Improving our understanding of moisture and other durability-related properties of wood in building envelope performance prediction
2011 - IRG/WP 11-20468
Building science has become an increasingly important field in recent years with rapid changes in construction methods, building materials and consumer expectations. The field has also been brought to prominence by a few large-scale premature building envelope failures in a few regions across the world. Considerable effort has been put into developing hygrothermal models to simulate heat, air, vap...
Jieying Wang, P Morris


Decay initiation in plywood, OSB and solid wood under marginal moisture conditions
2011 - IRG/WP 11-20469
Hygrothermal models are increasingly used as research tools by building scientists and and design tools by designers to simulate heat, air, vapour, and water movements within and through building envelope and even to predict the consequences in terms of mould/decay growth and metal corrosion. This work was designed to generate data on decay initiation under marginal moisture conditions to support...
Jieying Wang, P Morris


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher


Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani


Long term durability of the heartwood of seven common softwood species in above ground conditions
2012 - IRG/WP 12-10771
The natural durability for wood in above ground use has been evaluated based on results after 11 years of exposure in a test site situated at the Danish Technological Institute in Taastrup, Denmark. Selected results for seven common softwood species exposed horizontally are reported. The test results cover samples with direct rain exposure (use class 3 of the European standard EN335-1:2006) and sa...
E Tang Engelund, M Klamer, T Mark Venås, B Lindegaard


Influence of soil moisture, Sarawak soil types and decay types on decay susceptibility of rubberwood and kelempayan
2012 - IRG/WP 12-10780
Wood and soils are important natural resources of the land, the former widely used as structural supports in contact with the latter. Many low durability wood species exposed to soil contact has reportedly high incidence of decay failures in poorly treated and untreated materials depending on soil types, properties and soil microbial virulence. This paper probes the relationship of the main soil t...
A H.H. Wong, P K.F. Chong, J Sabang


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Plywood under the scanner: linking moisture dynamics and 3D structure
2012 - IRG/WP 12-20491
Plywood is highly esteemed as a construction material. Yet, the influence of moisture on both strength and durability are important factors. Especially the dynamics of moisture desorption and absorption should be taken into account when assessing the quality of a panel, which is a fact for all panel materials. This paper therefore focuses on the monitoring of the moisture dynamics of plywood subje...
J Van den Bulcke, I De Windt, N Defoirdt, J Van Acker


Comparative studies on the moisture performance and durability of wooden facades
2012 - IRG/WP 12-20492
Wooden claddings are traditionally used in many parts of the world. Also modern structures are frequently made from timber and timber engineering panel products. However, wood has to compete with other cladding materials and its durability needs to assure sufficient functional and aesthetic service life. Besides many other factors the durability of a wooden facade is dominated by its moisture perf...
T Bornemann, C Brischke, J-M Lück


Moisture performance based wood durability testing
2012 - IRG/WP 12-20495
In the frame of a scientific cooperation within the Swedish research program ‘WoodBuild’ comparative field and laboratory durability studies have been carried out by the Technical Research Institute of Sweden SP and Leibniz University Hannover. One objective was to improve test methods as well as evaluation systems in order to facilitate the use of (field) testing for service life prediction. ...
L Meyer, C Brischke, A Pilgård


Performance of wood treated with linseed and tung oil against wood decay fungi and wetting
2012 - IRG/WP 12-30598
Most of the European wood species does not have durable wood. In order to use it in outdoor conditions nondurable material has to be protected. Nowadays, non-biocidal solutions for wood protection are attracting a lot of attention, particularly in use class 2 and 3 applications. One of the non-biocidal techniques is treatment of wood with water repellents like wax emulsions and oils. Linseed oil a...
M Humar, B Lesar


Relationships between heat treatment intensity and some conferred properties of different European softwood and hardwood species
2012 - IRG/WP 12-40593
Effect of treatment intensity on conferred properties like elemental composition, durability, anti swelling efficiency (ASE) and equilibrium moisture content (EMC) of different European softwood and hardwood species subjected to mild pyrolysis at 230°C under nitrogen for different durations has been investigated. Independently of the wood species studied, elemental composition is strongly correl...
M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Influence of a pulsed electric field on the growth of surface fungi
2013 - IRG/WP 13-10795
The colonization of mold and staining fungi are not only an aesthetical problem. Blue stain fungi are able to penetrate paint films. Maintenance of coatings on wood are time consuming and costly. A new approach uses a pulsed electric field (PLEOT) in order to protect wood against surface fungi. This technology is evaluated in non-sterile laboratory conditions on different coated and uncoated Scots...
M Starck, A Treu


