Natural durability of some commercial timbers of Sarawak, Malaysia in tropical marine environment
2005 - IRG/WP 05-10561
The abundant supply of timber resources in Sarawak makes timber an ideal choice to be used for marine construction. The natural durability of the main commercial timber species of Sarawak in ground contact is well established but the same is not available for marine environment. This study was conducted to assess the natural durability of 28 commercial timber species in tropical marine environmen...
K Jenang, Wang Choon Ling


Heat treated timber in Finland
2000 - IRG/WP 00-40158
Heat treatment permanently changes the physical and chemical properties of wood by means of high temperatures (150 - 240°C). Heat treatment darkens the colour of the wood. Heat treatment improves the equilibrium moisture content of the wood and the shrinkage and swelling of the wood is reduced. Very high temperatures improve the resistance to rot and also reduce the susceptibility to fungal decay...
T Syrjänen, E Kangas


The leachability and specificity of the biological protection of timber using Scytalidium sp. and Trichoderma spp
1986 - IRG/WP 1302
The results of field experiments, using biological control against internal decay of creosoted poles, are briefly reviewed and the evidence concerning the leachability of the antibiotics produced by these species is presented. A pure culture miniblock decay test on biological control treated pine sapwood is described and the results compared to previously published data. The protection against Len...
P I Morris, N A Summers, D J Dickinson


Leaching of inorganic wood preservatives – Investigating the relationship between leachability, dissociation characteristics and long-term leaching potential
2003 - IRG/WP 03-50199
Estimation of the leaching properties of preservative components is greatly affected by the leaching test method applied since not all methods equally consider the physical components responsible for leaching. These include: wetting of the wood and penetration of water (affected by dimensions, amount of end grain, permeability, duration and nature of water exposure); solution of preservative comp...
L Waldron, Y T Ung, P A Cooper


Water-borne preservative marine trials in Western Canada
1981 - IRG/WP 470
Red pine boards treated with chromated copper arsenate, ammoniacal copper arsenate, copper zinc arsenic additive, a modified ammoniacal copper arsenate, and zinc arsenic additive, have been installed in a marine field test at West Vancouver, British Columbia. After two and a quarter years exposure, all the test samples are in excellent condition with the exception of those treated with the zinc ar...
J N R Ruddick


Quality control of microwave treatment of timber after dry rot attack
2001 - IRG/WP 01-40205
In Denmark microwave treatment of timber has been used during the last 15 years for eradication of dry rot (Serpula lacrymans). About 1500 microwave treatments have been employed in coorporation with Hussvamp Laboratoriet. Previously all the infected timber was removed plus an extra metre as a safety zone. This meant that all casting boards and plaster had to be removed as well and joists replaced...
J Bech-Andersen, J Andreasson, S A Elborne


Protection of beech veneer for fruit and vegetable boxes
1981 - IRG/WP 3176
In Yugoslavia about 50,000 m³ of low quality beech logs annually are rotary cut into veneer from which boxes are made for transporting fruit and vegetables. Because of steaming before rotary cutting, beech veneer becomes extremely sensitive to mould attack which decreases the quality and commercial value of the final product. To avoid mould attack, veneer sheets are dried to 16% moisture content ...
N Vidovic


Computer-assisted numerical clustering analysis of various strains of Serpula lacrymans (Wulfen:Fr.) Schroeter apud Cohn
1992 - IRG/WP 92-2396
Eight strains of Serpula lacrymans were compared in relation to their previously determined factors (5 physiological and 10 toxicometrical). A numerical clustering analysis was used along with, as coefficient of similarity, "cos Q" after standardization of all results. Results with respect to the combined factors showed a mutual similarity within four groups of strains. The first of these groups c...
J Wazny, J D Thornton, P Stenzel


