Comparison of thermally modified wood originating from four industrial scale processes – durability
2002 - IRG/WP 02-40229
This study examined the differences in biological wood properties of heat treated wood originating from four different European industrial heat treatment plants. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. The results of miniblock tests with basidiomyc...
C R Welzbacher, A O Rapp


The effect of heat treatment on the properties of spruce
1994 - IRG/WP 94-40032
The effect of high temperature treatment (above 150°C) on the wood quality is studied at the VTT. Improved dimensional stability, lower equilibrium moisture content and increased durability against biodeterioration is achieved, depending on the environmental factors. The biodeterioration resistance of spruce is improved due to changes in chemical composition and lower equilibrium moisture content...
H Viitanen, S Jämsä, L Paajanen, A J Nurmi, P Viitaniemi


Determination of bis-(N-cyclohexyl-diazeniumdioxy)-copper in different matrices by photometer, thermal energy analyzer and HPLC
1999 - IRG/WP 99-20179
For the quantitative analysis of bis (N-cyclohexyl-diazeniumdioxy)-copper (Cu-HDO) three analytical methods are used. The employment of the different methods depends on the matrices involved. For several years now, the colorimetric determination of Cu-HDO by photometer has been applied to solutions and concentrates of wood preservatives. In principle, the technique consists of a quantitative conve...
J Wittenzellner, W Hettler, M Maier


Dimensational stabilisation of wood
1981 - IRG/WP 3171
A review is given of the studies on the dimensional stabilisation of wood which have been carried out in the laboratory 5.14 "Wood Technology" since 1967. All stabilisation methods known have first been compiled from the available literature. Practical studies were then started. Wood was treated with monomers (styrene, methyl metacrylate, isocyanate), formaldehyde, tannin and sugar. Despite a sati...
A Burmester


Solution stability and Mechanical properties of Chitosan treated Pine
2005 - IRG/WP 05-30377
During the last years the research on chitosan as a wood preservative has been enhanced. Up to now, most of the research has been applied to the anti-fungal properties of chitosan, and no research was conducted on the solution stability of chitosan solutions in repeated trials by impregnation of wood, or on the mechanical properties of chitosan-treated wood. In this paper, the stability of high- a...
E Larnøy, M Eikenes, H Militz


Environmental characterisation of retification process by-products (liquid and gaseous wastes)
2005 - IRG/WP 05-50224-10
In order to reduce environmental risks during the service life of the treated wood and to find new alternative developments on the durability of wood, some research and technology development have been made on thermal treatment. The retification process is one of these processes. The retification process induces chemical modification of the lignin and cellulosic components and modifies the intrins...
G Labat, E Bucket, S Legay, C Yriex, P Marchal, E Raphalen, M Vernois, R Guyonnet, H Besset, E Fredon), G Vilarem, L Rigal, C Raynaud


Effect of aqueous polymer treatments on wood properties. Part 1: Treatability and dimensional stability
1990 - IRG/WP 3610
Partially air-dried sapwood of sweetgum (Liquidambar styraciflua) and southern pine (Pinus spp.) was treated with either aqueous polyacrylate or aqueous dimethyloldihydroxyethyleneurea (DMDHEU) solutions. Tests for dimensional stability were conducted on matched treated and untreated pieces. Measurement of the antishrink efficiency indicated that DMDHEU was a better stabilizer than the polyacrylat...
Z Ashaari, H M Barnes, R C Vasishth, D D Nicholas, D E Lyon


Impregnation of timber with tannin as a mean of improving its dimensional stability
1992 - IRG/WP 92-3695
The results of a joint project carried out at the Timber Division of LNEC under the 2nd research programme of the CEC DGXII - "Wood as a renewable raw material" entitled "Stabilization of wood by impregnation processes" is presented. Pieces Maritime pine timber was impregnated with tannin under pressure to see if the treatment with tannin improved the behavior of wood regarding its dimensional sta...
J S Machado


Determination of thermal degradation of isothiazolone treated wood
1997 - IRG/WP 97-30154
Wood treated with 4,5-dichloro-2-n-octyl-4-isothiazolin-3-one was the subject of thermal degradation study. The study included burning isothiazolone treated wood under various temperatures with and without oxygen. The result showed that no harmful combustion products, such as polychlorinated dibenzo-p-dioxins, polychlorinated dibenzo-p-furans and polychlorinated biphenyls, were detected. These fin...
Bing Yu


Stability of bifenthrin in a commercial phenol-formaldehyde plywood glue
2003 - IRG/WP 03-30311
Liquid phenol formaldehyde (PF) glue mixes used for plywood manufacture are strongly alkaline. At this pH insecticidal additives may not be stable for long periods. In order to establish practical working life of the synthetic pyrethroid insecticide, bifenthrin, in liquid PF glues the concentration of bifenthrin in the glue mix was measured under laboratory conditions over a 24 hour period. Glu...
M J Kennedy, P A Collins, R D Vella


A new process for in situ polymerization of vinyl monomers in wood to delay boron leaching
1998 - IRG/WP 98-40110
Efforts were accelerated on effective use of boron compounds in wood preservation owing to their environmentally safe characteristics and relatively low costs in addition to their well-known high bioactivity and fire resistant properties. Although having these unique favorable properties, they are readily leachable from treated wood at humid conditions. Therefore, they had limited market for exter...
M K Yalinkilic, W Dwianto, Y Imamura, M Takahashi


