IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3358 documents. Displaying 25 entries per page.


X-ray analysis of selected anatomical structures in copper/chrome/arsenic treated wood
1973 - IRG/WP 320
Application of analytical electron microscopy to problems in wood preservation has been very limited. Indeed, less than ten workers appear to have published their results using the technique, and of these' only two papers deal with energy dispersion procedures in the scanning electron microscope; the others employ the more familiar wavelength dispersive methods of the electron probe....
H Greaves


The potential of 2-deoxy-D-glucose as an active ingredient in wood preservation
1999 - IRG/WP 99-30205
2-deoxy-D-glucose (2-DOG) is a potential active ingredient against wood decaying fungi. When dissolved in water, it can be used in pressure treatment of wood. Thereby the wood is protected from attack by wood decaying fungi. A concentration of 1.5% (mean retention 9.7 kg/cubic meter sap-wood) is adequate for brown rot fungi, and 3% (mean retention 19.5 kg/cubic meter sapwood) will also provide protection against white rot fungi. 2-DOG is easily soluble in water, and is therefore easily leached from the wood upon completion of the preservation process. Different types of fixa-tion methods have been tried and evaluated. It is possible to produce 2-DOG by the hydrolysis of chitin, a constituent of the exterior skeleton of shellfish and insects. There is a potential for exploita-tion of this waste product provided by the crab and shrimp industry. The yield of 1 kg of fresh shrimp is 75 g of 2-DOG.
O V Frederiksen, A P Koch


Kinetic modelling of adsorption of quaternary ammonium compounds by Scots pine wood sawdust (Pinus sylvestris L.)
2005 - IRG/WP 05-30369
The adsorption of new quaternary ammonium compounds from aqueous solutions onto Scots pine wood (Pinus sylvestris L.) sawdust was studied. The pseudo first- and second- order kinetic models were used for the mathematical description of the sorption dynamic process of QACs onto wood. The highest correlation coefficients were obtained for the pseudo-second order kinetic model, those suggest that che...
J Zabielska-Matejuk


Specific gravity and moisture content of particleboards treated with various chemicals
2005 - IRG/WP 05-40310
The aim of the study was to investigated the effects of particleboard treated with various chemical substances on specific gravity and moisture content The wood raw material used in the experiments were the mixture of coniferous wood [70%, Pinus brutia Ten., Pinus nigra Arn (Lamb.), Cedrus libani Ait.] and black poplar (30%, Populus nigra L.). In this mixture, barks have been accepted up to 5 per...
Ü C Yildiz, A A Var, H Kalaycioglu, S Yildiz


Differences in feeding activity among colonies of Formosan subterranean termite Coptotermes formosanus Shiraki
1983 - IRG/WP 1202
Feeding activities of 7 colonies of the Formosan subterranean termite, Coptotermes formosanus Shiraki, were examined. Wood-consumption rates among colonies differed significantly, ranging from 23.80-78.48 mg/g/day. This large intraspecific variation raised a question of whether differences in feeding activity reported for other termite species were due to interspecific differences. When rates were...
N-Y Su, J P La Fage


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Questionnaire on university instruction in the subject of wood preservation
1977 - IRG/WP 79
J Wazny


Inventaire des "déchets" ou produits connexes de la filière bois
1993 - IRG/WP 93-50001-33
G Marcotte


Final draft of a monographic card for Pole Fungus A, L Harmsen, Rigidoporus vitreus (Fr.) Donk according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 178
L Harmsen


Wood preservatives ecotoxicology on Gammarus pulex (L.) - toward an environmental monitoring method and a getting rid of pollution process
2005 - IRG/WP 05-50224-9
Wood preservatives can have a strong impact on freshwater invertebrates when used close to aquatic ecosystems. It has been reported in Jura that different arthropod taxa, specially crustaceans, have disappeared along several kilometers downstream from factories using insecticides and fungicides as wood preservatives. The crustacean Gammarus pulex (L.) is a relevant bioindicator to characterize th...
O Adam, F Degiorgi, G Crini, P-M Badot


The rate of redistribution and loss of leachable preservatives under service conditions
1993 - IRG/WP 93-30026
This paper describes experiments carried out to determine patterns of preservative redistribution and any associated losses which occur when wood containing unfixed water-soluble wood preservatives is exposed to service conditions where leaching is possible. Scots pine sapwood treated with disodium octaborate was used as a model system. Results are recorded and discussed for trials representing pa...
R J Orsler, G E Holland


