Applications of immunological methods to the analysis and detection of Lentinus lepideus Fr
1989 - IRG/WP 1422
Polyclonal antisera have been raised against the brown rot fungus Lentinus lepideus, a major cause of rot induced pole failure in the UK. Specificity studies have indicated that the antisera cross-react with a number of basidiomycetes but to much lesser extent with other fungi. The antigenicity of Lentinus lepideus and hence its molecular composition shows some alteration with culture age and chan...
H Glancy, A Bruce, D Button, J W Palfreyman, B King


Further thoughts on standard principles of testing termiticides and/or wood preservatives
1992 - IRG/WP 92-1530
At the last annual meeting in Kyoto, Japan, there was a special session devoted to the standard principles of testing termiticides. There was definitely a perceived need by researchers and industry for some guidelines that spell out basic procedures required for any methodology in testing termiticidal formulations anywhere in the world. In the testing of new potential active ingredients, considera...
J R J French


A new technique for testing decay resistance of framing lumber
2002 - IRG/WP 02-20247
Model house frame units (two studs, top and bottom plates and a central “dwang”) were constructed using short (500-600 mm) lengths of framing timber. Constructed frames were impregnated with water using a mild pressure schedule to raise the initial moisture content to 35-40 % mc. The back face of each unit was then covered with black polyethylene. Two locations at the stud/dwang and stud/botto...
M E Hedley, D Page, B E Patterson


Contradiction between uptake of preservative in practical situation and laboratory testing
1992 - IRG/WP 92-2392
By brush treatment water- and solvent-based products were applied on boards of Scots pine and Norway spruce to achieve an uptake of 100 and 200 g/ml. In addition the scope of work to achieve the required uptake of preservative was determined under practical conditions for both product groups. EN 113 (RAL-GZ 830) tests were carried out to test the biological efficacy of products. After 18 months ex...
R Gründlinger, O Janotta, M Melzer


The effect of different concentrations of polesaver rods on the survival of selected decay fungi in liquid culture
1998 - IRG/WP 98-30166
An in-vitro method was developed to determine the effect of solutions of Polesaver Rods on the survival of selected decay fungi. Polesaver Rods are a diffusing preservative treatment containing fluorine and boron designed for the internal remedial treatment of power poles. Two white-rot fungi, Perenniporia tephropora and Trametes versicolor, and two brown-rot fungi, Polyporus verecundus and Gloeo...
M A Powell, T Deldot, C McEvoy


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Glulaminated poles - Progress report after 7 years' testing
1987 - IRG/WP 3444
In 1979 a number of glulaminated poles with various preservative treatments were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and under a power line just south of the Arctic circle in order to study their resistance against biological degradation. The tests have shown that the comparatively best performance will be obtained if each lamination is treated wi...
J Jermer, Ö Bergman


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


Laboratory induction of pupation and emergence in Anobium punctatum (Deg) (Col Anobiidae)
1973 - IRG/WP 219
The reluctance of Anobium punctatum to pupate and emerge outside its normal summer emergence period has led to attempts to induce pupation by artificial manipulation of the temperature conditions at which larvae are held. Infested hazel (Corylus avellana) twigs were subjected to temperature schedules which simulated some aspects of a spring climate. It was found that 40 days of a diurnal temperatu...
R W Berry


A novel device for detecting internal defects in wooden poles
1989 - IRG/WP 2329
The diagnosis of internal defects caused by termites and decay in hardwood transmission poles has been investigated using a novel Automatic Feed Drill (AFD) pole testing device. Internal defects were recognised by changes in drill feed-rate as the automatic air-driven drill traversed its 100 mm working stroke. The instrument is portable, simple to operate and recognises defects instantaneously. Te...
R A Eaton, R S Johnstone


Field testing of alkylammonium wood preservatives
1983 - IRG/WP 3248
The field test performance of five alkylammonium wood preservatives is described. The relative effectiveness of three unmodified formulations was determined by calculation of a Performance Index. Of the three, didecyldimethylammonium chloride was found to be superior to octyldecyldimethylammonium chloride, and both were more effective than alkyltrimethylammonium chloride. However, none were consid...
J N R Ruddick


