Optimization of oxalic acid production for bioleaching of metal components from CCA-treated wood by an unknown Polyporales sp. KUC8959
2010 - IRG/WP 10-50266
A brown-rot fungus, an unknown Polyporales sp. KUC8959, has recently been identified and proven as a prominent fungal species for bioremediation of CCA-treated wood wastes in our Lab. The fungus produced a larger amount of oxalic acid than other fungi tested, and removed 90 % or more of chromium, copper and arsenic from CCA-treated wood sawdust through bioleaching process. The bioleaching process ...
Yong-Seok Choi, Min-Ji Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Utilization of thermodesorption coupled to GC-MS to characterize volatiles formation kinetics during wood thermodegradation
2012 - IRG/WP 12-40587
Identification of volatile degradation products produced during wood mild pyrolysis is important to have better insight on thermodegradation mechanisms. Previous studies have shown that thermodesorption coupled to GC-MS is an attractive tool to characterize and quantify products formed during wood thermodegradation indicating an higher susceptibility of hardwoods to thermodegradation compare to so...
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Kamdem, P Gérardin


The effect on moisture content of water trapped in wood joints
2012 - IRG/WP 12-40613
To predict the service life of a structure, a model where the exposure of a structure is compared to its resistance can be used. Which exposure and resistance parameters that are relevant depend on which materials the structure consist of. This approach, with an exposure and a resistance parameter, is similar to the one used in structural engineering where a load (exposure) is compared to the bear...
M Fredriksson, L Wadsö, P Johansson


Influence of a pulsed electric field on the growth of surface fungi
2013 - IRG/WP 13-10795
The colonization of mold and staining fungi are not only an aesthetical problem. Blue stain fungi are able to penetrate paint films. Maintenance of coatings on wood are time consuming and costly. A new approach uses a pulsed electric field (PLEOT) in order to protect wood against surface fungi. This technology is evaluated in non-sterile laboratory conditions on different coated and uncoated Scots...
M Starck, A Treu


Surface moulds and staining fungi on acetylated wood – effect of increasing acetyl content
2013 - IRG/WP 13-10797
Wood used in outside applications is susceptible to weathering and photo degradation, which often leads to surface discoloration, loss of brightness and surface deterioration. Research has shown that acetylated wood is more resistant against brown rot, white rot and soft rot, and more dimensionally stable than untreated wood. However, acetylated wood seems still to be disfigured by surface moulds ...
L Ross Gobakken, S Bardage, C J Long II


Characterization of test fields
2013 - IRG/WP 13-20508
Test field characteristics and impact of test fields on wood degradation is important when testing wood protection. The current EN 252 standard has no requirement for knowledge of decay hazards, but most commonly a test field is known as a “brown”,- “white”,- or “soft rot” field. To understand which decay hazard wood preservatives are tested against, each test field should be character...
U Råberg, N Terziev, G Daniel


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


Performance of biocide-free preservative-protective systems modified with organosilicon compounds
2013 - IRG/WP 13-30628
The objective of the research was to determine the influence of organosilicon compounds in preservative-protective systems on the selected properties of pine wood aimed for outdoor use. The investigations were made for biocide-free systems based on alkyd resin and natural oils modified with alkylalkoxy-, amino- and glycidoxysilanes. The special attention was paid on the influence of hydrophobic pr...
B Mazela, P Hochmańska, T Krystofiak


Characterization of wood modification prepared by in situ polymerization with pre-polymer and the mechanism of modification
2013 - IRG/WP 13-40633
Chemical modification of wood is a potential way to obtain high quality wood. In this study, the fast-growing poplar was impregnated with modifier using a pulse-dipping machine by in situ polymerization. Fungal decay analysis, mechanical properties and dimension stability of the natural and modified woods were investigated. The wood samples were also characterized by X-ray diffraction (XRD) Therma...
Qian Lang, Zeng Bi, Junwen Pu


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


Molecular characterization and biodiversity of wood-decaying fungi in French Guiana
2014 - IRG/WP 14-10825
Fungi from tropical regions are currently under-represented in the classification system. Indeed, difficult access to tropical forests and irregular occurrence carpophores make it complicated to study fungus species in such environments, unlike in European zones where fungal diversity and taxonomy are better known. The purpose of this work was to enhance classification by integrating new data that...
A Zaremski, L Gastonguay, C Zaremski, J Beauchene


The Chelator Mediated Fenton System in the Brown Rot Fungi: Details of the Mechanism, and Reasons Why it has Been Ineffective as a Biomimetic Treatment in some Biomass Applications – a Review
2014 - IRG/WP 14-10828
The chelator-mediated Fenton (CMF) reaction requires the action of two types of chelating compounds. The first chelator, oxalate, solubilizes and then sequesters iron, and the second chelator reduces iron. Iron reduction must be controlled near the fungal hyphae to prevent damaging Fenton chemistry from occurring in that location. Similarly, iron reduction must be promoted within the wood/plant ce...
B S Goodell, M Nakamura, J Jellison


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar


Visualization of gold/silver nanostars in wood by surface enhanced Raman spectroscopy
2014 - IRG/WP 14-30653
Nanotechnology is a fast growing up-to-date technology and ventures expeditiously in the wood preservative market. However, there is still a huge lack of understanding about the interaction and incorporation of nanoparticles (NSs) in wood. Surface-enhanced Raman scattering (SERS) offers unique advantages as an analytical tool with a high selectivity and sensitivity without matrix interference. Her...
C Geers, L Rodríguez-Lorenzo, M Placencia Peña, P Brodard, T Volkmer, B Rothen-Rutishauser, A Petri-Fink


VOC-free remedial treatment agent on organic solvent basis with surface cleaning by photocatalysis using titanium dioxide
2014 - IRG/WP 14-40651
Due to the EU Regulations according to the harmonisation of the European market of biocidal products and the EU Regulations regarding emissions of volatile organic compounds in residential properties a new VOC free yet organic solvent based remedial treatment agent is introduced including a potential method to clean up the wooden surface of remaining biocides after a remedial treatment using photo...
H Ahl, J Fromm, P Jüngel, E Melcher, M Pallaske


The effect of UV irradiation on some technological properties of different polyurethane varnishes coated plywood panels from veneers dried at different temperatures
2014 - IRG/WP 14-40661
In this study, the effect of UV irradiation on some technological properties of three different polyurethane varnishes coated plywood panels produced from Scots pine (Pinus sylvestris L.) and Maritime pine (Pinus pinaster L.) veneers manuactured and dried at different temperatures was studied. Accordingly, 32°C log peeling temperature and three different veneer drying temperatures (110, 140 and ...
Ö Özgenç, C Demirkir, Ü C Yildiz, G Çolakoğlu


The role of hydrophobins in surface growth by the Blue Stain fungi Aureobasidium pullulans
2015 - IRG/WP 15-10837
Hydrophobins are small proteins found exclusively in filamentous fungi. These proteins are able to assemble spontaneously into amphiphilic monolayers at hydrophobic–hydrophilic interfaces. Hydrophobins have a diverse role, e.g. allowing the fungi to break through interfaces during aerial hyphae formation, sporulation, fruit body production and cell penetration. In this ongoing study, we are look...
J Stenbæk, L Riber, J Blæsbjerg Nielsen, C Møller Hansen, B Jensen


Effects of UV Radiation on Melanization and Growth of Fungi Isolated from Weathered Wood Surfaces
2015 - IRG/WP 15-10842
This research tests the hypothesis that fungi isolated from weathered wood will respond to elevated levels of UV radiation by increasing their melanin production. To test this hypothesis, we measured the melanin production and mycelial color of Aureobasidium pullulans and Cladosporium cladosporioides, before and after the fungi were grown under artificial UV, visible light and complete darkness. T...
V A Hernández, P D Evans


Acceptance levels of surface disfigurement - tolerance to defects of coated wood
2015 - IRG/WP 15-20564
Service life planning (PSL) has become an important issue in performance based building and substantial progress has been made in recent years. The role of predicting the aesthetical service life of wooden building components has been underestimated for quite long time but is recently attracting more and more notice. It is influenced by numerous factors such as discoloration, fading, flaking, crac...
C Brischke, P Kaudewitz


The effect of preservative treatment on mechanical strength and structural integrity of wood
2015 - IRG/WP 15-30667
The use of wood for demanding construction applications is increasing in Europe. Wooden constructions are frequently designed of susceptible conifer wood, which is endangered by wood decay fungi in wet applications. Therefore in many cases treating wood with preservatives is unavoidable to ensure the desired service life. However, chemical treatment of wood can result in changes of its mechanical ...
M Humar, D Kržišnik, C Brischke