Exterior birch plywood: potentiality of the thermo-hydro treatment
2016 - IRG/WP 16-40743
It has been found in the present study that, in laboratory fungi tests after leaching with water (EN 84), exterior birch (Betula spp.) plywood, as birch solid wood, is subjected to degradation by rot fungi. This limits the use of such plywood outdoors or in building structures in high humidity conditions. The possibility to improve the birch plywood fungal resistance was investigated in two ways: ...
B Andersons, I Andersone, A Meija-Feldmane, I Irbe, A Janberga, J Grinins


Creosote leaching from timber bridges in Norway – a practical classification approach
2016 - IRG/WP 16-40744
Creosote is widely used as a wood preservative for highway timber bridges in Norway. However, excessive creosote leaching at various highway timber bridge sites leads to a bad reputation for the use of creosote treated timber constructions and the use of wood in general. Macro- and micro anatomical factors such as amount of heartwood, annual ring width, annual ring orientation, ray- height and com...
A Treu, K Zimmer


The Environmental Impact of Timber Products Compared to other Building Materials - A Survey of Published Environmental Product Declarations
2016 - IRG/WP 16-50314
One of the positive aspects of using wood in construction is the environmental benefits that this can potentially bring. However, manufacturers of all construction products and materials make claims about the ‘environmental friendliness’ of their products, making it exceedingly difficult for the end user to make informed choices about the advisability of using one product over another. This st...
C Hill, J Dibdiakova


Development of a new method for wood hydrophobizing and fixation of copper compounds by chemical hardening of vegetable based modified oils
2016 - IRG/WP 16-40754
Wood products with ground and direct water contact, but without sufficient biological durability, have to be protected against biological degradation by fungi and other microorganisms. Due to European legislation (Biocidal Products Regulation 528/2012), the selection of possible chemical agents, which are still allowed to be used, is diminishing rapidly. The use of previously widely applied, very ...
C Swaboda, M Fischer, K Jacobs


Assessing the natural durability for different tropical timber species using the mini-block test
2017 - IRG/WP 17-10886
The Xylarium in the Royal Museum for Central Africa (RMCA, Tervuren, Belgium) contains over 60,000 wood-samples, comprising over 12,000 species. These samples are of great historical and scientific value yet have a random format, which complicates standard testing. The wood-durability against Coniophora puteana and Trametes versicolor was tested for 36 species. Due to the random sample sizes the s...
V Deklerck, I De Windt, N Defoirdt, J Van den Bulcke, H Beeckman, E Espinoza, J Van Acker


Genetic characterisation of the deathwatch beetle – Call for support
2017 - IRG/WP 17-10890
The deathwatch beetle (Xestobium rufovillosum) is one of the most important pests of historical wood constructions. Further analysis of the exact nature of the feeding habits regarding diet and wood characteristics might deliver answers for controlling this pest. Also there is little known about genetic variability and population structure within the species. For analysis of infested wood and also...
M Höpken, E Melcher, J Trautner


Influence of organosilicon compounds and nanocellulose treatment on dimensional stability of waterlogged elm wood
2017 - IRG/WP 17-10891
Commonly used agents for waterlogged wood consolidation (including the most popular polyethylene glycol) have proved ineffective and even dangerous to the preserved objects, jeopardising their integrity. Finding new, effective alternatives for safe preservation of wooden cultural heritage is therefore of key importance. The future conservation agents should, first and foremost, provide the integri...
M Broda, B Mazela, I Dąbek, A Dutkiewicz, H Maciejewski, R Markiewicz, M Grzeszkowiak, S Jurga


Underground timber constructions from the First World War are well preserved after 100 years
2017 - IRG/WP 17-10897
During the Great War or World War I many underground constructions have been built for protection from shelling. They were an important part of the trench warfare as they were used as an area to rest and carry out other activities such as eating. They would usually range in size from smaller constructions that could hold several men to larger entities that could hold thousands of soldiers. In the ...
J Van Acker, I De Windt, K Haneca, H Beeckman, F Claeys, S Vandenbussche, J Vandewalle, N Robeyst, A Willems


