Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Life Cycle Assessment of treated timber: methodological aspects and first results
2009 - IRG/WP 09-50264
Environmental information on products is more and more required as a key to the market, and the building sector in Europe is certainly advanced in that direction. In France, Environmental Product Declarations are becoming very common for construction products. Therefore, the CTB P+ and CTB B+ certification comity as commissioned FCBA to perform the Life Cycle Analysis of treated timber in order to...
E Vial, M Bertrand, C Cornillier, G Deroubaix


Differential response of wood to dry air thermal treatment (DATT) and soy oil thermal treatment (SOTT)
2009 - IRG/WP 09-40446
Thermal treatment is an alternative to chemical modification method which has been used to some extent in improving timber quality. In order to get the maximum benefits possible without compromising the various end-use quality requirements of timber, several possibilities have been and are still being investigated in relation to this technique. Clear wood samples (19 x 19 x 150mm) of kiln-dried re...
L Awoyemi


Microwave Surface Modification of Radiata Pine Peeler Cores for Preservative Treatment
2009 - IRG/WP 09-40453
Radiata pine peeler cores are classified as a by-product derived from the cores of logs left over after the veneer peeling process. The core can be potentially developed for value added solid wood products as it is abundantly available and has a constant diameter. However, the core needs to be preservative treated because of low durability in ground contact. An additional problem is that the wood ...
K Sugiyanto, G Torgovnikov, P Vinden


Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


A fast and economic method to produce grey wooden surfaces for decking and cladding: preliminary results
2009 - IRG/WP 09-40474
Uncoated wood is commonly used in France for cladding and decking to minimise maintenance. However wood surfaces progressively turn grey due to exposure to sunlight and water. This grey colour develops after several months depending on the wood species and the exposure: in the northern hemisphere surfaces facing south and west are most exposed and turn grey more rapidly than those facing north and...
L Podgorski, V Georges, I Garmendia, B Sánchez Sarachu


Qualitative - Quantitative Analysis of Wood-Inhabiting Fungi in External Wooden Structures of the Latvian Cultural Heritage
2010 - IRG/WP 10-10728
The frequency and diversity of wood inhabiting fungi in the exterior wood were established in the Araishi lake fortress, the Lielvarde wooden castle, the Latvian Ethnographic Open-Air Museum, Riga, and twelve wooden heritage objects in the Eastern part of Latvia (Latgale). The inspected wooden structures of the external woodwork included windows, stairs, walls, floorings, roofs, fences, and benche...
I Irbe, M Karadelev, B Andersons


Towards Understanding the Biology of Wood Decay
2010 - IRG/WP 10-10739
Our previous research has focused primarily on ways to identify the wood decay fungi and microbial community. We continue to explore this complex and dynamic community and its interactions through microbial community ecology studies, gene expression interactions and proteomics. However, in order to better understand the mechanisms of fungal decay, we have sequenced the genome of a copper tolerant...
J Tang, K Jenkins, L Parker, S V Diehl


Stress wave and visual analysis of treated and non treated fence posts after 15 years in field test
2010 - IRG/WP 10-20449
Wood preservation may play an important role in protecting tropical rain forest. Basically, it can reduce pressure on natural resources by increasing wood durability. Field tests are conducted to simulate final use of woods under different environmental conditions. Visual analysis, non destructive testing, and non destructive evaluation techniques were applied to assess wood resistance and chemica...
A Florian da Costa, R Faustino Teles, J Costa Gonçalves


Improved analysis of field test data related to service life prediction of tropical wood species
2010 - IRG/WP 10-20458
Long field trials of wood in ground contact give valuable data on the natural durability of the material. The European Standard EN 350 gives guidance on how to perform these durability classification, but is limited to the use of averages of in-service life of a set of specimens compared to a reference set. Starting from a database of visual assessment of field stake testing, it is possible to obt...
J Van den Bulcke, A Wong, Ling Wang Choon, Yoon Soo Kim, J Van Acker


Copper nanoparticles in southern pine wood treated with a micronised preservative: Can nanoparticles penetrate the cell walls of tracheids and ray parenchyma?
2010 - IRG/WP 10-30547
This study tests the hypothesis that copper nanoparticles can penetrate the cell walls of southern pine wood treated with a micronised preservative. We examined the nanodistribution of particles in tracheid and ray parenchyma cell walls using state-of-the-art HR (High Resolution)-TEM and HR-STEM (Scanning Transmission Electron Microscope)-EDX. These devices are capable of atomic-scale resolution. ...
H Matsunaga, Y Kataoka, M Kiguchi, P Evans


Analysis of phenolic extractives from various Tunisian species trees -Study of its potential valorisation
2010 - IRG/WP 10-30552
Phenol extractives are naturally synthesized compounds taken from several trees. It is well demonstrated that the presence of phenol compounds is positively correlated with the durability of wood. This property is very interesting for outdoor uses of wood with a limited treatment. Phenol compounds may also be used in the formulation of glue. In the aim to improve the knowledge on Mediterranean tr...
I Oueslati, F Charrier, K Seffah, A Moubarik, N Ayed, A Zerizer, B Charrier


