Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown


Alternatives to CCA for ground contact protection of timber: a perspective from UK on performance and service life expectations
2002 - IRG/WP 02-30289
The proposed amendment to the European Union's Marketing and Use Directive (1976/769/EEC) in respect of arsenic in CCA wood preservatives seeks to restrict the use of CCA across the European Union. CCA is an extremely important wood preservative in the UK from the manufacturing of the product to the extent of use of CCA-treated timber. Based on our experience and judgement on the use of ...
E D Suttie, A F Bravery, T B Dearling


Recycling of treated timber by copper smelter
1994 - IRG/WP 94-50030
A preliminary trial was carried out to see whether copper smelting process is able to recycle CCA treated timber. As a result of the first trial almost a full recovery of both copper and arsenic was achieved. Recovered metals were utilized in manufacturing CCA preservatives. The energy bound in wood is utilized in the flash smelting process and the burning gases are fed to the sulphuric acid plant...
A J Nurmi, L Lindroos


The mechanism of leaching of copper-chrome-arsenic preservatives from treated timber in saline waters
1976 - IRG/WP 374
A mechanism for the leaching of copper-chrome-arsenic preservatives is proposed on the basis of theoretical calculations and experimental studies using timber subjected to a range of water types of different ionic compositions. Complex formation by copper (II) and chromium (III) with chloride and hydroxide ions is shown to affect the leaching rate. Of even greater importance is the salt effect on ...
J Irvine, S-E Dahlgren


Isolation of soil borne bacteria and fungi from treated timber
2001 - IRG/WP 01-50174
Most research in the last few decades has focused on the development of new strategies to control biological attack and the means to quantify this. Comparatively little work has been done to examine the effect that treated timber might have on its surrounding environment. This presentation will describe a methodology that attempts to detect any changes which might occur in the soil microflora foll...
I Stephan, A Stegemann, G Heidrich


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 21: Report of eighth inspection (7 years) in Australia
1985 - IRG/WP 4119
This report tabulates the seven year (86 month) inspection results, obtained on 28 Fabruary l985, of the IRG/COIPM International Marine Test at Goat Island, Australia. This test was installed in December 1977. The results are given in Tables 1-6. Table 7 lists the number of marine borers identified from blocks (2 cm and 6 cm long respectively) cut from the ends of specimens removed at the previous...
L J Cookson, J E Barnacle


Volatile organic compounds (VOC) measured during drying of impregnated timber
2004 - IRG/WP 04-50216
Discussion about drying of impregnated timber has taken place in the Nordic countries under eighties and nineties and goes on nowadays. The drying increase the value of production and the customer gets fewer problems when handles the timber. This introduces a positive attitude to the impregnation as a process and its products. Beside the important information about the advantages of impregnated ti...
N Terziev, V Djokic


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


Premature failure of treated timber in wharfs in Papua New Guinea, attributed to defects in design
1991 - IRG/WP 4158
The performance of timber in wharfs in Papua New Guinea has been monitored for a number of years. Premature failure of wharf structures was found in many cases to be due to defects in design rather than ineffective preservative treatment. Above-water timbers were found to be prone to severe checking followed by decay. Protection for the end grain of pile tops and the limiting of radial checking in...
S M Cragg


Interim report on world survey of sap displacement impregnation of timber
1974 - IRG/WP 329
At the 4th Annual Meeting of the IRG held in West Berlin in October 1972 it was suggested that a survey of sap displacement impregnation of timber would be of interest. Accordingly through the courtesy and co-operation of the New Zealand Department of Trade and Industry a questionnaire was circulated to the Trade Commissioners for transmission to the relevant organisations in various parts of the ...
F B Shorland, C G W Mason


Leaching of active components from preservative-treated timber - Ongoing research: Status after approx. 4 months’ out-door exposure
2003 - IRG/WP 03-20276
The Danish Technological Institute is together with manufacturers of active ingredients and formulators of wood preservatives running a project aiming at finding realistic leaching rates from preservative treated wood in hazard class 3 (above ground). The project is focussed on developing a field trial method for investigating leaching. According to BPD hazard assessment has to be carried out f...
N Morsing


Bacterial brown stain on sawn timber cut from water-stored logs
1992 - IRG/WP 92-1532
Brown stains which appear on the surface of sawn radiata pine cut from water-stored logs were identified as tannin-like compounds. They are derived from bacterial breakdown of flavanoid-glucosides. When timber is sawn from infected logs, the free flavanoids migrate to the wood surface as the timber dries. There, they condense and oxidise to form permanent brown discolourations. Stains occurred on ...
M E Hedley, R Meder


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 6: Report of third inspection (24 months) in Australia
1980 - IRG/WP 456
This report presents the results of the third inspection of the IRG/COIPM International Marine Test specimens installed at the Goat Island Marine Biological Station of the Maritime Services Board of New South Wales, in Sydney Harbour. The inspection was completed on 5th December, 1979, after 24 months exposure. As on previous occasions, this inspection was carried out in conformity with the provis...
J Beesley


The natural durability assessments of secondary timber species - field trials
1998 - IRG/WP 98-10297
Secondary or 'alternative' hardwood timber species can replace traditional hardwoods and contribute significantly to satisfying the overall demand for hardwoods in the UK timber market. A selection of these 'alternative' hardwoods is currently being tested at BRE-WTC for natural durability both in ground contact (to EN252) at two field sites, and out of ground c...
E D Suttie, R J Orsler


