Effect of soil contact on reacted copper(II) levels in micronized copper treated wood
2013 - IRG/WP 13-30616
Small 3 to 4 mm thick and approximately 80 to 100 mm long, samples were removed from wood treated with micronized copper quat (MCQ) or micronized copper azole (MCA) and buried full length in a soil bed. Samples were removed after 2, 4 and 8 weeks. The total copper was determined by x-ray fluorescence (XRF) spectroscopy and the amount of reacted micronized copper measured by electron paramagnetic r...
Wei Xue, P Kennepohl, Xingguo Jin, J N R Ruddick


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Selection of Wood-Rotting Basidiomycetes for Inoculation of an Accelerated Soil Bed Test
2014 - IRG/WP 14-20543
There is a need for a test method that guarantees exposure of treated wood to soil and preservative-tolerant wood-rotting basidiomycetes as standard field tests do not do this reliably. The ability of a range of selected wood-rotting basidiomycetes to grow through unsterile forest soil was investigated in a Mason jar test assembly. None of the white-rot fungi in test grew through this soil. Fou...
P I Morris, A Uzunovic, J Ingram


Potential for migration of boron from fused boron rods used as internal remedial treatments of utility poles
2014 - IRG/WP 14-50301
The distribution of boron in Douglas-fir utility poles and in the surrounding soil was assessed over a 54 month period following application of fused boron rods. Boron levels in the wood never reached the levels that might be predicted if diffusion were to produce a uniform chemical distribution, nor did levels in the soil suggest that boron was becoming more concentrated. The results suggest th...
M Konkler, C Freitag, C S Love, J J Morrell, J Renfroe


Laboratory Study of Relative Leachability of Chromated Copper Arsenate Preservative from Treated Woods among Soil Types of Sarawak
2014 - IRG/WP 14-50307
Wood and soils are important natural resources from the environment and serves mankind well respectively as structural materials and natural platform erecting such materials. With shortfalls of naturally durable timber species for protected in-ground uses under Malaysian environments, Chromated Copper Arsenate (CCA) treated woods are widely used instead, incurring serious potential threats of pres...
A H H Wong, P K F Chong


Termite Management and the U.S. Experience: A Case for Wood Treatment & Integrated Control
2015 - IRG/WP 15-30678
A brief overview of termite control is given using specific experiences from the U.S.A. Five major types of termite treatment now prevail: soil applied chemical barriers, in-structure chemical barriers (in-situ applied wood and foundation treatments), physical barriers, treated wood and termite baits. In general, ‘stand-alone’ pretreatments or ‘primary’ treatments are often discussed and ...
J D Lloyd, K van den Meiracker


Laboratory evaluations of woods from Pakistan and their extractives against Postia placenta and Trametes versicolor
2016 - M Mankowski, B Hassan, A Bishell, G Kirker
Natural durable wood species are those which exhibit innate tolerance to wood decay organisms such as fungi and termites. The goal of this study was to evaluate 4 wood species (Dalbergia sissoo, Cedrus deodara, Morus alba and Pinus roxburghii) from Pakistan in order to determine their resistance to both a model brown (Postia placenta) and white (Trametes versicolor) rot fungus compared to a durabl...
M Mankowski, B Hassan, A Bishell, G Kirker


Variation in moisture content in field trials according to use class 3.2 conditions
2016 - IRG/WP 16-20580
Different test methods to determine the durability of wood in use class 3 (EN 335:2013) are available. Fungal degradation of wood requires liquid water. Different Standards (EN 335-1:2006; DIN 68 800:2011) specify the risk for decay with moisture content (mc) of above 20%. EN 335 (2013) does not specify moisture content but rather defined limited wetting conditions (use class 3.1) or prolonged wet...
S Bollmus, A Gellerich, H Militz


Evidence for a role for precipitated copper on the chemistry of micronized copper treatments
2016 - IRG/WP 16-30690
Micronized copper preservative treatments of softwoods, result in mobile copper being formed by reaction of the basic copper carbonate (BCC) with the carboxylic acid functional groups in hemicellulose and pectic substances present in wood. Typically, the amount of reacted copper formed is approximately 0.3% Cu m/m. In this paper, two examples are discussed where remaining unreacted basic copper ca...
Wei Xue, P Kennepohl, J N R Ruddick


