and favourable strength to weight ratio and its relative ease of fabrication make it an...
J R Williams


Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori


Protecting Sustainable Wood Infrastructure ̶ Improving the Performance of Poles, Piles, Ties & Timbers with Dual Treatments
2019 - IRG/WP 19-30735
Wood is by far the best structural material in terms of environmental impact, as shown by a number of LCA studies. This environmental impact superiority can be improved if the longevity of the commodity is extended. The main durability concern in large cross-section treated materials is the susceptibility of the heartwood to decay, as it is not typically treatable using traditional methods. This ...
J Lloyd, A Taylor, C Brischke, N Irby, M Manning


Chemical Analysis of Southern Pine Pole Stubs Sixty Months Following Treatment with a Methylisothiocyanate-Based Solid Fumigant Stick
2019 - IRG/WP 19-30740
Methylisothiocyanate-based fumigants have been commercially used in the United States for over 35 years to control internal decay in utility poles and other wooden structures with little technological advancement. The most recently commercialized methylisothiocyanate-based fumigant is chemically known as dazomet. Dazomet is a free-flowing powder or granule that decomposes in the presence of mois...
D J Herdman, T Pope, R R Browning


The use of bicine and tricine as possible Maillard reagents in a combined thermal/chemical modification of beech
2019 - IRG/WP 19-40852
The effects of thermal modification have been well established, particularly in terms of reductions in mechanical performance. In recent years, there has been an increase in studies related to the Maillard reaction. More commonly associated with food chemistry, it involves the reaction of amines and reducing sugars during cooking procedures. This paper has attempted to combine the use of amines an...
D Jones, C-M Popescu, D Krzisnik, M Hocevar, M Humar, M-C Popescu


Antifouling wood matrix with natural water transfer and micro reaction channels for water treatment
2019 - IRG/WP 19-40853
Wood with abundant nutrition transport channels could be considered as a kind of natural water purifier due to quick and effective passages for separation. Nevertheless, microporosity as main porous structure of initial wood are not enough to effectively separate small molecular, such as organic dye pollutants. Meanwhile, like most filters the fouling resulting in blocking and poor water flux will...
G Liu, D Xu, S Chang, J Hu, Xianjun Li5, Y Liu


Development of beech wood thermo-chemical modification treatments based on different vinylic derivatives of glycerol and polyglycerol
2019 - IRG/WP 19-40855
In this study, a combination between chemical and thermal wood modification has been investigated. Seven types of a low concentration of 10% aqueous additive solution of vinylicglycerol [glycerol-maleic anhydride (Gly-MA), glycidyl methacrylate (GM), and Glycerol methacrylate-maleic anhydride (GM/MA(2eq))], vinylicpolyglycerol [polyglycerol-maleic anhydride (PG-MA), polyglycerol methacrylate (PGM...
M Mubarok, S Dumarcay, H Militz, K Candelier, M-F Thevenon, P Gerardin


Suggestive remarks for designing of experimental samples and trial devices to treat wood by pre-vacuumed immersion method
2019 - IRG/WP 19-40862
This study was conducted to test the impregnability of wood material according to the pre-vacuumed immersion process and to reveal the usability of cylindrical (plug) samples in impregnation experiments in addition to the cuboid or cubic samples. In this context, cuboids were prepared 30 mm in length, 20 mm in width and 20 mm in thickness, whereas plugs were prepared radially and longitudinally wi...
I Usta


Treatability of native and exotic alternative timber species
2019 - IRG/WP 19-40864
The service life of moderately durable species can be extended significantly if the challenge of effective treatment of refractory wood species can be overcome. Along with preservative effectiveness, the performance of preservative in treated wood depends on factors such as retention and penetration in treated wood, the wood anatomy, the uniformity of penetration and micro-distribution within the ...
D Page, T Singh


Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama


Improvement of wood decay and termite durability resulting from combined treatments based on borax/phenol-formaldehyde impregnation followed by thermal modification
2019 - IRG/WP 19-40871
This study determined the factors influencing the boron content after leaching of pine blocks impregnated with aqueous solution of phenol-formaldehyde (PF) resin with or without borax and subjected to heat treatment by response surface methodology. An experimental design permits to analyze the effects of heat treatment temperature (150, 185 and 220°C), curing time (5, 12, 5 and 20 hours), resin c...
S Salman, M-F Thevenon, A Petrissans, S Dumarcay, P Gerardin


Thermal performance and fire safety properties of traditional circumferential log-cabin walls
2019 - IRG/WP 19-40872
The paper describes the experiment of fire resistance of a circumferential log-cabin wall fragment using various structural modification of the gap between two log members. The influence of the gap structural modification on the criterion of fire resistance E (envelop integrity) and I (insulation) is evaluated. The evaluating criteria are represented by the development of temperatures measured in ...
S Jochim, L Makovicka Osvaldova, M Zachar, Z Danihelova


