IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1058 documents. Displaying 25 entries per page.


An engineering model for the decay of timber in ground contact
2003 - IRG/WP 03-20260
To predict the residual strength of an engineered structure, it is first necessary to predict the effect of decay. A model was developed in which the effective area of structural decay in large section timbers was defined as that area that could be picked out with a pen-knife. Some limited studies indicated that for practical purposes the remaining wood could be assumed to have its full residual s...
R H Leicester, C-H Wang, M N Nguyen, J D Thornton, G Johnson, D Gardner, G C Foliente, C MacKenzie


The performance of water repellants on radiata pine exposed to the weather
1989 - IRG/WP 3553
The effectiveness and resistance to weathering of four water repellent treatments, a commercial timber stain, and an oil-based clear finish, was assessed using 20x20x6 mm³ samples of untreated, copper-chrome-arsenic (CCA)-treated, and tributyltin oxide (TBTO)-treated radiata pine exposed to the weather over a four month period. The water repellency of each preservative/water repellent combination...
D V Plackett, F M Cameron


An evaluation on durability of untreated mining timber support
1997 - IRG/WP 97-20121
Wedge blocks in dimension of 5 x 7 to 8 x 155 cm3 were cut from indigeneous scots pine pitprops. Each of wedge block pairs were numbered and half of them were placed as the test blocks between the steel arches and the strata in a hard coal pit. Controls in laboratory and test wedge blocks in the mine were then sawn into 20 by 20 by 300 mm standard test sticks. Impact bending, static bending and MO...
A Bobat


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests. Results after 40 months fungal cellar exposure
1983 - IRG/WP 2200
Decay rates of preservative-treated Pinus radiata stakes during 40 months exposure in the FRI fungus cellar were compared with those of similarly treated material in a field test. Decay rates in the fungus cellar were from 4 to 100 times higher than in the field, although for the majority of preservatives the rate was between 7 and 12 times higher. The lag phase before onset of decay, noticeable w...
M E Hedley


Chromium on the surface of CCA-treated wood
1978 - IRG/WP 386
Chromium in solutions of CCA preservatives is predominantly in the hexavalent state (Cr VI). It is well known that Cr VI is associated with dermatitis and skin ulceration in workers handling chromium containing products and processes. When reduced to the trivalent state, however, chromium is considerably safer. An essential part, therefore, of safety procedures in any chromium - using industry is ...
C R Coggins, P Hiscocks


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Methyl bromide eradication of the oak wilt fungus in logs. Laboratory and field fumigation
1981 - IRG/WP 3168
Concern over accidental introduction of the oak wilt fungus (Ceratocystis fagacearum) into oak-importing nations has prompted a study supported by the U.S. National Lumber Exporter's Assn. to assess the efficacy of methyl bromide fumigation to eradicate the fungus from logs and lumber. Laboratory and field fumigation trials to develop a reliable and realistic treatment were performed on r...
E L Schmidt, M M Ruetze, D W French


Chemical Analysis of Southern Pine Pole Stubs Thirty-Nine Months Following Treatment with Three Methylisothiocyanate-Based Fumigants
2004 - IRG/WP 04-30349
Agricultural fumigants have been commercially used in the United States for over 20 years to control internal decay in utility poles and other wooden structures. Of the four fumigants which are currently used in the remedial treatment of utility poles, three are based on methylisothiocyanate (MITC) as being the principal fungitoxic component. Two of these MITC-based fumigants, liquid metham sodi...
R J Ziobro, J Fomenko, D J Herdman, J Guzzetta, T Pope


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Preliminary field and laboratory findings regarding the efficacy of a novel anti-marine wood borer agent
2000 - IRG/WP 00-10380
Blocks of sapwood of Pinus nigra were treated by vacuum impregnation with Biocide A to retentions of 0.5, 1 and 2 kg m-3. Similar blocks were vacuum-pressure impregnated with CCA to retentions of 2, 24 and 38kg m-3. The blocks were exposed subtidally in Mourilyan Harbour (Queensland, Australia). After 5 and 10 months exposure, blocks were removed, examined for superficial signs of attack by wood b...
A Praël, S M Cragg, R A Eaton


Development on Damage Functions of Wood Decay for Building Envelope Design
2005 - IRG/WP 05-10556
For the hygrothermal analyses of building envelope systems for insulation design, we tried a natural decay test of wetted wood specimens without any inoculation of fungi. Three principal experimental types: under steady-state conditions (Experiment A), at a cyclic water dripping under Non-steady conditions (Experiment B) and at a cyclic water dipping under-steady conditions (Experiment C), were ca...
H Suzuki, Y Kitadani, K Suzuki, A Iwamae, H Nagai


Sludge formation in timber treatment with CCA preservatives. Origin and elimination
1984 - IRG/WP 3276
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, are repor...
A Pizzi, W E Conradie, A Jansen