Evaluation of advanced tannin-boron preservative in unsterile soil-bed tests
2016 - IRG/WP 16-30693
In Europe, boron compounds are facing restrictions, and due to their natural solubility into water, the only way to keep using them for wood protection is to fix them into the wood, at very low level (Obanda et al. 2008). In the meantime, the idea of protecting wood with natural preservatives has been back into favour (Lotz and Hollaway 1988, Nakayama et al. 2001, Singh and Singh 2012). Tannin a ...
Jinbo Hu, Yiqiang Wu, Shanshan Chang, Guangming Yuan, G Tondi, M-F Thévenon


Resistance of heat treated Ash wood under steam pressure: rot fungi, soil micro-organisms and termites
2016 - IRG/WP 16-40724
Thermal modification processes have been developed to increase the biological durability and dimensional stability of wood. The aim of this paper was to study the influence of ThermoWood® treatment intensity on wood decay resistance improvement against soil-inhabiting micro-organisms, brown/white rots and termite’s exposures. All of the tests were carried out in the laboratory with two differen...
K Candelier, S Hannouz, M-F Thévenon, D Guibal, P Gérardin, M Pétrissans, R Collet


A Case Study of Long-term CCA Preservative Leaching from Treated Hardwood Poles in a Humid Tropical Condition
2016 - IRG/WP 16-50324
Chromated copper arsenate (CCA)-treated Malaysian hardwoods have long been used as utility poles, posts, construction piles and motorway fencing in soil contact exposed to the threats of decay fungi and termites. Despite global concerns citing predominantly temperate conditions of long-term leaching of CCA toxic heavy metals from wood into surrounding soils and groundwater since the 1990’s, the ...
A H H Wong, W S M Chin


Assessing the natural durability for different tropical timber species using the mini-block test
2017 - IRG/WP 17-10886
The Xylarium in the Royal Museum for Central Africa (RMCA, Tervuren, Belgium) contains over 60,000 wood-samples, comprising over 12,000 species. These samples are of great historical and scientific value yet have a random format, which complicates standard testing. The wood-durability against Coniophora puteana and Trametes versicolor was tested for 36 species. Due to the random sample sizes the s...
V Deklerck, I De Windt, N Defoirdt, J Van den Bulcke, H Beeckman, E Espinoza, J Van Acker


Agar block durability test of plywood made of neem (Azadiracta indica) leaves treated veneer using two white rot fungi
2017 - IRG/WP 17-40782
This study has been undertaken to investigate the durability of plywood made from non-durable wood (simul, Bombax ceiba) veneer treated by neem (Azadiracta indica, A. Juss.) leaves. The veneers were treated with cold and hot water solution of neem leaves of different concentrations (10%, 5%, 2.5%) and treatment durations (1, 2, 3 days) for cold water and 20, 40 and 60 minutes for hot water. The pl...
K Akhter, M A Hashem, S Akhter


Solid Timber Bridges – Latest Developments
2017 - IRG/WP 17-40788
The technology of gluing in wood construction has evolved considerably in recent years. This has been shown especially in timber bridges that Glulam is now the main building material. A further development is the so-called block gluing, which provides a good basis for supporting structures. Numerous bridges, especially in central Europe, appeal by unique design and monolithic and solid construction. These structures base on two main developments: block lamination of glulam and the composite of timber and concrete to one structural system.
F Miebach


Fipronil Concentrations in Soil after Vertical Termiticide Applications Using the “Termidor®H•P High Precision Injection System”
2017 - IRG/WP 17-20630
Termidor®H•P II High Precision Termiticide concentrations in sandy-loam and sandy-clay-loam building foundation soil were measured 1.0-hour after high-pressure vertical liquid injections into the soil using the Termidor®H•P High Precision Injection System. Cylindrical, vertical 30.5-cm-deep soil cores were extracted and separated into four 7.6-cm-long sequential partitions, and fipronil res...
B M Kard


