IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 933 documents. Displaying 25 entries per page.


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Decay patterns observed in butylene oxide modified ponderosa pine after exposure in unsterile soil
1982 - IRG/WP 3211
Small blocks of ponderosa pine (Pinus ponderosa Laws) chemically modified with butylene oxide to three different weight gains were exposed for 6 weeks in unsterile soil. Severe surface decay caused by soft rot fungi and tunnelling bacteria was observed in blocks with 8 weight percent gain. The soft rot attack was restricted to the outer parts of the radial walls in the latewood tracheids. Bacteria...
T Nilsson, R M Rowell


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Biological control of blue stain on wood with Pseudomonas cepacia 6253. Laboratory and field test
1989 - IRG/WP 1380
Pseudomonas cepacia strain 6253 was tested as a biological control agent on wood samples under laboratory conditions, as well as in the field. In the laboratory this bacterium controlled blue stain on Pinus radiata, but field test were not totally satisfactory. However, after 2 months of field test, the test samples were 1/3 to 1/2 less stained then the control samples....
R Benko


Results of field tests on the natural durability of timber (1932-1975)
1976 - IRG/WP 3105
This paper describes a continuing field stake trial to determine the natural resistance of different species of timber to decay. Data are presented for about 180 timbers, covering over 6000 stakes, and the results are discussed in terms of a natural durability classification....
D W Purslow


Isolation and identification of the fungal flora in treated wood
1976 - IRG/WP 144
J F Levy


Programme Section 2 Test methodology and assessment
1999 - IRG/WP 99-20180
IRG Secretariat


Methods for testing fumigant efficacies against termites
1986 - IRG/WP 1297
Methodologies for testing fumigants against termites are reviewed and factors needed to be taken under consideration for standardization listed. Toxicity should be defined by both direct exposure to the gas and under more practical "barrier" conditions which include test enclosures simulating abiotic surroundings of the termites, i.e. wood, nest material, etc. To observe latent effects, mortality ...
N-Y Su, R H Scheffrahn


Soil contamination at the wood preservation industry: Treatment technologies
2001 - IRG/WP 01-50166-16
The soil is a specific compartment of the biosphere, because it is not only a geochemical sink for contaminants, but it also acts as a natural buffer, controlling the transport of chemical elements and substances to the atmosphere, hydrosphere, and biota. Soil contamination problems are expected at wood preservation sites, particularly at those which use(d) inorganic wood preservatives or creosote...
A B Ribeiro, L M Ottosen


A case for adopting a standardised protocol of field and laboratory bioassays to evaluate a potential soil termiticide
2003 - IRG/WP 03-20275
The rationale for adopting a new approach to the field testing of potential soil termiticides is advocated on the grounds that current testing methods are limited to termite bioassays and do not address quantitatively the persistence and bioavailability of soil termiticides to foraging subterranean termites over time and in different soil types. Furthermore, the present testing regimes assume fiel...
J R J French, B M Ahmed


Final proposals for collaborative work on laboratory soft rot testing
1987 - IRG/WP 2292
In this paper proposals are made to scope, timbers, preservatives, leaching, drying, soil type, moisture content, soil burial (blocks and stakes), incubation and dry weight determination and the expression of results....
D J Dickinson, S M Gray


Occurrence of manganese deposits in test stakes exposed in groung contact situations
1996 - IRG/WP 96-10182
Dark spots and flecks were frequently recognized on the surface and within non-preservative treated hard- and softwood test stakes placed in soil contact. Energy dispersive X-ray microanalysis in conjunction with electron microscopy showed the flecks to be composed primarily of manganese dioxide. Detailed transmission electron microscopy observations indicated intrusion of manganese into the wood ...
G F Daniel, T Nilsson, J Volc


Comparison of the effect of different soil sources on the type and rate of decay of CCA-treated pine exposed in a soil-bed
1984 - IRG/WP 2213
The types of decay observed in CCA-treated pine posts in horticultural situations in New Zealand can be reproduced using a soil-bed exposure. Radiata pine stakelets, untreated or treated to 1.4, 2.7, or 5.4 kg/m³ with Tanalith NCA, were exposed to six different soil sources. The local nursery soil used for all standard laboratory tests was found to represent the greatest decay hazard to untreated...
J A Drysdale


