Towards designing eco-friendly buildings with in-built termite protection
2010 - IRG/WP 10-50273
The increase in greenhouse gases, leading to global warming, is considered by a consistent scientific worldview not due to natural variation, but due to the growing concentration of carbon dioxide (CO2), methane (CH4) and other atmospheric pollutants. Global emissions of carbon dioxide from fossil fuel combustion and cement production rose from 22.6 billion tons in 1990 to an estimated 31.2 billio...
J R J French, B M Ahmed Shiday, B Maggiolo, D Maggiolo


Chapter 5 - Nursing of bamboo
2007 - IRG/WP 07-10635-05
In this chapter various procedures and steps of nursing of bamboo have been described with introduction, methodologies, examples and photographs. The propagation, improvement and sustainable growth of bamboo are possible through proper nursing of bamboo. The nursing of bamboo includes proper felling or extraction, fertilization and earth filling, protection from diseases and injuries, silvic...
A K Lahiry


Wood protectors sensitivity of Fusarium circinatum, a quarantine organism in Europe
2011 - IRG/WP 11-10755
In the last decade, two new organisms with a high potential damage in Conifer forests have been detected in Europe. They are the nematode Bursaphelenchus xylophilus and the fungus Gibberella circinata (anamorf: Fusarium circinatum), and have driven the European Union to protect the stands from propagation and dispersion of these new pathogens. The nematode was detected first in Setubal (Portugal)...
Y Serrano, S Cobacho, A Navas, M Conde, R Raposo, M T Troya


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Tannin resin-boron for outdoor wood protection and fire retardancy
2011 - IRG/WP 11-30567
Boron in the form of boric acid is well known for its efficacy against wood destroying organisms, as well as for its high leachability from treated wood when in outside exposure. Moreover, due to the European directive 2008/58/EC, boric acid is only authorized at low levels. In order to keep considering boric acid as an interesting active ingredient for wood protection, the issue is now to fix it ...
M-F Thévenon, G Tondi, N Leménager, S Wieland, A Pizzi


Effectiveness of Water Based Bentonite-Borate Slurry for In-situ Remedial Protection of Historic Wooden Piles: The Eurobor Protocol, Part 2
2011 - IRG/WP 11-30574
The study of the biocide product Eurobor®, water mixture of boric acid, borax and sodium bentonite, aimed to verify previous findings regarding borates penetration from a clay-water mixture of foundation timber. The product was applied on samples from 100 year old timber foundation from the city of Göteborg. Although in ground for this long the timber was in acceptable god condition due to groun...
M. Theorin, K. Fimmerstad, K-M. Bandh


Design, synthesis, characterisation and effectiveness of ‘Locked-in-Boron’ chemicals for H3.2 level of wood protection
2011 - IRG/WP 11-30577
Boratrane molecules with five-membered and six-membered molecular ring systems, and with various ring substituents were synthesised, characterised and formulated for wood treatment for accelerated laboratory bioassays using wood decay fungi as test organisms. Six-membered ring boratranes showed lower efficacy in laboratory assays than five-membered ring boratranes. One alkyl-substituted boratran...
R Franich, H Kroese, S Gallagher, S Hill, B Kelly, G Billett, R Meder, W Rae


Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher


Challenges and new developments in testing electro osmotic pulsing technology (PLEOT) by means of conventional laboratory methods
2011 - IRG/WP 11-40555
A new wood protection system, electro-osmotic pulsing technology, called PLEOT, is tested in lab trials using different test setup. The technology is tested on Scots pine sapwood and beech wood samples exposed to brown- and white rot fungi. Mass loss and moisture content is calculated after testing and a chitin analysis are performed on the sample powder. Two different electrodes are used in ord...
A Treu, E Larnøy


Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani


The Significance of Natural Durability of Croatian Mediterranean Wood Species for their Traditional and Present Protection Methods and Use
2012 - IRG/WP 12-10770
The aim of this article is to contribute to the better cognition of the protection and use of some most important Croatian autochthonous Mediterranean wood species. Their traditional use and protection are observed by two aspects. The first one is the presence of these species in the Croatian Mediterranean regions for many centuries, and the long tradition of their use, regardless of their natural...
R Despot, M Hasan


Use of the durable species Coast Redwood as a reference system for field testing of Wood Protection systems
2012 - IRG/WP 12-20486
Data is provided and discussed for a number of field exposure tests where the naturally durable wood species Coast redwood, Sequoia sempervirens, was included along with untreated pine and standard preservative treatments. In general, there is potential for higher variability of results with this naturally durable species, but it does suggest that redwood can be a useful reference material for te...
A Zahora, A Preston, L Jin


