IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1715 documents. Displaying 25 entries per page.


Soft Rot Decay of Cengal (Neobalanocarpus heimii) Heartwood in Ground Contact in Relation to Extractive Microdistribution
2003 - IRG/WP 03-10501
The heartwood of cengal (Neobalanocarpus heimii, fam. Dipterocarpaceae) is naturally durable. A square-sawn utility pole specimen of cengal heartwood, after 30 years in ground contact, showed 10-15 mm surface decay all around the ground line position, accompanied with isolated surface termite attack at the decayed region. Light and transmission electron microscopy (TEM) of the decayed regions prov...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi, Kwang Ho Lee


Decay resistance of densified ammonia-plasticized stems of oil palm (Elaeis guineensis)
1991 - IRG/WP 3673
When wafers of oil palm stems (Elaeis guineensis) were plasticized with 28% aqueous ammonia and immediately compressed mechanically, the treated material, gained 73% in basic density (average basic density, 0.695 g/cm³), and was highly resistant to decay by wood rot basidiomycetes. Compared with the control specimens (density, 0.403 g/cm³), resistance to decay of the densified specimens by Corio...
A H H Wong, M P Koh


Dimensional lumber model demonstrates the sensitivity of the particle capture immunoassay in early detection of brown-rot fungi
1995 - IRG/WP 95-20058
A dimensional lumber model was designed to test the sensitivity of the particle capture immunoassay (PCI) compared to traditional methods of culturing and microscopic examination for detection of brown-rot fungi. Southern yellow pine 2 x 4's (5.1x10.2 cm²), and 86.4 cm in length, were inoculated on one end with the brown-rot fungus, Postia placenta, and tested over the full length of the...
C A Clausen, L Ferge


New approaches to practical evaluation method of bio-degradation of wooden construction - Non-destructive detection of defects using radar technique
2000 - IRG/WP 00-20214
There have been a number of researches and developments on the techniques and apparatus for the nondestructive evaluation of the biological deterioration in wood and wooden constructions, such as decay or insect attack in house, public buildings or in historically important architectures. As for the detection of the decay in wood, techniques using sound in audible or in ultrasonic frequency ranges...
Y Fujii, Y Komatsu, Y Yanase, S Okumura, Y Imamura, M Tarumi, H Takiuchi, A Inai


Treatment application method and CCA efficacy in Corsican pine - Assessment by serial exposure and soil burial tests
1993 - IRG/WP 93-40006
A previous report on this research (Newman and Murphy, 1992) identified possible variation in the efficacy of a CCA preservative applied to Corsican pine (Pinus nigra var. maritima) dependant upon the treatment application method (Bethel, Lowry or Steam/Bethel). This paper presents further data from biological testing of CCA treated Corsican pine using serial exposure and unsterile soil techniques...
P R Newman, R J Murphy


Severe decay damages of bridges made of ekki (Lophira alata) wood known as a durable species
2000 - IRG/WP 00-10383
Bridges made of ekki (azobe, bongossi, Lophira alata Banks et Gaertn.) timbers were severely decayed only 10 years after the construction possibly caused from no maintenance for the periods. The reason of no maintenance is due to the misunderstandings on wood durability against wood-decaying fungi. Some civil-engineers and architectures understand "durable species" means "absolutely decay-durable ...
S Doi, T Sasaki, Y Iijima


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


The WOODCARE project: Development of detection methods for Death watch beetle larvae and fungal decay
1999 - IRG/WP 99-20172
Woodcare was a European project coordinated by English Heritage. The aim of the research was to develop more targeted and more environmentally friendly treatment methods for Death watch beetle infections in Oak constructions of historical buildings. TNO has developed two new methods for fast and reliable detection of Death watch beetle larvae and related fungal decay in Oak. The problem with Death...
P Esser, P Van Staalduinen, A C Tas


Durability of surface coating systems. Mycologg - an accelerated mycological test.
2004 - IRG/WP 04-20301
Field testing and natural aging/degradation of test sample, e.g. coated wooden surfaces is a slow process. Accelerated tests focus on mechanical properties, water uptake or sometimes stain fungi. Artificially weathered coated panels are not easily compared with naturally aged panels, and show the importance of involving the biological component among the degrading facors. It is a need for acce...
L Ross Gobakken, J Mattsson, B Jacobsen, F G Evans


Aspects of leaching
1976 - IRG/WP 267
With respect to Document No: IRG/WP/246, and the recommendation that an economic leaching test can be based on a non-changing volume of water (500 ml/block), I would like to relate our experiences with this suggestion. Following 14 days of continuous immersion in de-ionized water it was found that blocks treated with moderate and above concentrations of a preservative gave no problems, but those b...
R S Smith


Biological resistance of wood treated with waterbased resins and drying oils in a mini-block test
1998 - IRG/WP 98-40107
In recent years it was found that the resistance of wood against fungal degradation could be increased by impregnation with an etherificated melamine formaldehyde resin. Using this resin as a reference, a waterbased fatty acid modificated alkyd-resin and two drying-oils were assessed for their biological performance in a mini-block laboratory test. Although drying-oils, like linseed-oil, are often...
M Sailer, A O Rapp, R-D Peek


