Biostatic film as a primary treatment against pole failure in soil
1995 - IRG/WP 95-40053
Field liners of low density polyethylene (LDPE) film applied as primary treatment of soil-contact surfaces of creosote-treated poles prevented their detoxification and premature failure by establishing hurdles against microbiological colonisation. These hurdles include low water activity, low oxygen tension and nutrient limitations. Moreover, under conditions of high soil moisture, field trials sh...
A A W Baecker, M Behr


Environmental risk assessment of treated wood - A mesocosm study
2005 - IRG/WP 05-50224-8
In order to evaluate the environmental impact of treated poles, we have developed physical models (mesocosms) containing around 250 kg of natural soil and a treated pole. On the top of each mesocosm, a spraying mechanism, which can distribute ultrapure water through several nozzles, was built. On the lower part of each mesocosm, a small tank, which can contain some litres of leachate, was placed...
P Marchal, F Poly


The effect of wood preservatives on the relation between the electric resistance and moisture content in scots pine (Pinus sylvestris L.) sapwood
1998 - IRG/WP 98-20142
The effect of two types wood preservatives (TBTO and CuHDO) on moisture content measurements with an electric resistance meter in pine sapwood is assessed. High and low concentration impregnated pine sapwood is climatized at different relative humidities. Once climatized the samples are weighed and the moisture content is measured with an electric resistance meter by fixed stainless steel, isolate...
B W Holleboom, W J Homan


Evaluation of bacteria for biological control of wood decay
1990 - IRG/WP 1426
Laboratory soil-block and agar-block tests were carried out to evaluate the efficacy of bacteria as biological control agents against 5 brown-rot and 3 white-rot fungi. Pretreatment of Southern pine and sweetgum with a bacterial solution prevented decay in agar-block tests. However, the bacteria were generally ineffective in preventing decay in Southern pine, Douglas-fir, sweetgum and yellow popla...
R Benko, T L Highley


The natural durability assessments of secondary timber species - field trials
1998 - IRG/WP 98-10297
Secondary or 'alternative' hardwood timber species can replace traditional hardwoods and contribute significantly to satisfying the overall demand for hardwoods in the UK timber market. A selection of these 'alternative' hardwoods is currently being tested at BRE-WTC for natural durability both in ground contact (to EN252) at two field sites, and out of ground c...
E D Suttie, R J Orsler


Dip-diffusion of dressed timber - Effect of drying
1990 - IRG/WP 3603
The effect of drying on BFCA dip-diffused, dressed, freshly sawn timber was determined by the depth of penetration of boron achieved on two test timber species, White Cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that the light density White cheesewood was completely penetrated even after 3 days drying while Light Hopea, treated immediately achieved 5...
H C Konabe


Fungi causing sap stain in wood
1980 - IRG/WP 199
The present paper is a revised edition of former Document No: IRG/WP/125. It contains some additions and an explanation of terminology, as was suggested at a previous meeting of the Group. The paper is a compilation based mainly on available literature. Some of my own unpublished results have been added together with other unpublished data which have been received from the Bundesanstalt für Mater...
A Käärik


Influence of CCA and TnBTO on wood decay, under different oxygen levels and various initial moisture content
2001 - IRG/WP 01-10415
Fagus sylvatica (beech) and Pinus sylvestris (Scots pine) were impregnated by TnBTO (tributyl-tin oxide) and CCA (chromated copper arsenate). In wood blocks two levels of moisture content (50% and 100% of saturation point) were used. Three levels of oxygen concentrations (10, 21, and 50%) were chosen. Treated and untreated wood were exposed to three fungi (C. versicolor a white rot, C. puteana, a ...
S M Kazemi, R J Murphy, D J Dickinson


The Efficacy of Wood Preservative Treatments in Laboratory Soil-Bed Test
2004 - IRG/WP 04-20289
The efficacy of wood preservatives were determined in laboratory soil-bed test. Pine and alder wood samples (10 x 10 x 10 mm) were treated with CCA (1, 2%), ACQ-1900 (2, 3%), ACQ-2200 (1, 2%), Tanalith E 3491 (2, 2,8%), Wolmanit CX-8 (1, 2%). The leached and unleached samples were exposed 76 days at Simlångsdalen soil and determined mass loss. The results of this study showed that mass losses o...
A Temiz, T Nilsson, Ü C Yildiz, E D Gezer, S Yildiz


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


IUFRO rating system compares favourably to weight loss for soil-bed testing
1990 - IRG/WP 2343
The soil-bed/small stake test is commonly used for rapidly evaluating the performance of new, more environmentally acceptable, preservatives. In a 1.5 year experiment with three copper-based waterborne preservatives, visual evaluation and probing using the IUFRO performance rating scale (0-4) gave very similar toxic thresholds to those derived from measurement of weight loss at the end of the expe...
P I Morris