Performance of treated and untreated sawn fence posts of Scots pine and Norway spruce
2000 - IRG/WP 00-30247
Sawn fence posts are a rather important product and the objective of this trial was to assess their durability. In 1985 a field trial with treated and untreated fence posts of Scots pine (Pinus sylvestris L.) and Norway spruce (Picea abies (L.) Karst.) was set out at the test field in Ultuna, Uppsala, Sweden. The posts had a dimension of 75 x 100 x 1400 mm3. The preservatives applied were a CCA, a...
Ö Bergman


Less environmental impact of wood preservatives by considering the risk of attack in addition to the hazard class system
1995 - IRG/WP 95-50040-10
Hazard classes, which are standardized in Europe in EN 335, are most useful to direct chemical wood preservation towards the organisms which may attack wood in the various fields of utilisation. However, hazard only signifies the fact that an attack may occur without considering the actual risk to attack. To minimize the application of chemicals with respect of less environmental impact it is nece...
H Willeitner


Water-borne wood preservatives against marine borers. Results from NWPC marine trials started in 1972 and 1976
1990 - IRG/WP 4162
The paper presents the results from NWPC (Nordic Wood Preservation Council) marine trials started in 1972 and 1976. The trials are carried out according to the NWPC Standard No. 1.4.2.2./73 "Marine test - a test against marine wood boring organisms in sea water". The test site is Kristineberg Marine Biology Station on the west coast of Sweden. The wood blocks used in the trials were made from sapw...
Ö Bergman, C Lundberg


Wood preservation in Turkey
1982 - IRG/WP 3216
The report reviews the forestry potential of Turkey and also the historical background of wood preservation in the country. The wood preservation industry in Turkey is mainly concentrated on the treatment of poles and railway sleepers. There is no official body responsible for wood preservation activities, and therefore its promotion depends mainly on the voluntary research efforts carried out by ...
R Ilhan, R Cockcroft


The use of ESR spectroscopy to assess the photostabilising effects of wood preservatives
2000 - IRG/WP 00-20186
The degradation of wood surfaces exposed to UV light which leads to poor performance of clear coatings is understood to be due to delignification via a mechanism involving free radicals. Certain wood preservatives most notably CCA are able to photostabilise wood and therefore they may reduce the concentration of free radicals formed when treated wood is exposed to ultraviolet light. As a first ste...
S Schmid, R D Webster, P D Evans


Aspergillus fumigatus Fresenius resistance to chemical preservatives in piles of pine and birch wood chips
1981 - IRG/WP 1146
Investigation has been carried out on the communities of fungi developing in birch and Scots Pine chip piles in the Ostroleka Pulp and Paper Mill in the North-East of Poland The species composition or fungal communities and their development in a dozen of chip piles during storage was investigated. Untreated and chemically treated birch and pine wood chips were investigated. In all samples the gre...
M H Zielinski


Test methods used for approval of wood preservatives in Indonesia
1994 - IRG/WP 94-20045
Indonesian regulation stipulates that all pesticides, including wood preservatives, must be registered and obtain legal permit from the Minister of Agriculture, c.q. the Pesticide Committee before they are eligible for public use. For that purpose they have to meet safety and efficacy requirements approved by the Pesticide Committee. To meet the efficacy requirements, wood preservatives must be te...
A Martawijaya


Wood preservation in Thailand
1983 - IRG/WP 3265
The report gives a background to Thailand and its timber resources, production and consumption. The history of wood preservation in the country and its modern industrial development are described. Its 19 preservation plants are listed and the production figures of the two major ones given. The wood preservatives in use are noted and the costs of treating a railway sleeper in three different ways c...
A Rananand, R Cockcroft


Phytotoxicity of selected wood preservatives
1999 - IRG/WP 99-50133
The treated wood is used commonly around our environment. The aim of the study was to determine the reaction of plants to the wood preservatives and wood treated with preservatives. The study was made comparatively with ten types of organic and water-borne preservatives. The white mustard (Sinapis alba L.) was chosen for use as bioindicator and the tests were carried out to determine the response ...
P Witomski, J Wazny


