Thermal modification of non-durable wood species 2. Improved wood properties of thermal treated wood
1998 - IRG/WP 98-40124
Properties of wood treated in a new heat-treatment process called the PLATO-process have been studied. Several wood species have been treated using this new thermal modification process using a range of process conditions (mainly time and temperature). In this study the characteristics of the treated wood were determined using samples from whole planks treated on pilot plant scale. The modified ch...
B F Tjeerdsma, M J Boonstra, H Militz


Effects of heat treatment on modulus of elasticity of beech wood
2002 - IRG/WP 02-40222
Heat treatment is the oldest, simplest and cheapest method for reducing hygroscopicity of wood. The heat treatment protects wood against to biological organisms as well as giving wood dimensional stabilization without damaging environment. The effects of heat treatment on modulus of elasticity (MOE) of beech wood (Fagus orientalis Lipsky) naturally grown and intensively used in forest products in...
S Yildiz, G Çolakoglu, Ü C Yildiz, E D Gezer, A Temiz


Development of a disinfection treatment for oak logs to be imported from the USA
1984 - IRG/WP 3283
The European veneer industry depends greatly on oak supplies from the USA. To prevent the accidental introduction of the American Oak Wilt Disease (Ceratocystis fagacearum) into the member states of the EC, a disinfection treatment was developed for oak logs under consideration of the technical requirements of veneer production. Laboratory experiments and field trials in Germany and in the USA sho...
W Liese, M M Ruetze


Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Effect of point of preservative addition on the mechanical and physical properties of strandboard treated with Tanalith 3485
2000 - IRG/WP 00-40152
Preservative has been added to a PF bonded strandboard at various different stages in the manufacturing cycle and the physical and mechanical properties of the boards have been evaluated (modulus of elasticity, modulus of rupture, thickness swelling, water absorption, internal bond strength, and shear strength). Preservative addition has been examined at five different stages namely green strand d...
G J Goroyias, M D C Hale


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Remedial treatment of creosoted railway sleepers of redwood by selective application of boric acid
1980 - IRG/WP 3134
An ideal preservative for remedial treatment must primarily be characterized by two requirements. First, it must have an ability to diffuse and distribut evenly into the wood and secondly, it must be fixed properly so that it does not leach out too fast. However, these two characteristics conflict with each other, and the choice of preservative must of necessity be a compromise. Wood preservatives...
C Bechgaard, L Borup, B Henningsson, J Jermer


Evaluation of the insecticidal efficacy of deltamethrin and the fungicidal efficacy of its association with TCMTB + MBT in the field of wood preservation
1986 - IRG/WP 1289 E
Deltamethrin possesses many advantages for the insecticidal protection of wood: relatively low toxicity, very reduced evaporation, very prolonged retention in the wood, very slight leaching after having penetrated the wood, and absence of odour. Its association with other active agents or solvents is being studied with regard to chemical compatibility. Compatibility studies have proved positive fo...
J S Duguet


Characteristics and quantity of impregnated wood waste in Germany
1995 - IRG/WP 95-50041
The disposal of wood waste in Germany is one of the main problems not only for the wood preservation industry but also for all concerned with wood waste. Data on characteristics and quantity of wood waste are still needed. Based on criterions given in a previous paper (IRG/WP 93-50006), several assortments have been characterized with regard to their hazardous potential and their logistical aspect...
A Voss, H Willeitner


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Dutch national environmental policy strategy (NMP): Implications throughout the life cycle of treated timber and for the Dutch preservation industry
1993 - IRG/WP 93-50001-31
All overview of relevant environmental legislation and instruments for control is given for each stage of the life cycle of treated timber. Recent policy in the Netherlands has been focused around the "National Environmental Policy Strategy", in which a general policy with regard to reduction of pollution to the air, soil and water is described. The principle is one of an "Integrated Chain of Cont...
P Esser, D A Lewis, A J Pendlebury


Revised South African standards for wood preservation: Protocols for approval of wood preservatives
1995 - IRG/WP 95-20072
In 1994 the South African timber treatment industry completed its revision of the South African Bureau of Standards (SABS) Code of Practice for the preservative treatment of timber. These revisions were undertaken in parallel with changes to the SABS specifications for preservative treated timber. As a result of shortcomings in the previous wood preservative classification system which was based o...
D Conradie, P Turner, W E Conradie, A D Currie, I S J Burger


