Wood-Plastic Composites preservation against fire: Nanofillers as fire retardant alternative
2018 - IRG/WP 18-40843
The purpose of this study is to improve fire resistance of Wood-Plastic Composites (WPCs) by adding inorganic nanofillers. Indeed, the main components of WPC, namely wood and polymer are both flammable materials despite the fact that WPCs are used in the field of construction. The effect of nanofillers on fire retardancy of Wood-High density polyethylene Composites was studied with three nanofille...
D Ben Ammar, A Koubaa, S Migneault, H Bouafif


Performance of wood exterior structures above ground in Spain built with softwood species. The situation case of a shelter bridge
2018 - IRG/WP 18-40844
Across Europe is very common to find wood exterior structures build in sawn and glue-laminated wood. Most of these exterior wood structures use softwood wood species such as: fir, spruce, larch and pine. In Spain exterior wood structures, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wood structures in overall Spain. This paper s...
D Lorenzo, M Touza, J Fernández-Golfín, A Lozano, J Benito


Developments within COST Action FP1303 related to the modification of wood
2018 - IRG/WP 18-40847
COST Action FP 1303 (Performance of bio-based building materials) was established in 2013 with the main aim to improve the knowledge on the performance of bio-based materials used as building products and the assessment of factors influencing these, with the aim of increasing their service life. This Action has helped in understanding the interlinked relationships between durability, product aesth...
D Jones


Non-stochiometric oxidation and ROS generation promoted by guaiacol lignin structures and lignocelluose surfaces may be a component of brown rot fungal degradation mechanisms
2019 - IRG/WP 19-10937
Model guaiacol compounds representing lignin monomers, as well as DHP-lignin and wood flour of controlled particle size were used to assess iron reduction at the pH of the natural wood cell wall. All compounds functioned as electron donors for ferric iron, with the lignin monomers demonstrating capacity for non-stochiometric reduction of iron with multiple moles of ferric ion reduced per mole of l...
Y Tamarua, M Yoshidaa, L D Eltisb, B Goodell


Exploring the use of X-ray micro CT as a tool for the monitoring of moisture production and mass loss during lab-based fungal degradation testing
2019 - IRG/WP 19-20654
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, J Van den Bulcke, A De Muynck, J M Baetens, B De Baets, L Van Hoorebeke, J Van Acker


The use of bicine and tricine as possible Maillard reagents in a combined thermal/chemical modification of beech
2019 - IRG/WP 19-40852
The effects of thermal modification have been well established, particularly in terms of reductions in mechanical performance. In recent years, there has been an increase in studies related to the Maillard reaction. More commonly associated with food chemistry, it involves the reaction of amines and reducing sugars during cooking procedures. This paper has attempted to combine the use of amines an...
D Jones, C-M Popescu, D Krzisnik, M Hocevar, M Humar, M-C Popescu


Development of beech wood thermo-chemical modification treatments based on different vinylic derivatives of glycerol and polyglycerol
2019 - IRG/WP 19-40855
In this study, a combination between chemical and thermal wood modification has been investigated. Seven types of a low concentration of 10% aqueous additive solution of vinylicglycerol [glycerol-maleic anhydride (Gly-MA), glycidyl methacrylate (GM), and Glycerol methacrylate-maleic anhydride (GM/MA(2eq))], vinylicpolyglycerol [polyglycerol-maleic anhydride (PG-MA), polyglycerol methacrylate (PGM...
M Mubarok, S Dumarcay, H Militz, K Candelier, M-F Thevenon, P Gerardin


An overview of recent studies involving the thermal modification of hardwood species
2019 - IRG/WP 19-40869
This paper outlines recent activities related to the thermal modification of hardwood species, and particularly to tropical hardwood species. Timber demand is ever increasing, but this is being limited by the necessity to protect virgin forest stands. As such, the majority of supply of popular species is being met from juvenile short rotation stands. The limited age from these stands often plays a...
D Jones, M Gaff, F Kacik


Charring of Norway spruce wood surface – an alternative surface modification technique?
2019 - IRG/WP 19-40870
Charring is an old wood surface treatment technique, mainly performed on wooden façade elements with the aesthetical aims, but also with the purpose of protection. This flame treatment method can be grouped into heat treatment processes. Below the top charred layer of damaged wood there is a layer which is during flame treatment exposed to high temperatures in anoxic or semi-anoxic conditions. Th...
M Petric, M Pavlic, J Zigon


Improvement of wood decay and termite durability resulting from combined treatments based on borax/phenol-formaldehyde impregnation followed by thermal modification
2019 - IRG/WP 19-40871
This study determined the factors influencing the boron content after leaching of pine blocks impregnated with aqueous solution of phenol-formaldehyde (PF) resin with or without borax and subjected to heat treatment by response surface methodology. An experimental design permits to analyze the effects of heat treatment temperature (150, 185 and 220°C), curing time (5, 12, 5 and 20 hours), resin c...
S Salman, M-F Thevenon, A Petrissans, S Dumarcay, P Gerardin


Thermal performance and fire safety properties of traditional circumferential log-cabin walls
2019 - IRG/WP 19-40872
The paper describes the experiment of fire resistance of a circumferential log-cabin wall fragment using various structural modification of the gap between two log members. The influence of the gap structural modification on the criterion of fire resistance E (envelop integrity) and I (insulation) is evaluated. The evaluating criteria are represented by the development of temperatures measured in ...
S Jochim, L Makovicka Osvaldova, M Zachar, Z Danihelova


Protecting wood exterior infrastructures above ground in Spain. The importance of protection by design in the performance
2019 - IRG/WP 19-40874
Across Spain is very common to find wood exterior infrastructures build mainly in sawn and glue-laminated wood. Most of these exterior wood infrastructures use softwood wood species such as: fir, spruce, larch and pine. In Spain exterior wood infrastructures, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wood infrastructures in o...
D Lorenzo, M Touza, J Fernandez-Golfín, A Lozano, J Benito, M T Troya, L Robertson


