IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 604 documents. Displaying 25 entries per page.


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 4: Report of second inspection (12 months) in Australia
1979 - IRG/WP 448
Previous reports have presented full details of the treatment and installation of the test specimens in Sydney Harbour during December, 1977, and of the results of the first (6 months) inspection made during June, 1978. At the June inspection it was apparent that the plastic tubing used to make up the frames from which to suspend the specimens was inadequate for the job and not strong enough to su...
J Beesley


Leaching of CCA preservative from treated timber in marine environment
2001 - IRG/WP 01-30254
Knowledge on the amount of preservatives leaching out of treated wood is essential to optimise the chemical loading in various species of timber required for different end uses. In order to gain more insight into this aspect, the residual CCA content in 40 treated timber panels belonging to 14 species removed on destruction by marine organisms from a series of durability tests conducted in Kochi w...
M V Rao, V Kuppusamy, K S Rao, L N Santhakumaran


Inhibition of wood decay and termite damage by calcium precipitation
1996 - IRG/WP 96-30111
Fungal decay of wood in service, especially brown rot, results in billions of dollars (US) of losses annually. Recent environmental restrictions, both U.S. and international, are limiting or eliminating the use of broad spectrum biocides for wood preservation, primarily due to problems with disposal. In order to design new, environmentally benign methods for control of wood decay fungi, it is esse...
F Green III, T A Kuster, L Ferge, T L Highley


The yeast Pichia sp. As a short-term biological control agent to fungal spoilage of sawn softwood timber
2000 - IRG/WP 00-10362
Previous work has found isolates of the yeast Pichia to be a successful biological control agent toward moulding of fruits. An isolate was tested for the ability to protect sapwood of Pinus sylvestris timber against visual degrade by surface growth of moulds and staining fungi. Successful protection of autoclaved wood sprayed with a mixture of common wood moulding fungi was achieved when the yeast...
C Payne, H J Staines, A Bruce


Changes to New Zealand Timber Treatment Specifications
2004 - IRG/WP 04-20288
Changes have been made to the New Zealand timber treatment specifications in response to frequent incidences of decay in framing timber and doubts about the long-term performance of tributyltin formulations when used in exposed situations. Changes have been made to Hazard Class H1 to allow a level of treatment to provide short to medium decay resistance to framing which would protect it, should l...
M E Hedley


Incursion of Hylotrupes bajulus Linnaeus (European House Borer) into Western Australia
2005 - IRG/WP 05-10558
In January 2004, an adult Hylotrupes bajulus Linnaeus was detected emerging from a beam of Pinus pinaster in a house in Perth, Western Australia. The timber had been locally grown and milled. Surveys to define the extent of the infestation show it is restricted to dead pine trees in 28 sites around Perth. The biological and economic feasibility of eradication is being assessed. Since about 2001, k...
M Grimm


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Chemical analyses of IRG/COIPM INTERNATIONAL MARINE TEST (to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water) samples
1987 - IRG/WP 4114
Chemical analysis of CCA and CCB treated timber was carried out after exposure at tropical and temperate marine sites. Results indicated that losses of all elements had occurred. In particular, losses of boron were severe. Arsenic and copper were also lost. The chromium components in both formulations was the most dominant metal remaining. The results suggest that chromium modification was importa...
L E Leightley


Detection of Acoustic Emission (AE) generated by termite attack in a wooden house
1999 - IRG/WP 99-20166
Recently, considerable attention has been paid to methods for termite control, which involves few or no chemicals. To reduce the amount of termiticide needed, it is necessary to detect termite attack in wood as early as possible. The feasibility of acoustic emission (AE) monitoring for the nondestructive detection of termite attack has been discussed previously. In this study, we propose some tech...
Y Fujii, Y Yanase, T Yoshimura, Y Imamura, S Okumura, M Kozaki


Wooden windows, avoidance of damage via constructional measures
1990 - IRG/WP 3591
Increasing awareness of the environment reinforces the trend to use wood as a building material for windows in modern building constructions. Wood is a natural building and construction material. Under certain circumstances such as persistent humidity exceeding 30%, wood is rapidly degraded by decay fungi into CO2 and inorganic salts. The cost caused by damage (e.g. replacement of windows) represe...
R Gründlinger, K Messner


An engineering model for the decay of timber in ground contact
2003 - IRG/WP 03-20260
To predict the residual strength of an engineered structure, it is first necessary to predict the effect of decay. A model was developed in which the effective area of structural decay in large section timbers was defined as that area that could be picked out with a pen-knife. Some limited studies indicated that for practical purposes the remaining wood could be assumed to have its full residual s...
R H Leicester, C-H Wang, M N Nguyen, J D Thornton, G Johnson, D Gardner, G C Foliente, C MacKenzie