Proposal for a simple methodology for the evaluation of the preventive effectiveness of protectors applied in superficial treatments against basidiomycetes fungi
1999 - IRG/WP 99-20167
Due to the considerable effect that the relation between the lateral surface and the volume of wood blocks has on superficial treatments, this work has attempted to determine the ideal size which allows to evaluate the effectiveness of a preservative in the shortest possible time. Three wood blocks of different dimensions were tested. In addition, as it is necessary to neutralise the effect of the...
M T De Troya, A Navarrete, F Rubio, M Yuste, C Rodríguez-Borrajo, D Muñoz-Mingarro, F Llinares


Leaching of arsenic, copper and chrome from preservative-treated timber in playground equipment
1984 - IRG/WP 3149
Samples were taken from CCA-treated timber in sand play boxes and other play ground equipment. Sand was also sampled. Sand and wood samples were analysed for copper, chrome and arsenic by AAS. About 20-25% of the arsenic had leached from the timber after 2-4 year's exposure in the playgrounds. Very little of the copper and chrome had been leached. Sand collected in the close vicinity of t...
B Henningsson, B Carlsson


Collaborative soft rot tests: Statistical treatment of results of soil analyses
1971 - IRG/WP 29
Institutes taking part in the collaborative experiments already reported forwarded samples of the soils employed in the tests to the Forest Products Research Laboratory, England. The soils were then autoclaved sterilised under uniform conditions and sent to the Department of Forest Soils, the Royal College of Forestry, Stockholm, Sweden. The results of the soil analyses are given in Table 1, toget...
A F Bravery


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 5: Interim report
1980 - IRG/WP 454
Wood samples (15 x 2 x 2 cm³) were treated with one copper/chrome/arsenic (CCA) and one copper/chrome/boron (CCB) preservative using the following concentrations - O, 3, 6, 10%. Treated samples of three reference wood species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were supplied to all participants. Additional local species were chosen by participants and included in the test at t...
R A Eaton


A report on the development of "Technical Recommendations Document for the Canadian wood preservation and protection facilities"
1987 - IRG/WP 3447
The wood preservation and wood protection industry uses chemicals which are similar. However, because the methods of applications of preservatives are different in wood preservation (pressure treatment) and wood protection (surface treatment) plants, their problems need to be resolved separately. As a part of a federal strategy to protect the environment and human health from potentially toxic com...
G Das, V N P Mathur


Bibliographie sur les produits organiques en solvant pour la préservation du bois
1972 - IRG/WP 313
Le présent travail exécuté dans le cadre do la Section III du Groupe International de la Préservation du bois a pour but de rassembler, en vue d'éventuelles études plus approfondies sur le sujet ou sur l'un de ses aspects, les principales et relativement récentes références sur les produits de protection des bois en solvant, souvent appelés, et parfois improprement, pro...
H Alliot


The effect of a chelator mediated fenton system on activation of TMP fibres and decolorization of synthesized dyes
2004 - IRG/WP 04-50223
The purpose of this work is to improve our current knowledge of the non-enzymatic mechanisms involved in the brown rot degradation of wood, but also to study the potential applications of a chelator-mediated Fenton system in activation of wood fibers and decolorization of synthesized dyes. In this work, Electron Spin Resonance (ESR) spin-trapping techniques were used to study the generation of hyd...
Yuhui Qian, B Goodell, J Jellison


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


Silafluofen: Novel chemistry and versatility for termite control
1995 - IRG/WP 95-30069
A novel silicon - containing insectizide, HOE 084498 ('Silafluofen'), with a favourable toxicological profile, has shown activity against a broad spectrum of agricultural and environmental health pests. Results from laboratory and field studies around the world have demonstrated that silafluofen is effective at protecting timber from attack by various species of termite and wood-...
A J Adams, A Jermannaud, M-M Serment


Remedial ground-line treatment of CCA poles in service. A progress report after 28 months' testing
1988 - IRG/WP 3481
Remedial treatments of CCA-treated poles in service with incipient soft rot were carried out with boron rods, boron/glycol solution, boric acid paste, copper/creosote paste and a commercial product (DFCK paste) respectively. The micro-flora before remedial treatment and 6 months after as well as the spread of chemicals in the poles were reported in Document No: IRG/WP/3388. In this progress report...
B Henningsson, H Friis-Hansen, A Käärik, M-L Edlund


Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver


Rapid fixation of Chromated Copper Arsenate (CCA) wood preservatives by microwave treatment
2000 - IRG/WP 00-40184
Rapid microwave heating of freshly chromated copper arsenate (CCA) treated timber indicates that rapid preservative fixation is possible within approximately 40 seconds. The leaching of CCA was evaluated using simulated rainfall. Cost analyses indicates that microwave fixation using an on-line conveyor belt fixation process with an output of 4m3/hour using a microwave power supply of 230 kW costs ...