Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III


Termite resistance of DMDHEU-treated wood
2008 - IRG/WP 08-40401
Chemical wood modification with dimethyloldihydroxy-ethyleneurea (DMDHEU) or its derivatives are applicable to both solid lumber and wood-based composites. Advantages of DMDHEU-based modification are an increase of dimensional stability and high durability against white, brown and soft rot fungi. At higher chemical loadings, the hardness of the wood is considerably increased. Due to the durabil...
H Militz, S Schaffert, B C Peters, C J Fitzgerald


Cantilever bending test of furfurylated poles
2008 - IRG/WP 08-40424
Ten, 8 m long poles of Scots pine (Pinus sylvestris) were treated with furfuryl alcohol to a WPG of approximately 40 %. A bending test was performed according to the principles in the draft European standard for wooden poles, prEN 14229 - Structural timber - Wood Poles for overhead lines. The bending strength and stiffness (MOE) for the poles tested were compared to an earlier study by the Swedish Wood Preservation Committee. In the latter study untreated, CCA-treated, ammoniacal Cu-PCP treated and creosoted poles were tested in bending. These types of poles were considered not to differ in strength and stiffness. The results of the furfurylated poles fit well with the results from the previous study. The bending strength and MOE values obtained are compared to the upper and lower 95-percentile values of the results from the previous study and all poles treated with furfuryl alcohol fit within this interval.Thus, this study indicates that a treatment with furfuryl alcohol does not result in a decrease of strength or stiffness. Further testing with a larger population of poles is necessary in order to get a statistically reliable result. In addition to further demonstration of the durability, the treatment process must be optimised to ensure full sapwood penetration and measures have to be taken to avoid the serious cracking observed in this trial before furfurylation can be considered for treatment of Pinus sylvestris poles.
R Ziethén, J Jermer, A Clang


Emission Rates of Active Substances from Preserved Wood in Use Class 3
2008 - IRG/WP 08-50256
The evaluation of an active substance or a biocidal product under the Biocidal Products Directive (BPD) requires that an environmental risk assessment is carried out. The risk assessment for wood preservatives includes scenarios for preserved wood (e.g. cladding on a house), in which the predicted environmental concentration (PEC) in soil is calculated, using an emission rate for the active subs...
E F Baines


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


To decay or not to decay: An accelerated field test of the validity of the Scheffer index
2008 - IRG/WP 08-20392
The Scheffer Index was introduced in 1971 to predict the relative decay hazard of untreated wood exposed above-ground. Precipitation and temperature parameters are used in the calculation. A higher Scheffer Index value implies a greater risk of decay. An accelerated 18-month study using seven field sites with Scheffer Indices ranging from 35 to 400 and two wood types (Populus tremuloides and Pi...
G M Larkin, P E Laks


Above Ground Field Testing – Influence of test method and location on the relative performance of various preservative systems
2008 - IRG/WP 08-20393
Standardized above ground tests such as the lap-joint or test deck methods can be very slow in producing useful information on the relative performance of wood preservative systems. It often requires many years for decay to develop in wood treated to sub-optimal concentrations of standardized preservatives, making relative comparisons of performance between new systems and established preservativ...
A Zahora


Effectiveness of MOQ® OX 50 (CCB-Oxide) wood preservative – Part 2: Field tests
2008 - IRG/WP 08-30483
MOQ® OX 50 is a chromated copper borate preservative known around the world as CCB. In Brazil, this product is the only CCB-oxide type preservative with fungicide and insecticide properties registered at the Brazilian Institute for the Environment and Renewable Resources (IBAMA) that complies with the requirements of the Brazilian and European markets for preserved wood. For over five decades, s...
A Gandolfi Jr, C Salvela, D R Macedo, J M Vidal


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Laboratory and field exposures of FRT plywood: Part 1. Physical test data
2008 - IRG/WP 08-40426
Our understanding of the laboratory induced degradation with fire retardant systems is currently limited since we are unable to correlate laboratory steady-state experiments with actual in-service field degradation. Current model studies have generally been limited to isothermal rate studies with selected model FR chemicals. Other factors also play a major role in the degradation of FR-treated woo...
H M Barnes, J E Winandy, C R McIntyre


Termite resistance of pure and mixed heartwood-sapwood Cypress (Cupressus sempervirens L.) plywoods
2009 - IRG/WP 09-10693
The main objective of this research was to evaluate the ability of different plywoods made of durable heartwood and/or non-durable sapwood to resist termite damage. The well-known durable cypress (Cupressus sempervirens) was chosen for this study. The natural durability of cypress solid wood, divided into sapwood and heartwood, as well as the durability of 17 different laboratory manufactured plyw...
F Faraji, M-F Thévenon, B Thibaut


Prevelence of termite infestation and wood preferences in Pakistan
2009 - IRG/WP 09-10695
In order to know about prevalence of termite infestation in Pakistan, A study was carried out to know the intensity of infestation of different species of termites to different types of woods used in buildings as well as in the forests. Heterotermes indicola was the most notorious species of termite present in buildings, grounds throughout the year while Odontotermes obesus was most common in for...
F Manzoor, S Asma Malik


