IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 209 documents. Displaying 25 entries per page.


The resistance of composite boards protected with azole and inorganic nanoparticles to basidiomycetes and moulds
2015 - IRG/WP 15-40688
This paper presents a study on the resistance of wood composite boards, glued with silicone adhesive and obtained from chips of Scots pine Pinus silvestris L. and willow Salix viminalis L., to basidiomycetes and mould. The boards were protected in the production processes with fungicides based on metal nanoparticles, as well as on derivatives of 1,2,4-triazole, benzimidazole, and thiazole. The bio...
J Zabielska-Matejuk, I Frąckowiak, A Stangierska


Termiticide Residues in Building Foundation Aggregate Fills After Trench and Surface Applications
2015 - IRG/WP 15-30679
Termiticide concentrations (ppm) in aggregate fill were determined by measuring active ingredient (a.i.) residues of two pyrethroid termiticides, Up-Cyde Pro® 2EC-cypermethrin, and BaseLine® EC-bifenthrin, at 24.0 hours, and then at 6.0- and 12.0-months after ‘horizontal’ surface applications, perimeter ‘trenching and rodding’ applications, or ‘rodding only’ trench applications at lo...
B M Kard, C E Koneman, K T Shelton, C C Luper, R A Grantham


Simulation of surface climate and mould growth on wooden façades
2016 - IRG/WP 16-20585
The weathering of wooden surfaces is normally caused by mould growth, lignin deterioration and leaching of extractives. For well insulated buildings, the effect of the interior climate on the outer surface is small and sometimes negligible. This paper describes simple models for surface temperature and moisture conditions on a wooden façade that can further be used to model weather degradation an...
T K Thiis, I Burud, D Kraniotis, L Ross Gobakken


Assessment of the biological durability of wood treated with organosilicon compounds
2016 - IRG/WP 16-30685
The European wood construction market is in need of environmentally friendly wood-based products whose service life meets the expectations of end users. Non-biocidal silicon-based water repellents, which can be applied to different materials, help minimize their vulnerability/susceptibility to liquid water. Consequently, they have the potential of increasing wood’s resistance against decay fungi...
M Kutnik, M Montibus, S Derocker, S Salivati, J-P Lecomte


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti


Superhydrophobic treatment of Norway spruce wood for improvement of its resistance against brown rot and moulds
2016 - IRG/WP 16-40734
Water repellence of wood can be increased and its some other properties influenced by introduction of hydrophobic chemicals into and on cell walls without affecting the wood’s bulk density due to lumen filling. Herein, a simple dipping method to insert octadecyltrichlorosilane (OTS) into cell walls and to deposit the self-assembled hydrophobic monolayers (SAMs) of OTS is reported. It was found o...
A Kumar, P Ryparová, P Hajek, B Kričej, M Pavlič, A S Škapin, M Šernek, J Tywoniak, J Žigon, M Petrič


Formation of hydrophobic wood surface by means of thermal treatment and surface modification with alkyl ketene dimer (AKD)
2016 - IRG/WP 16-40738
One of the major shortcomings of wood-based materials compared to technical materials is attributed to their poor dimensional stability in changing climates and in contact with liquid water. Heat treatment induces chemical change with a consequent decreasing of reactivity of the material showing unwanted surface inactivation. Alkyl ketene dimer (AKD) is a widely used sizing agent in papermaking, w...
T Lovaglio, T Meints, L Todaro, W Gindl-Altmutter


The influence of log soaking temperature and thermal modification on the properties of birch veneers
2016 - IRG/WP 16-40749
In veneer manufacture the logs are routinely soaked in heated water baths in order to soften the wood prior to peeling. The temperature of the water may vary greatly between batches; however, the influence of log soaking temperature on veneer properties has had little research attention. Uncontrolled moisture is known to cause problems in wood-based materials, while thermal modification offers a m...
S Källbom, K Laine, M S Moghaddam, A Rohumaa, K Segerholm, M Wålinder


Evaluation of surface cracks on wood – physical assessment versus subjective sensation
2017 - IRG/WP 17-20617
In the presented studies from the University of Goettingen (Study I) and the University of Hannover (Study II), the assessment of cracks with different methods and their acceptance in general as well as depending on different target groups are investigated. The aim was to determine which factors are relevant for a crack evaluation and which visual impression of a wooden surface is tolerable for co...
A Gellerich, C Brischke, L Emmerich, L Meyer-Veltrup, P Kaudewitz


