Biochemical relationships between biodegradation of cellulose and formation of oxalic acid in brown-rot wood decay
1991 - IRG/WP 1472
Non-enzymic hydrolysis of cellulose with low concentrations of oxalic acid was examined. The incubation of pine wood pulp with 1% oxalic acid (pH 1.3) at 35°C for 4 weeks reduced the original viscosity to 60%. Reducing sugars were liberated from various cellulosic samples by the oxalic acid treatment. However, crystallinities of cellulose in those samples did not change before and after the treat...
M Shimada, Y Akamatsu, A Ohta, M Takahashi


Accelerated decay tests on DNBP-treated Pinus patula and Eucalyptus grandis
1987 - IRG/WP 3441
Blocks (10 x 10 x 5 mm³) of Pinus patula and Eucalyptus grandis were impregnated to 0, 1.5, 3.0 and 4.5 kg/m³ 2-sec-butyl, 4, 6 dinitrophenol (DNBP). They were monitored microscopically and for weight losses over 16 weeks against monocultures of Coriolus versicolor and Coniophora puteana. Treated ministakes (10 x 10 x 100 mm³) and blocks in soil contact were similarly monitored to determine wei...
L D Abraham, A A W Baecker


A rapid method for collecting large numbers of subterranean termites from wood
1982 - IRG/WP 1165
A corrugated fiberboard trap is described which attracts large numbers of subterranean termites from infested logs. Single-trap collections in excess of 63 grams (wet wt.) for Reticulitermes virginicus (Banks) and 43 grams for Coptotermes formosanus Shiraki were taken one to three days following discovery by termites. If traps are removed from the source logs shortly after beeing attacked, termite...
J P La Fage, N-Y Su, M Jones, T Lawrence


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman


Analysis of D-glucose metabolism of wood decay fungi using 13C-NMR and 13C-labeled substrates
2003 - IRG/WP 03-10475
D-Glucose metabolism is thought to be important during wood decay by fungi, not only for anabolic and catabolic purposes of central metabolism, but also as a potential source of peroxide required by extracellular peroxidases. There has been some confusion in the literature as to whether this peroxide-generating activity is of the glucose 1-oxidase or pyranose 2-oxidase (glucose 2-oxidase) type wi...
T H de Koker, M D Mozuch, P J Kersten


L-joint trials: Part 3: Relative performance of a range of preservative products
2002 - IRG/WP 02-30292
Long-term trials using the L-joints described in BS EN 330 and AWPA Standard E9-97 have been in progress at BRE since 1982. This paper records the current assessments of decay of L-joints in trials started between 1982 and 1994 with treatments applied to both Scots pine sapwood (Pinus sylvestris) and spruce (Picea sp.). Data are provided on a range of active ingredients including TnBTO, PCP, a...
J K Carey


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Preservation of robinia wood (Robinia pseudoacacia L.) stakes by vintners
1982 - IRG/WP 3194
This work discusses decay resistance of robinia wood to fungi Trametes versicolor (L.ex Fr.) Pil. and Coniophora puteana (Schum. ex Fr.) Karst., and also the possibility of influencing its resistance by means of chemical protection. The results showed that natural resistance of robinia wood to these two different agents of wood decay is not the same. It is much less resistant to the fungus Conioph...
R Benko


The natural durability story
1997 - IRG/WP 97-20119
Wood species with superior natural durability were in use since the beginning of timber utilisation. Their importance decreased with increasing industrial timber impregnation. In recent time, however, they gained worldwide new interest due to environmental problems involved with treated timber. In Europe a special Standard (EN 350) has been published and a multinational research project on testing...
H Willeitner, R-D Peek


A technique for assessing the preventive efficacy against decay fungi of preservative treatments applied to wood
1988 - IRG/WP 2309
A method is described in which test blocks with envelope preservative treatments can be challenged by selected test fungi previously established on an untreated feeder block. The progress of the test fungus through the treated zone is monitored using novel baits or sensors inserted in holes drilled into blocks to within predetermined distances of the face being challenged. Preliminary results show...
J K Carey, A F Bravery


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 1: Laboratory screening tests using a filter paper technique
1977 - IRG/WP 290
Thirty-one miscellaneous formulations have been screened using a filter paper assay technique, for their efficacy in controlling the growth of Chaetomium globosum, Cephalosporium acremonium, and a mixed inoculum of finely ground soft-rotted wood obtained from preservative treated transmission poles. The formulations consisted of various organic compounds and inorganic preparations made from differ...
H Greaves


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Statistical evaluation of 'micro-bending' samples for classification of wood attacking fungi
1992 - IRG/WP 92-1544
Micro-specimens from both hardwood and softwood were exposed to selected species of field isolated fungi. The strength reduction and weight loss caused by these fungi were determined. A statistical procedure was then developed to classify the fungi into brown-, white-rot, or non-decay fungal categories based on these data. The procedure reveals the extent of hazard a fungus poses to wood members. ...
B Goodell, Jing Liu, A Homola, J Jellison, J Shottafer


