Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Wood preservative obtained by recycling – preliminary selection of leaching inhibitor
2008 - IRG/WP 08-50252
Based on recycling of used household batteries, a process was developed to enable the recovery of major manufacturing components, leading to a solution of zinc (32 g.l-1) and manganese (15 g.l-1) salts, free of heavy metals. The potential use of the above solution as wood preservative was demonstrated by means of assays both of fungicidal activity -using white and brown rot fungi- and of insectici...
C Ibáñez, C Mantero, G Cecchetto, M Rabinovich, M Cerdeiras


Categorization of 300 timber, bamboo and cane grown in Bangladesh based on their families, origins, growths, physical and mechanical properties
2009 - IRG/WP 09-10684
In this study the 300 timber, bamboo and cane plants grown in Bangladesh have been classified into various categories based on their taxonomic families, origin of species, rate of growth, color of wood, texture of wood, shrinkage of wood, equilibrium moisture content (EMC) of wood, flammability of wood, cutting and sawing properties of timber, finishing and polishing qualities of wood, machining p...
A K Lahiry


Durability and fungal colonisation patterns in wood samples after six years in soil contact evaluated with qPCR, microscopy, TGA, chitin- and ergosterol assays
2009 - IRG/WP 09-20402
There is a need to establish new objective and sensitive methods for early detection and quantification of decay fungi in wood materials. Molecular methods have proven to be a useful tool within wood protection issues, however, this field is still poorly explored and so far relatively few have used these methods within the field of wood deterioration. Among the techniques used in the indirect quan...
A Pilgård, G Alfredsen, I Børja, C Björdal


Copper to quat ratio in alkaline copper quat (ACQ) wood preservative - Effects on fixation and leaching of preservative components in red pine
2009 - IRG/WP 09-30496
This study investigates the effect of the relative proportion of copper oxide (CuO) to didecy dimethyl ammonium carbonate (DDACb) in an alkaline copper quat (ACQ) formulation on the rate of copper fixation or stabilization and the resistance of treated wood to leaching of copper and quat (DDACb). Red pine samples were treated with ACQ, having CuO to DDACb ratios of 2:1 (the normal ratio for ACQ-D...
S Pankras, P A Cooper, T Ung, L Awoyemi


A theoretical-industrial correlation and perspective on copper-based wood preservatives - a review of thermodynamic and kinetic aspects on copper-wood fixation mechanism
2009 - IRG/WP 09-30499
Copper was and it will continue to remain one of the key active component in wood protection industry. Over the past decades, a significant effort from R&D teams in industry, academia and research institutes was directed toward understanding the copper-wood fixation mechanism, optimising the copper retentions in the wood and reduce leaching in order to maximized performance, prolong the lifetime o...
R Craciun, M Maier, J Habicht


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Factors affecting sodium hypochlorite extraction of CCA preservative components from out of service treated wood for recycling
2009 - IRG/WP 09-50263
Significant amounts of chromated copper arsenate (CCA) treated wood products such as utility poles and residential constructions remain in service. There is an increasing public concern about environmental contamination from CCA treated wood when it is removed from service for reuse or recycling, placed in landfills or burned in commercial incinerators. In this paper, we investigate the effects of...
E D Gezer, P A Cooper


Microwave Surface Modification of Radiata Pine Peeler Cores for Preservative Treatment
2009 - IRG/WP 09-40453
Radiata pine peeler cores are classified as a by-product derived from the cores of logs left over after the veneer peeling process. The core can be potentially developed for value added solid wood products as it is abundantly available and has a constant diameter. However, the core needs to be preservative treated because of low durability in ground contact. An additional problem is that the wood ...
K Sugiyanto, G Torgovnikov, P Vinden