Surface Protection of Wood with Metal Acetylacetonates
2017 - IRG/WP 17-40802
Metal acetylacetonates are coordination complexes of metal ions and the acetylacetonate anion. They have diverse uses as catalysts, cross-linking and curing agents and adhesion promotors. Some metal acetylacetonates can photostabilise polymers whereas others are photocatalysts. We hypothesise that the ability of metal acetylacetonates to photostabilise wood will vary depending on the metal in the ...
Yuner Zhu, P D Evans


Aesthetic changes of coated thermally modified wood after artificial weathering
2017 - IRG/WP 17-40819
The thermal modification process affects the chemical configuration of the wood matrix improving some physical properties and durability. In addition, the distinctive dark tones of thermally modified timber increase the economic value of several light-coloured species. However, heat-treatment alters the substrates and it could influence in the application of coating products, necessaries to mainta...
R Herrera, J Sandak, E Robles, J Labidi


Rapid Screening test of potential antimicrobial agents for wood coatings
2018 - RG/WP 18-20644
A two-part screening test has been developed to evaluate additives for wood coatings. First, an additive is tested in the microbial laboratory and evaluated based on its inhibitory properties against selected test organisms, directly on agar plates. A microbial growth analysis is prepared and evaluated. If the additive is considered effective, it will be tested in a standard top coating (acrylic o...
J Stenbæk, E Morsing, T Østergaard Jensen


Wood Hydrophobic Modification by Mixed Wax Emulsions
2018 - IRG/WP 18-40839
An environmental-friendly, economical and facile method to construct hydrophobic system for improving wood repellency was applied in this study. Using paraffin wax and carnauba mixed wax O/W emulsions can simultaneously fabricate continuous wax films and rough structures in wood internal and external surface under appropriate heat treatment. In the study, single and mixed wax emulsions of 4% solid...
C Chen, W Wang


Visual appearance of unpainted wooden claddings during the first year of outdoor exposure: Evaluation of surface mould growth, lightness (L*) and wasp attack
2018 - IRG/WP 18-40841
This study addresses changes in visual appearance of unpainted wood materials exposed outdoors. Specimens of Norway spruce (Picea abies) Scots pine (Pinus sylvestris), aspen (Populus tremula), acetylated Radiata pine (Pinus radiata) and DMDHEU-modified Scots pine sapwood were exposed facing south in Ås, Norway for 60 weeks. During this period, surface mould growth development and wasp attack were...
S Karlsen Lie, L Ross Gobakken, G I Vestøl, O Høibø


Charring of Norway spruce wood surface – an alternative surface modification technique?
2019 - IRG/WP 19-40870
Charring is an old wood surface treatment technique, mainly performed on wooden façade elements with the aesthetical aims, but also with the purpose of protection. This flame treatment method can be grouped into heat treatment processes. Below the top charred layer of damaged wood there is a layer which is during flame treatment exposed to high temperatures in anoxic or semi-anoxic conditions. Th...
M Petric, M Pavlic, J Zigon


Improvement of wood decay and termite durability resulting from combined treatments based on borax/phenol-formaldehyde impregnation followed by thermal modification
2019 - IRG/WP 19-40871
This study determined the factors influencing the boron content after leaching of pine blocks impregnated with aqueous solution of phenol-formaldehyde (PF) resin with or without borax and subjected to heat treatment by response surface methodology. An experimental design permits to analyze the effects of heat treatment temperature (150, 185 and 220°C), curing time (5, 12, 5 and 20 hours), resin c...
S Salman, M-F Thevenon, A Petrissans, S Dumarcay, P Gerardin


Application of diverse hyperspectral imaging systems for evaluation of heritage objects
2020 - IRG/WP 20-10971
Advanced imaging techniques are able to non-invasively characterize, monitor and evaluate the impact of conservation treatments on cultural heritage (CH) objects. In this specific field, hyperspectral imaging (HI) allows non-destructive characterization of materials by identifying and characterizing colouring agents, binders and protective coatings as constituents of an object’s original constru...
J Sandak, A Sandak, L Legan, K Retko, M Kavčič, J Kosel, F Poohphajai, R Herrera Diaz, V Ponnuchamy, N Sajinčič, Č Tavzes, P Ropret


