Your search resulted in 717 documents. Displaying 25 entries per page.
Interactions between water-borne preservatives and emulsion additives that influence the water repellency of wood
1991 - IRG/WP 2374
Incorporation of non-polar additives into water-borne treatments through of emulsion technology can greatly improve the physical characteristics of wood in service. Of specific interest with these emulsions is their effectiveness in reducing the rate of wood swelling. We have observed that the presence or absence of preservatives can often significantly influence the resultant effectiveness of the...
A R Zahora
Design of a laboratory method for evaluating the effectiveness of soft rot preservatives
1988 - IRG/WP 2312
This purpose of this work was to design a method which makes it possible to evaluate the effectiveness of products which present protect wood against soft rot, using new products·of a different nature, on wood of·Pinus sylvestris L. and Fagus sylvatica L., and which, suitably applied, avoid big economic losses deriving from lack of knowledge of the active principles suitable to present protect w...
M T De Troya, A M Navarrete
CCFZ, a new type of water-borne wood preservative for vacuum pressure impregnation
1991 - IRG/WP 3643
By combination of CCF-Salt types with zinchexafluorosilicate a remarkable improvement of efficacy is achieved. In the same time the ecotoxicoligical data become more save. As well as the efficacy against wood-destroying organisms (Basidiomycetes, Soft rot and Long horn beetle) the basic data to evaluate the ecotoxicological behaviour of a CCFZ-Salt are described and compared with the properties of...
W Metzner, D Seepe, H-W Wegen
Preliminary pole treatment trials with chlorothalonil in hydrocarbon solvent
1994 - IRG/WP 94-40027
A series of 460-mm long, end-sealed southern pine pole stubs were treated with chlorothalonil in hydrocarbon solvent. Over sixty sections were treated using various combinations of initial seasoning (kiln-drying, steam-conditioning), treating temperature (ambient, 200°F), initial air pressure, and final conditioning (steam flash + vacuum, expansion bath + vacuum, steam distillation + vacuum). Dis...
H M Barnes
The effect of oil-borne preservative treatments on the shear strength of FRP/wood composite adhesive bonds
2003 - IRG/WP 03-40265
Reinforcement of structural wood components with Fiber Reinforced Polymer (FRP) will enhance the beam’s strength, but actual data on long-term durability is sparse, not well documented or not readily accessible. In this study, bond properties of FRP-wood composite materials were investigated following treatment with creosote or copper naphthenate preservatives. The properties investigated inclu...
B Herzog, B Goodell, R Lopez-Anido
Application of paint primers after light organic solvent preservative treatment
1986 - IRG/WP 3381
The application of three alternative paint primers is investigated, including a slow-drying oil-based primer, a fast-drying oil-based primer, and a fast-drying water-based primer. The treatment schedules employed, in particular the evacuation period after treatment, have a marked effect on subsequent paintability. Priming can potentially be carried out immediately after treatment with approved Tim...
P Vinden
Soft rot in heartwood of preservative-treated pole stubs of Eucalyptus cypellocarpa L. Johnson
1983 - IRG/WP 1204
Pole stubs of Eucalyptus cypellocarpa L. Johnson, treated in the sapwood with certain waterborne preservatives and exposed for 21 to 23 years in a dry tropical region were severely soft-rotted in the heartwood, as well as the sapwood. They broke with a brash fracture when stress tested (loaded as a cantilever) in the field. The severe soft rot in the heartwood was not detected by the knife test or...
J E Barnacle, G C Johnson, M A Tighe
Efficacy of a novel copper-based organic solvent preservative in laboratory and fungus cellar tests
1995 - IRG/WP 95-30071
The efficacy of Chemicca 4, a novel copper-based organic solvent preservative, was compared with that of other LOSP in pure culture laboratory decay tests and with that of CCA and TBTO in a fungus cellar exposure. It was markedly superior to copper and zinc naphthenates at equivalent metal retentions in laboratory decay tests, and similar in activity to TBTO. After 60 months' fungus cella...