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 9: Report of third inspection (2 years) in Italy
1980 - IRG/WP 461
The wood samples were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitudine 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian sea. The recorded temperature varies between 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 1 year (4/1978) and 2 years (4/1979)....
A Gambetta, E Orlandi


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 7: Second report on the samples in Papua New Guinea
1980 - IRG/WP 459
This report presents the findings to date regarding specimens installed in Papua New Guinea, as part of a world-wide marine trial of certain timbers treated with CCA or CCB preservatives. The details of the trial are set out in document number IRG/WP/414. The report discusses the findings in the context of the conditions prevailing at the trial site and of the properties of the trial timbers. The ...
S M Cragg, C R Levy


Virulence tests with fungal strains used in EN 113 CEN ring test. Results with Coniophora puteana (Schum.ex Fr.) Karst
1986 - IRG/WP 2249
D Dirol


Soil chemistry and wood decay
1978 - IRG/WP 2109
Soil is a most complex biological, chemical and physical material; its study is effectively a separate branch of science but almost entirely in relation to ist ability to grow plants - this paper is intendet just to note some known facets that might have relevance to the decay of wood and the performance of wood preservatives....
E A Hilditch


Co-operative field experiment. Performance of preservative-treated hardwoods with particular reference to soft rot: Report of condition of specimens installed in Victoria, Australia
1978 - IRG/WP 3118
J Beesley


Ekki heartwood - is “Durable”
2002 - IRG/WP 02-10444
Severe decay damages of bridges made of ekki (Lophira alata Banks) wood which is classified as a durable species in the EN 350:2 as already reported at the 31 IRG annual meeting. This paper deals with results of long-term decay tests of ekki heartwood specimens using 3 isolates (Loweporus tephroporus 2 strains and a fungus of other sp. from damaged ekki bridges) and Trametes versicolor as a refere...
S Doi, R Itoh, S Horisawa


Test Methods – Performance Based Requirements
2004 - IRG/WP 04-20297
In this paper is briefly described the present approach to service life prediction as an essential part of the architectural engineering process. The system of testing the durability of wood is described more in detail including laboratory tests as well as field trials. It is concluded that the system has a lot of weaknesses which makes it less well suited for practical building applications. A le...
M-L Edlund, F Englund, J Jermer, T Nilsson, M Westin, K Ödeen


Evaluating the natural durability of a number of lesser known species of Ghanaian hardwoods using a short term laboratory assay
2004 - IRG/WP 04-10540
Resistance of a number of Ghanaian hardwoods to attack by the crustacean Limnoria quadripunctata was assessed by measuring the production of faecal pellets under forced feeding conditions over a two week period. Small sticks of commercially available, lesser known timber species, were leached in seawater for one week then placed in a cell culture chamber with one animal and 4 ml of seawater. At in...
J R Williams, S M Cragg, L M S Borges, B Shayler


Test methods used for approval of wood preservatives in Indonesia
1994 - IRG/WP 94-20045
Indonesian regulation stipulates that all pesticides, including wood preservatives, must be registered and obtain legal permit from the Minister of Agriculture, c.q. the Pesticide Committee before they are eligible for public use. For that purpose they have to meet safety and efficacy requirements approved by the Pesticide Committee. To meet the efficacy requirements, wood preservatives must be te...
A Martawijaya


Effect of soft-rot decay on the static bending strength of wood
1991 - IRG/WP 2361
In this study, a modified static bending test has been developed as a method for measuring soft-rot decay in soil bed studies. A good correlation was found between the strength loss of the southern pine test specimens and extent of decay. This data suggests that it may be possible to develop a dynamic test based on stress relaxation that is more sensitive than static bending....
D D Nicholas, J A Wilson, R C Vasishth


Questionnaire concerning assessment of test data from laboratory and field tests
1992 - IRG/WP 92-2418
During the WG II session in Harrogate, UK it was announced, that possibly a working-session on the assessment of test data and correlation between laboratory and field tests might be organised during next year's meeting in Orlando. For that pupose a questionnaire was prepared. The valuable comments and input of Prof. Thomas Nilsson from Sweden is hereby greatly acknowledged....
A R Valcke


Previous Page | Next Page