Estimation of residual compressive strength on cross laminated timber with biodeterioration damage
2021 - IRG/WP 21-40918
CLT is susceptible to biodeterioration such as fungal decay and termite attack during long-term use for buildings. It is necessary to know the residual strength performance of biodegraded CLT for estimating future performance and aging of CLT. In this study, compression tests of CLT damaged by brown rot fungi and termites were conducted to clarify the relationship between residual strength and mas...
R Inoue, T Mori, K Kambara, W Ohmura


Influence of weathering on the mechanical properties and performance of exterior wood coatings
2022 - IRG/WP 22-40951
Three commercial coatings were exposed to artificial (EN 927-6) and natural weathering (EN 927-3) on wood samples. Cracking was visually assessed as well as Persoz hardness. Free films of the same coatings were also exposed to the same weathering tests before their tensile properties were measured. Results show that artificial and natural weathering modified the overall mechanical properties of wo...
L Podgorski, J-D Lanvin


Make do and mend: Re-using timber in Smithfield Market
2022 - IRG/WP 22-50371
Historic buildings are part of our built environment. They are a record of how construction and use of materials have evolved and provide excellent opportunities for regeneration of urban areas. Moreover, re-using these buildings and as much of the material within, contributes to the Green Revolution. Currently, there is tremendous growth in green construction and as Bob Dylan once said, “the t...
J R Williams


A simple method for assessing the effects of lyctid beetle attack on longitudinal compressive strength of spotted gum sapwood
2023 - IRG/WP 23-20700
Lyctid beetle attack is commonplace in a significant proportion of spotted gum utility poles that are air seasoned prior to chromated copper arsenate (CCA) treatment. While this damage is allowed, there are no reports quantifying the effects of the beetle galleries on pole properties. Full scale testing would require substantial quantities of poles in order to obtain a range of degrees of damage....
M Powell, J J Morrell


Longitudinal tensile shear properties of polyurethane-bonded preservative-impregnated Eucalyptus grandis laminates subjected to varied simulated climatic conditions
2023 - IRG/WP 23-40967
Bonding process adaptations have yielded improvements in the adhesive bonding of Eucalyptus grandis wood for manufacturing hardwood laminates. However, there are still concerns over the adhesive-bond performance, particularly preservative-impregnated E. grandis laminates, under exposure to varying climatic conditions. These concerns could limit the implementation of E. grandis laminates, especiall...
A A Alade, C B Wessels


Estimation of single shear strength performance of screw joints with decayed wood
2023 - IRG/WP 23-40968
In order to use existing wooden structures for a long term, it is necessary to evaluate appropriately the damage degree of bio-deterioration of the structural performance including the members and joint systems. As one for them, it is necessary to estimate more accurate the single shear strength performance of screw joints with decay. Therefore, we proposed the model considering the yield strength...
R Inoue, K Tanaka, T Mori


Effect of incised pattern on flexural strength of CLT
2023 - IRG/WP 23-40993
As a study aimed at developing preservation methods suitable for CLT, investigations have been carried out using “deep penetration treatment”. This treatment method was originally developed as a treatment method for sawn lumber and glulam used as sill members. In the treatment, materials are incised using specially designed blades and immediately sprayed with an oil-based wood preservative. Th...
T Mori, R Takanashi, T Miyauchi, Y Ohashi, S Isaji


Relationships between deterioration part and structural performance in wooden houses
2023 - IRG/WP 23-50376
Based on the survey examples, there are four patterns of deterioration that tend to occur in plywood bearing walls of wooden houses in Japan. The first is a pattern in which wall is in a whole deterioration. It is a no damage wall or test specimen. The second is a pattern in which only the sill is deteriorating. It is caused by moisture or termites from ground to the base. In addition, there is a ...
Y Ota, H Ishiyama, S Okamoto


Manufacturing of bamboo hybrids with high strength, superior fire retardancy, and dimensional stability
2024 - IRG/WP 24-30808
Bamboo, renowned for its rapid growth, high strength-to-weight ratio, and eco-friendly attributes, has found extensive use in decorative building materials and glue-laminated beams. However, the inherent challenges of dimensional instability and flammability in natural bamboo restrict its broad application. This research introduces a range of environmentally friendly techniques aimed at producing ...
W He, Rui Wang, W Li, G Hu, T Singh, Q Fu