Limitations of the Pilodyn when assessing decay in graveyard test stakes
1982 - IRG/WP 2168
The following examination was designed to evaluate more precisely the usefulness of the Pilodyn for routine, objective assessments of the condition of field test stakes and to examine its limitations, particularly in respect to: 1.) The importance of variables other than extent of decay which may affect Pilodyn readings; 2.) Practicality of obtaining multiple readings in decayed and non-decayed re...
M E Hedley


Co-operative research project on L-joint testing. Sampling after 4 years exposure
1987 - IRG/WP 2274
In September 1983, Document No: IRG/WP/2208 was distributed giving guidance on sampling after 8 months exposure and including tables on which to record the test results. Similarly in September 1984, Document No: IRG/WP/2233 was distributed concerning sampling after 18 months exposure. No major problems have been notified to Princes Risborough Laboratory concerning the sampling method. It is theref...
J K Carey, A F Bravery


Treatment groups and remedies for CCA treated hardwood and softwood poles
1999 - IRG/WP 99-40142
Different hardwood and softwood species from Bangladesh and Bhutan was investigated regarding density, green fiber stress, natural durability of heartwood and CCA treated sapwood, CCA treatability grades, sapwood thickness, and kiln-drying properties for long term use as electric poles. These properties along with the past service records for nineteen years, separated ten heardwood and five softwo...
A K Lahiry


Surface checking of CCA-treated radiata pine decking timber exposed to natural weathering
2000 - IRG/WP 00-40165
A field trial was established at four locations in Australia to assess the effect of CCA and CCA-wax treatment on the checking (cracking) of radiata pine decking timber exposed to natural weathering. Untreated decking timber and timber that had been pressure treated with water acted as controls. After 1 year's exposure the number and sizes of checks occurring in treated timber and control...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Surface protection of wood with titanium, zirconium and manganese compounds
2005 - IRG/WP 05-30376
Thin radiata pine veneers were treated with a range of titanium, zirconium and manganese compounds and exposed to natural weathering. Veneer weight and tensile strength losses were used to assess the protective efficacy of the compounds. The oxidative manganese compounds potassium permanganate and manganic acetate restricted both weight and tensile strength loss of treated wood veneers during weat...
K J Schmalzl, P D Evans


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


A technique for determining the efficacy of water diffusible preservative plugs for implanting in joinery in service
1987 - IRG/WP 2291
A technique is described for determining the efficacy of soluble, diffusible preservative plugs for eradicating decay in joinery. It uses blocks of Scots pine sapwood or heartwood adjusted to known moisture contents prior to the establishment of the test fungus Coniophora puteana, from a single longitudinal dowel and the subsequent introduction of the preservative plugs. Prevention of decay, eradi...
J K Carey, A F Bravery


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Application of oscillating pressure to improve treatability of refractory species
1987 - IRG/WP 3449
Under practical conditions a minimum moisture content of 80% demande by the German quality standard RAL-RG 411 can not be guaranteed throughout the year. Storage of logs with bark prolonges the drying process; a storage without bark must be avoided. A sufficient penetration according the standard can be achieved at least with a moisture content of 60%, optimal conditions may prevail between 100% a...
R-D Peek


Quantification of creosote migration down wooden poles and the prevention of its depletion during flood irrigation
1994 - IRG/WP 94-50032
Polyethylene field liners heat-shrunk onto soil-contact surfaces prevented decay of creosote-treated Eucalyptus grandis vineyard poles under flood-irrigation. The present work quantified losses of creosote from these poles after six and 24 months' service. After six months' service the mean creosote retention of unlined poles above the ground line was 12.62% (m/m dry wood), with ...
M Behr, A A W Baecker


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek


The effect of moisture content on the electrical resistance of timber as detected by a pulsed current reistance meter (Shigometer)
1984 - IRG/WP 2212
The literature concerning the use of the Shigometer® for detecting decay in standing trees and wood poles is reviewed and the differences of opinion over the effect of timber moisture content on electrical resistance are highlighted. A simple experiment designed to test this effect is described and the implications of the results for testing poles in service are discussed. There was a large diffe...
P I Morris, D J Dickinson


Preliminary observations of the effect of growth ring orientation on the surface checking of flat sawn Southern pine decking
2005 - IRG/WP 05-20313
Checking in decking timber is a serious defect and methods of reducing its severity are required to ensure that wood can compete with alternative decking materials. The first aim of this research was to test the hypothesis that flat sawn Southern pine decking boards with growth rings oriented concave to the exposed surface will develop less severe checking when exposed outdoors than similarly expo...
K Urban, P D Evans


The study of blue stain found in coniferous timber in SR Slovenia (Yugoslavia)
1983 - IRG/WP 1177
The report concerns the problems connected with blue stain in coniferous timbers stored in warehouses at wood-processing plants in SR Slovenia (Yugoslavia). The amounts of spruce-wood (Picea abies Karst.) found to have been infected with blue stain have been measured and some of the fungi causing the stain have been identified and their biology studied. It was found that the percentage of spruce-w...
R Benko


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


Whitewood - An external joinery timber?
1975 - IRG/WP 253
The timber used traditionally for softwood joinery in the UK is redwood (Pinus sylvestris). In the past its ready availability in the desired sizes and quality and its durability in service encouraged little competition. However, the past decade has seen some erosion of this position, particularly through the increased proportion of sapwood in redwood supplies. Since the sapwood is less durable th...
J W W Morgan


The use of lap-joints in natural durability testing: moisture content development during 36 months outside exposure trials
2000 - IRG/WP 00-20217
Lap-joint trials (following European Standard ENV 12037) were set up with 11 different softwood and hardwood species. The main aim was to evaluate the suitability of this test standard (developed for testing wood preservative effectiveness) for natural durability testing. The moisture development has been followed during a 36 months period. In this paper, the outcomes of different moisture content...
H Militz, C J Bloom


Moisture Adsorption Behaviour of Rubber Wood Decayed by Brown and White rot Fungi
2005 - IRG/WP 05-40306
Moisture adsorption behaviour of rubber wood blocks decayed by each brown rot and white rot fungi was studied. The adsorption isotherms of decayed wood were compared with the isotherm of undecayed wood. The wood decayed by brown rot adsorbed less moisture as compared to sound or undecayed wood at all humidity levels. No significant difference was observed in adsorption behaviour of white rot dec...
S S Chauhan, H C Nagaveni


Why don't more people work with Serpula lacrymans nowadays? A discussion of some of the different approaches to experimenting with this unique fungus
1989 - IRG/WP 1383
Remarkably few laboratories are currently investigating this well-known fungus. Not only has it failed to gain acceptance as a standard test organism (for wood preservative evaluation) in many countries, but is also sometimes excluded from pure research studies when it ought to be an obvious first choice as a representative basidiomycete. This paper discusses some different approaches that have be...
J D Thornton


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


A new process for in situ polymerization of vinyl monomers in wood to delay boron leaching
1998 - IRG/WP 98-40110
Efforts were accelerated on effective use of boron compounds in wood preservation owing to their environmentally safe characteristics and relatively low costs in addition to their well-known high bioactivity and fire resistant properties. Although having these unique favorable properties, they are readily leachable from treated wood at humid conditions. Therefore, they had limited market for exter...
M K Yalinkilic, W Dwianto, Y Imamura, M Takahashi