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Natural Durability Variations of Malaysian Timbers from Sarawak after 26 Years Exposure by Stake Test
2009 - IRG/WP 09-10704
An extensive graveyard stake test site was established in 1977 in Sibu, Sarawak, Malaysia, to evaluate the in-ground durability of 132 Sarawak wood species, mainly hardwoods. Test samples were planted at 100 x 50 cm spacing. Authenticated wood specimens from 3 trees of each of 132 species were processed into 20 replicated outer heartwood (or else undifferentiated heartwood) stakes of 19 x 19 x 457...
A H H Wong, Ling Wang Choon


What Can Fecal Pellets Tell Us About Cryptic Drywood Termites (Isoptera: Kalotermitidae)?
2009 - IRG/WP 09-20407
Drywood termites (Isoptera: Kalotermitidae) are serious economic pests of both plants and seasoned wood (furniture, wood frame structures). Currently, five species of kalotermitids are known to occur in the Hawaiian Islands: Neotermes connexus, Incisitermes immigrans, Incisitermes minor, Cryptotermes brevis, and Cryptotermes cynocephalis. These termites are difficult to detect and observe due to ...
J K Grace


Ensure Durable Wood-Frame Construction under the Climate and Biological Hazards in Shanghai
2009 - IRG/WP 09-20413
This paper provides technical background for developing durability-related provisions for the Shanghai wood-frame construction code. It summarizes the related climate, decay and termite hazards in this area as well as traditional durability solutions used for wood and wood hybrid constructions in China. The overall durability principles or philosophy used throughout this durability chapter are to ...
Jieying Wang, Chun Ni, Jiahua Zhang


Review of candidate graded particle barrier testing methods in Australian Standard (AS 3660.3 – 2000): Assessment criteria for termite management systems
2009 - IRG/WP 09-20417
The Australian Standard (AS. 3660.3 – 2000) for assessment of candidate graded particle termite barriers is reviewed and suggestions for amendments are made. Areas requiring amending in light of current biological knowledge involve the inclusion of proprietary or patented systems rather than generic types; selection of test termites in the genus Coptotermes; duration of test periods; and inadequ...
J R J French, B M Ahmed (Shiday), B L Schafer


Effectiveness of sol-gel treatments coupled with copper and boron against subterranean termites
2009 - IRG/WP 09-30493
Wood modification by sol-gel treatments shows many positive features, like antimicrobial properties. Wood was also successfully modified with alkoxysilanes enhancing its resistance against soil micro-organisms. Silver, copper, zinc compounds, boric acid or organic biocides such as alkylammonium compounds may be added to the sol-gel to enhance its biocidal properties. Nevertheless, if some of these...
E Feci, L Nunes, S Palanti, S Duarte, G Predieri, F Vignali


Leaching performance, decay and termite resistance of wood treated with boron compounds incorporated with phenol-formaldehyde resin
2009 - IRG/WP 09-30503
A resol-type phenol-formaldehyde (PF) resin was synthesized and designed to penetrate wood incorporated with boron compounds in order to immobilize boron in wood. The leaching performance, decay and termite resistance of treated wood was investigated. Three kinds of boron compounds, that is, boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT), were selected to mix with PF and tw...
Liping Yu, Jinzhen Cao


Resistance to decay fungi of ammonium borate oleate treated wood
2009 - IRG/WP 09-30505
Ammonium borate oleate molecule (ABO) produced from reaction between boric acid, ammonia and oleic acid was tested as wood preservative treatment against brown and white rot fungi according to European standards. This compound was prepared according to a previous study which has proved existence of synthesis reaction and effectiveness against termites (Lyon et al. 2007b). Four solutions of ABO in ...
F Lyon, M-F Thevenon, A Pizzi, J Gril


Laboratory test of some formulations against stain and mould fungi isolated from bamboo wood
2009 - IRG/WP 09-30508
To screen the effective anti-mould formulations, fungicides such as carbendazim, tebuconazole, fludioxonil, difenoconazole, prochloraz, benomyl and 8-hydroxy-quinoline copper (copper oxine) were selected to conduct the laboratory test of fungicidal activity by method of inhibition zone against Botryodiplodia theobromae Pat., Fusarium sp., Alternaria tenuis Nees., Penicillium purpurogenum Stoll, Tr...
Xingxia Ma, Airui Sun, Mingliang Jiang, Daochun Qin


Environmental Emission of Wood Preservatives: Interpretation of Data Relevant to BPD Risk Assessments
2009 - IRG/WP 09-50259
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. The leaching rates can be derived from laboratory testing and from field testing. The relationship between laboratory and f...
D G Cantrell


Modification of Wood by a Water-Repellent Compound Used in the Textile Industry: Boron Release and Termite Resistance
2009 - IRG/WP 09-40447
In the study, wood specimens were treated with disodium octoborate tetrahydrate (DOT) and a commercial water and oil repellent compound, FORGUARD M®, a weak cationic emulsion containing dipropylene glycol monomethylether, water and solids in its formulation and used in the textile industry. There were two different processes for preservative treatments: double and single treatments. The leaching ...
S N Kartal, E Terzi, B Erilkun, Y Imamura


Termite resistance of some modified wood species
2009 - IRG/WP 09-40449
During the last few decades, researchers worldwide have investigated and developed new treatment techniques to improve intrinsic wood properties. Some of these techniques were introduced to the market recently and are gaining in importance.. Various wood properties of these new materials have been studied intensively. These include physical-mechanical properties (dimensional stability, moisture ...
H Militz, B C Peters, C J Fitzgerald


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...