IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1378 documents. Displaying 25 entries per page.


In-ground field test of scots pine (Pinus sylvestris L.) sapwood and heartwood
2004 - IRG/WP 04-30336
Scots pine (Pinus sylvestris L.) sapwood and heartwood stakes treated with CCA-C and creosote were tested for one- year in a field plot in Bartın region in Turkey. Scots pine heartwood stakes had lower preservative retention than sapwood stakes. Bending strength of the stakes was decreased after impregnation and one-year field test. While the bending strength of untreated sapwood was 93....
H Sivrikaya, H Hafizoglu


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


Performance trials of treated hardwood fences
2002 - IRG/WP 02-30281
This paper examines the performance of the traditional hardwood paling fence used in Australia, after preservative treatment. Unseasoned rails, palings and plinths of the low natural durability species Eucalyptus regnans (mountain ash) and E. obliqua (messmate) were treated with PEC (pigment emulsified creosote) or PROCCA (an oil emulsion of CCA). Treated posts of these species were also compared ...
L J Cookson D Scown, B Iskra


Performance of borate-treated sill plates (dodai) in a protected, above-ground field test in Japan
2002 - IRG/WP 02-30278
This document is supplemental to the previous IRG document (IRG/WP 2000-30239). An experiment to simulate the dodai (sill plate) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. DOT...
K Tsunoda, A Adachi, A Byrne, P I Morris, J K Grace


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


New conception for shortering the duration of fungitoxic test of wood preservatives. Part 2: Computer-assisted miniaturisation of wood specimens
1994 - IRG/WP 94-20052
The mass loss of wood used as a criterion in the standarised agar-block method of evaluation of toxic value of preservatives depends upon the relationship between volume of specimens, their outspread planes and ratio of areas of particular anatomic sections. Upon the computer-assisted mathematical basis the dimensions of miniaturized specimens which make 1/2, 1/4, and 1/8 part of standarized ones ...
J Wazny, K J Krajewski


Evaluating the potential of amine chemicals for use as wood protecting agents. Part 1: Investigation of cation components of quaternary ammonium compounds
1994 - IRG/WP 94-30049
Quaternary ammonium compounds (quats) have shown a great potential as more environmentally acceptable wood preservatives. In order to identify chemicals possessing the wood protecting potential, an evaluation was carried out of a range of commercially available 'quats', using a modified soil block test. Ponderosa pine sapwood blocks were treated with selected 'quat&a...
Hang Tang, J N R Ruddick


Decay resistance of densified ammonia-plasticized stems of oil palm (Elaeis guineensis)
1991 - IRG/WP 3673
When wafers of oil palm stems (Elaeis guineensis) were plasticized with 28% aqueous ammonia and immediately compressed mechanically, the treated material, gained 73% in basic density (average basic density, 0.695 g/cm³), and was highly resistant to decay by wood rot basidiomycetes. Compared with the control specimens (density, 0.403 g/cm³), resistance to decay of the densified specimens by Corio...
A H H Wong, M P Koh


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


Durability of surface coating systems. Mycologg - an accelerated mycological test.
2004 - IRG/WP 04-20301
Field testing and natural aging/degradation of test sample, e.g. coated wooden surfaces is a slow process. Accelerated tests focus on mechanical properties, water uptake or sometimes stain fungi. Artificially weathered coated panels are not easily compared with naturally aged panels, and show the importance of involving the biological component among the degrading facors. It is a need for acce...
L Ross Gobakken, J Mattsson, B Jacobsen, F G Evans


Distribution of the three symbiotic protozoa in Formosan subterranean termite, Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae)
1993 - IRG/WP 93-10010
Six colonies (three each from laboratory and field) of Formosan subterranean termite, Coptotermes formosanus Shiraki, were served for investigating the abundance and distribution of three symbiotic protozoa in the hindgut of workers. The total protozoan number amounted to 6,000-10,000 per a worker, and the order of the abundance of the three protozoa and the proportional distribution of each speci...
T Yoshimura, K Tsunoda, M Takahashi


Comparison of methods for monitoring CCA fixation
1994 - IRG/WP 94-40023
The CCA fixation status in the outer 12.5 mm of pole sections of southern pine (Pinus sp.), red pine (Pinus resinosa) and lodgepole pine (Pinus contorta var. latifolia) were followed during fixation at 21°C under non-drying conditions by the following procedures: - Qualitative CrVI indication by the chromotropic acid spot test. - Quantitative CrVI in the expressate by the diphenylcarbazide method...
P A Cooper, Y T Ung, G Zanjani