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Disodium octaborate tetrahydrate, alone and in conjunction with a selected isolate of Trichoderma viride, reduces decay of fresh felled pine independent of the effect of weathering
1994 - IRG/WP 94-10054
Unpeeled billets of Corsican pine were treated with the following: 5% aqueous disodium octaborate tetrahydrate (DOT) solution; 5% DOT solution with an isolate of Trichoderma viride with a low susceptibility to borate; the Trichoderma viride isolate alone. Half of the billets in each treatment group were also placed in large-diameter plastic pipes to protect the billets from the weather. All three ...
M W Schoeman, D J Dickinson, J F Webber


Kiln drying of poles as a means of solving the problems of pre-treatment decay in poles
1985 - IRG/WP 1263
The concept that pre-treatment decay can cause wide variation in the treatability of wood and especially wood poles has caused much discussion and debate in wood preservation circles. Yet it seem only logical that if decay has effected the strength characteristics of the wood and caused a differential moisture content in the wood the treatment of the end product will be highly variable and the lon...
J A Taylor


Occurrence of termite species on decaying heartwood specimens exposed 18 to 23 years at an Australian site
1998 - IRG/WP 98-10270
The occurrence of species of subterranean termites on hardwood and softwood specimens (including preservative-treated), exposed in-ground at a semi-arid site at Walpeup (north-western Victoria), 18 to 23 years after installation, is reported. This paper presents maps of the cumulative occurrence on specimens, after six annual inspections, of the following species: Coptotermes acinaciformis, Hetero...
J W Creffield, J-D Thornton, G C Johnson


Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier


On the laboratory use of X-rays in timber decay evaluations
1981 - IRG/WP 2144
The paper reports the results of laboratory experiments on the X-raying of some Pinus radiata sapwood blocks infected with Serpula lacrymans to determine the effect of density and moisture content on the absorption of X-rays by wood. It is concluded that with increasing moisture content there is a very marked increase in time required to pass a constant quantity of X-rays through a test block and ...
J D Thornton, J W Creffield, O Collett


The wood-attacking insects in wooden houses of an old open air museum in southern Finland
1989 - IRG/WP 1409
Harmful insects of wood in a open-air museum were investigated in 1985-1988 by order of the National Board of Antiquities and Historical Monuments of Finland in nine old log houses. Many thousands of insects and altogether 1073 anobiids (Coleoptera, Anobidae) were obtained by window and light traps. The most common Anobiidae-species were Hadrobregmus confusus (Kraatz) 60.3%, Hadrobregmus pertinax ...
H Viitanen, M Pulkkinen


On the occurrence of Phialophora species in preservative treated wood in ground contact
1977 - IRG/WP 163
Phialophora is a fairly large genus comprising about thirty described species. They are widespread in very diverse environments, such as soil, sea water, wood and wood pulps. Some species are known as parasites on plants and animals, including man. Phialophora species were early known for their ability to produce blue stain in timber. Later it was discovered that several species were able to produ...
T Nilsson, B Henningsson


The long road to understanding brown-rot decay. A view from the ditch
1995 - IRG/WP 95-10101
Interest in understanding how brown-rot fungi decay wood has received increasing interest in recent years because of a need to identify novel targets that can be inhibited for the next generation of antifungal wood preservatives. Brown-rot fungi are unique in that they can degrade holocellulose (cellulose and hemicellulose) in wood without first removing the lignin. Furthermore, they degrade holoc...
F Green III, T L Highley


Assessment of the Inhibition of wood decay fungi by volatile organic compounds identified from Trichoderma spp.
1999 - IRG/WP 99-10302
Previous research identified five volatile organic compounds produced by Trichoderma spp. that may be inhibitory to wood decay fungi. The effects of four of these volatile organic compounds, 2-propanone, 2-methyl-1-butanol, heptanal and octanal were tested over a range of concentrations against four selected wood decay fungi. The fungi were incubated in malt extract broth under appropriate conditi...
S N Humphris, R E Wheatley, A Bruce, C Payne


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 18. Report of seventh inspection (72 months) in Australia
1984 - IRG/WP 4108
This report includes the results for the 72 month inspection of the IRG/COIPM International Marine Test installed in Sydney Harbour. Although, overall, attack by teredinid and limnorid borers have been most commonly encountered in test specimens at this site, slight attack, mainly by sphaeromatids, has recently been initiated on some hitherto unattacked treated Alstonia scholaris and Pinus sylvest...
L J Cookson, J E Barnacle


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


A shower test protocol for measuring antisapstain wash-off from small individual log billets
1996 - IRG/WP 96-50069
According to New Zealand Timber Industry Federation statistics New Zealand exported 4,835,000 m³ of logs in 1994 and it is estimated that c. 20% were anti-sapstain treated. Loss of preservative from logs as a result of rain impact after application is of considerable concern both with respect to potential loss of efficacy and environmental contamination. Whilst Environment Canada have a proposed ...
A J Pendlebury, H Pearson


Bestimmung der pilzwidrigen Wirksamkeit von Holzschutzmitteln gegen Moderfäule-Erreger
1977 - IRG/WP 2125
Ziel der vorliegenden Arbeit war der Vergleich der in verschiedenen Ländern zur Bestimmung der pilzwidrigen Wirksamkeit von Holzschutzmitteln gegen Moderfäule-Erreger angewandten Methoden. Als Vergleichsmaterial dienten drei normierte Methoden: die britische (42), skandinavische (45) und die in der DDR angewendete (47) sowie wichtige, von verschiedenen Fachleuten ausgeführte Arbeiten experiment...
J Wazny