Surface characteristics of wood treated with various AAC, ACQ and CCA formulations after weathering
1991 - IRG/WP 2369
Wood samples treated with various alkylammonium compounds (AACs) as well as ammoniacal copper quat (ACQ) and chromated copper arsenate (CCA) have been studied in accelerated weathering experiments. Microscopic examination of the surfaces of these samples after exposure in a weatherometer revealed several different changes. Samples treated with didecyldimethyl ammonium chloride (DDAC) show consider...
L Jin, K J Archer, A F Preston


Screening of bacteria, yeasts and Trichoderma isolates for antagonism toward stain and mould fungi on agar media and wood
1999 - IRG/WP 99-20159
A screening programme of soil bacteria for antagonism toward mould and wood stain fungi was undertaken on 8 types of agar-based media by application of several bacteria to each plate. The rapid screening method was subsequently verified by testing antagonism of the most promising bacteria on Scots pine sapwood. Most of the 64 bacterial showed antagonistic effects on certain media against individua...
C Payne, A Bruce


The importance of blue stain attack for the colonization by wood-rotting fungi of wood not in contact with the ground
1988 - IRG/WP 1349
When used in constructions not in contact with the ground, wood has been shown often to proceed from blue stain to moulds. The appearance of wood rotting fungi is normally delayed. Solid wood artificially inoculated with the blue stain fungus Pullularia pullulans was shown to permit germination of Pycnoporus cinnabarinus basidiospores. This was demonstrated by the use of an indirect and a direct b...
J Bjurman


An appraisal of anti-sapstain chemicals in Queensland, Australia
1985 - IRG/WP 3331
Eleven formulations were tested in the field for effectiveness against sapstain, mould and fungi on Pinus elliottii in Queensland. The commercially used sodium pentachlorophenoxide (0.5% a.i.) and Captafol (0.2% a.i.) performed well. Busan 1009 (0.3% a.i.), Protek T (5.0% a.i.), Woodgard E.S. and E.C. (0.8% a.i.), together with sodium tetrachlorophenoxide (0.5% a.i.) offer potential as anti-sapsta...
L E Leightley


Japanese standardized method for evaluating effectiveness of anti-sapstain and anti-mould chemicals
1988 - IRG/WP 2299
Japan Wood Preserving Association established a method for testing effectiveness of chemicals against sapstain and mold fungi on wood in 1979. The method is concerned with a laboratory technique using small timber specimens (20 x 50 x 3 mm³), petri dish and 5 test fungi. Effectiveness of each candidate chemical is evaluated on the basis of the relative resistance to sapstain and mold fungi which ...
K Tsunoda, K Nishimoto


Field evaluation of alternative antisapstain chemicals
1982 - IRG/WP 3198
Seven alternative antisapstain formulations containing four different active ingredients were field tested during the summer and fall of 1981. The test was designed to evaluate the potential long term effectiveness of PQ-8 (Chapman Chemical Co.) containing copper-8-quinolinolate, Busan 30 (Buckman Laboratories) containing 2-(thiocyanomethylthio)benzothiazole, BL2398 (Buckman Laboratories) containi...
D V Plackett


A field test on susceptibility of wood-based board materials to moulds
1989 - IRG/WP 3545
A field test on susceptibility of wood-based board materials to mould growth was carried out under practical, but severe, service-conditions. A total of 19 commercially available composite boards were investigated. It was found that all board materials tested were not completely immune to mould attack. Test results revealed that among the three main categories of wood-based boards involved, partic...
Qiao Wang, B Henningsson


Moisture distribution in coated wooden panels. Studies of moisture dynamics by computerized axial tomography
1992 - IRG/WP 92-2413
Certain modern coatings have been held responsible for the rot damages in wood sidings, which have, during the past few years, appeared at an increasing extent in Scandinavia and which have occurred rather soon after the application of the coating. In this study, the moisture excluding effect of different coating systems intended for sidings have been studied with the help of an X-ray technique, c...
J Ekstedt, L O Lindgren, S Grundberg


Field evaluation of anti-sapstain products
1987 - IRG/WP 3402
Product A based on methylenebisthiocyanate, product B based on methylenebisthiocyanate plus 2-thiocyanomethylthio-benzothiazole, product C based on 2-thiocyanomethilthio-benzothiazole and product D based on didecyl dimethil ammonium chloride plus 3-iodo-2 propynil butyl carbarnate were evaluated on Pinus radiata sawn timber as fungicides for sapstain and mould in the Sawmill Division of the Univer...
M C Rose, A Bedoya


Evaluation of the effectiveness of Tuff Brite C in the control of sapstain in laboratory and field tests
1992 - IRG/WP 92-3718
Since 1990, the anti-sapstain product Tuff Brite C (ASC 66898) has been evaluated internationally in laboratory and field tests, and has been commercially introduced in New Zealand. The product is an aqueous flowable formulation of chlorothalonil and carbendazim. Efficacy tests which have been carried out in New Zealand, Australia, USA, South Africa and Europe are described and summarized. Tuff Br...
T L Woods, C J Klaver