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Tolerance of Wood Decay Fungi to Commercial Copper Based Wood Preservatives
2002 - IRG/WP 02-30291
Due to the use of copper based preservatives like CCB or CCA for more than a century, copper tolerant fungi have appeared in some European countries in recent times. It is therefore important to find out whether this phenomenon is specific for only classical copper ingredients, or generally for all copper based formulation. Thus, we tested the tolerance of three commercial copper based pres...
F Pohleven, M Humar, S A Amartey, J Benedik


Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


Anti-feedant activity of stilbenic components from bark of Picea glehnii against a subterranean termite, Reticulitermes speratus
2002 - IRG/WP 02-10447
Stilbenic components, one of polyphenolic groups, widely distributed in plant bodies have been known as anti-microbial agents, but not known whether to have anti-termite activities. A stilbene glucoside, isorhapontin, from the bark of Picea glehnii was examined on the anti-feedant activity against a subterranean Reticulitermes speratus. Isorhapontigenin, the aglycone of isorhapontin, induced from ...
S Shibutani, M Samejima, S Doi


On the occurrence of Phialophora species in preservative treated wood in ground contact
1977 - IRG/WP 163
Phialophora is a fairly large genus comprising about thirty described species. They are widespread in very diverse environments, such as soil, sea water, wood and wood pulps. Some species are known as parasites on plants and animals, including man. Phialophora species were early known for their ability to produce blue stain in timber. Later it was discovered that several species were able to produ...
T Nilsson, B Henningsson


Acceleration of boric acid uptake into the subterranean termite, Coptotermes formosanus Shiraki using steamed larch wood
2000 - IRG/WP 00-10353
Laboratory tests were done to measure the efficacy of addition of steamed larch (Larix leptolepis (Sieb. et Zucc.) Gord.) heartwood extracts for the uptake of boric acid against the termite, Coptotermes formosanus Shiraki. Paper discs were treated with the water-soluble fraction obtained from hot-water extracts of steamed larch wood (S-Water) with or without 0.01-2.0% boric acid, followed by expos...
W Ohmura, S Doi, S Ohara


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 18. Report of seventh inspection (72 months) in Australia
1984 - IRG/WP 4108
This report includes the results for the 72 month inspection of the IRG/COIPM International Marine Test installed in Sydney Harbour. Although, overall, attack by teredinid and limnorid borers have been most commonly encountered in test specimens at this site, slight attack, mainly by sphaeromatids, has recently been initiated on some hitherto unattacked treated Alstonia scholaris and Pinus sylvest...
L J Cookson, J E Barnacle


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


A shower test protocol for measuring antisapstain wash-off from small individual log billets
1996 - IRG/WP 96-50069
According to New Zealand Timber Industry Federation statistics New Zealand exported 4,835,000 m³ of logs in 1994 and it is estimated that c. 20% were anti-sapstain treated. Loss of preservative from logs as a result of rain impact after application is of considerable concern both with respect to potential loss of efficacy and environmental contamination. Whilst Environment Canada have a proposed ...
A J Pendlebury, H Pearson


Effect of test site, preservative and wood species on decay type Glenbervie pastoral and radiata pine forest sites
2000 - IRG/WP 00-30248
Pinus radiata stakes were treated with 0.8, 1.2, 1.8, 2.7 and 4.1 kg/m3 of CCA and Fagus sylvatica with 2.7, 4.1 and 6.1 kg/m3 of CCA. Both wood species were also treated with equivalent retentions of a copper plus triazole preservative (CT) (0.89, 1.3, 2 and 3 kg/m3 of copper for pine & 2.5 and 4 for beech) and chlorothalonil plus chlorpyriphos in oil (CC) (1.4, 2.1, 3.2 and 4.8 kg/m3 of chlo...
R N Wakeling


Proposing innovative technologies in the control of dry-wood insects
1985 - IRG/WP 1262
This paper discusses the social-economic problems involved in the biological evaluation of dry-wood insects with particular reference to Nigeria. It also discusses prospects of applying non-conventional methods of control against such insects, integrating these with the conventional preservatives as a control strategy. This discussion follows attempts made to identify the major dry-wood insects in...
M O Akanbi


New boron-based biocides for the protection of wood
2002 - IRG/WP 02-30283
Boric acid and other simple inorganic oxides of boron are amongst the oldest wood preservatives currently in use. Their relatively low toxicity and broad-spectrum activity are just some of their desirable characteristics. The primary disadvantage associated with conventional boron-based preservatives is their lack of permanence in exposed applications. A collaborative project between CSIRO and the...
D G Humphrey, P J Duggan, E M Tyndall, J M Carr, L J Cookson


Previous Page | Next Page