Surface chemical wood densification through in situ electron beam polymerization: description and dose study
2022 - IRG/WP 22-40933
Traditional wood chemical densification processes can be used to improve wood mechanical properties by increasing density of the material throughout its thickness. While mechanical surface densification has heavily been investigated, surface treatments involving impregnation of monomers remain unexplored. This study describes a new material, surface densified through lateral impregnation of acryla...
J Triquet, P Blanchet, V Landry


Biological assessment of bio-based phase change materials in wood for construction applications
2022 - IRG/WP 22-40935
Solid wood can serve multi-functionality for energy savings in buildings. The study reveals the results of bio-deterioration and degradation of solid Scots pine wood used to incorporate single or multicomponent fatty acid mixtures as bio-based phase change materials (BPCMs). The sapwood samples were impregnated with capric acid (CA), methyl palmitate (MP), lauryl alcohol (LA) and a mixture of coco...
S Palanti, A Temiz, G Köse Demirel, G Hekimoğlu, A Sari, M Nazari, J Gao, M Jebrane, T Schnabel, N Terziev


Comparative study of the properties of silicate coatings with different mineral pigments (titanium dioxide, iron (III) oxide, copper (II) oxide) on the surface of wood
2022 - IRG/WP 22-40936
Silicate coatings are attractive alternatives to conventional organic-based coatings for wood protection. In this work, silicate coatings were prepared with a potassium silicate binder modified with a methyl siliconate solution, and three types of mineral pigments titanium dioxide, iron (III) oxide and copper (II) oxide. The coatings were applied on beech wood and cured under ambient conditions. T...
A M Cheumani Yona, M Petrič


Effect of nano-particle characteristics and concentration on UV protection of timber: A field exposure test
2022 - IRG/WP 22-40941
Wood has a well-known susceptibility to ultra-violet light degradation, leading to premature replacement. A variety of products have been developed to protect against this damage, but most provide less than 12 months of protection and must be regularly reapplied. Developing improved coatings would help reduce wood losses and reduce maintenance costs. Nano-particles have a variety of attractive pro...
T Yi, J J Morrell


The influence of thermal modification and surface charring to different levels on wettability of Norway spruce wood
2022 - IRG/WP 22-40942
The wood can alternatively be protected from water absorption by thermal modification and charring. Both techniques cause certain chemical and physical changes in the wood, the extent of which depends on the level of temperature applied. The objective of this study was to determine how the combination of charring to different levels and thermal modification affects the chemical, morphological, and...
J Žigon, C Gerardin, M E P Wålinder, P Gerardin


Characterization of the fungal communities associated with Aquilaria crassna Pierre ex Lecomte plantations in French Guiana
2023 - IRG/WP 23-11001
Aquilariais a tree species belonging to the family of the Thymeleaceae. When the tree is wounded, it can produce a blackened wood, also known as agarwood. The blackened wood has a darker colour than healthy wood and gives off a strong fragrance greatly appreciated by perfumers and by certain oriental religious communities. Production of this blackened wood is deemed to depend on environmental fact...
C Zaremski, C Malandain, O Sibourg, B Heuclin, N Amusant, M Ducousso, A Zaremski


Accelerated surface mould testing for exterior wood treatment in Temperate, Tropical and Laboratory environments
2023 - IRG/WP 23-20699
Mould attack is a very common cause of discoloration on wooden surfaces and can subsequently promote development of wood decay by other organisms. Prevention of mould growth is relevant for both pigmented wood paints as well as more transparent systems with a high or low amount of binder. The use of commercial biocides has led to effective microbiological inhibition in many contexts, but the incre...
A Nazeri, J Stenbaek, T R Laursen, A H H Wong, B M Hasnul


Starch modified with silanes – high hydrophobic surface treatment for wood protection
2023 - IRG/WP 23-40981
The great potential of silanes for starch modification and their utility as surface wood protection is still not sufficiently assessed. The work aimed to analyze the crosslinking process's effect on starch modification with silane and tested the hydrophobic properties of surface-treated wood. The starch treatment was modified with methyltrimethoxysilane or N-octyltriethoxysilane. SEM-EDX with a cr...
W Perdoch, M Bajstok, B Mazela, I Siemińska, B Peplińska


Characterization of cell wall morphology and water-soluble extractives in Japanese larch decayed by white-pocket-rot fungi
2024 - IRG/WP 24-11034
Porodaedalea chrysoloma (Fr.) Fiasson & Niemelä is a basidiomycete that can cause white-rot decay in Japanese larch (Larix kaempferi) heartwood. P. chrysoloma is a white-rot fungus with a unique pattern that causes white-pocket-rot in the xylem of Japanese larch. However, the mechanism by which P. chrysoloma yields the pattern of white-pocket-rot in Japanese larch heartwood remains unclear. Thus,...
Y Mori, H Arai, T Ito, H Hashitani, K Yamashita, Y Ota, M Kiguchi


Surface treatment of cross-laminated timber to improve water repellency and UV resistance
2024 - IRG/WP 24-20716
Cross-laminated timber (CLT) has emerged as a revolutionary building material, offering a sustainable alternative to traditional construction methods. By layering and bonding multiple layers of wood at right angles, CLT creates a robust and versatile structural element capable of supporting significant loads while promoting eco-friendliness and design flexibility. However, despite its numerous adv...
M Chen, S Uphill, J Hilsenbeck, A Hughes


Natural weathering of modified pine and Eucalyptus woods by surface charring
2024 - IRG/WP 24-30801
Within various wood modification techniques, surface charring is anticipated to extend the lifespan of wooden components in building facades; however, visual deterioration of charred cladding materials has become a notable concern. This study, conducted through international collaboration, aimed to assess the resistance of bio-based facade materials to weathering in the Turkish climate. The natura...
E E Soyturk, E N Kavakli, S N Kartal, C M Ibanez


Physical, durability and chemical characterization of Gmelina arborea (Roxb.) wood treated with lactic acid
2024 - IRG/WP 24-30803
The increase in demand for durable wood has drawn attention to the use of fast-grown plantation species across the globe. Chemical modification was used to treat Gmelina arborea wood with lactic acid for property enhancement. The treated samples were obtained from two different ages of 15 and 10 years and sawn into (20 x 20 x 60) mm and (20 x 20 x 20) mm for physical, durability and chemical chara...
T O Akinwamide, J M Owoyemib, E A Iyiolac


Developing thermal-energy storage systems based on Kraft lignin-glyoxal and organic phase-change material modified wood
2024 - IRG/WP 24-30810
This study investigated the use of modified wood as a thermal-energy storage material through the integration of paraffin-based phase-change materials (PCMs). The objective was to evaluate the influence of Kraft lignin-glyoxal prepolymer on the properties of wood modified with PCMs. The implementation of the modified wood involved preparing PCM emulsions, synthesizing lignin-glyoxal prepolymer, an...
C-F Lin, O Karlsson, D Jones, D Sandberg


A novel treatment for increasing UV stabuility of wood based on citric acid and urea
2024 - IRG/WP 24-30811
Wood, a fundamental material in the Built Environment, faces challenges related to durability and weathering, notably UV degradation leading to colour changes. This study explored a novel treatment method utilising citric acid and urea to enhance the UV stability of wood. The reaction between these compounds forms fluorescent species and insoluble nanoparticles upon thermal treatment. Two treatmen...
S Jué, A Scharf, C-F Lin, R Moutou Pitti, D Sandberg, D Jones