Performance of wood-based composites in a protected aboveground test in southern Japan
2008 - IRG/WP 08-40391
Five kinds of untreated wood-based composites (medium density fiberboard, hardwood plywood=HP, softwood plywood, particleboard and aspen oriented strand board, hereinafter abbreviated as MDF, HP, SP, PB and OSB, respectively) were exposed to subterranean termites and microbial (decay) attack under protected aboveground conditions in a southern part of Japan (Kagoshima Prefecture) for six years. An...
K Tsunoda


Effect of CCA and Tanalith E on the performance of surface finishing
2008 - IRG/WP 08-40405
Effect of CCA and Tanalith E treatment on the performance of surface finishing properties was the objectives of this study. Sapwood of scots pine, (Pinus sylvestris L.) and oriental beech (Fagus orientalis Lipsk.) specimens (300 x 100 x 15 mm along the grain) were impregnated with aqueous solution of CCA 2% and Tanalith E 2%. Surface roughness, dry film thickness, adhesion strength, gloss measur...
T Ozdemir, A Temiz, I Aydin


Near infrared spectroscopy for the quantification of wood preservatives
2008 - IRG/WP 08-20391
Near infrared (NIR) spectroscopy is a rapid, flexible, inexpensive and non-destructive technology that has many applications, including the evaluation of many wood properties. Initial studies have indicated the potential to apply NIRS for the quantification of wood preservatives. However, further evaluation with borate and azole preservative systems has revealed that NIRS technology is challenged ...
A M Taylor, Seung H Baek, Myong K Jeong, J D Lloyd, J J Morrell


Above Ground Field Testing – Influence of test method and location on the relative performance of various preservative systems
2008 - IRG/WP 08-20393
Standardized above ground tests such as the lap-joint or test deck methods can be very slow in producing useful information on the relative performance of wood preservative systems. It often requires many years for decay to develop in wood treated to sub-optimal concentrations of standardized preservatives, making relative comparisons of performance between new systems and established preservativ...
A Zahora


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Performance of dip and pressure treated wood in termite ground proximity exposures in Hilo, HI, and Colombia
2008 - IRG/WP 08-30491
A number of preservative systems were evaluated for their ability to control termite attack when applied as both dip and pressure treatments. With dip treatments, better performance was observed with southern pine than spruce-pine-fir using the same solution strength treatment, probably as a result of the about 50% greater uptake with southern pine and associated deeper preservative penetration. B...
P Walcheski, A Zahora


Alkaline copper treated wood for use in residential decking
2008 - IRG/WP 08-30490
Alkaline copper quaternary ammonium compound (ACQ) treated decking was exposed in a field experiment and the mobile copper assessed based on that collected in the leachate. The amount of copper which leached was modeled after 4 years. The results showed that boards which leached most chemical initially provided the greatest loss over four years. The reduction in the mobility of copper with time wa...
J N R Ruddick


Field Stake Performance of Parallel Strand Lumber Treated with Waterborne Copper Naphthenate
2008 - IRG/WP 08-40435
Wood and wood products have been considered a premium building material for residential and industrial structures for many centuries. More recently, structural composite lumber (SCL) products have played an increasing role in satisfying the needs of the building industry. However, both wood and wood composites are naturally biodegradable materials which require enhanced durability when used in ce...
G P Merrick, M H Freeman, J A Brient


Wood preservative obtained by recycling – preliminary selection of leaching inhibitor
2008 - IRG/WP 08-50252
Based on recycling of used household batteries, a process was developed to enable the recovery of major manufacturing components, leading to a solution of zinc (32 g.l-1) and manganese (15 g.l-1) salts, free of heavy metals. The potential use of the above solution as wood preservative was demonstrated by means of assays both of fungicidal activity -using white and brown rot fungi- and of insectici...
C Ibáñez, C Mantero, G Cecchetto, M Rabinovich, M Cerdeiras


Comparison of laboratory and natural exposure leaching of copper from wood treated with three wood preservatives
2008 - IRG/WP 08-50258
Standard and non-standard laboratory and field leaching tests were used to compare copper leaching from wood treated to above ground and ground contact specified retentions for three wood preservative systems, CCA-C, ACQ-D and a micronized copper formulation with quat DDAC as co-biocide. Copper leaching was highest for the ACQ formulation. Percent leaching was lowest for the micronized copper sy...
P A Cooper, Y T Ung


Categorization of 300 timber, bamboo and cane grown in Bangladesh based on their families, origins, growths, physical and mechanical properties
2009 - IRG/WP 09-10684
In this study the 300 timber, bamboo and cane plants grown in Bangladesh have been classified into various categories based on their taxonomic families, origin of species, rate of growth, color of wood, texture of wood, shrinkage of wood, equilibrium moisture content (EMC) of wood, flammability of wood, cutting and sawing properties of timber, finishing and polishing qualities of wood, machining p...
A K Lahiry


