Virulence of two Laboratory Test Strains and one Natural Isolate of Rhodonia (Oligoporus) placenta against Thermally Modified Pine and Beech Wood
2013 - IRG/WP 13-20524
Rhodonia (Oligoporus) placenta is known as a relative aggressive basidiomycete fungus against thermally modified timber. In durability lab tests, this often results in a lower durability class, compared to other test fungi. In the reported work, the virulence of three different strains of Rhodonia placenta for untreated and thermally modified timber was determined and compared. Therefore, two lab ...
K Plaschkies, W Scheiding, K Jacobs, N Rangno


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


Development of a rapid method to assess the rate of fungal colonization of wood
2013 - IRG/WP 13-20531
Testing of wood durability is today done mainly with accelerated exposure tests under rather realistic conditions (in ground, outdoors with moisture traps etc). Although such tests are accelerated with respect to the conditions that outdoor exposed wood structures are exposed to, they tend to take rather long time. The present paper presents the development of a rapid method intended to assess at ...
L Wadsö


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2013 - IRG/WP 13-20535
A round robin involving 15 European participants was set up in 2006. The round robin consists of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. When comparing EN 84 preconditioning (two weeks water leaching) with natural preconditioning (1 year in field, above ground) according to CEN/TS 15397, no significant difference...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, B Mazela, E Melcher, R Möller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Methylene Chloride compared with white spirit as a treatment solvent for wood preservation – results from decay and termite studies
2013 - IRG/WP 13-30611
Non-aqueous solvents have a long history in the treatment of wood products in various parts of the world. The most familiar solvent treatment is the ‘light organic solvent preservative’ (LOSP) treatment based on low density solvents such as white sprit. Until recently white spirit was the only non-aqueous solvent approved for use in wood preservation in New Zealand. Australia also permitted...
A Siraa, P Lobb, C Molloy


Effect of Nano and Micronized Particles as Wood Preservatives for Termite Control
2013 - IRG/WP 13-30620
Subterranean termites are a major factor in the biodegradation of wood constructor products. In this study the efficacy of wood treated with micronized copper, zinc oxide and their mixture was compared to that of wood treated with soluble amine copper oxide with subterranean termites in a laboratory test. All of the formulations tested were effective in controlling wood degradation by the termites...
M Akhtari, D Nicholas, A Rowlen, M Arefkhani


40 year results from the largest preservative in-ground stake trial conducted in Australia
2013 - IRG/WP 13-30624
The final results from Australia’s largest preservative in-ground stake trial are listed. There were eight test sites, six in Australia and two in Papua New Guinea. The preservatives tested include low and high temperature creosotes, PCP and various water-borne preservatives including CCA and copper chromate. The main timbers examined were sawn Pinus radiata sapwood, sawn Eucalyptus regnans hear...
L J Cookson


Potential valorization of wood extractives from waste products of steam distillation of Aniba rosaeodora: antitermitic activity
2013 - IRG/WP 13-30629
Aniba rosaeodora, is a slow growing evergreens of the Lauraceae family which are indigenous over a wide range of the Greater Amazon Region (the Guianas and Venezuela, Brazilian Amazon…). The essential oil obtained from the wood has a characteristic aroma and is a long-established ingredient in the more expensive perfumes. The wood is also composed with alkaloid compounds like anibin. These compo...
N Amusant, A Digeon


Decay resistance of thermally modified Scots pine after 6 years’ exposure above ground
2013 - IRG/WP 13-40624
In the present study the performance of boards treated by ThermoWood process were studied above ground and the results given are based on a “modified” horizontal double- layer test. The base layer of boards was in direct contact with ground and the conditions were much harder than in the standard method. After six years’ exposure clear differences were found between untreated Scots pine and ...
H Viitanen, S Metsä-Kortelainen, A Nurmi, S Jämsä


Resistance of WPC against wood destroying fungi
2013 - IRG/WP 13-40627
The investigation of biological durability is a fundamental topic to assess the performance of Wood Plastic Composites (WPC) particularly for outdoor applications. In the last years, different test setups based on existing standards on the field of wood as well as the field of plastics were used for WPC. But the test methodologies give different information about the durability of the tested mater...
A Gellerich, S Bollmus, A Krause