An evaluation on durability of untreated mining timber support
1997 - IRG/WP 97-20121
Wedge blocks in dimension of 5 x 7 to 8 x 155 cm3 were cut from indigeneous scots pine pitprops. Each of wedge block pairs were numbered and half of them were placed as the test blocks between the steel arches and the strata in a hard coal pit. Controls in laboratory and test wedge blocks in the mine were then sawn into 20 by 20 by 300 mm standard test sticks. Impact bending, static bending and MO...
A Bobat


Chromium on the surface of CCA-treated wood
1978 - IRG/WP 386
Chromium in solutions of CCA preservatives is predominantly in the hexavalent state (Cr VI). It is well known that Cr VI is associated with dermatitis and skin ulceration in workers handling chromium containing products and processes. When reduced to the trivalent state, however, chromium is considerably safer. An essential part, therefore, of safety procedures in any chromium - using industry is ...
C R Coggins, P Hiscocks


Detection of termite attack in wood using AE monitoring
1990 - IRG/WP 2355
An acoustic emission (AE) monitoring method for detecting termite activity in wood was applied to lumber of 3 by 3 cm to 10 by 10 cm square, 1 m long. Furthermore, the propagation of AEs due to the feeding activities of termites in the specimens and the locations of AE sources were analyzed. Also discussed was the feasibility of the method applied to posts out in the field of subterranean termites...
Y Fujii, M Owada, M Noguchi, Y Imamura, M Tokoro


Investigation of microwave as a means of eradicating dry rot attack in buildings
1992 - IRG/WP 92-1545
A microwave-apparatus developed for treatment of building-structures infested by dry rot was tested in the laboratory. The test-conditions simulated treatment of either infested timber or infested brickwork. Sawdust samples, both wet and dry, infested by viable mycelium of Serpula lacrymans were packed in glass-tubes. The tubes were then placed in the middle of either 20 cm thick wooden beams or 3...
C Kjerulf-Jensen, A P Koch


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Development on Damage Functions of Wood Decay for Building Envelope Design
2005 - IRG/WP 05-10556
For the hygrothermal analyses of building envelope systems for insulation design, we tried a natural decay test of wetted wood specimens without any inoculation of fungi. Three principal experimental types: under steady-state conditions (Experiment A), at a cyclic water dripping under Non-steady conditions (Experiment B) and at a cyclic water dipping under-steady conditions (Experiment C), were ca...
H Suzuki, Y Kitadani, K Suzuki, A Iwamae, H Nagai


Sludge formation in timber treatment with CCA preservatives. Origin and elimination
1984 - IRG/WP 3276
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, are repor...
A Pizzi, W E Conradie, A Jansen


Survey of maintenance management of a residence
2001 - IRG/WP 01-10405
The following points were clarified from the responses to the questionnaire. Termite damage was most common in the bathroom, washroom, and entrance, in that order. Termite damage was most commonly found beneath floors, followed by floor surfaces, and inside walls, in that order. Damage in framing was minimal. Damage in all structural components was most common in the Kyushu region, with the most s...
Y Yamaguchi, M Azuma, Y Hikita, K Nishimoto


The use of a physical field model to study the effects of remedially treated timber on the growth of perennial ryegrass (Lolium perenne) and rye (Secale cereale), and the accumulation of toxic preservative constituents in Lolium perenne
1995 - IRG/WP 95-50040-02
Low cost laboratory model systems can be used to give relatively rapid indications of the environmental effects of preservative treated timber in soil contact. This paper details the effects of remedially treated timber on the growth of crops of Lolium perenne and Secale cereale seeded on soilbeds of different texture in close proximity to remedially treated creosoted pole sections. Lolium perenne...
D C R Sinclair, G M Smith, A Bruce, H J Staines


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


Novel observations on the micromorphology of soft rot attack of wood
1996 - IRG/WP 96-10176
Electron microscopic examinations of decaying Pinus radiata horticultural posts which had been treated with CCA preservative prior to being placed in service about nine years ago showed the presence of soft rot fungi and tunnelling bacteria. Some novel observations on the micromorphology of the soft-rotted areas of tracheid walls are described here. The micromorphology of soft-rotted areas was hig...
A P Singh, R N Wakeling


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980's against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


The possible significance of the lignin content and lignin type on the performance of CCA-treated timber in ground contact
1988 - IRG/WP 1357
The lignin in wood samples of Alstonia scholaris, Octomeles sumatrana and a Simaruba species have been analysed. These timbers are characterised by a high lignin content and low syringyl:guaiacyl ratios. Decay tests with two soft rot fungi showed that the timbers were less susceptible than timbers with a low lignin content and higher syringyl:guaiacyl ratios. Numerous data for field performance of...
T Nilsson, J R Obst, G F Daniel


An environmental assessment of timber treatment plants in Australia
1999 - IRG/WP 99-50124
Australian Standard AS 2843 Timber Preservation Plant Safety Code, sets the specifications for the design and operation of timber treatment plants in Australia. The Timber Preservers' Association of Australia has carried out an environmental survey of timber treatment plants throughout Australia using the operational checklist provided in Appendix C of Part 2 of the Standard. Third party ...
J Norton, K Riley


Previous Page | Next Page