Biological Performance of Boron-based Chemicals Treated Wood Composites
2009 - IRG/WP 09-40464
In this study, the biological performance of wood-based composites panels treated with boron containing chemicals against to a fungus was determined. Boric acid, borax, zinc borate and agricultural borate (Tarım-bor™), developed and patented by National Boron Research Institute, were mixed with wood chips or fibers and then particleboard, medium strand board and middle density fiberboar...
Ü C Yıldız, H Kalaycıoğlu, S Yıldız, A Temiz, E Tomak Dizman, A Çavdar Dönmez


Extensive review of fire-retardant wood composites researches
2009 - IRG/WP 09-40471
The increased demand for public safety has led to greater interest in fire retardant materials in the recently years. Legislation relating to safety in the home, in work locations, on transport facilities and in public places continues to produce new regulation. There is average 524 thousand structure fires occurred every year in US, 3757 civilian in death, about 20 thousand civilian in juries, di...
Zhilin Chen, Zhiyong Cai, Feng Fu


Progress in Fire-Retardant Research on Wood and Wood-Based Composites: a China Perspective
2009 - IRG/WP 09-40476
The fire retardant research on wood and wood-based composites, which was carried out in China in the past two decades, was reviewed with 55 references. While many kinds of fire retardants for wood and wood-based composites have been studied, the mainstream is still the compound or the mixture containing phosphorus, nitrogen and boron elements, which can be used in the form of water solution in th...
Wang Qingwen, Wang Fengqiang, Hu Yunchu, Li Jian


Microscopy evaluation of microbial decay patterns in wood stakes after 6 years in soil contact
2010 - IRG/WP 10-10715
Most studies on wood modification have so far been concerned with service life predictions rather than investigating the decay protection mechanism. Very little is known about the mode of action of these new treatments and about the strategies used by wood degraders in order to utilize the wood material despite a treatment. Access to such knowledge would allow further modification and improvement ...
A Pilgård, C G Björdal


Seasonal shifts of fungal community structure at the interface of treated or untreated wood and soil
2010 - IRG/WP 10-10721
Many wood species are degraded rapidly in soil by the fungal community. In order to preserve wood and structures in which it is used, chemical preservatives are used. Little is known about the interaction of treated wood and the surrounding soil fungal community. For this work, presented at IRG 41, wooden specimens (Pinus sylvestris sapwood, sizes 25 mm x 50 mm x 500 mm (longitudinal)) were treate...
M Noll, I Stephan


Determination of a fixation time of wood preservatives: A discussion paper
2010 - IRG/WP 10-20436
The intention of that paper is to initiate a discussion on the basis of a French method in combination with a German approach regarding the need of a method for the determination of a fixation time and especially to obtain input as well as ideas concerning a possible test design. Since no harmonised European approach exists up to now concerning the determination of a fixation time, CEN TC 38 (2009...
E Raphalen, E Melcher


DNA-based tools for rapidly detecting, quantifying and monitoring ophiostomatoid fungi on beetles, in trees and wood products
2010 - IRG/WP 10-20450
Approximately half of the trees harvested for commercial purposes are lost because of native or introduced insects or insect-vectored microorganisms. Ophiostomatoid fungi, which are well adapted to dissemination by insects, include ~140 species of saprobes and pathogens. They are present worldwide, have high economical impact and many are subject to quarantine regulation. Thus, it is necessary to ...
L Khadempour, Young Woon Lim, S Massoumi Alamouti, C Breuil


The use of thermal desorption and pyrolysis combined with a semiconductor VOC detector for the on-site detection of preservative-treated wood
2010 - IRG/WP 10-20456
The purpose of this study was twofold; to identify possible marker molecules released from preservative-treated wood upon heat treatment and then develop a prototype detector for this marker. Two methods for heating the samples were used: Pyrolysis combined with Gas-Chromatography with IR-detection and Thermal Desorption combined with Gas-Chromatography with mass detection. A first prototype detec...
I Svensson, A Gonzalez, L Irusta, Mª J Fernandez-Berridi, O Munné