M E Hedley, P N Maynard
Growth and succession of mould on commercial paint systems in two field sites
2007 - IRG/WP 07-30421
Discolouring fungi reduce the service life of coated wooden claddings in façades and increase the total cost of ownership due to shorter maintenance intervals. It is of major importance to find paint systems for wood which are durable and have a high resistance to mould growth. A total of 15 paint systems from 9 different manufacturers were exposed on two field sites, Sørkedalen and Birkenes, ...
L Ross Gobakken, K M Jenssen
Preservative treatment of Golla cane (Daemonorops jenkinsiana) by pressure process
2007 - IRG/WP 07-40379
The feasibility of preservative treatment of golla cane (Daemonorops jenkinsiana (Griff) Mart). by pressure process has been studied using water borne preservatives CCB (copper-chrome-boron). Cane samples of three different lengths 1m, 2m and 3 m. were treated at different pressure and time period to evaluate the extent of penetration and retention of preservative chemicals. It was observed that t...
K Akhter, M Hoque Chowdhury
VOC-free remedial treatment agent on organic solvent basis with surface cleaning by photocatalysis using titanium dioxide
2014 - IRG/WP 14-40651
Due to the EU Regulations according to the harmonisation of the European market of biocidal products and the EU Regulations regarding emissions of volatile organic compounds in residential properties a new VOC free yet organic solvent based remedial treatment agent is introduced including a potential method to clean up the wooden surface of remaining biocides after a remedial treatment using photo...
H Ahl, J Fromm, P Jüngel, E Melcher, M Pallaske
A non-VOC approach of solvent-based wood preservatives for remedial treatment
2016 - IRG/WP 16-30681
Solvent-based wood preservatives are the workhorses in the field of remedial treatment. Due to new European regulations on the indoor air quality there is an increasing pressure on the VOC-content on these solvent-based product types. The transfer of these European regulations into national law is left up to each European member state and handled in different ways. E.g. France has introduced a VO...
M Pallaske, S Hellkamp, P Jüngel
Relative efficacy of various oxine copper formulations against brown-rot fungi
2019 - IRG/WP 19-30741
This paper investigates the relative resistance of three different oxine copper formulations (oil-borne, water-borne, water-borne with pH-adjustment) as a preservative treatment for wood against brown-rot fungi. Impregnated southern pine sapwood cubes were exposed to R. placenta and G. trabeum cultures in a soil-block test. After eight weeks, the weight losses of the cubes were examined in relatio...
M Petruch, J Lloyd, A Taylor
Adhesion durability of the thinnest CLT in Japan treated by solvent recovery system
2019 - IRG/WP 19-40882
The purpose of this study is to clarify the adhesion durability of the thinnest CLT (36 mm thickness) in Japan impregnated with preservatives (azole neonicotinoid compounds (AZN)) under solvent recovery system so called “dry pressure process” for long-term durability. The adhesion durability tests were conducted in accordance with the Japanese Agricultural Standard (JAS) of Cross-Laminated-Tim...
K Kawakami, W Ohmura
Alternative products enhancing dimensional stability comparing to conventional treated products in Japan
2019 - IRG/WP 19-40885
The Act on the Promotion of the Utilization of Wood in Public Buildings (2010) in Japan has made a new stream of the utilization field of timber from housing constructions to larger scale non-housing constructions. After the act, the performance of dimensional stability in preservative treated products becomes more important factor than before. Therefore, various technologies have been developed, ...
K Yamamoto, D Tezuka, Y Sugai, S Maeda, I Momohara
Preliminary investigation for preservation method of CLT using non-pressure treatment
2021 - IRG/WP 21-40919
Cross-laminated Timber (CLT) is increasingly being used in residential and non-residential construction around the world, and some of these areas are at high risk of biodeterioration. Addition to moisture management of construction, preservative treatment of CLT may be needed to prevent decay and termite attack in the area. Pressure treatment being most reliable, is not feasible due to the large d...
