IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 503 documents. Displaying 25 entries per page.


Effects of Nano-Zycosil on Liquid and Gas Permeability of MDF
2012 - IRG/WP 12-40578
Effects were studied of zycosil nanoparticles, with size range from 30 to 90 nm, on liquid and gas permeability of medium density fiberboard. 100 g of nanozycosil was added to each kg of dry fibers. Density was kept constant at 0.67 g/cm3. The obtained results indicated that addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the ...
H Reza Taghiyari, K Heidarhaee, P Noori, A Karimi


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Effects Of Wood Preservative On Mechanical Properties Of Glulam Manufactured From Lower Density Malaysian Tropical Timber
2012 - IRG/WP 12-40590
This study is to investigate the effect of wood preservative on the mechanical properties of glulam timbers made from low density Malaysian hardwood timbers. Utilization of lower density Malaysian tropical timber for structural applications have not exploited extensively due to their inferior strength. By converting into treated glued laminated (glulam) timbers it could offer the possibility of th...
L Francis, Z Ahmad


Guideline for Environmental Product Declaration for Thermally Modified Timber
2012 - IRG/WP 12-50287
Environmental Product Declarations (EPD) intend to enable the comparison of the environmental attributes of products that meet equivalent functional requirements. This guideline describes the proceedings of EPD for thermally modified timber (TMT). The main objective is the general survey on requirements on EPD which are based on European and international standards.Up to now only a few EPDs for na...
L Clauder


Seed oil and defatted cake proximate composition of non timber product Annona squamosa (Annonaceae) grown in Benin
2012 - IRG/WP 12-30607
Annona squamosa L. is a small tree which grows wild in many places in the tropical regions, locally called “xwingle” in Benin. Its produces edible fruits, typically globular or heart-shaped which are highly appreciated and the seeds are not used. In the course of work about identifying new oil sources from a large number of oil bearing seeds grown in Benin, we report here on the chemical compo...
T S Djenontin, J Dangou, P Lozano, D Pioch, D C K Sohounhloue


Survival of Bursaphelenchus xylophilus exposed to different active ingredients of wood protectors
2013 - IRG/WP 13-10802
The pine wilt nematode (PWN) Bursaphelenchus xylophilus (Steiner and Buhrer 1934) Nickle, 1970 is a quarantine organism with a high potential to damage Conifer forests in Europe. This has driven the European Union to protect forest stands from the propagation and dispersion of this pathogen.The nematode was first detected in Europe in Setubal (Portugal) in 1999 and eradication measures were taken....
S C Arcos, M T Troya, L Robertson, F Llinares, M Conde, A Navas


Quasi-in-situ durability tests on oak timber bridges
2013 - IRG/WP 13-20510
This study aims on developing a method for determination of wood durability on samples taken from real structures in service. Therefore quasi-in-situ durability tests have been conducted exemplarily on timber bridges made from English oak (Quercus robur L.). Drilling cores were found to be a feasible alternative to standard specimens for laboratory durability tests against pure cultures of Basidio...
C Brischke, C J Behnen, M-T Lenz, K Brandt, E Melcher


Testing the performance of timber using 27 different field test methods
2013 - IRG/WP 13-20517
Numerous test methods to determine the durability of timber and timber products have been described in relevant literature. However, only some of these methods have been standardized and thus only very few are regularly used for resistance tests in the field. Since results from extensive comparative field studies have shown differences in moisture performance between different test methods, the ai...
L Meyer, C Brischke, J Rieken


Extraction and analysis of DNA from green and seasoned timber as basic methods for determination of wood species and origin
2013 - IRG/WP 13-20523
Against the background of the European timber trade regulation EUTR, commenced to law by March 2013, the determination of wood species and tracing of its origin is getting a great importance. A promising approach for establishing fast and reliable tracking systems for wood products is DNA analysis. A critical point is the extraction of analysable DNA from the wood and its lignified cell walls. Thu...
K Jacobs, H Mende, W Scheiding


Virulence of two Laboratory Test Strains and one Natural Isolate of Rhodonia (Oligoporus) placenta against Thermally Modified Pine and Beech Wood
2013 - IRG/WP 13-20524
Rhodonia (Oligoporus) placenta is known as a relative aggressive basidiomycete fungus against thermally modified timber. In durability lab tests, this often results in a lower durability class, compared to other test fungi. In the reported work, the virulence of three different strains of Rhodonia placenta for untreated and thermally modified timber was determined and compared. Therefore, two lab ...
K Plaschkies, W Scheiding, K Jacobs, N Rangno


Application of a model for the prediction of fungal degradation of thermally modified beech timber by Trametes versicolor
2013 - IRG/WP 13-40622
Colour measurement technology is found to be feasible for characterization of the property changes of thermally modified timber (TMT). In opposite to time-consuming and expensive laboratory tests a non-destructive test represents an improvement for the manufacturer of TMT. Therefore the aim of this study was to develop a method which allows sorting the different treatment intensities after the man...
Clauder, L., Richter S., Unger, W., Pfriem, A


Conclusions and Summary Report on an Environmental Life Cycle Assessment of ACQ-Treated Lumber Decking with Comparisons to Wood Plastic Composite Decking
2013 - IRG/WP 13-50295
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of ACQ (alkaline copper quaternary)-treated lumber decking and wood plastic composite decking using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood decking are significant. • Less En...
AquAeTer, Inc.