Field performance of wood impregnated with siloxanes using supercritical carbon dioxide
2013 - IRG/WP 13-40632
This paper presents preliminary results from a 13-month field test containing pine sapwood samples (Pinus sylvestris) impregnated with a mixture of siloxane and organic biocides using supercritical carbon dioxide as carrier. Samples were exposed above ground at a Danish field test site using matched non-treated sapwood controls for every treated sample. All samples were painted before exposure. Pi...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Quantification of copper and chromium in field stakes after different exposure times: Remaining metal content and distribution
2013 - IRG/WP 13-50291
In order to determine the distribution of copper and chromium as well as their remaining concentration EN 252 specimens and thicker pine sapwood stakes (non standard format) were treated with a commercial CC salt in a vacuum pressure process. The stakes were installed in the test field of the Institute of Wood Research, Hamburg, in August 2010. In all cases three stakes were removed after 4, 8, 12...
T Liese, M Bahmani, E Melcher


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Estimation of service life of treated wood in ground contact based on early indicators
2013 - IRG/WP 13-20536
A well-known problem with field testing is that it takes a long time before meaningful and reliable results are achieved. Only when a trial has come to an end the so called average life for the samples in a group can be calculated and compared with other samples. The aim of the present study was to investigate if it is possible to get a reasonable and good estimation of the average life long befor...
M Hansson, J Jermer, P Larsson Brelid, N Terziev


Effect of Nano and Micronized Particles as Wood Preservatives for Termite Control
2013 - IRG/WP 13-30620
Subterranean termites are a major factor in the biodegradation of wood constructor products. In this study the efficacy of wood treated with micronized copper, zinc oxide and their mixture was compared to that of wood treated with soluble amine copper oxide with subterranean termites in a laboratory test. All of the formulations tested were effective in controlling wood degradation by the term...
M Akhtari, D Nicholas, A Rowlen, M Arefkhani


Is there a role for termite alates in colony expansion in Wisconsin?
2014 - IRG/WP 14-10820
Termite colonies in Wisconsin tend to be large and widely spread out geographically, and separated by distances up to 1342km. We recently completed a study to determine the genetic diversity and population substructure of thirteen existing colonies of Reticulitermes flavipes using amplified fragment length polymorphism to determine patterns of termite dispersal in Wisconsin. Measures of inbreedin...
F Green III, R A Arango, G R Esenther, T G Shelton


The effects of copper proximity on oxalate production in Fibroporia radiculosa
2014 - IRG/WP 14-10823
Copper remains a key component used in wood preservatives available today. However, the observed tolerance of several critical wood rotting organisms continues to be problematic. Tolerance to copper has been linked to the production and accumulation of oxalate, which precipitates copper into insoluble copper-oxalate crystals, thus inactivating copper ions. The purpose of this study was to assess d...
K M Jenkins, C A Clausen, F Green III


Nondestructive Detection of Biodeterioration in Indonesian Traditional Wooden Construction of “Joglo”
2014 - IRG/WP 14-10834
To decide the repairing and reinforcement method for wooden constructions, it is necessary to get the enough and precise information on the status of the construction beforehand, especially the distribution and the degree of the biodeterioration, such as decay or insect attack (e.g. termite attack). In this study, damage of biodeterioration to teak wood used in Indonesian traditional wooden const...
Y Yanase, T Mori, T Yoshimura, Y P Prihatmaji, J Sulistyo, S Doi


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of wood. The moisture performance of wood and wood-based products has been recognized as key...
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


Selection of Wood-Rotting Basidiomycetes for Inoculation of an Accelerated Soil Bed Test
2014 - IRG/WP 14-20543
There is a need for a test method that guarantees exposure of treated wood to soil and preservative-tolerant wood-rotting basidiomycetes as standard field tests do not do this reliably. The ability of a range of selected wood-rotting basidiomycetes to grow through unsterile forest soil was investigated in a Mason jar test assembly. None of the white-rot fungi in test grew through this soil. Fou...
P I Morris, A Uzunovic, J Ingram


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar


Screening method to test efficacy of fumigants against fungi and preliminary data on the efficacy of sulfuryl fluoride
2014 - IRG/WP 14-20551
Methyl bromide is being phased out and there is an urgent need to find a suitable replacement that is effective in reducing exotic pest establishments via trade in wood products. Efficacy data for established phytosanitary fumigants were mostly developed for arthropods and nematodes, and limited information exists for plant pathogens. Increased interest in developing a fast screening process for f...
A Uzunovic, A Mukherjee, R Mack, P Elder, S Myers