Durability of five wood species against Coriolus versicolor
1992 - IRG/WP 92-1578
The durability of following five wood species Zelkova carpinifolia, Ulmus glabra, Carpinus betulus, Acer trauvetteri and Pterocarya fraxinifolia were studied against Coriolus versicolor under laboratory conditions according to DIN 52176 standards. Zelkova caprinifolia shows a reduction in weight of 2.19%, Ulmus glabra 41.69%, Carpinus betulus 45.64%, Acer trauvetteri 53.05%, and Pterocarya fraxini...
S M Kazemi


Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown


An Australian test of wood preservatives. Part 1: Preservatives, principles and practices
1978 - IRG/WP 2123
Between November, 1963, and July, 1964, a graveyard test of some 6000 preservative-treated stakes was installed at 8 sites equally distributed between Papua New Guinea in the tropics, through Queensland and New South Wales to Victoria. More than 40 different preservatives and preservative mixtures, mostly at several different levels of retention, were used to impregnate sawn specimens of Pinus rad...
J Beesley


Analysis of water repellents in wood treated with water borne formulations using FTIR
2000 - IRG/WP 00-40176
The use of aqueous water repellent emulsion formulations has increased significantly in the wood treatment industry. These products are primarily used to enhance the weathering characteristics of wood products treated with water borne preservatives systems used in exterior above ground applications. They are also used in pole treatments to improve climbing characteristics and in low VOC millwork t...
P J Walcheski, L Jin


SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown on inert surfaces
1997 - IRG/WP 97-10194
A range of wood inhabiting and wood decay fungi have been studied for their production of extracellular mucilage when grown on inert surfaces, for comparison with their growth on wood. The species tested were: Coniophora puteana, Coriolus versicolor, Chaetomium globosum, Trichoderma harzianum, Ceratocystis coerulescens, Ophiostoma piceae, Mucor sp. and Penicillium sp. They were grown on plastic me...
A R Abu, R J Murphy, D J Dickinson


The practice of using concrete on wood piling for marine use in Thailand
1982 - IRG/WP 492
The practice of using concrete on wooden poles has been carried on in Thailand for a long time in pile-houses and pier constructions which have been situated in, or partly in the sea. In such instances, the hewed round and/or square-sawn heartwood poles of naturally durable timber species have been coated with concrete of about 5 to 10 cm or more in thickness, and to about 100 cm above the highest...
B Anuwongse


Utilization of nitrogenous substance by Serpula lacrymans
1989 - IRG/WP 1397
When Serpula lacrymans degrades wood, the fungus is considered to have to assimilate nitrogen, which is not abundant in the wood, from the third material. The strands/mycelium has grown into the soil under the floor of the wooden house damaged by the dry rot fungus. The authors analyzed the soil samples collected from the ground under the floors of the dryrotted houses. The samples which were coll...
S Doi, I Togashi


Oxalic acid quantification, oxaloacetase assay and ESI localization of P, C, and Fe from the brown rot fungus Postia placenta
1994 - IRG/WP 94-10063
The mechanism by which brown-rot fungi initiate depolymerization of holocellulose in wood remains unknown. Recently, oxalic acid (OA) has received considerable attention in cellulose breakdown by brown-rot fungi. The OA could serve as a proton donor for hydrolytic or an electron donor for oxidative (Fenton's reaction-H2O2/Fe2+) cleavages of cellulose. The acid may originate via oxaloaceta...
C R Jordan, W V Dashek, T L Highley


Report on the co-operative leaching tests
1975 - IRG/WP 246
The Work reported here was undertaken at the request of CEN to see (1) whether the standard beaker leaching method under discussion at CEN, and based on the German DIN could be made less labour intensive; and (2) whether the leaching parameters could be expressed in more general terms so that alternative procedures could be used. A co-operative experiment was set up in which the amount of leaching...
J W W Morgan


Isolation of soil borne bacteria and fungi from treated timber
2001 - IRG/WP 01-50174
Most research in the last few decades has focused on the development of new strategies to control biological attack and the means to quantify this. Comparatively little work has been done to examine the effect that treated timber might have on its surrounding environment. This presentation will describe a methodology that attempts to detect any changes which might occur in the soil microflora foll...
I Stephan, A Stegemann, G Heidrich


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 21: Report of eighth inspection (7 years) in Australia
1985 - IRG/WP 4119
This report tabulates the seven year (86 month) inspection results, obtained on 28 Fabruary l985, of the IRG/COIPM International Marine Test at Goat Island, Australia. This test was installed in December 1977. The results are given in Tables 1-6. Table 7 lists the number of marine borers identified from blocks (2 cm and 6 cm long respectively) cut from the ends of specimens removed at the previous...