Evaluation of the pulsed-current resistance meter (Shigometer®) for determination of the internal condition of utility poles
1979 - IRG/WP 2128
A number of Telecom poles, which had been removed from service to be replaced by a radio link, were inspected using an electrical resistance meter (Shigometer®). These poles were creosoted, non-durable Victorian species in service in New South Wales. Six of these poles, chosen to represent various internal conditions typical of the range of the population tested, are discussed here. Data, from tr...
J D Thornton, W G Seaman, M McKiterick


The natural durability of wood in different use classes
2003 - IRG/WP 03-10457
The natural durability of important European wood species has been tested on 3970 specimen in field trials. The wood was exposed at five test fields in Germany with different climates at each site in European hazard class 4 and 3 (with and without soil contact). Within EHC 3 it was distinguished between tree different expositions (end grain sheltered, unsheltered and with water trap). The test is...
U Augusta, A O Rapp


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


Blue Stain Testing of Alkyd and Acrylic Stains
2003 - IRG/WP 03-20273
Resistance against blue stain of semi-transparent alkyd and acrylic stains was tested by both EN 152 and the so-called reverse exposure test methods. Comparison of the results, obtained by both methods was the most important aim of this study. As expected, performance of the water-borne acrylic paint was lower compared to protective effectiveness of the alkyd stain. This difference was even more p...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


On the effectiveness of fumigants against wood-destroying insects and fungi in wooden cultural property
1993 - IRG/WP 93-10030
Based on a survey of the history of the use of fumigants the actual agents are mentioned in relation to their biogenic effect on wood-destroying insects and fungi as well as their corrosive behavior on cultural property. Furthermore the conditions for the use of reactive fumigants in buildings are discussed. Trials to control wood-destroying insects and fungi by nitrogen and bromomethane are the m...
W Unger, A Unger


Unsuitability of the limiting dose as a criterion for assessing the toxicity of preservatives to wood-destroying fungi
1974 - IRG/WP 243
In the majority of methods for investigating preservatives for wood-destroying fungi their toxicity is assessed by determining what is called the "limiting dose". This normally denotes a range of preservative solution concentrations or retentions of dry preservative in the timber, the lower value serving to indicate the amount of preservative at which is observed the expected effect, e.g. the grow...
D A Belenkov


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Preservation of robinia wood (Robinia pseudoacacia L.) stakes by vintners
1982 - IRG/WP 3194
This work discusses decay resistance of robinia wood to fungi Trametes versicolor (L.ex Fr.) Pil. and Coniophora puteana (Schum. ex Fr.) Karst., and also the possibility of influencing its resistance by means of chemical protection. The results showed that natural resistance of robinia wood to these two different agents of wood decay is not the same. It is much less resistant to the fungus Conioph...
R Benko


The natural durability story
1997 - IRG/WP 97-20119
Wood species with superior natural durability were in use since the beginning of timber utilisation. Their importance decreased with increasing industrial timber impregnation. In recent time, however, they gained worldwide new interest due to environmental problems involved with treated timber. In Europe a special Standard (EN 350) has been published and a multinational research project on testing...
H Willeitner, R-D Peek


A technique for assessing the preventive efficacy against decay fungi of preservative treatments applied to wood
1988 - IRG/WP 2309
A method is described in which test blocks with envelope preservative treatments can be challenged by selected test fungi previously established on an untreated feeder block. The progress of the test fungus through the treated zone is monitored using novel baits or sensors inserted in holes drilled into blocks to within predetermined distances of the face being challenged. Preliminary results show...
J K Carey, A F Bravery


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 1: Laboratory screening tests using a filter paper technique
1977 - IRG/WP 290
Thirty-one miscellaneous formulations have been screened using a filter paper assay technique, for their efficacy in controlling the growth of Chaetomium globosum, Cephalosporium acremonium, and a mixed inoculum of finely ground soft-rotted wood obtained from preservative treated transmission poles. The formulations consisted of various organic compounds and inorganic preparations made from differ...
H Greaves


An Australian test of wood preservatives. Part 1: Preservatives, principles and practices
1978 - IRG/WP 2123
Between November, 1963, and July, 1964, a graveyard test of some 6000 preservative-treated stakes was installed at 8 sites equally distributed between Papua New Guinea in the tropics, through Queensland and New South Wales to Victoria. More than 40 different preservatives and preservative mixtures, mostly at several different levels of retention, were used to impregnate sawn specimens of Pinus rad...