Long term performance of CCA preservatives in ground contact
2000 - IRG/WP 00-30223
Copper-chrome-arsenate (CCA) preservatives have been use extensively in New Zealand since the mid-1950s for a wide range of ground contact uses, radiata pine being the main species treated. They have been the subject of a comprehensive field testing programme in up to five sites in New Zealand, the earliest tests being established in 1955. Main factors affecting performance have been formulation t...
M E Hedley, D R Page, B E Patterson


Preservative performance of copper naphthenate (SANPRESER-OGR) in brush treatment of timber
1991 - IRG/WP 3663
Preservative efficacy of copper naphthenate (SANPRESER-OGR) was evaluated in the laboartory and field trials when timber was treated by brushing. Results of field trial indicated that service life of the brush-treated timber could be approximately 10 years or longer under ground contact conditions, although life span was slightly varied with timber species and test sites. After four years&apos...
Y Sugai, K Hamada, M Kitada, K Tomoi


Co-operative field trial. Background notes and questionnaire for field sites
1992 - IRG/WP 92-3733
The first co-operative field trial was designed to study the occurrence of soft-rot in CCA treated hardwoods. Generally speaking very similar results were obtained from the different field sites. In the early part of the trial considerable variability was evident with regard to the rate and type of attack which occurred in the untreated material. With the CCA treated timber the type of decay was p...
D J Dickinson


Amines – Promising Wood Preservatives
2002 - IRG/WP 02-30287
Environmental concerns require a new approach in the field of wood protection. Band of many traditional wood preservatives has lead to intense researches for new environmental-friendly wood preservatives. Amines seem to be promising substitutes for classical biocides. Fungicidal and leaching resistance as well as some other chemical analysis of beach and Norway spruce samples treated with ethanola...
M Humar, F Pohleven, Š Kesnar, P Kalan


Review of remediation methods of sites contaminated by wood preservatives - testing of filter material for use in permeable barrier technology
1999 - IRG/WP 99-50141
Several treatment methods are currently available for treatment of contaminated sites. Soil and water can be treated by immobilisation, separation or destruction of contaminants. It has been common to use intensive treatment methods starting with soil excavation to reach strict purification goals. However, technical and financial reasons make it difficult to reach the desired treatment criteria. A...
G Rasmussen, H Iversen, S Andersen


Copper-resistant fungi on pressure impregnated wood in Denmark
1994 - IRG/WP 94-10078
The occurence of Amorphotheca resinae Parbery and its asexual stage Cladosporium resinae (Lindau) de Vries on CCA and CCB treated wood has previously been shown. In the autumn 1993 some other blue stain fungi were found on CCP and CCB treated pine timber, such as Ophiostoma minus (Hedgc.) H. and P. Sydow, Ophiostoma pilifera (Fr.) H. and P. Sydow and Ophiostona piceae (Munch) H. and P. Sydow. The ...
J Bech-Andersen, S A Elborne


The course of fixation of Cu-Cr-As wood preservatives
1972 - IRG/WP 307
Copper-chrome-arsenic (CCA) preservatives in contact with wood result in an instant extensive increase of pH, because of ion-exchange and adsorption reactions with the wood. During precipitation of the active elements the pH continuously increases but reaches a maximum, when all chrome is consumed. Some of the early reaction products are unstable and slowly convert via dissolution into stable comp...
S-E Dahlgren


Relative performances of DNBP and CCA wood preservatives in accelerated decay tests
1988 - IRG/WP 3496
The effectiveness of 2-sec-butyl-4,6-dinitrophenol (DNBP) was compared with that of CCA. Test blocks of Pinus patula and Eucalyptus grandis were impregnated to precisely known retentions of approximately 3, 6, and 10 kg/m³ CCA and solvent-borne DNBP respectively. They were then challenged in decay tests comprising soil burial and exposure to monocultures of Chaetomium globosum, Coriolus versicolo...
W H Schnippenkoetter, L D Abraham, A A W Baecker