T Miyauchi, Y Ohashi, J Miyazaki, R Takanashi, H Shibui, S Isaji, T Shigeyama, Y Sugai, A Yamamoto, T Hramiishi, T Mori, H Matsunaga
Treatability of South African-grown Eucalyptus grandis with water-borne copper azole and disodium octaborate tetrahydrate wood preservatives
2021 - IRG/WP 21-40920
This study investigated the treatability of the sapwood and heartwood of sawn Eucalyptus grandis with copper-azole (CuAz) and disodium octaborate tetrahydrate (DOT) water-borne preservatives towards improving its durability for enhanced use in structural solid wood applications. The results obtained showed that, at a moisture content of 12 ± 1%, sawn E. grandis sapwood can be impregnated to a mea...
A A Alade, Z Naghizadeh, C B Wessels
Influence of plasma treatment on the coatability of wood primer with a topcoat for exterior use
2025 - IRG/WP 25-30828
The coatability of oil, or of solvent-borne alkyd resin wood primers with waterborne acrylic finish is the subject of much debate, but not much information can be found in the scientific literature on this topic. The aim of our study was therefore to evaluate the adhesion strength of the waterborne acrylic coating on oiled wood or wood with a solvent-based alkyd primer and to test the recoatabilit...
M Petrič, L Albreht, N B Štrus, E Keržič, M Pavlič, J Žigon, S Dahle
Effect of biodiesel-containing solvents on the performance of Copper Naphthenate and Pentachlorophenol: 118-month assessment and depletion analysis
2025 - IRG/WP 25-41022
Solvent systems are incredibly important in determining the performance of oilborne wood preservative systems and they can cause early failures in commodities treated with an otherwise effective preservative system. It is important to assess new solvent performance with oilborne preservative systems to ensure these systems continue to function with the changes. One solvent/preservative combination...
J Cappellazzi, M J Konkler, J J Morrell, C S Love, G Presley
Durability evaluation of outdoor-exposed CLT treated with various wood presevatives using CT scans
2025 - IRG/WP 25-41035
Methods for wood preservation treatment of large materials such as Cross Laminated Timber (CLT) are limited. It is unclear which wood preservation treatment methods can effectively protect CLT from rot risk. In this study, accelerated rot tests (fungus cellar test) of CLT treated with the solvent-borne wood preservative by non-pressure treatment, named ‘deep penetration treatment’, were conduc...
Y Sakurai, T Shigeyama, Y Sugai
Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh
Solvent drying and preservation of timber
1977 - IRG/WP 381
Processes which combine drying and preservation are first reviewed. Some preliminary experiments are then described in which blocks of green Sitka spruce sapwood were immersed, in a solution of tributyltin oxide (TBTO) in methanol at 60°C. Satisfactory penetration of the preservative and exchange of methanol and water occurred in a few hours. The methanol was removed rapidly from the wood by evap...
J A Petty
Status of the research and development of a new preservative system (EFPL) for pressure treatment of spruce in Canada
1975 - IRG/WP 348
Our work has been to develop a system which would have the stability of the ACA system and the formulation flexibility of the CCA system enabling properties such as fixation of arsenic, water repellency, appearance and cost to be controlled. Our permeability studies of spruce using a method previously developed indicated that an ammoniacal solution of copper arsenate is an excellent candidate for ...
J Rak, M R Clarke
IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 2: Report of treatment and installation in Australia
1978 - IRG/WP 440
The purpose of this test and the procedures to be followed have been fully set out in documents distributed by the International Research Group on Wood Preservation and numbered IRG/WP/414 and IRG/WP/420. The prescriptions set out in these two documents have been closely followed....
J Beesley
Field test evaluation of preservatives and treatment methods for fence posts
1985 - IRG/WP 3347
This work presents the field test results after fifteen years exposure of Eucalyptus saligna fence posts treated with six different preservatives and five treatment methods. All the combinations with oil-borne preservatives presented the best results and among the waterborne preservatives, the fence posts treated by immersion method were with the lowest performance in the field test....
G A C Lopez, E S Lepage