Durability testing of mass timber building elements: a call for a collaborative trial
2019 - IRG/WP 19-40875
Mass timber buildings have captured the imagination of architects and engineers seeking more environmentally friendly building materials. The mass timber movement has tremendous potential to markedly increase timber use in mid-rise to high rise buildings. With great promise, however, comes great risk. Most mass timber structures that have been built or are being planned use no protective treatm...
J J Morrell


Fungal damages in Norwegian massive timber elements – causes and measures
2019 - IRG/WP 19-40879
Massive wood elements are relatively new in Norway but the use is growing quickly, primarily the use of cross-laminated timber (CLT). Moisture performance of massive timber elements has been examined by some researchers, but more knowledge is needed. There is uncertainty regarding the need for vapour barriers or retarders in roof assemblies, and for practical reasons buildings are rarely assembled...
M S Austigard, J Mattsson


Adhesion durability of the thinnest CLT in Japan treated by solvent recovery system
2019 - IRG/WP 19-40882
The purpose of this study is to clarify the adhesion durability of the thinnest CLT (36 mm thickness) in Japan impregnated with preservatives (azole neonicotinoid compounds (AZN)) under solvent recovery system so called “dry pressure process” for long-term durability. The adhesion durability tests were conducted in accordance with the Japanese Agricultural Standard (JAS) of Cross-Laminated-Tim...
K Kawakami, W Ohmura


Experimental study on compressive strength performance of cross laminated timber with biodeterioration damage
2019 - IRG/WP 19-40883
The mass timber construction has attracted attention around the world. The reasons are due to the environmental impacts and the potential of the strength performance and quantity of the wood. Nowadays, CLT is one of the most important materials for the timber constructions. If we use CLT as a building material, we should consider the biodegradation risk for long time use. From an estimation of fut...
T Mori, Y Otsubo, R Inoue, M Ikeda, K Kambara, W Ohmura


Wood veneer with high flexible decorated with nanoparticles for highly efficient water treatment
2019 - IRG/WP 19-50347
Natural wood is mainly comprised of numerous long, partially aligned channels (lumens) as well as nanochannels. Wood with these quick and effective passages is suitable for a membrane/separation material. However, a suitable thickness range of wood along its growth direction is essential to effectively separate small molecular, and the wood membrane is too thick to clean easily. In this paper, woo...
S Chang, D Xu, G Liu, J Hu, X Li, Y Liu


Outbreak of timber pest in Philippines: A consequence of frequent typhoons
2019 - IRG/WP 19-50348
Evidence of climate change and its impact are now visible in many parts of the world. This report presents impact of natural disasters in particular typhoons on trees as it passes across the Philippines archipelago every year. Typhoons damage and destroy large number of trees which soon rot under moist and warm conditions. Wood beetles and termites find these sources very quickly, breaking down th...
P Dhang


Study on Nailed Joint with Iron Contamination. Part1: Shear Performance of Nailed Joint with Iron Contamination
2019 - IRG/WP 19-50349
In Japan, The building standard law was amended in 2000.1) The use of metal joint was obligated by this law. Since then, metal joints have been largely used for wooden buildings. Also, Act on the Promotion of Popularization of Long-life Quality Housing was enacted in 2009 and leaving Long-life Quality Housing has been focused on2). However, leaving houses to posterity for a long time causes severa...
R Nakano, D Nakano, H Ishiyama


Moisture and temperature conditions in an old, highly moisture-loaded timber building in the Røros municipality, Norway
2020 - IRG/WP 20-10966
A 150 years old log building near Røros, Norway, has been in active use as a cowshed since its erection. The animals are kept inside the cowshed all winter and this causes a situation of a high moisture load on the wooden floor, wooden walls and ceiling. Logging of temperature and humidity over one year shows that there are favourable levels of moisture in the wood and air for development of moul...
M Sand Austigard, J Mattsson


Observed and projected changes in the climate based decay hazard of timber in the United Kingdom
2020 - IRG/WP 20-20665
The risk of microbiological attack on wood is determined by both material and climatic factors and indeed the hazard for a component is based on its intrinsic durability and the conditions in which it is used. The use of wood and organic materials in construction is increasing but ultimately all these materials will be susceptible to microbiological attack. The Scheffer Climate index applies clima...
S F Curling, G A Ormondroyd


Self-regulating heating cables for conductive heat transfer in pest control
2020 - IRG/WP 20-40895
Pest control by means of conductive heating of wooden elements requires considerable measuring and control efforts in order to avoid overheating of wooden surfaces, damage of structural elements and risk of fire. The usage of self-regulating heating cables might overcome such problems. In laboratory tests and under real conditions the applicability of self-regulating heating cables is tested with ...
J Müller, E Melcher, J Welling


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Comprehensive protection of timber in seawater
2020 - IRG/WP 20-10970
The hazard of wood in seawater can be divided into two areas: Below the water level, shipworm (Teredo navalis) and gribble (Limnoria lignorum) can attack non-resistant or insufficiently protected wood; above the water level, there is a risk by wood-destroying fungi and, to a lesser extent, insects. In a national project funded by the Deutsche Bundesstiftung Umwelt (DBU, German Federal Environmenta...
E Melcher, J Müller, T Huckfeldt