Survey of maintenance management of a residence
2001 - IRG/WP 01-10405
The following points were clarified from the responses to the questionnaire. Termite damage was most common in the bathroom, washroom, and entrance, in that order. Termite damage was most commonly found beneath floors, followed by floor surfaces, and inside walls, in that order. Damage in framing was minimal. Damage in all structural components was most common in the Kyushu region, with the most s...
Y Yamaguchi, M Azuma, Y Hikita, K Nishimoto


Chemical, physical and biological factors affecting wood decomposition in forest soils
2003 - IRG/WP 03-20281
Organic matter (OM) decomposition is an important variable in determining the potential of forest soils to sequester atmospheric CO2. Studies using OM from a particular location gives site-specific decomposition information, but differences in OM type and quality make it difficult to compare results among soils and forest ecosystems. By using a “standard” OM in decomposition studies, OM qual...
M Jurgensen, P Laks, D Reed, A Collins, D Page-Dumroese, D Crawford


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Biological control of sapstain fungi in wood
1996 - IRG/WP 96-10158
Sapstain fungi can cause serious damage to wood and wood products, resulting in a significant economic loss for the wood products industry. The purpose of the present investigation was to determine whether the sapstain in wood caused by sapstain fungi could be biologically controlled. Biological control of sapstain fungi in wood was demonstrated in field trials with nonpigmented isolates of Cerato...
S C Croan


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980's against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


Premature decay of CCA-treated pine posts in horticultural soils - An overview
1984 - IRG/WP 1241
The recent discovery in New Zealand of early decay in CCA-treated pine posts set in horticultural soils led to the establishment of a comprehensive research programme. The objectives and outline of this programme are presented together with an overview of research progress to date. Results suggest that premature decay of CCA-treated timber is restricted to material placed in highly cultivated soil...
J A Butcher


Assessing the performance of wood preservatives from biological tests - the European approach
1994 - IRG/WP 94-20040
The impetus for the European Standardisation Committee to undertake the development of a performance standard for characterising the effectiveness of wood preservatives from biological tests, lies in the Construction Products Directive. This is effectively the European Community law which provides the basis for Construction Products to be traded across all member states without technical or regula...
A F Bravery


Effect of treatment process on performance of copper-chrome-arsenate. Part 2: Field stake tests
1995 - IRG/WP 95-40046
Pinus radiata sapwood stakes 20 x 20 x 400 mm³ were treated with CCA Type C using a range of concentrations and three treatment processes; Bethell, Lowry and Rueping. Preservative retention was determined by chemical analysis of treated material. Following fixation stakes were installed in a randomised plot in the Whaka graveyard located on the FRI campus. Stakes were inspected at yearly interval...
M E Hedley, J Anderson, J B Foster, B E Patterson


Calculation of preformance index of Bardac 20 (an alkylammonium compound) evaluated in a field stake test
1982 - IRG/WP 3206
Bardac 20 treated stakes have been in test for three years at the Westham Island test site near Vancouver, B.C. The Performance Index for the preservative was calculated and found to be 0.009 which infers that, at the standard retention, Bardac 20 added 0.9 y to the life of the stake. It may be concluded that when tested using a standard field stake test using ponderosa pine (Pinus ponderosa Laws)...
J N R Ruddick


Correlation between different international standard assessment procedures with termites. Part 1: Field exposure
1983 - IRG/WP 1198
Ramin treated with copper-chrome-arsenic (CCA), pentachlorophenate and lindane, each at three retentions, and three other untreated timbers were assessed in the field against Coptotermes lacteus and Nasutitermes exitiosus. Replicate specimens were exposed around five mounds of each termite species over a period of five years in south-eastern Australia. The field results provided the basis for judg...
M Lenz, C D Howick, N Tamblyn, J W Creffield, M Westcott


The possible significance of the lignin content and lignin type on the performance of CCA-treated timber in ground contact
1988 - IRG/WP 1357
The lignin in wood samples of Alstonia scholaris, Octomeles sumatrana and a Simaruba species have been analysed. These timbers are characterised by a high lignin content and low syringyl:guaiacyl ratios. Decay tests with two soft rot fungi showed that the timbers were less susceptible than timbers with a low lignin content and higher syringyl:guaiacyl ratios. Numerous data for field performance of...
T Nilsson, J R Obst, G F Daniel


An environmental assessment of timber treatment plants in Australia
1999 - IRG/WP 99-50124
Australian Standard AS 2843 Timber Preservation Plant Safety Code, sets the specifications for the design and operation of timber treatment plants in Australia. The Timber Preservers' Association of Australia has carried out an environmental survey of timber treatment plants throughout Australia using the operational checklist provided in Appendix C of Part 2 of the Standard. Third party ...
J Norton, K Riley


Moisture condition in treated wood exposed outdoors. A progress report
1989 - IRG/WP 3533
Wood treated with water-borne preservatives, mainly CCA (copper/chromium/arsenic), CCB (copper/chrome/boron) or CC (copper/chrome) is often said among users in Sweden to absorb more water than untreated wood. In laboratory tests this statement has not been confirmed but no field tests have been carried out in Sweden to study this phenomenon. In 1986 a project was started to compare water absorptio...
M-L Edlund, C E Sundman


Previous Page | Next Page