The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell


Biodegradation of creosote/naphthalene-treated wood in the marine environment
1977 - IRG/WP 428
The present study was undertaken to determine the biodegradability of marine grade creosote and selected components, including naphtalene, and to determine the effectiveness of (up to 40%) creosote in protecting wood from microbial attack. Also, the impact(s) of creosote and naphtalene-enriched creosote on the microbial ecology os estuarine environments was examined....
P A Seesman, R R Colwell, A Zachary, A J Emery


Safety technique in wood preservation
1974 - IRG/WP 54
S N Gorshin, I G Krapivina, B I Telryatnikova


Framework document for an international code of good practices for wood preservation and wood protection (anti-sapstain) facilities
1992 - IRG/WP 92-3683
At the Kyoto meeting, the Health & Safety committee agreed to form a task force to prepare a global plan for writing a code of good practices (Code) for wood protection and preservation facilities (Doc. No. IRG/WP/3681). The Canadian document had been presented to the IRG group earlier (Doc. No. IRG/WP/3447) and similar documents were solicited from other countries for preparing a framework do...
V N P Mathur, G Das


Above ground testing of wood preservatives - some experiences from Sweden
1995 - IRG/WP 95-20079
Field stake tests for the evaluation of wood preservatives have been used for more than 50 years in Sweden. In the Nordic countries a system for approval of wood preservatives, which includes field test, has also been in operation for more than 25 years. This system has been described in an IRG Document by Henningson & Jermer (1988). The Nordic system is now in a process of harmonization with ...
B Henningsson, Ö Bergman


Information from COIPM Wood Group
1985 - IRG/WP 4120
During the last COIPM Meeting (which took place in Athens, Greece in September 1984) the Wood Group met and discussed the co-operative work 'Durability in sea-water of wood with plastic wraps and wood treated with polymere'....
A Gambetta


The Sixteenth Report of the International Research Group on Wood Preservation 1986-1987
1987 - IRG/WP 5283
R Cockcroft


Bacteria and wood. A review of the literature relating to the presence, action and interaction of bacteria in wood
1971 - IRG/WP 101
S E Rossell, E G M Abbot, J F Levy


Bibliography: Interactions of wood preservatives with wood, metals, glues, paints and concretes
1983 - IRG/WP 3271
H Becker


Effects of the anaerobic wood decay bacterium Clostridium xylanolyticum on unbleached Pinus and Eucalyptus pulp
1991 - IRG/WP 1506
Clostridium xylanolyticum has been shown to produce extracellular enzymes capable of degrading wood. The present work was conducted to quantify growth on various lignocellulosic substrates and degradation of pulped wood fibre. In the latter tests Clostridium xylanolyticum was incubated at 35°C under anaerobic conditions in a medium containing 0.2% (w/v) peptone and 4% (w/v) unbleached Pinus and E...
G D Shelver, U Matai, W Van Wyk, A A W Baecker


Decay resistance of resin treated wood
1999 - IRG/WP 99-30206
Selected natural resin systems were evaluated for their potential as wood protecting agents according to standard test procedures. As indicated by the European standard EN 599 both a Basidiomycete test according to EN 113 and a ENV 807 soil bed test were carried out. Six resin treatments were tested using 3 concentration or treatment levels. Using the biocidal activity criteria as usually applied ...
J Van Acker, A J Nurmi, S M Gray, H Militz, C Hill, H Kokko, A O Rapp


Wood decay in Danish buildings
1985 - IRG/WP 1261
At Technological Institute identification of fungi and advisory activity concerning repair of damages has taken place since 1935. Statistical analyses based on material from 1982 and 1983 are compared to earlier investigations worked out by L. Harmsen. The material shows that building traditions influence the diversity and frequency of fungal species. Many fungal damages in the last decade have sh...
A P Koch


Monographic information on Serpula (Merulius) lacrymans (Schum. ex Fr.) S. F. Gray according to the "Model Questionnaire forpreparation of monographic cards for wood-destroying fungi"
1975 - IRG/WP 133
J Segmüller, O Wälchli


The influence of building design on wood decay
2000 - IRG/WP 00-10339
The cheapest and most effective way to prevent wood decay is to KEEP THE WOOD DRY! You and I know that, but we often forget and attempt a preservative solution to a problem better solved with good design and construction. It's also the answer to a frequently missed exam question in my Architecture class. Just as caulking is a poor substitute for proper design, so preservative treatment sh...
W W Wilcox


Previous Page | Next Page