Biofinish: A Functional Wood Surface Treatment based on Aureobasidium
2020 - IRG/WP 20-40903
Xyhlo Biofinish is a natural and environmentally friendly wood protection concept based on linseed oil impregnation and a fungal-based coating. It emerged in the late 1990s and has been developed over the past 15 years into an industrially applicable process in the Netherlands. The combination of linseed oil impregnation and a surface treatment with the living fungus Aureobasidium extends the serv...
S Rensink, M Sailer, S Roukens, J Gerber, H van der Mel, K Potgieter, J Spit, R Bulthuis, C Struck, M Bennink


The influence of chemical compounds on wood cell wall to surface cracks
2020 - IRG/WP 20-40908
Degradation due to cracking and dimensional changes caused by drying, have a significantly negative impact on the preservation and durability of wood. Therefore, the prevention of surface cracking, which tends to occur during the drying process, is vital. High temperature set drying is one of the most effective methods for preventing wood surface cracking. It begins with softening the wood at a hi...
R Suzuki, Y Mori, K Yoshihiro, K Yamashita, M Kiguchi


Plasma treatment of wood - a review of 15 years of research in Göttingen
2021 - IRG/WP 21-40913
Wood is an important renewable resource and can be found omnipresent in everyday life. Its natural properties offer numerous advantages regarding physical, mechanical but also aesthetic aspects, but also challenges that one has to address with various modification methods. Driven by the desire to promote the use of promising new technologies using plasmas, there has been a close research network ...
P Sauerbier, R Köhler, G Avramidis, W Viöl, H Militz


Influence of weathering on surface roughness of thermally modified wood
2021 - IRG/WP 21-40915
Thermally modified wood is exposed to weathering similarly as other wood-based building materials. It has been reported that if thermally modified wood is exposed to weathering, its moisture performance might decrease fairly fast. The aim of this study was to determine whether this phenomenon is associated with crack formations or roughness. Norway spruce, thermally modified spruce, wax-treated th...
E Kerzic, B Lesar, M Humar


Surface morphology and short-term water uptake of charred and coated wood
2021 - IRG/WP 21-40916
Charring of the wood surface represents a traditional alternative surface treatment technique with the purpose of aesthetics and protection. By the treatment with flame the surface of wood becomes carbonized and a few millimetres thick charred layer is formed on the top of the wooden element. Further, the charred layer can be removed by brushing, which accentuates the structure of the surface. Add...
J Zigon


Dynamics of fungi colonization on the surface of Scots pine wood during natural weathering in different European climate zones
2022 - IRG/WP 22-10984
Wood The presence of fungi leads to biomaterial decay and/or changes in aesthetical appeal. The start of fungi colonization as well as the following growth on wood are primarily influenced by four factors: ambient temperature, moisture history of the object, access to oxygen, and intrinsic properties of the exposed wood, considered here as a source of nutrients for microorganisms. A prevalence of ...
F Poohphajai, O Myronycheva, O Karlsson, L Rautkari, J Sandak, A Sandak


Impact of wetting agents on polyelectrolyte complex impregnation for wood fire-retardancy
2022 - IRG/WP 22-30768
Wood fire performance is a great concern in interior finishing due to the high risk of flame spread. To increase the use of wood in high building while ensuring the safety of building occupants, fire retardant (FR) treatments are required. Traditionally, two fireproofing strategies are employed: impregnation and coatings. They have been widely studied but they, respectively, are time and chemicals...
M Soula, J B Grenier, S Duquesne, F Samyn, V Landry


Surface chemical wood densification through in situ electron beam polymerization: description and dose study
2022 - IRG/WP 22-40933
Traditional wood chemical densification processes can be used to improve wood mechanical properties by increasing density of the material throughout its thickness. While mechanical surface densification has heavily been investigated, surface treatments involving impregnation of monomers remain unexplored. This study describes a new material, surface densified through lateral impregnation of acryla...
J Triquet, P Blanchet, V Landry


Previous Page | Next Page