Preliminary laboratory and field evaluation on the performance of Rubbermite as a graded physical barrier against subterranean termite species in Australia
2012 - IRG/WP 12-10766
This paper describes the performance of Rubbermite as a potential graded particle barrier against two subterranean termite species of Coptotermes in laboratory and field test. The results of these bioassays suggest that Rubbermite is a viable control option against Coptotermes species in Australia, particularly against Coptotermes acinaciformis (Froggatt) and Coptotermes lacteus (Froggatt). Rubber...
B M Ahmed (Shiday), J R J French


Laboratory and Field evaluation on Natural Resistance and Feeding Preference of Different Wood Species to Subterranean Termites (Isoptera: Rhinotermitidae, Termitidae) in Pakistan
2012 - IRG/WP 12-10769
The resistance of twenty four different woods to attack and damage by subterranean termite species Heterotermes indicola (Wasmann) and Coptotermes heimi (Wasmann) was evaluated by choice and no choic in laboratory and field trials. Mean wood mass loss was calculated for both laboratory and field trials results using Analysis of Variance (ANOVA). Mean percentage termite mortality was calculated fo...
S A Malik; F Manzoor, B M Ahmed (Shiday)


The importance of proper taxonomic identification, a case study with Reticulitermes spp. from USA
2012 - IRG/WP 12-10774
Taxonomy has been evolving with recent advancement in molecular and internet technologies. The importance of a stable taxonomic foundation is unquestionable as this science provides crucial information about evolutionary relationships and allows questions about the life history and ecology of organisms to be asked. We hope to highlight the issues and lessons we have learned from revising the taxon...
Su Yee Lim, B T Forschler


Decay factors in termite in-ground monitoring stations
2012 - IRG/WP 12-10775
Subterranean termites are serious pests of wood in service in much of the world. One of the most common techniques for monitoring and controlling termites is the use of in-ground monitoring stations which comprise a wood or other cellulosic material monitor (cellulosic matrix) and/or a termiticide bait held in a open plastic holder so facilitates examination and the termite access. Wood and other ...
S Duarte, A M Taylor, Jae-Woo Kim, J D Lloyd, M Duarte, L Nunes


Influence of soil moisture, Sarawak soil types and decay types on decay susceptibility of rubberwood and kelempayan
2012 - IRG/WP 12-10780
Wood and soils are important natural resources of the land, the former widely used as structural supports in contact with the latter. Many low durability wood species exposed to soil contact has reportedly high incidence of decay failures in poorly treated and untreated materials depending on soil types, properties and soil microbial virulence. This paper probes the relationship of the main soil t...
A H.H. Wong, P K.F. Chong, J Sabang


Coconut lumber for wood decks (Cocos nucifera L.): decay resistance against Basidiomycetes fungi
2012 - IRG/WP 12-10784
Since a couple of years, manufactured products of coconut wood for outdoor uses like wood decks have been proposed on the European market. These are presented as an alternative for traditional tropical timbers. In the past, coconut wood was neglected and burned for sanitary reasons and lack of interest at industrial scale. Plantation coconut trees at end of production of copra constitute a renewab...
B Jourez, C Verheyen, J Van Acker


Managing termite risks – An Australian perspective and a cautionary tale
2012 - IRG/WP 12-20482
The management of the risks of termite attack on new buildings in Australia falls to a range of agencies and is mostly achieved through controlling the process by which structures are certified as complying with the Building Code of Australia. Australian Standard AS3660 parts 1, 2 & 3 have historically been the core of this function but now the Building Codes Board's own certification scheme,...
D Ewart


A survey on Bio-Resistance of Oak and Elm in Caspian Sea Water
2012 - IRG/WP 12-20483
Logs of Oak (Quercus castanifolia) and Elm (Zelkova carpinifolia) have been cut to lumbers with dimensions of 300×100×30 mm. The oven dried samples have been impregnated with CCA (Chrome–Cupper-Arsenic). Treated and untreated (natural as a control) woods have been established for 3, 6, 9 and 12 months in Amirabad beach of Behshare under fishing environment. The observation results shows that i...
S M Kazemi


Durability of timber products – Part 2: Proposal for an IRGWP - Durability Database
2012 - IRG/WP 12-20497
A proposal for a web-based platform for scientific exchange of test data in the field of wood durability and wood protection has been made. The overall aim of the durability data base is to improve the usability of existing test data and to create an added value for durability research and service life prediction. The database allows for test results from standardized and non-standardized laborat...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis


Durability of timber products –Part 1: Inventory and evaluation of above ground data
2012 - IRG/WP12-20498
The material-inherent resistance of wood is one of the most important qualities influencing the durability of timber. Hence, it has also a major effect on the service life to be expected from a timber construction. In addition, design details and the respective climatic conditions determine durability and make it impossible to treat wood durability as an absolute value. Moreover, the reference mag...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis, P O Flæte, P Larsson Brelid


Mould resistance of bamboo timber treated with tebuconazole-loaded micells
2012 - IRG/WP 12-30586
In this paper both anti-mould test through inhibition zone and mould resistance test on bamboo samples were carried out evaluate mould resistant effect of tebuconazole (TBA) loaded micells. Results showed that TBA loaded micells prepared with a ratio of TBA to PEG113-b-PCL28 50:25 had the best mould resistance, followed by micells prepared with a ratio of TBA to PEG113-b-PCL28 50:50. PEG113-b-PCL2...
Sun Fangli, Chen Anliang, Bao Binfu, Zhou Yueying, Zhang Shaoyong, Zhang Xu