Long-time efficacy of some soil termiticides tested according to “Modified Ground Board Test”
2018 - IRG/WP 18-10935
Field trials of efficacy of soil termiticides available in Thailand were started back in the 1980s at four different locations representing different unique weather types of the country. The method used in the trials (Modified Ground Board Test) is the compulsory test for every soil termiticides aiming to be registered for termite control in Thailand. The ongoing record reveals that some particula...
C Vongkaluang, K Charoenkrung, N Same Rain


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


The biodegradation of creosote oil by various species of white rot fungi and bacteria isolated from the contaminated soil
2018 - IRG/WP 18-50334
The aim of the study was to determine biodegradation effectiveness of the selected polycyclic aromatic hydrocarbons (PAHs) contained in creosote oil, by two white rot fungal species (Bjerkandera adusta and Irpex lacteus) and three bacterial species (Pseudomonas putida, Pseudomonas sp. OS4 and Rahnella aquatilis). Bacteria were isolated from the soil contaminated with petroleum hydrocarbons from th...
M Sydow, J Zabielska-Matejuk, E Kaczorek, AStangierska, A Kropacz


Preserved Wood in the Story of Sustainable Forestry
2018 - IRG/WP 18-50344
Sustainable forestry, at its simplest, is about growing trees. The full story, though, is much more complex. An important chapter of that story is the role that preserved wood plays in ensuring sustainability. Too often, this part of the sustainability story is rarely mentioned. It is time for the preserved wood industry to deliver a unified message of our critical role in sustainability. By res...
D Brookes


Determining the natural durability on xylarium samples: mini-block test, wood powder and chemical profiling
2019 - IRG/WP 19-10944
Xylaria, or wood collections, can be considered sleeping beauties in terms of wood technological and biological output. In this study we focus on determining the natural durability of xylarium specimens from the Federal Xylarium in the Royal Museum for Central Africa. The Federal Xylarium contains over 80,000 specimens, covering more than 13,000 species, mainly from Central Africa. These specimens...
V Deklerck, L De Ligne, J Van den Bulcke, E Espinoza, H Beeckman, J Van Acker


From fungal detoxification systems to wood durability in neotropical forests
2019 - IRG/WP 19-10946
White-rot fungi are able to mineralize all the wood components due in particular to an efficient detoxification system. We hypothesised that components of this detoxification systems, glutathione transferases, could be used as tools to explore the natural durability of neotropical wood species. Analysis of the interactions between six glutathione transferases of Trametes versicolor and extracts of...
T Perrot, G Salzet, N Amusant, J Duchene, E Gelhaye


Performance of modified wood in service - multi-sensor data fusion and its multi-way analysis
2019 - IRG/WP 19-20660
Recent developments in the field of electronic sensors and analytics provide new opportunity for accurate characterization of materials often based on portable and non-destructive methods. By using several complementary techniques, the material description is precise and complete. The data provided by multiple equipment, however, are often not directly comparable due to different resolution, sensi...
A Sandak, J Sandak, M Cocchi


Impact of water holding capacity and moisture content of soil substrates on the moisture content of wood in terrestrial microcosms
2019 - IRG/WP 19-20662
Terrestrial microcosms (TMC) are frequently used for testing the durability of wood and wood-based materials as well as the protective effectiveness of wood preservatives. In contrary to experiments in soil ecology sciences, the experimental set-up is usually rather simple. However, for service life prediction of wood exposed in ground, it is of immanent interest to better understand the different...
C Brischke, F L Wegener


The role of specimen format in wood durability testing
2020 - IRG/WP 20-20672
The experimental basis for testing the biological durability of wood are often incubation experiments with wood-destroying basidiomycetes. Numerous parameters can affect the mass loss by fungal decay (MLF) in laboratory durability tests and therefore being decisive for the resulting durability classification. Among others, the dimension of the wood specimen and the time of incubation impact on fun...
C Brischke, L K Grünwald, S Bollmus