Exotic timber insect species intercepted in the UK since 1945
1978 - IRG/WP 182
Since the formation of an entomology section at the former Forest Products Laboratory, Princes Risborough, the Laboratory has been called upon to identify and comment upon a wide range of insects and insect damage in imported timber. Very often only the damage remains and frequently dead insects are associated with it, but on other occasions living exotic wood-boring insects enter the UK. Followin...
J M Baker, R W Berry


Dip-diffusion of dressed timber - Effect of drying
1990 - IRG/WP 3603
The effect of drying on BFCA dip-diffused, dressed, freshly sawn timber was determined by the depth of penetration of boron achieved on two test timber species, White Cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that the light density White cheesewood was completely penetrated even after 3 days drying while Light Hopea, treated immediately achieved 5...
H C Konabe


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 14: Report of fifth inspection (48 months) in Australia
1982 - IRG/WP 484
This report presents the results of the fifth inspection of the IRG/ COIPM Internatlonal Marine Test specimens installed in Sydney Harbour in December, 1977. This inspection took place on 9th December, 1981, just 48 months after the specimens were installed. Earlier reports have contained full details of the treatment and installation of the specimens as well as results of all previous inspections...
J Beesley


The colonisation pattern of anaerobic fungi in wood
1989 - IRG/WP 1403
Timber foundations may be degraded in service in anaerobic conditions. The present work was conducted to investigate whether anaerobic fungi could colonise wood, using rumen fungi as test microorganisms. Strictly anaerobic fungi were isolated and purified from cow dung and goat and sheep rumen fluids respectively. Colonisation of Eucalyptus grandis and Pinus patula by these fungi and Neocallimasti...
A H Wiederhold, M Morrison, A A W Baecker


Structural defects in CCA treated timber fence posts: A case study.
1997 - IRG/WP 97-40084
Since 1983 an environmental improvement programme has been in progress in the city of Dundee. This programme included the erection of rail and pale timber fencing throughout the city. The timbers had been pressure treated with CCA prior to painting with 2 coats of an exterior wood stain finish. However, the larger dimension timber fence posts (100 x 125 x 1500 mm3) regularly developed severe check...
S Muhsin, D C R Sinclair, A Bruce, H J Staines


Ecotoxicological behaviour of leachates from superficially treated timber as an approach for a test strategy of environmental risk assessment in wood preservation
1998 - IRG/WP 98-50101-09
At present for wood preservatives, which in Germany are subject to the quality mark of the RAL-GĂĽtegemeinschaft Holzschutzmittel, health and safety as well as environmental aspects are evaluated by official authorities, as BgVV (Federal Institute for Consumer Health Protection and Veterinary Medicine) and the UBA (Federal Environmental Agency). From the environmental point of view to day there a...
H W Wegen, U J Lucks


Durability of Anogeissus acuminata timber used for plank-built catamarans
2005 - IRG/WP 05-10551
Catamaran, the most versatile traditional fishing craft used along the Indian coast is made hitherto of solid timber of a few selected species of broad-leaved soft woods. Due to scarcity coupled with high cost of these timbers, the craft, of late, are fabricated from the wooden planks of an indigenous hardwood species, namely, Anogeissus acuminata (Yon) belonging to the family Combretaceae. Infor...
M V Rao, M Balaji, V Kuppusamy, K S Rao


Natural durability of fifty species of Indian timber in Goa waters against marine wood-borers
1989 - IRG/WP 4150
Results of the investigations on the natural durabilitv of fifty species of Indian timber, based on data collected bv exposing test panels at Betim near Panaji (Goa) continuously for a period of 11 months are presented. The study revealed that none of the timber species tested has any natural resistance at this locality and all the panels were completely destroyed within 11 months. Details on the ...
L N Santhakumaran, S Udaya Bhaskar, J C Jain


Performance of preservative-treated timber against biodeterioration in Indian waters
1984 - IRG/WP 4106
Results on the investigation on the durability of panels of 32 timber species, pressure-treated with various preservatives and exposed along the Indian coast for varying periods upto a maximum of 15 years, are summarised. Panels of even non-durable timber gave excellent results against biodeterioration after treatment. Their life was comparable to that of treated durable timber. The preservative t...
L N Santhakumaran, J C Jain, M C Tewari


Losses of CCA components and creosote from treated timber to soil
1997 - IRG/WP 97-50098
Components of creosote and CCA preservatives can migrate within the wood and move into surrounding soil. However, at present, the ecological significance of such losses is uncertain. This paper examines the distribution of four target polyaromatic hydrocarbons (PAHs ) and of copper, chromium and arsenic in treated stakes and surrounding soil after long term exposure in field trials. Concentrations...
N J Hudson, R J Murphy


Timber deterioration and its prevention in marine environment
2005 - IRG/WP 05-10559
Wood-borer activity is an established fact in Mumbai harbour that leads to severe deterioration of timber. In order to prevent the deterioration caused by wood borers three resin preservatives containing Zinc borate, Organo-copper polymer (4 wt% Cu) and Organo-Tin polymer Copoly(TBTM-MMA) were used for timber treatment. Test panels were treated using standard method and the...
B S Swami, M Udhayakumar, P Kumar, A B Samui


Previous Page | Next Page