Tannin resin-boron associations: Leaching and biological resistance
2012 - IRG/WP 12-30587
The easy leaching of boron in wood preservation formulations has allowed to use this fungicide only for short term applications. The recently discovered adduct with flavonoids allows boron to resist longer periods of time within wood and consequently extend its life. Two different leaching treatments were compared and the fungal and termite decay was examined. The biological tests have shown extre...
G Tondi, S Wieland, N Lemenager, A Petutschnigg, A Pizzi, M-F Thevenon


Thiacloprid as a glueline termiticide for veneer based wood products
2012 - IRG/WP 12-30592
Thiacloprid is an insecticide commonly used in the agricultural industry. No evidence of its commercial use in wood has been discovered by the authors. Results are reported for veneer based wood products treated with thiacloprid via the glueline. Thiacloprid was tested against Coptotermes acinaciformis following the brick assembly technique as described in the Australasian Wood Preservation Com...
K Day, A Siraa, P Lobb


Biological performance of wood- and bamboo-polypropylene composites: Effects of particle content, particle size and Zn borate
2012 - IRG/WP 12-40577
Particle content and size of wood material in wood plastic composites (WPCs) can affect efficacy of WPCs against fungi and termites. This study evaluated fungal and termite resistance of WPCs manufactured by using two different levels of particle content (50 and 70%) and three different particle sizes (30, 60, and 100 mesh). In fungal resistance tests, Tyromyces palustris, a standardized test fung...
S N Kartal, S Aysal, E Terzi, T Yoshimura, K Tsunoda


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


The resistance of thermo and thermo-oil modified black poplar wood (Populus nigra L.) to Basidiomycetes fungi
2012 - IRG/WP 12-40585
The share of area taken by poplar tree species in Poland account for 2.0% of the area of state forests, 4.8% of national parks and for 2.3% in the privately-owned forests. It is shown and expected an increase in the share of poplar stands connected with plantation of fast growing trees. The poplar wood is not resistant to Basidiomycetes fungi, easy attacked by insects and in consequence is regarde...
A Fojutowski, A Kropacz, A Noskowiak


A survey of factors affecting decay resistance of wood modified with acetic anhydride
2012 - IRG/WP 12-40594
From the range of information published, acetylation appears well suited to provide adequate protection against biological attack for materials derived from typically non-durable wood species. Acetylated wood is now commercially available both in Europe and in the USA. But still there are a lot of unanswered questions related to fungal decay mechanisms in acetylated wood. The paper summarize exist...
G Alfredsen, P O Flæte, H Militz


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Classifying white rot decay resistance of some hardwoods from Sarawak and Peninsular Malaysia and correlations with their tropical in-ground durability
2012 - IRG/WP 12-10788
White rot wood decay under Malaysian (humid tropical) terrestrial conditions pose more serious threats to the in-ground service life of hardwoods than other common fungal decay types. A study is made on decay resistance variation for a total combined list of 30 Peninsular Malaysian and Sarawak timber species (plus 6 exotic reference temperate commercial woods for comparison) using the laboratory s...
A H H Wong, J M E Jem, Lai Jiew Kok


Hydrogels: a solution to reduce boron leachability without reduction of its biodisponibility to wood decaying fungi?
2012 - IRG/WP 12-30602
Products used today for wood protection must fulfill to more and more environmental constraints, such as being of low toxicity in answer to the Biocidal Product Directory, but also to involve waterborne treatments to limit rejection of volatile organic compounds in the atmosphere. Boron preservatives have been described as valuable alternatives for wood protection for non-ground contact applicatio...
F Obounou Akong, P Gérardin, M-F Thévenon, S Parant, C Gérardin-Charbonnier


The chemistry of wood degradation by Basidiomycetes studied in a van Krevelen diagram
2013 - IRG/WP 13-10805
The atomic composition ratios of decayed wood by Basidiomycetes are mapped in a van Krevelen diagram. It is shown that the wood residue after decay is chemically reduced, rather than oxidized. A previously developed and verified theoretical model for thermal wood modification, relating atomic composition ratios to moisture sorption and fungal resistance properties has tentatively been applied to w...
W Willems, H Militz


Transferable Durability: Enhancing decay resistance of non-durable species with extractives from durable wood species
2013 - IRG/WP 13-10808
Extractive content and composition is a vital component of naturally durable woods; however, variability in extractives can limit their usefulness in the field. Two extractive-free, non-durable wood species were pressure treated with ethanol-toluene extractives from 8 durable wood species. Extracted Southern pine, Paulownia and unextracted Southern pine blocks were treated and challenged in soil b...
G T Kirker, A B Blodgett, S Lebow, C A Clausen


Focus on the European standardization - Towards a revision of the EN 350 natural durability standard: a different approach to the inherent resistance and performance of wood and wood-based materials
2013 - IRG 13-10811
The European standard EN 350 “Natural durability of solid wood”, Parts 1 and 2, is one of the fundamental standards developed by the CEN/TC 38 “Durability of wood and wood-based products”. This standard is widely used by wood industries as the reference document which provides information on the resistance of wood species used in mainly the construction sector against decay fungi, wood-bor...
M Kutnik


Resistance of Consolidated Deteriorated Wood to Wood Decay Fungi
2013 - IRG 13-10812
The main purpose of the experiment was to establish which consolidating products in impregnated wood are the most effective against wood decay fungi. Five different consolidators were tested: Paraloid B-72, Consolidating restaurateur, SG 715 BLANC (epoxy resin), R.712 polyester and the wood consolidant agent containing nano particles, which is still in development. From the already damaged wood ...
F Pohleven, A Valantič, M Petrič