New research data confirming the suitability of bifenthrin as a wood preservative
1996 - IRG/WP 96-30116
Bifenthrin has been further tested against wood destroying insects, and its behaviour in wood has been extensively studied. Bifenthrin proved to be highly effective as a curative and preventative treatment against Anobium punctatum and Hylotrupes bajulus, after both leaching and evaporative ageing. Results of penetration tests with water and solvent based formulations, applied by brushing, dipping...
S Shires, P Héloir, B Chen, G Rustenburg


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


The commercialisation of ThermoWood® products
2006 - IRG/WP 06-40339
The concept of thermally modifying timber is well established, which has achieved a limited market breakthrough to date. Commercial application has mainly occurred within Finland, though recent years has seen market gain in several other European countries. This paper reviews the known properties of ThermoWood® timber, based on the combined work of the Finnish ThermoWood® Association, alongside ...
D Jones, E Suttie, J Ala-Viikari, N Bergstrom, D Mayes


The Effect of Flavonoids on Colour and Spectral Changes of the Wood Surface Caused by Heat Treatment or Ultra-violet Irradiation
2006 - IRG/WP 06-40341
Both heat treatment and UV irradiation can cause discolouration and change in the spectral properties of wood surface. Some of the characteristic flavonols have significant role on colour and spectral changes, despite of their relative small quantities in wood. Colour changes and spectral properties of natural and extracted black locust (Robinia pseudoacacia L.) and poplar (Populus nigra L.) were...
R Csonka-Rákosa, L Molnár-Hamvas, E Börcsök, J Molnár, K Németh


Thermal decomposition behavior of CCA-treated wood for safe disposal and the safe recovery of heavy metals through pyrolysis
2006 - IRG/WP 06-50238
If we could estimate the chemical changes in heavy metals by temperature in chromated copper arsenate (CCA)-treated wood during pyrolysis, it is expected that we could solve the environmental problems of heavy metals, which may occur during pyrolysis, and therefore, the thermal decomposition behavior of effective elements of CCA-treated wood was examined to find a safe disposal method. First, CCA-...
Dong Won Son, Dong-heub Lee, Sun-hae Cheon, Myung Jae Lee


Fire, flame resistance and thermal properties of oil thermally-treated wood
2007 - IRG/WP 07-40361
Oil thermal treatment, first developed by German scientists, is a promising technology for improving the durability and dimensional stability of wood for outdoor above-ground residential uses such as siding and shingles. The present authors’ previous research showed that 220ºC is an optimal treatment temperature, with 2 hours’ treatment producing wood with significantly improved moisture and ...
Jieying Wang, P Cooper


Water repellency and dimensional stabilIty of wodd treated with waterborne resin acids/TOR
2007 - IRG/WP 07-40364
Wood used in above ground applications such as decking undergoes undesired dimensional changes leading to the lumber warping, cupping, splitting, etc. This is a major concern to consumers but it can be reduced by treating lumber with a water repellent. The ability of resin acids, hydrophobic compounds naturally present in southern yellow pines, was examined as a possible water repellent. A wate...
T P Schultz, D D Nicholas, J Shi


Multivariate analysis of infrared spectra for the prediction of the mechanical performance and dimensional stability of thermally modified wood
2007 - IRG/WP 07-40367
The use of calibrated mid-infrared Fourier transform (FTIR) spectroscopy for predicting the main bending strength parameters of thermally modified wood is described for the first time. The analysis is based on the handling of OSC-filtered FTIR data from control and treated wood samples, using partial least squares (PLS) regression. Sets of Norway spruce, Scots pine and Beech wood samples were th...
M M González-Peña, M D C Hale


A step towards a better understanding of fungal colonization of modified wood - QRT-PCR studies
2008 - IRG/WP 08-10653
The area of wood protection is in a period of change. New wood protection systems have been developed while their mode of action remains insufficiently understood. The development of molecular methods provides potential tools to investigate the interaction between modified wood and decay fungi. One small step to tackle some of the unsolved questions about the mode of action of modified wood is tak...
G Alfredsen, A Pilgård, A Hietala


Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III


Heat treatment, thermal treatment, thermal degradation of wood, carbon nanotubes and Damascus steel swords. What do they all have in common?
2008 - IRG/WP 08-40399
Thermal degradation of wood is a well known phenomenon. Yet heat-treatment of wood can also provide protection for wood against certain environmental hazards. This paper explores some of the aspects of thermal degradation of wood fiber at relatively low temperatures with a surprising result. Carbon nanotubes (CNTs) were produced when a specific heating regime was used to carbonize the wood fiber. ...
Xinfeng Xie, B Goodell, Yuhui Qian, G Daniel


Thermal treatment of Nigerian-grown Albizzia zygia and Funtumia elastica wood in soy oil medium.
2008 - IRG/WP 08-40413
Thermal treatment in soy oil medium is one of the techniques used as a substitute to the chemical treatment in wood preservation. However, the effects of this technique vary from one species to another and hence the need to investigate the response of individual species to it. Thermal treatment of air-dried Nigerian-grown Albizzia zygia and Funtumia elastica wood was carried out in a vessel contai...
L Awoyemi


The Effect of Heat Treatment on Water Absorption and Dimensional Stability of Anatolian Chestnut (Castanea sativa Mill.) wood
2008 - IRG/WP 08-40407
The heat treatment of wood is an environment-friendly method for wood preservation. This process improves wood’s resistance to decay and its dimensional stability. However, mechanical properties decrease in different ration because of density loss as a result of heat treatment. In this study, the effect of heat treatment on water absorption and dimensional stability at different relative humidit...
G Gunduz, D Aydemir


Previous Page | Next Page