Novel wood treatments improve resistance to the wood-boring marine isopod Limnoria quadripunctata
2017 - IRG/WP 17-10899
The marine isopod Limnoria quadripunctata degrades wooden structures in the sea and causes significant economic damage. Broad-spectrum biocides and naturally resistant tropical hardwoods have failed to prevent feeding by Limnoria and have caused ecological damage. Wood modification is now the favoured method, and resin-based modifications have been effective, while the efficacy of silica-based mod...
H Bowen, M Montibus, M Kutnik, S M Cragg


Case study: “Riesenbühlturm”
2017 - IRG/WP 17-20599
In this case study four 7 m long Douglas fir crossbeams were investigated regarding the remaining metal and moisture content. The crossbeams were replaced from a timber tower after 10 years of service in the Black Forest region (South Germany) due to fungal decay. From each of the crossbeams five stem discs were taken and relevant parameters (density, moisture and remaining metal content) were de...
E Melcher, J Müller


Design and performance prediction of timber structures based on a factorization approach
2017 - IRG/WP 17-20603
Service life of timber structures in outdoor conditions is predominantly affected by the climatic conditions in terms of moisture and temperature over time. On the one hand, the two parameters moisture content and temperature determine the exposure-induced dosage that can lead to fungal infestation and subsequent decay. On the other hand, the material resistance of wood stands in opposition to exp...
L Meyer-Veltrup, C Brischke


Laboratory test to determine the effect on durability of combining biobased building materials with timber in construction
2017 - IRG/WP 17-20604
The use of Structural Insulated panels is a construction approach that is seeing more abundant use and is becoming a widely available method. Preformed units are usually a composite structure which often include a range of bio-based materials such as timber, wool or straw. Traditional laboratory based wood decay tests do not take into account this combination of biobased materials and it may be po...
S F Curling, G A Ormondroyd


Modelling of moisture content in timber bridge details
2017 - IRG/WP 17-20613
The design of details is an important aspect in durability design of timber bridges. Details are often considered the weakest points in bridges due to their tendency to trap and accumulate moisture and thus facilitate decay. When designing maintenance plans and inspection intervals, it is important to know how design choices will come to influence the service life. Moreover, service life and wood ...
J Niklewski, C Brischke, E Frühwald Hansson, L Meyer-Veltrup


Comparative Durability of Timber Bridges in the USA
2017 - IRG/WP 17-20615
As engineers begin to utilize life-cycle-cost design approaches for timber bridges, there is a necessity for more reliable data about their durability and expected service life. This paper summarizes a comprehensive effort to assess the current condition of more than one hundred timber highway bridge superstructures throughout the United States. This national study was jointly administered by the ...
J P Wacker, B K Brashaw


Moisture content as a quality control parameter in thermally modified timber production
2017 - IRG/WP 17-20622
Quality assurance (QA) or factory production control (FPC) is necessary to ensure a proper production process. The requirements of QA/FPC can result from EN and national standards, quality assurance systems, or producer-specific rules. TMT producers must ensure that the process was correct, and to ensure traceability of products. In addition to the electronic records, the material should be che...
W Scheiding, H Turkulin, S Stein


An experimental study of mould growth and wood decay in timber frame walls
2017 - IRG/WP 17-20623
This paper deals with parameters related to the occurrence of mould growth and wood decay in timber frame walls. In a first part, the hygrothermal conditions inside a timber frame wall finished with brick veneer cladding are analysed to get an idea of possible moisture related problems. It is shown that, based on the VTT mould prediction model, there is a mould risk on the interface between the in...
M Vanpachtenbeke, J Van den Bulcke, I De Windt, J Langmans, S Roels, J Van Acker


Efficacy of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsamdua) water extractives on the durability of five Ghanaian less used timber species of varying perviousness and retentiveness
2017 - IRG/WP 17-30705
Conventional wood preservatives are not only toxic to target bio-deterioration organisms but also to humans, other organisms and the environment. In an effort to find preservatives that are less toxic or non-toxic to man, other organisms and the environment, efficacy of branch bark and heartwood water extracts (0.65 g/ml) of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsa...
A Asamoah, K Frimpong-Mensah, C Antwi-Boasiako