Comparison of colour change in wood clear-coating systems including inorganic and organic UV absorbers for exterior use
2010 - IRG/WP 10-40499
The aim of this work is to compare the performance of inorganic and organic UV absorbers used in a wood coating application against weathering. Our study has investigated the colour changes of selected UV absorbers; hombitec 402 RM from the Sachtleben Company as an inorganic UV absorber, tinuvin 477 DW from the Ciba Company as an organic UV absorber. The study was carried out on two wood species; ...
Ö Özgenç, B Forsthuber, A Teischinger, C Hansmann


Optimization of oxalic acid production for bioleaching of metal components from CCA-treated wood by an unknown Polyporales sp. KUC8959
2010 - IRG/WP 10-50266
A brown-rot fungus, an unknown Polyporales sp. KUC8959, has recently been identified and proven as a prominent fungal species for bioremediation of CCA-treated wood wastes in our Lab. The fungus produced a larger amount of oxalic acid than other fungi tested, and removed 90 % or more of chromium, copper and arsenic from CCA-treated wood sawdust through bioleaching process. The bioleaching process ...
Yong-Seok Choi, Min-Ji Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Gene expression analysis of a copper-tolerant brown rot fungus on MCQ-treated wood
2011 - IRG/WP 11-10748
Most brown rot fungi are copper-tolerant, which makes them difficult to control with copper-based wood preservatives like MCQ. To better understand what biological processes are regulated, we used our model species, Antrodia radiculosa, to examine expression of genes on MCQ-treated wood. Our hypothesis was genes that decreased copper bioavailability would be up-regulated early, when wood showed ...
J D Tang, A Perkins, S V Diehl


Comparative investigations between thermal and microwave assisted digestion as a novel tool for the chemical analysis of inorganic wood preservative components
2011 - IRG/WP 11-20461
The correct chemical impregnation of wood requires an internal as well as external quality control of the treated wood. The active is located in a solid matrix, therefore it is often difficult to analyse such material since most analytical procedures are based on liquid systems. Because of this quite a number of methods – like extraction or thermal digestion - were developed in order to transfer...
H Ahl, J Fromm, E Melcher


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Classification of wood materials using Fourier Transform Near Infrared Spectroscopy and multivariate analysis
2011 - IRG/WP 11-20471
A distinction between preservative-treated wood and non-treated wood can be demonstrated by the combination of Fourier Transform-Near Infrared Spectroscopy (FT-NIRS) and Multivariate Analysis (MVA). This technique is non-destructive, quick, easy to use and can be portable. The calibration models for different heavy metals are set up using principal component analysis (PCA) to classify species of t...
M A Bouslamti, M A Irle, C Belloncle, V Salvador, S Hulot, B Caron, E M Qannan


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


Slice - Cut and Analyze Laser Microdissection (LMD): A method to produce sample material from modified wood for chemical quality analysis
2011 - IRG/WP 11-20478
Wood modification with its various systems is an established way to enhance a wood products’ service life in outdoor applications. Per definition, selected material properties are enhanced by means of modification without producing toxic substances or residues during service life and combustion afterwards. The systems of impregnation modification include a physical and often chemical alteration ...
K Zimmer, E Larnøy, A Treu, M Fongen


LOSP for glulam, when should the treatment be applied?
2011 - IRG/WP 11-30555
Treatment options for outdoor above-ground (H3) exposed glulam of Pinus radiata and P. elliottii were examined. Beams were treated with azole LOSP (containing a zinc tracer) aiming for retentions of 35-40 l/m3 or 70-80 l/m3. Treatment was conducted either before or after gluing. TBTN LOSP and CCA were included as comparative treatments. Test specimens for exposure were cut after treatment, while w...
L J Cookson


Copper Nanoparticles in Southern Pine Wood Treated with a Micronised Preservative: Nanodistribution of Copper in the Pit Membrane and Border of an Earlywood Bordered Pit
2011 - IRG/WP 11-30566
Copper nanoparticles can penetrate the cell walls of unlignified parenchyma cells in southern pine wood treated with a micronised wood preservative, but they are excluded from lignified tracheid walls. This paper extends these observations to include the cell wall layers of the bordered pit. Focused ion beam and ion milling were used to make an ultra-thin section of the cell wall layers of an earl...
H Matsunaga, Y Kataoka, M Kiguchi, P Evans


Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani


Above Ground Field Evaluation and GC-MS Analysis of Naturally Durable Wood Species
2012 - IRG/WP 12-10764
Nine wood species are being evaluated in above ground field studies in Mississippi and Wisconsin. Candidate naturally durable wood (NDW) species are being rated at yearly intervals for resistance to decay, cupping, and checking. Field ratings after 12 months exposure are presented. To date, Paulownia tomentosa (PAW) and southern yellow pine (SYP) are least durable and cedars are the most durable i...
G T Kirker, A B Blodgett, S T Lebow, C A Clausen


Previous Page | Next Page