Surface checking of CCA-treated radiata pine decking timber exposed to natural weathering
2000 - IRG/WP 00-40165
A field trial was established at four locations in Australia to assess the effect of CCA and CCA-wax treatment on the checking (cracking) of radiata pine decking timber exposed to natural weathering. Untreated decking timber and timber that had been pressure treated with water acted as controls. After 1 year's exposure the number and sizes of checks occurring in treated timber and control...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Surface protection of wood with titanium, zirconium and manganese compounds
2005 - IRG/WP 05-30376
Thin radiata pine veneers were treated with a range of titanium, zirconium and manganese compounds and exposed to natural weathering. Veneer weight and tensile strength losses were used to assess the protective efficacy of the compounds. The oxidative manganese compounds potassium permanganate and manganic acetate restricted both weight and tensile strength loss of treated wood veneers during weat...
K J Schmalzl, P D Evans


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Biological control of sapwood-inhabiting fungi by living bacterial cells of Streptomyces rimosus as a bioprotectant
1992 - IRG/WP 92-1564
The objective of this study is to evaluate the efficacy of antifungal activity of living bacterial cells for the protection of wood against sapwood-inhabiting fungi. The following sapwood-inhabiting fungi were selected: sapstain --Ceratocystis coerulescens, Ceratocystis minor, Ceratocystis pilifera, and Aureobasidum pullulans; mold fungi --Aspergillus niger, Penicillium spp, and Trichoderma spp. L...
S C Croan, T L Highley


Quantification of creosote migration down wooden poles and the prevention of its depletion during flood irrigation
1994 - IRG/WP 94-50032
Polyethylene field liners heat-shrunk onto soil-contact surfaces prevented decay of creosote-treated Eucalyptus grandis vineyard poles under flood-irrigation. The present work quantified losses of creosote from these poles after six and 24 months' service. After six months' service the mean creosote retention of unlined poles above the ground line was 12.62% (m/m dry wood), with ...
M Behr, A A W Baecker


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek


Shorter-term biological control of wood decay in pre-seasoning pine roundwood as an alternative to chemical methods
1992 - IRG/WP 92-1555
Previous studies on the long-term control of decay in creosoted transmission poles, using Trichoderma and other antagonistic moulds, have met with limited success. However, it is possible biological control is more suited to control of decay on shorter time scales. An earlier study, focusing on pre-seasoning treatment of transmission poles showed that favourable porosity increases could be brought...
M W Schoeman, D J Dickinson


Preliminary observations of the effect of growth ring orientation on the surface checking of flat sawn Southern pine decking
2005 - IRG/WP 05-20313
Checking in decking timber is a serious defect and methods of reducing its severity are required to ensure that wood can compete with alternative decking materials. The first aim of this research was to test the hypothesis that flat sawn Southern pine decking boards with growth rings oriented concave to the exposed surface will develop less severe checking when exposed outdoors than similarly expo...
K Urban, P D Evans


Why don't more people work with Serpula lacrymans nowadays? A discussion of some of the different approaches to experimenting with this unique fungus
1989 - IRG/WP 1383
Remarkably few laboratories are currently investigating this well-known fungus. Not only has it failed to gain acceptance as a standard test organism (for wood preservative evaluation) in many countries, but is also sometimes excluded from pure research studies when it ought to be an obvious first choice as a representative basidiomycete. This paper discusses some different approaches that have be...
J D Thornton


Laboratory evaluation of anti-sapstain formulations
1989 - IRG/WP 3510
Four formulations were tested for their efficacy in controlling molds and sapstaining fungi on wood according to the Standard-II of Japan Wood Preserving Association (JWPA). Relative efficacy was compared on the basis of visual rating of the fungal growth on the treated and untreated wood surfaces when the wood specimens were exposed to each monoculture of 5 test fungi at 26±2°C and 70-80% for 4...
K Tsunoda


Antifungal activity in metabolites from Streptomyces rimosus
1991 - IRG/WP 1495
The objective of this study was to evaluate the efficacy of antifungal metabolites from Streptomyces rimosus for controlling the growth of sapwood-inhabiting fungi: sapstain fungi - Ceratocystis coerulescens, Ceratocystis minor, Ceratocystis pilifera, and Aureobasidum pullulans; mold fungi - Aspergillus niger, Penicillium spp, and Trichoderma spp. Production of antifungal metabolites by Streptomyc...
S C Croan, T L Highley


Sawmill Evaluation of a Bioprotectant against Moulds, Stain and Decay on Green Lumber
2003 - IRG/WP 03-10460
Moulds, stain and decay cause serious problems on wood utilization. Though a growing volume of wood is kiln-dried, the market for green exports remains significant, and environment-friendly wood protection is required to replace traditional chemicals. As a solution to this problem, Forintek Canada Corp. developed a bioprotectant for protecting logs and green lumber from moulds, stain and decay, wh...