Copolymers of tannin extracts as wood protection agents
2017 - IRG/WP 17-30709
Wouldn´t be a dream to preserve wood with the substances which the nature already synthesizes for protecting itself? The idea we would like to pursue is simple: Increase the concentration of these substances, the tannins, trying to fix them properly in wood. It appears easy but it is not. Sensibility against leaching, fungal decay and weathering were observed. In this paper new flavonoid co-polym...
G Tondi, L Sommerauer, A Oberle, A Petutschnigg, M-F Thevenon


Possibility of using lichen (Usnea filipendula) and mistletoe (Viscum album L.) extracts as potential natural wood preservative
2017 - IRG/WP 17-30712
Increasing environmental pressures on toxic chemical wood preservatives lead to the development of natural and environmentally friendly wood preservatives. In this study, using possibilities of lichen (Usnea filipendula) and leaves of mistletoe (Viscum album L.) as potential natural wood preservative were researched. Treatment solutions have been prepared with two different solvents, water and met...
Ü C Yildiz, C Kiliç, A Gürgen, S Yildiz


Weathering protection of European hardwoods through double modification
2017 - IRG/WP 17-30715
Beech and poplar were thermally modified, treated with melamine resin and both treatments were combined. The weathering performance (cracks and general appearance) of modified beech and poplar was assessed in natural weathering and correlated to material properties such as work in bending (WB) and Brinell hardness. In addition, the equilibrium moisture content after exposure of 12 months and subse...
G Behr, A Gellerich, S Bollmus, H Militz


Effects of heat treatment on sound absorption coefficients in nanosilver-impregnated and normal solid woods
2017 - IRG/WP 17-40770
Effects of impregnation with silver nano-suspension as well as heat-treatment on sound absorption coefficients (AC) were studied in tangential direction of five different solid woods based on their importance. AC was measured at two frequencies of 250 and 500 Hz. A 400 ppm nanosuspension was used for the impregnation; silver nanoparticles had a size range of 30-80 nm. Based on the obtained results...
A Esmailpour, J Norton, H R Taghiyari, H Zolfaghari, S Asadi


Permeability of Eucalyptus wood improved by microwave treatment
2017 - IRG/WP 17-40773
The wood species with low permeability may cause many problems during timber manufacturing. Extreme difficulties take place in fabricating new wood-based composites by impregnating low- permeability timber with functional materials, such as flame retardant, preservatives and resins. Microwave (MW) treatment can increase the permeability of wood both in transverse and longitudinal directions. The e...
Xia He, Xianjun Li, Jie Xie, Xingyang Xiong


Is the SPM 15 effective? Survival of Pine Wood Nematode under thermal treatments
2017 - IRG/WP 17-40775
The pine wood nematode Bursaphelenchus xylophilus (Steiner and Buhrer) Nickle (PWN) is the causal agent of “Pine wilt disease” affecting coniferous forests, and since its detection in 1999 in Portugal, has obligated the European Union to take action to prevent its spread (Decision 2006/133/CE). The main measure applied is the International Standard for Phytosanitary Measures ISPM No. 15 (ISPM ...
L Robertson, M Conde, J C Cabrero, F Llinares, M T Troya


Evaluation of timber bridges with special consideration of detail design
2017 - IRG/WP 17-40781
Since 1997 the use of wood in bridge construction has been increasingly criticized by the Hamburg federal state authority supposedly because of shortened service life due to decay. With regard to wood research, however, it is often suggested that use of timber is suitable for weathered structures as long as constructive protection measures will be observed. In order to unravel the reasons for the ...
K Robbers, J Fromm, E Melcher


Prefacricated modular wooden bridges
2017 - IRG/WP 17-40785
The bridge consists of simple, identical pre-fabricated triangular wooden panels joined top and bottom to make up trusses. These trusses are in turn joined together side by side in pairs and are braced to one another to create a girder construction. The deck is carried on top of the trusses, an arrangement which has several advantages for such an uncomplicated structure. It is built up on site, af...