Novel approaches for improvement of dimensional, photo- and thermal stability of wood through liquefied wood polyols impregnation
2019 - IRG/WP 19-40884
The major problems encountered in both indoor and outdoor utilization of wood are due photo instability and dimensional instability. The modification of Melia dubia wood for ultraviolet resistance and dimensional stability with liquefied wood has been carried out through impregnation method under solvent free conditions. The level of impregnation in modified wood was estimated by weight perc...
A Kumar, A John, T S Mehra


Durability and climate change - implications for wood building structures
2019 - IRG/WP 19-50361
Sustainable building practices are rooted in the need for reliable information on the long-term performance of building materials; specifically, the expected service-life of building materials, components, and assemblies. This need is ever more evident given the anticipated effects of climate change on the built environment and the many governmental initiatives world-wide focused on ensuring that ...
M Lacasse


Different levels of acetylation lead to groupwise upregulation of non-enzymatic wood degradation genes of Rhodonia placenta during initial brown-rot decay
2020 - IRG/WP 20-10958
Rhodonia placenta, often used as a model fungus to represent brown rot fungi, uses a two-stepped degradation mechanism to degrade wood. Regarding the overcoming of wood protection systems the initial degradation phase seems to be the crucial point. A new laboratory test enables the separation of the non-enzymatic oxidative and the enzymatic degradation phases, which has previously been proven chal...
M Kölle, R Ringman, A Pilgård


FTIR analysis of wood blocks decayed by brown-rot fungi
2020 - IRG/WP 20-10959
Calibration curves of the relative lignin contents in Cryptomeria japonica decayed by brown-rot fungi were developed with Infrared Spectroscopy and Klason technique. First, wood decay test was conducted using brown-rot fungi (Fomitopsis palusris, F. pinicola, Wolfiporia cocos, Gloeophyllum trabeum, and Neolentinus suffrutescens) and white-rot fungus (Trametes versicolor) was used as a comparison. ...
R Kondo, Y Horikawa, R Kose, M Yoshida


Moisture and temperature conditions in an old, highly moisture-loaded timber building in the Røros municipality, Norway
2020 - IRG/WP 20-10966
A 150 years old log building near Røros, Norway, has been in active use as a cowshed since its erection. The animals are kept inside the cowshed all winter and this causes a situation of a high moisture load on the wooden floor, wooden walls and ceiling. Logging of temperature and humidity over one year shows that there are favourable levels of moisture in the wood and air for development of moul...
M Sand Austigard, J Mattsson


Profiling fungal degradation of Scots pine sapwood by short wave infrared hyperspectral image analysis
2020 - IRG/WP 20-20667
Hyperspectral image analysis of Scots pine sapwood wood affected by decay fungi has been carried out as part of a Ph.D. thesis within the project Remote Inspection of Wooden Utility Poles (RIWUP). In a lab experiment, Petri-dishes with Scots pine sapwood samples on malt agar medium were infected with two types of decay fungi, a brown rot and a white rot. The wood samples were scanned with a HySpe...
A Jochemsen, G Alfredsen, I Burud


Studying amount, location and state of water in modified wood at moisture levels relevant for fungal degradation
2020 - IRG/WP 20-40889
Water is an essential parameter for fungal degradation of wood, but degradation primarily occurs at high moisture levels at water potential in the range of -4 to -0.1 MPa, which corresponds to 97-99.9% relative humidity. At these moisture levels, water is present in the wood structure both in and outside of cell walls. The majority of previous studies on the interaction between wood and water for ...
M Fredriksson, E Engelund Thybring, Ramunas Digaitis


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Macro biological degradation of wood treated with sorbitol and citric acid – first results from marine environment and termite exposure
2020 - IRG/WP 20-40901
Most European wood species are rapidly and severely degraded in termite-infested areas and the marine environment. There is a need for new solutions, especially in the marine environment, since we lack wood preservatives approved for marine applications in Europe. Several wood modification systems show high resistance against both marine borers and subterranean termites. However, the existing comm...
A Treu, L Nunes, E Larnøy


PlasmaSolution – Curing of coating formulations using non-thermal plasmas
2020 - IRG/WP 20-40904
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, M Petrič


Thermal spray coatings to protect wood from termites
2020 - IRG/WP 20-40905
Protecting buildings and construction materials against subterranean termites in Europe relies on combined physical and chemical approaches. Buildings can be protected by physical or physico-chemical barriers such as gravel aggregates, steel mesh or plastic films impregnated with insecticides. Wood and wood-based materials are traditionally protected by insecticides applied on the surface or deepl...
L Podgorski, H Myalska, A Dinoirjean, M Kutnik


NewSiest-Enhancement of UV stability of thermally modified wood through envelope impregnation with nanobased stabilisers
2020 - IRG/WP 20-40909
Thermal modification is a process which improves the properties of wood, resulting in a material that can be disposed at the end of the product life cycle without presenting an environmental hazard. Thermally modified wood retains as a natural product and the grain, original colour variances and characteristics of wood are still present. However, exposure to daylight causes brightening or greying ...
K Srinivasa, M Petrič


Enhancing the durability of low durability Eucalyptus plantation species: a review of strategies
2020 - IRG/WP 20-40910
Eucalyptus species native to Australia have shown excellent growth rates, good physical properties and resistance to diseases. As a result, they are widely planted globally for a variety of uses. One negative aspect of many of these faster growing species is that they have a high percentage of low durability heartwood that resists preservative treatment. In Australia, large plantations of these sp...
K C Wood, J J Morrell, W Leggate