Surface moulds and staining fungi on acetylated wood – effect of increasing acetyl content
2013 - IRG/WP 13-10797
Wood used in outside applications is susceptible to weathering and photo degradation, which often leads to surface discoloration, loss of brightness and surface deterioration. Research has shown that acetylated wood is more resistant against brown rot, white rot and soft rot, and more dimensionally stable than untreated wood. However, acetylated wood seems still to be disfigured by surface moulds ...
L Ross Gobakken, S Bardage, C J Long II


The influence of microclimate on the moisture conditions in a Norway spruce (Picea abies (L.) Karst.) joint exposed to artificial rain
2013 - IRG/WP 13-20505
Wood structures outdoors are susceptible to decay if they are exposed to high moisture contents during long periods of time. Structures with joints that act as water traps are especially exposed since high moisture contents are reached in such positions. This paper presents a part of a laboratory study that concerns the relationship between the microclimate and the material climate, i.e. the moist...
M Fredriksson, L Wadsö, P Johansson


Testing the performance of timber using 27 different field test methods
2013 - IRG/WP 13-20517
Numerous test methods to determine the durability of timber and timber products have been described in relevant literature. However, only some of these methods have been standardized and thus only very few are regularly used for resistance tests in the field. Since results from extensive comparative field studies have shown differences in moisture performance between different test methods, the ai...
L Meyer, C Brischke, J Rieken


Climatic impacts on the moisture performance of wooden decking and facades
2013 - IRG/WP 13-20518
In outdoor usage wood is exposed to a variety of influences, which reduce its durability against biological deterioration and wetting. Besides many other factors the service life of wooden facades and cladding is dominated by occurring moisture loads on the one hand and their capability to withstand moisture on the other hand. Hence, climatic factors have a direct impact on the material climate an...
T Bornemann, C Brischke, G Alfredsen


Predicting the Rate of Decay, and the Potential for Misinterpretation of Proper Scientific Method
2013 - IRG/WP 13-20525
Predicting the rate of fungal attack in wood-based materials and its effect on properties remains the holy grail of wood products pathologists; however, achieving this goal is difficult because of the many variables associated with the process. This paper reviews some of the more important aspects of the decay process in relation to test methodology and then discusses how data are sometimes used b...
B S Goodell, J J Morrell


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


Surface energy characterization of thermally modified wood using inverse gas chromatography
2013 - IRG/WP 13-20532
The objective of this work is to characterize surface energetics of thermally modified wood. Such information may be useful for a better understanding and predictions of adhesion properties between the modified wood and other material systems, e.g. coatings, adhesives or matrices in composites. Inverse gas chromatography (IGC) was used to study the surface energy characteristics of thermally modif...
S Källbom, K Segerholm, D Jones, M Wålinder


System treatments of Pinus sylvestris - influence on moisture, decay and discoloration
2013 - IRG/WP 13-30612
Biological activity can cause challenges for the use of wood in outdoor exposure. Decay and discolouring fungi influence the service life of wooden constructions, and the moisture content of the wood is often an important factor. The aim of this study was to evaluate the performance of different combinations of preservative/modified wood protection treatments and surface treatments for wooden deck...
A Schabacker, G Alfredsen, L Ross Gobakken, H Militz, P O Flæte


Performance of biocide-free preservative-protective systems modified with organosilicon compounds
2013 - IRG/WP 13-30628
The objective of the research was to determine the influence of organosilicon compounds in preservative-protective systems on the selected properties of pine wood aimed for outdoor use. The investigations were made for biocide-free systems based on alkyd resin and natural oils modified with alkylalkoxy-, amino- and glycidoxysilanes. The special attention was paid on the influence of hydrophobic pr...
B Mazela, P Hochmańska, T Krystofiak