Harmonisation of technical requirements of treated wood in Europe. What can we learn from the experience in the Nordic countries?
1995 - IRG/WP 95-50040-20
In the Nordic countries the Nordic Wood Preservation Council (NWPC) has since 1972 harmonised the technical requirements for pressure treated timber in a Nordic standard. These requirements were used by the control schemes that exist in every country. In 1976 the first Nordic standard for pressure treated wood was accepted and in 1978 NWPC changed from recommendations to approvals for the preserva...
F G Evans


FTIR characterization of copper ethanolamine - wood interaction
1999 - IRG/WP 99-20154
The interaction of copper ethanolamine (Cu-EA) and wood components was studied by using Fourier transform infrared spectroscopy (FTIR). In Cu-EA treated wood, significant reduction was noticed on the band attributed to carbonyl vibration from carboxylic groups at 1735±5 cm-1 and an increase in band intensity was obtained from carbonyl in carboxylate at 1595±5 cm-1. The same observation was made ...
Jun Zhang, D P Kamdem


The examination of preservative-treated radiata pine using electron spin resonance spectroscopy
1987 - IRG/WP 3423
Electron spin resonance spectroscopy (ESR) may be used to characterise the molecular environment of chemical species containing unpaired electrons. These species include free radicals, bi-radicals, point defects in solids, localised crystal imperfections and many transition metal ions. ESR has previously been applied to the examination of wood weathering or wood pyrolysis and now FRI and Massey Un...
D V Plackett, E W Ainscough, A M Brodie


Screening of the technical performance and aquatic toxicity of N-methylolacrylamide treated wood
2000 - IRG/WP 00-40166
In the course of the last decades chemical modification of wood species, with a limited natural durability, has been subjected to intensive research. As a possible alternative and supplementary treatment of non-durable wood in a range of applications it remains one of the major topics in the wood preservation world. Different modification systems have been scaled-up and are now in an industrialisi...
V Rijckaert, S De Geyter, J Van Acker, M Stevens


Surface protection of wood with titanium, zirconium and manganese compounds
2005 - IRG/WP 05-30376
Thin radiata pine veneers were treated with a range of titanium, zirconium and manganese compounds and exposed to natural weathering. Veneer weight and tensile strength losses were used to assess the protective efficacy of the compounds. The oxidative manganese compounds potassium permanganate and manganic acetate restricted both weight and tensile strength loss of treated wood veneers during weat...
K J Schmalzl, P D Evans


Micromorphological and chemical changes of archaeological woods from wrecked ship's timbers
1987 - IRG/WP 4136
Micromorphological and chemical alterations of sea-waterlogged woods obtained from the ship-wrecked materials which had been submerged in Yellow Sea for over 700 years were investigated. The woods were deteriorated in varying degrees by marine organisms depending on species and parts of the woods. Under the light and scanning electron microscope the morphological characteristics of deteriorated wo...
Y S Kim


FTIR studies on the weathering of didecyldimethylammonium compound (DDAC) treated wood
1993 - IRG/WP 93-30013
Wood treated with alkylammonium compounds (AACs), such as DDAC, weathered more rapidly than untreated wood. In order to examine the influence of DDAC treatment of wood on its weathering, treated and untreated microtomed sections of southern yellow pine earlywood of various thicknesses, were prepared and weathered for approximately one month. The changes in these samples were monitored using FTIR. ...
R Liu, J N R Ruddick


Defining fungal decay types - A proposal for discussion
1985 - IRG/WP 1264
The present definitions of the fungal decay types, white rot, brown rot, and soft rot are somewhat vague. The definitions are based on a mixture of criteria involving morphological and chemical aspects of decay as well as taxonomic affiliation of the responsible fungal species. The present vague definitions have led some fungi being erroneously places in a wrong decay type. Furthermore, some fungi...
T Nilsson


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek


A substantively bonded water repellent treatment based on chromium carboxylates
1985 - IRG/WP 3344
Chromium carboxylates soluble in toluene have been synthesised and applied to Scots pine (Pinus sylvestris) sapwood. Without any further treatment, the compounds may be readily leached from wood surfaces with toluene. After a period of heating however, they become fixed to the cell wall, substantial amounts being resistant to leaching even under reflux conditions for several hours. Treatment of wo...
J K Wright, W B Banks, W J Eilbeck


Wood preservation in Canada - Regulation and Registration
2001 - IRG/WP 01-50166-02
The Canadian wood preservation industry is at a critical juncture now as a number of initiatives converge on the industry over the next few years. Issues facing the industry include: Re-evaluation of the conventional wood preservative chemicals - inorganic arsenicals, creosote and pentachlorophenol targeted for July 2001. Delayed registration of new actives as a result of re-evaluation activity an...
P A Cooper


Fixation of chromated wood preservatives through technical drying
1990 - IRG/WP 3623
Twin samples of sawn timber of Pinus sylvestris and Picea sp. were treated with copper-chromate-containing wood preservatives and subsequently kiln resp. air dried. After drying, the distribution of preservative and rate of fixation were determined. Drying of freshly treated wood in a condenser type kiln at temperatures of 60°C and 80°C and in a vacuum type kiln at 55°C with a pressure of about...
R-D Peek, H Klipp


Experimental variations in the distribution of CCA preservative in lignin and holocellulose as a function of treating conditions (temperature, concentration, pH, species, and time)
1984 - IRG/WP 3277
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a 3x3x4x2 factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, a...
A Pizzi, E Orovan, M Singmin, A Jansen, M C Vogel


Extracellular laccase production in brown-rot fungus Coniophora puteana
2001 - IRG/WP 01-10391
Coniophora puteana, one of representing brown-rot fungus, was investigated in terms of extracellular ligninolytic enzyme production. Three fungal strains of C. puteana were inoculated in liquid culture medium with sawdust of pine and oak wood. Extracellular laccase production was observed in some strains of C. puteana in the culture medium with sawdust of oak wood. The highest activity occurred at...
Kwang-Ho Lee, Seung-Gon Wi, Yoon Soo Kim


Immunolabelling studies on the detection of enzymes during the degradation of wood by Phanerochaete chrysosporium
1988 - IRG/WP 1364
The degradation of lignin in native lignocellulosic substrates by white rot fungi is poorly understood. Biochemical studies have shown the involvement of a number extracellular ligninolytic enzymes released by white rot fungi which are capable of the oxidative conversion of DHP's (lignin model compounds) in vitro, but to date conclusive evidence for occurrence of these enzymes in wood und...
G F Daniel, T Nilsson, B Pettersson


Influence of ethanolamine on lignin depolymerization and copper leaching from treated Norway spruce and beech wood
2007 - IRG/WP 07-30423
Copper-ethanolamine based wood preservatives are replacing several classical copper-chromium based solutions, due to foreseen ban of chromium. Fixation of copper-ethanolamine based wood preservatives is not as good as fixation of copper-chromium ones. The main object of this manuscript was to prove, that ethanolamine is the prime reason for insufficient fixation of copper-ethanolamine formulations...
M Humar, B Bucar, M Zupancic, D Žlindra, F Pohleven


Anatomical, physical and chemical changes of Bamboo (Phyllostachys puberscence ) during weathering processes
2008 - IRG/WP 08-10650
Bamboo (Phyllostachys puberscence) culms with 1, 2, 3 year old were exposed to natural weathering condition in Gwangju, Korea for 12 months. Changes in color, surface topography, strength and chemical properties were investigated using various microscopic and instrumental techniques. After one year’s weathering, the color of bamboo became lighter but strengths of bamboo did not change significan...
Jong Sik Kim, Kwang Ho Lee, Mi Young Cha, Yoon Soo Kim


Oxidative stress and lignin peroxidase production in Phanerochaete chrysosporium
2008 - IRG/WP 08-10655
In Phanerochaete chrysosporium liquid cultures, the induction of lignin peroxidases is directly related to accumulation of reactive oxygen species at the mitochondrial level. In this study, we demonstrate that the expression of the mitochondrial thiol-related antioxidant system is not directly coupled to the LiPs expression. When the antioxidant systems are not able to cope with ROS accumulation, ...
M Morel, L Diss, C Fourrey, M Chalot, M Droux, J P Jacquot, E Gelhaye


Degradation of polychlorinated organic biocides by the wood decaying fungi
2008 - IRG/WP 08-50253
Organochlorine biocides such as lindane, pentachlorophenol sodium salt, and polychlorinated biphenyl 153 have been widely used as wood preservatives. Due to their low degradability by soil bacteria, treated waste wood products pose a serious threat to the environment. Consequently, there is an increased need for development of new strategies for their detoxification. In this work, the bioremediati...
I Vidic, L Zupancic-Kralj, K Sepcic, F Pohleven


Fungal Attack on Lignin and Cellulose: Elucidation of Brown- and White-Rot Mechanisms Comparing Biomimetic and In-Vivo Degradation Patterns
2010 - IRG/WP 10-10714
This paper examines research and hypotheses that have been developed over several years on wood degradation mechanisms. This information is combined with new data and analyses to explain why wood decay patterns caused by brown-rot fungi and specific types of white-rot fungi are different. New data, including work with both biomimetic studies on low molecular weight compounds, degradative enzymes, ...
V Arantes, B Goodell, A M F Milagres, Yuhui Qian, T Filley, J Jellison, S Kelley


Lignin blocking effects on weathering process of wood plastic composites
2010 - IRG/WP 10-40529
The weathering of wood–plastic composites (WPC) causes discoloration which affects their aesthetic aspects. It has been proved that these discolorations are due to lignin degradation. Effects of blocking the susceptible structure of lignin assessed by chemical treatment such as acetylation and methylation are reported in this study. Surface chemical change of wood plastic composite (WPC) formula...
P Darabi, A Naghi karimi, S Ahmade Mirshokraie, M-F Thévenon


Micromorphological and chemical characteristics of waterlogged archaeological bamboos excavated from the Yellow Sea
2012 - IRG/WP 12-10785
Bamboos have widely used as documentation material in Far Eastern countries such China, Korea and Japan. In particular, bamboo slips as documentation material were extensively used even after the wide spread of paper in those countries. A large number of bamboo slips have been excavated from the shipwreck since 2009 in Korea. Understanding the cause of deterioration of ancient bamboos is crucial f...
Mi Young Cha, Yoon Soo Kim


The Technical Criteria on Biological Evaluation of Wood Preservatives for Use Category C4.1 in Southern China
2012 - IRG/WP 12-20481
According to the Regulations on Pesticide management of the People's Republic of China, wood preservatives belong to agrochemicals. The establishment of registration system on wood preservatives would be benefit to management of preservatives, including the market entrance and safety insurance to the human beings, livestock and the environment associated by the application of these preservati...
Xingxia Ma, Mingliang Jiang


Study of the use of organosolv lignin as bio-preservative of wood
2012 - IRG/WP 12-30603
The service life of wood depends on the species, use and environmental conditions of exposure. The treatment of wood protects it against degradation by xylophagous agents, enhancing the durability of material up to 10 times, and reducing the deforestation around 12.5%. In this way, the use of treatments is necessary because increases the service life of material and protect against xylophagous age...
P S B dos Santos, A Garcia, P H G de Cademartori, D A Gatto, J Labidi


Scanning Transmission X-ray Microscopy as a tool for examining chemical changes in wood cell walls due to enzymatic activity
2014 - IRG/WP 14-20556
As development of techniques for examining enzymatic activity on solid, complex biological materials, is considered to be an important factor in further development of enzyme applications and for understanding the decay of plant materials, this study explores applicability of Scanning Transmission X-ray Microscope (STXM) for determining chemical changes in enzymatically treated samples at the cell...
D Jeremic, R Goacher, R Yan, C Karunakaran, E R Master