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Performance of Wood Protection Systems at Multiple Field Test Sites Using the Ground Proximity Test Method
2012 - IRG/WP 12-20499
A series of preservative systems were used to treat southern pine ground proximity test samples which were then exposed at a range of test sites located throughout the world. The sites were chosen on the basis of having vastly different Scheffer Climate decay indices. After almost 14 years exposure, distinct differences are apparent in how different preservative systems perform at the different ...
A Zahora, A Preston, L Jin


Survival of Bursaphelenchus xylophilus exposed to permethrins
2012 - IRG/WP 12-30585
The pine wilt nematode Bursaphelenchus xylophilus (Steiner and Buhrer 1934) Nickle, 1970 is a quarantine organism with a high potential to damage Conifer forests in Europe. This has driven the European Union to protect forest stands from the propagation and dispersion of this pathogen.The nematode was first detected in Europe in Setubal (Portugal) in 1999 and eradication measures were taken. Howev...
S C Arcos, M T Troya, L Robertson, F Llinares, M Conde, A Navas


Efficiency of the Amazon Forest Oils as Preservatives to the Attack of cellulolytic fungi in Pine Wood
2012 - IRG/WP 12-30599
The bobbins of wood are used for storage and field installation of cables from the electricity and telecommunications sectors. There are legal requirements governing the Brazilian ways of treating the wood used in these sectors, aimed at preventing pollution and protecting nature. When exposed to severe environmental conditions in Brazil these products are degraded and occurs many operational prob...
S Silveira, I M S Mendes, R S Paiva, J E Volponi, R C G Comar, R S Cruz


Wood protection in the Sierra Nevada National Park, Venezuela
2012 - IRG/WP 12-50290
The use of wood without the respective protection inevitably leads to its replacement. When this wood is used in a national park call attention to public opinion because the consequences generated by the very short life service, and replacement is required, means more wood not preserved, rapidly deteriorated in a constant repeated cycle. This becomes an environmental problem, especially when the ...
O Erazo, O Encinas, Y Molina


Recommendations for handling of mold infestation of wooden artifacts
2012 - IRG/WP 12-10790
The presentation gives an overview of the handling of wooden artifacts with mold infestation. The causes of mold deterioration are demonstrated by investigations in a church, a historic library and a monastery in Germany. Investigated infested wooden artifacts were altars, sculptures, picture frames and sarcophagi. Important investigation methods including indoor climate measurement, material an...
K Plaschkies, B Weiss, W Scheiding


Triazole – based ionic liquids to protect of lignocellulosic materials against fungi
2012 - IRG/WP 12-30601
In presented paper we examined on biotic properties of novel structure of tebuconazole derivatieves: tebuconazole hydrochloride, allyltebuconazole chloride, methyltebuconazole iodide, tebuconazole dihydrocitrate. Our investigation against wood-degrading fungi were contained also the didecyldimethylammonium 3-aminotriazolate as well as didecyldime-thylammonium nitrate(V) with tebuconazole or wit...
J Zabielska-Matejuk, J Pernak, I Frąckowiak, A Stangierska, W Przybylska, M Kot


The effect on moisture content of water trapped in wood joints
2012 - IRG/WP 12-40613
To predict the service life of a structure, a model where the exposure of a structure is compared to its resistance can be used. Which exposure and resistance parameters that are relevant depend on which materials the structure consist of. This approach, with an exposure and a resistance parameter, is similar to the one used in structural engineering where a load (exposure) is compared to the bear...
M Fredriksson, L Wadsö, P Johansson


Wood-leather panels – A biological, fire retardant building material
2012 - IRG/WP 12-40615
The poor flame retardant properties of wood-based products are among the severest obstacles, hindering its use in the commercial building sector. Recently, some attempts to improve the fire properties, relying on inflammable salts or reactive halogen compounds, have been presented, although they either cause problems with machining or embody harmful compounds (halogen derivates). In this paper, ...
S Wieland, U Stöckl, T Grünewald, S Ostrowski, A Petutschnigg


Influence of a pulsed electric field on the growth of surface fungi
2013 - IRG/WP 13-10795
The colonization of mold and staining fungi are not only an aesthetical problem. Blue stain fungi are able to penetrate paint films. Maintenance of coatings on wood are time consuming and costly. A new approach uses a pulsed electric field (PLEOT) in order to protect wood against surface fungi. This technology is evaluated in non-sterile laboratory conditions on different coated and uncoated Scots...
M Starck, A Treu


Surface moulds and staining fungi on acetylated wood – effect of increasing acetyl content
2013 - IRG/WP 13-10797
Wood used in outside applications is susceptible to weathering and photo degradation, which often leads to surface discoloration, loss of brightness and surface deterioration. Research has shown that acetylated wood is more resistant against brown rot, white rot and soft rot, and more dimensionally stable than untreated wood. However, acetylated wood seems still to be disfigured by surface moulds ...
L Ross Gobakken, S Bardage, C J Long II