Conclusions and Summary Report Environmental Life Cycle Assessment of Marine Pilings
2013 - IRG/WP 13-50298
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of treated wood, concrete, galvanized steel, and plastic marine piles using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood piles are significant. • Less Energy & Resource Use: Tre...
AquAeTer, Inc.


Modelling the risk for mould growth on timber stored outdoors protected from rain
2013 - IRG/WP 13-20529
A mould resistance design (MRD) model was used to calculate the maximum duration of storage of timber outdoors under cover (protected from rain) before the onset of mould growth on the surface of wood. The prediction model is based on laboratory tests performed in constant and cyclic climates and were also confirmed against exposure tests in attics and crawl spaces. The prediction model presented ...
E Frühwald Hansson, S Bardage, S Thelandersson


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


On-site remediation treatments for framing timber in leaky buildings
2014 - IRG/WP 14-20549
Weathertightness failures in New Zealand buildings due to the combined effects of cladding choices, design and construction faults and the use of untreated framing timber has led to the so called ‘leaky building syndrome’. The latest estimated cost of the leaky building crisis in New Zealand is about NZ$11 billion. This research was conducted to provide a better understanding of the option...
T Singh, D Page, A Bennett


Efficacy of commercial wood preservatives against Bursaphelenchus xylophilus, a quarantine organism in Europe
2014 - IRG/WP 14-30638
Bursaphelenchus xylophilus (Steiner and Buhrer 1934) Nickle, 1970, pine wilt nematode (PWN), is a quarantine organism with a high potential to damage Conifer forests in Europe. This has driven the European Union to protect forest stands from the propagation and dispersion of this pathogen. Since the nematode was detected in Europe, eradication measures were taken. However, these measures were unsu...
C S Arcos, A Navas, L Robertson, M T Troya, M Conde, F Llinares


Laboratory investigation of fire protection coatings for creosote-treated timber railroad bridges
2014 - IRG/WP 14-30639
As the incidence of timber railroad bridge fires increases, so has the need to develop protective measures to reduce the risk from accidental ignitions primarily caused by hot metal objects. Of the six barrier treatments evaluated in the laboratory for their ability to protect timbers from fires sourced with ignition from hot metal objects only one intumescent coating provided adequate fire prote...
C A Clausen, R H White, J P Wacker, S T Lebow, M A Dietenberger, S L Zelinka, N M Stark


CreoSub – New protection technology to substitute creosote in railway sleepers, timber bridges, and utility poles
2014 - IRG/WP 14-30644
Creosote oil is one of the oldest industrially used wood preservatives. Due to its toxic profile, the European Commission has restricted the use of creosote specific applications, but it is highly controversial within the European Commission. Its approval for use after 2018 is very questionable and may depend on derived research results until then, i.e., the viability of alternatives developed to ...
U Hundhausen, K-C Mahnert, A Gellerich, H Militz


Nano-Zycosil in MDF. Part I: Gas and Liquid Permeability
2014 - IRG/WP 14-40652
Effects were studied of zycosil nanoparticles, with size range from 20 to 80 nm, on liquid and gas permeability of medium density fiberboard. Nanozycosil was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. The obtained results indicated that the addition of zycosil to the mat resulted in a significant increase...
H Reza Taghiyari, A Karimi, P M D Tahir, O Schmidt, E Bari, P Nouri , A Jahangiri


Effect of silver nanoparticles on the rate of heat transfer to the core of the medium-density fiberboard mat
2014 - IRG/WP 14-40653
Effect of silver nanoparticles on the rate of heat transferred to the core section of medium-density fiberboard (MDF) mat was studied here. A 400 ppm aqueous nanosilver suspension was used at three consumption levels of 100, 150, and 200 mL/kg based on the weight of dry wood fibers; the results were then compared with the control MDF panels. The size range of silver nanoparticles was 30-80 nm. Res...
H Reza Taghiyari, O Schmidt, E Bari, P M Tahir, A Karimi, P Nouri, A Jahangiri


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


Development of composite furniture using bamboo strips, bamboo mat and rubber wood veneer
2014 - IRG/WP 14-40679
Bamboo offers cost-effective component in panel form is well suited to wood substitute can be used as furniture components. In the present study, borak (Bambusa balcooa ) bamboo were used for manufacturing bamboo panel. Mitinga (B. tulda) bamboo were used for making mat and rubber wood veneers were used for manufacturing mat overlaid veneer board. Borax-boric acid (BB) treatments were given to enh...
K Akhter, M Mahabubur Rahaman, M H Chowdhury, M Zahirul Alam


Compatibility of Acetylated Wood and Wet Concrete
2014 - IRG/WP 14-40673
One of the newer commercial technologies to provide stability and durability to wood and wood composites is the process of acetylation (the reaction of acetic anhydride with wood). Wood is often used in contact with concrete, although only a very limited amount of species are suitable for this type of application because of durability issues. From this perspective durability class 1 timber such ...
R Rowell, C Lankveld, J Alexander


Douglas-fir PSL Treated with Oilborne Copper Naphthenate – Treatment Experience & Efficacy
2014 - IRG/WP 14-40687
Treating characteristics, field stake efficacy and the results from treatment trials for oilborne copper naphthenate (CuNap) and Douglas-fir parallel strand lumber (PSL) are summarized in this paper. Treatment with a P9 Type-C based solution in laboratory tests showed full cross section penetration of large cross sections could be achieved. Commercial treatment trials using a P9 Type-A solution ...
G P Merrick


Previous Page | Next Page