European House Borer Hylotrupes bajulus Linnaeus in Western Australia: the anatomy of an eradication program
2009 - IRG/WP 09-20403
In January 2004, European house borer (EHB) Hylotrupes bajulus Linnaeus was detected in Perth, Western Australia. A containment program was set up and expanded to a full eradication campaign in 2008. The program is projected to eradicate EHB by 2021. This paper describes research work and assumptions on the biology and behaviour of EHB in Western Australia, surveillance and control methods, commun...
M Grimm, R J Cunningham, M Castalanelli, D Collins, L Vagg


Review of candidate graded particle barrier testing methods in Australian Standard (AS 3660.3 – 2000): Assessment criteria for termite management systems
2009 - IRG/WP 09-20417
The Australian Standard (AS. 3660.3 – 2000) for assessment of candidate graded particle termite barriers is reviewed and suggestions for amendments are made. Areas requiring amending in light of current biological knowledge involve the inclusion of proprietary or patented systems rather than generic types; selection of test termites in the genus Coptotermes; duration of test periods; and inadequ...
J R J French, B M Ahmed (Shiday), B L Schafer


Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston


The Promotion of Timber and Timber Product uses in China - Government's Role in Regulation and Standardization
2009 - IRG/WP 09-20424
Chinese Government always pays special attention to resource and environmental issues, therefore, resource saving and environmental protection are part of the basic state policies. This paper provides a brief summary of the key policies which guide the practices in promoting timber conservation and efficient utilization in order to meeting social demands of the wood uses. In the paper, the develop...
Liu Nengwen


A theoretical-industrial correlation and perspective on copper-based wood preservatives - a review of thermodynamic and kinetic aspects on copper-wood fixation mechanism
2009 - IRG/WP 09-30499
Copper was and it will continue to remain one of the key active component in wood protection industry. Over the past decades, a significant effort from R&D teams in industry, academia and research institutes was directed toward understanding the copper-wood fixation mechanism, optimising the copper retentions in the wood and reduce leaching in order to maximized performance, prolong the lifetime o...
R Craciun, M Maier, J Habicht


Antifungal Activities of Three Supercritical Fluid Extracted Cedar Oils
2009 - IRG/WP 09-30501
The antifungal activities of three supercritical CO2 (SCC) extracted cedar oils, Port-Orford-cedar (POC) (Chamaecyparis lawsoniana), Alaska yellow cedar (AYC) (Chamaecyparis nootkatensis), and Eastern red cedar (ERC) (Juniperus virginiana L), were evaluated against two common wood decay fungi, brown-rot fungi (Gloeophyllum trabeum) and white-rot fungi (Trametes versicolor). The statistical analysi...
Tianchuan Du, T F Shupe, Chung Y Hse


Leaching performance, decay and termite resistance of wood treated with boron compounds incorporated with phenol-formaldehyde resin
2009 - IRG/WP 09-30503
A resol-type phenol-formaldehyde (PF) resin was synthesized and designed to penetrate wood incorporated with boron compounds in order to immobilize boron in wood. The leaching performance, decay and termite resistance of treated wood was investigated. Three kinds of boron compounds, that is, boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT), were selected to mix with PF and tw...
Liping Yu, Jinzhen Cao


Effects of new fixative additives on leachability of boron wood preservatives
2009 - IRG/WP 09-30507
Borates are well known with their protective capacity against both fungi and insects with low mammalian toxicity and environmental acceptable. However, boron itself does not ensure the appropriate protection for wood in the exterior applications because of their easily depletion from the treated wood under wet conditions. In this study, the potential use of monoglyceride and polyvinyl alcohol prod...
A Mohareb, J Henry, E Wozniak, P Gérardin


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Enhanced uptake of wood modification agents in “bioincised” wood
2009 - IRG/WP 09-40445
The permeability of refractory wood species e.g. Picea abies and Abies alba is reduced resulting in a radial penetration of chemical solutions of only a few millimetres. Exploitation of these wood species is therefore not possible for many applications. A novel biotechnological method (European patent 05027812.6) based on the pre-treatment of wood with the white-rot fungus Physisporinus vitreus si...
F W M R Schwarze, M Schubert


Environmental Emission of Wood Preservatives: Interpretation of Data Relevant to BPD Risk Assessments
2009 - IRG/WP 09-50259
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. The leaching rates can be derived from laboratory testing and from field testing. The relationship between laboratory and f...
D G Cantrell


Life Cycle Assessment of treated timber: methodological aspects and first results
2009 - IRG/WP 09-50264
Environmental information on products is more and more required as a key to the market, and the building sector in Europe is certainly advanced in that direction. In France, Environmental Product Declarations are becoming very common for construction products. Therefore, the CTB P+ and CTB B+ certification comity as commissioned FCBA to perform the Life Cycle Analysis of treated timber in order to...
E Vial, M Bertrand, C Cornillier, G Deroubaix


Barefoot-heat-impact of oil-heat-treated wood: An important thermal property of decking boards
2009 - IRG/WP 09-40458
In this study the phenomenon of sensual heat impression was examined, when walking with bare feet on sun exposed wood based decking boards. A suitable method for measuring the heat flux from decking boards into an artificial foot was developed. The method and measuring device is described as well as results from measuring three different decking board materials: Oil-heat-treated spruce (OHT), untr...
A O Rapp, C R Welzbacher, C Brischke


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp