IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 214 documents. Displaying 25 entries per page.


Wet and dry adhesion of coatings on modified and unmodified wood: comparison of the pull-off test and the cross-cut test
2010 - IRG/WP 10-40524
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, thermal modification) on coatings adhesion and to compare two methods of assessing the adhesion: the cross-cut test and the pull-off test both tested in dry and wet conditions. The study also investigates the effect of other parameters of the wood substrates on adhesion like the ring...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, V Georges, S Bollmus


Silicon compounds as additives improving alkyd-based wood coatings performance
2010 - IRG/WP 10-40531
The reactivity of cellulose with solvent-born alkyd-based wood coatings supplemented with organosilanes was analyzed. Structural analysis of cellulose subjected to the reaction with organosilanes and following extraction with water was performed using Fourier-transform infrared spectroscopy (FTIR). The analyzed IR spectra comprise bands 1250 cm-1 typical for the SiC group and 800 cm-1 typical for ...
B Mazela, I Ratajczak, K Wichłacz-Szentner, P Hochmańska


Optimization of oxalic acid production for bioleaching of metal components from CCA-treated wood by an unknown Polyporales sp. KUC8959
2010 - IRG/WP 10-50266
A brown-rot fungus, an unknown Polyporales sp. KUC8959, has recently been identified and proven as a prominent fungal species for bioremediation of CCA-treated wood wastes in our Lab. The fungus produced a larger amount of oxalic acid than other fungi tested, and removed 90 % or more of chromium, copper and arsenic from CCA-treated wood sawdust through bioleaching process. The bioleaching process ...
Yong-Seok Choi, Min-Ji Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Effects of intumescent formulation of vinyl acetate-based coating on flame-retardancy of thin painted red lauan (Parashorea spp.) plywood
2011 - IRG/WP 10-40537
Using intumescent coatings on wood-based materials is an effective method for fire safety. The intumescent coatings consist of four major components: (1) binder resin (BR), (2) carbonizing substance (CS), (3) foam producing substance (FPS) and (4) dehydrating agent (DA). Previous studies have demonstrated that the formulation of the four components strongly influences the performance of coatings. ...
Chih-Shen Chuang, Kuang-Chung Tsai, Te-Hsin Yang, Ming-Kuang Wang, Chun-Han Ko


Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher


Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani


Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin


Comparison of exterior performance of two coating systems based polyurethane applied Pinus sylvestris L. and Picea orientalis L. wood
2012 - IRG/WP 12-40588
Some surface changes in sapwood and heartwood of two species before applying clear-coating were characterized after accelerated weathering time. Wood specimens covered with two types polyurethane (PU) films were also observed in accelerated weathering exposure. In this study, changes on the wood surface were compared of between wood specimens covered with two types polyurethane (PU) films after ir...
Ö Özgenç, Û Cafer Yıldız


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


The effect on moisture content of water trapped in wood joints
2012 - IRG/WP 12-40613
To predict the service life of a structure, a model where the exposure of a structure is compared to its resistance can be used. Which exposure and resistance parameters that are relevant depend on which materials the structure consist of. This approach, with an exposure and a resistance parameter, is similar to the one used in structural engineering where a load (exposure) is compared to the bear...
M Fredriksson, L Wadsö, P Johansson


Protective nanoparticle coating reducing water absorption of wood species
2012 - IRG/WP 12-40614
Nanoparticle coatings were deposited onto different tropical wood samples for controlling the surface hydrophobicity. The styrene(maleimide) nanoparticles were synthesized in aqueous dispersions under pure conditions or in combination with 70 wt.-% palm oil. A first evaluation of the non-coated wood surfaces indicates a high dependence between the water contact angles, the average surface roughnes...
P Samyn, A Paredes, G Becker, H Van den Abbeele, L Vonck, D Stanssens


Influence of a pulsed electric field on the growth of surface fungi
2013 - IRG/WP 13-10795
The colonization of mold and staining fungi are not only an aesthetical problem. Blue stain fungi are able to penetrate paint films. Maintenance of coatings on wood are time consuming and costly. A new approach uses a pulsed electric field (PLEOT) in order to protect wood against surface fungi. This technology is evaluated in non-sterile laboratory conditions on different coated and uncoated Scots...
M Starck, A Treu


Detection of Aureobasidium as the dominant fungus on coated wood
2013 - IRG/WP 13-10796
Wood is often covered with a coating in order to protect the surface. Unwanted dark mold growth on paint covered surfaces in external conditions is a familiar phenomenon. Simple microbial techniques have commonly been used to determine the dominant fungal species present in the discoloured area, for example morphological analysis of microscopic preparations of fungal pieces sticking to an adhesive...
E J Van Nieuwenhuijzen, M F Sailer, R A Samson, O C G Adan


Surface moulds and staining fungi on acetylated wood – effect of increasing acetyl content
2013 - IRG/WP 13-10797
Wood used in outside applications is susceptible to weathering and photo degradation, which often leads to surface discoloration, loss of brightness and surface deterioration. Research has shown that acetylated wood is more resistant against brown rot, white rot and soft rot, and more dimensionally stable than untreated wood. However, acetylated wood seems still to be disfigured by surface moulds ...
L Ross Gobakken, S Bardage, C J Long II


Inhibitory extractives or nutrients? Mould growth on coated heartwood and sapwood of Pinus sylvestris and Gleditsia triacanthos
2013 - IRG/WP 13-10806
Sometimes mould fungi grow over weathered coated sapwood, whereas the coated heartwood is not colonised. Two factors may be responsible for these differences: Either the larger content of nutrients in the sapwood, or the content of biocidal extractives in the heartwood. In this study the factors for the difference in mould growth on coated heartwood and sapwood of Pinus sylvestris (Scots Pine) and...
D Lukowsky, N Buddruhs


Surface energy characterization of thermally modified wood using inverse gas chromatography
2013 - IRG/WP 13-20532
The objective of this work is to characterize surface energetics of thermally modified wood. Such information may be useful for a better understanding and predictions of adhesion properties between the modified wood and other material systems, e.g. coatings, adhesives or matrices in composites. Inverse gas chromatography (IGC) was used to study the surface energy characteristics of thermally modif...
S Källbom, K Segerholm, D Jones, M Wålinder


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


Copper Coating on Wood: a New Way of Protecting Wood
2013 - IRG/WP 13-30617
Thermal spray metal coating technology was used to apply a thin layer of copper on the surfaces of a number of wood species. The adhesion of metal coating to mahogany, oak, soft maple, spruce, white pine and medium density fibreboard (MDF) was evaluated by pull off adhesion test. The resistance of copper coated wood samples to mildew were assessed in the lab. Also, the decay resitance and water re...
M Nejad, R Shafaghi, L Pershin, J Mostaghimi, P Cooper


Performance of biocide-free preservative-protective systems modified with organosilicon compounds
2013 - IRG/WP 13-30628
The objective of the research was to determine the influence of organosilicon compounds in preservative-protective systems on the selected properties of pine wood aimed for outdoor use. The investigations were made for biocide-free systems based on alkyd resin and natural oils modified with alkylalkoxy-, amino- and glycidoxysilanes. The special attention was paid on the influence of hydrophobic pr...
B Mazela, P Hochmańska, T Krystofiak


Study of UV resistance and natural weathering of coatings on chemically modified wood
2013 - IRG/WP 13-40629
In this study, UV resistance and weathering performance of rubberwood (Hevea brasiliensis) and radiata pine (Pinus radiata) modified with benzoyl chloride and acetic anhydride was studied. Performance of polyurethane based wood coatings on modified wood was also evaluated. Unmodified and chemically modified specimens were exposed to accelerated and natural weathering. Modified and unmodified woo...
K K Pandey, K Srinivas


Protective effectiveness of antifouling coatings for wooden boats in the Northern Adriatic Sea
2013 - IRG/WP 13-40634
There are various conventional biocide containing antifouling coatings and some more environmentally friendly paints for boats on the market. However, the question of their performance in accordance with the manufacturers’ statements or guaranties arises. The aim of our preliminary investigation was to state which type of antifouling coating exhibits better effectiveness against fouling organism...
M Petrič, M Humar, J Adamek, B Kričej


Preparation and characterization of activated carbon fibers prepared from liquefied wood
2013 - IRG/WP 13-40636
Activated carbon fibers were prepared from liquefied wood through stream activation. The effects of activation temperature and time on the microstructure and surface functional groups of the liquefied wood activated carbon fibers (LWACFs) were studied using analysis of burning behavior, X-ray diffraction, nitrogen adsorption-desorption isotherms, X-ray photoelectron spectroscopy, and SEM. The resu...
Wenjing Liu, Guangjie Zhao


Previous Page | Next Page