A comparison of the chemistry of alkaline copper and micronized copper treated wood
2010 - IRG/WP 10-30528
This paper discusses the chemistry of the reaction of alkaline copper and micronized copper with wood. The objective of this study is to examine the copper species produced in wood during the fixation reaction using electron paramagnetic resonance (EPR) spectroscopy. The initial experiments (phases 1 to 2) were designed to confirm the effect of time of treatment and solution concentration on the s...
Wei Xue, P Kennepohl, J N R Ruddick


Distribution and availability of preservative components in ACQ treated wood - effects of coatings and weathering
2010 - IRG/WP 10-30537
Copper and quaternary ammonium compound (quat) distributions across lumber (gradients) and availability, as measured by amount removed by intensive leaching of wood flour, were measured in ACQ treated southern pine lumber. Samples were evaluated just after treatment and stabilization, or after 3 years of laboratory storage, or after 3 years of natural weathering exposure. The objective was to in...
T Ung, M Nejad, P Cooper


Antifungal and wood preservative efficacy of IPBC is enhanced by α - aminoisobutyric acid
2010 - IRG/WP 10-30544
There is currently a need to reduce the biocide content of wood preservatives, without decreasing efficacy. The nonmetabolised amino acid analogue α-aminoisobutyric acid (AIB) acts as a translocated inhibitor of mycelial spread in basidiomycete wood decay fungi, although it does not kill the organism. Factorial combinations of AIB with either the azole fungicide tebuconazole, or 3-iodo-2-...
P Bota, E Baines, A Mead, S C Watkinson


Copper nanoparticles in southern pine wood treated with a micronised preservative: Can nanoparticles penetrate the cell walls of tracheids and ray parenchyma?
2010 - IRG/WP 10-30547
This study tests the hypothesis that copper nanoparticles can penetrate the cell walls of southern pine wood treated with a micronised preservative. We examined the nanodistribution of particles in tracheid and ray parenchyma cell walls using state-of-the-art HR (High Resolution)-TEM and HR-STEM (Scanning Transmission Electron Microscope)-EDX. These devices are capable of atomic-scale resolution. ...
H Matsunaga, Y Kataoka, M Kiguchi, P Evans


Evaluation of formulation type on the efficacy of bifenthrin as a glueline termiticide for veneer based wood products
2010 - IRG/WP 10-40486
Field trials were carried out in Australia on Coptotermes acinaciformis to evaluate the efficacy of various bifenthrin formulations. One trial tested plywood made by Zelam at their research facility in New Zealand and compared three emulsifiable concentrate formulations (EC), a suspension concentrate (SC) and an encapsulated formulation (CS). A second trial compared laminated veneer lumber (LVL)...
P Lobb, A Siraa


Extruded wood plastic composites based on ACQ and MCQ-treated wood materials
2010 - IRG/WP 10-40495
This paper deals with wood plastic composites manufactured using ACQ and MCQ-treated wood fibers recovered from a wood treatment plant. The goal was to investigate the effect of coupling treatments on the properties of manufactured wood plastic composites (WPCs) through injection molding and to manufacture co-extruded WPC with treated wood fibers. The result demonstrated sound mechanical propertie...
Qinglin Wu, Fei Yao, K Ragon, J Curole, M Voitier, T Shupe


Influence of Copper Preservative Type on Earlywood and Latewood Distribution of Copper in Treated Wood
2010 - IRG/WP 10-40507
Some of the new water based copper containing wood preservative systems use particulate “micronized” copper as the primary biocide instead of the more traditional soluble amine copper based systems. Studies were conducted to investigate how this difference in the type of copper system might impact both initial and post drying distribution of the preservatives in wood. Of specific interest wa...
A Zahora


A comparison of the corrosion of alkaline copper and micronized copper treated wood
2010 - IRG/WP 10-40515
With the replacement of chromate copper arsenate (CCA) by alkaline copper wood preservatives, there have been reports of increasing corrosion of metal fasteners and connectors in contact with treated wood. This may be explained by the presence of more mobile copper in the treated wood. One novel industrial response has been to develop a wood preservative based on an aqueous solution containing sus...
M Kofoed, J N R Ruddick


Previous Page | Next Page