Field test design for service life prediction of wooden components
2005 - IRG/WP 05-20308
Wood is predominantly degraded by organisms. Thus, compared to other building materials, service life of wooden material is influenced by many more factors, which are divided into direct and indirect factors. Climate, geographical position, and construction criteria count to the indirect decay factors. Besides material inherent properties (natural durability, wood preservatives), wood temperature...
A O Rapp, C Brischke


Field Liners™ prevent creosote migration from transmission poles to soil during service
1996 - IRG/WP 96-40067
A full scale trial utilised 150 12m Eucalyptus grandis transmission poles treated with standard retentions of creosote according to SABS Method 457. One hundred poles had Field Liners™ applied while 50 did not. The 150 poles were used to complete an electricity transmission line in Southern KwaZulu-Natal. After 18 months service, incremental cores were taken from 15 cm below the ground lines of ...
M R Behr, G D Shelver, A A W Baecker


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


Long term experiments for assessing the diffusion of boric acid and diluorides from local preservative pills in spruce and pine
1996 - IRG/WP 96-40065
For the experimental assessment of the diffusion of boric acid and difluorides over a three year period 2 tests were set up. In a test with large spruce blocks (150 x 150 x 300 mm³) 3 different pill types were exposed to 3 different climates: climate room (20°C, 65% r.h.), wet room (20°C, 95% r.h.), and to outside exposure. In a test with open L-joints without paint, with an alkyd paint and wit...
W J Homan, H Militz


Borate diffusion in wood from rods and liquid product. Application to laminated beams
1988 - IRG/WP 3482
In the aim to use borate preservatives (fused rods and boracol) in fields of building construction other than external joineries, tests of diffusion of borate rods and secondary boracol, were carried out on different species of woods exposed to different moisture conditions. Tests were also applied on laminated beams very often subjected to high moisture contents and thus decay of rot fungi. Diffu...
D Dirol


Evaluating the potential of amine chemicals for use as wood protecting agents. Part 1: Investigation of cation components of quaternary ammonium compounds
1994 - IRG/WP 94-30049
Quaternary ammonium compounds (quats) have shown a great potential as more environmentally acceptable wood preservatives. In order to identify chemicals possessing the wood protecting potential, an evaluation was carried out of a range of commercially available 'quats', using a modified soil block test. Ponderosa pine sapwood blocks were treated with selected 'quat&a...
Hang Tang, J N R Ruddick


Termites in Uruguay; control, prevention and environment
1991 - IRG/WP 1474
When Prof. La Fage's questionaire on termites was received by 1987, few were aware of termite damage in Uruguay and infestations were not much reported. Further contacts between scientists, operators and homeowners, are now shaping the real threat of termite attack. Before letting the problem faIl in the hands of the layman, with all ist environmental risks, it seemed reasonable to: 1) re...
A Aber, G Baillod


Treatment application method and CCA efficacy in Corsican pine - Assessment by serial exposure and soil burial tests
1993 - IRG/WP 93-40006
A previous report on this research (Newman and Murphy, 1992) identified possible variation in the efficacy of a CCA preservative applied to Corsican pine (Pinus nigra var. maritima) dependant upon the treatment application method (Bethel, Lowry or Steam/Bethel). This paper presents further data from biological testing of CCA treated Corsican pine using serial exposure and unsterile soil techniques...
P R Newman, R J Murphy


Losses of CCA components and creosote from treated timber to soil
1997 - IRG/WP 97-50098
Components of creosote and CCA preservatives can migrate within the wood and move into surrounding soil. However, at present, the ecological significance of such losses is uncertain. This paper examines the distribution of four target polyaromatic hydrocarbons (PAHs ) and of copper, chromium and arsenic in treated stakes and surrounding soil after long term exposure in field trials. Concentrations...
N J Hudson, R J Murphy


Remediation of a large CCA-impregnation plant
1998 - IRG/WP 98-50101-13
During 1949-85 the Swedish Telecom ran a plant for pressure impregnation of poles in Hjältevad, 80 km east of Jönköping in the southern part of Sweden. About one million poles were treated with CCA-preservaties. Leaks and accidential spills have contaminated soil and groundwater within the 5 ha large site. The total amount of released arsenic, the main pollutant, is estimated to 6-7 metric tons...
P Englöv


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


On the laboratory use of X-rays in timber decay evaluations
1981 - IRG/WP 2144
The paper reports the results of laboratory experiments on the X-raying of some Pinus radiata sapwood blocks infected with Serpula lacrymans to determine the effect of density and moisture content on the absorption of X-rays by wood. It is concluded that with increasing moisture content there is a very marked increase in time required to pass a constant quantity of X-rays through a test block and ...
J D Thornton, J W Creffield, O Collett


A comparison of the migration behaviour in soil of different waterborne wood preservatives and their leachates
1997 - IRG/WP 97-50091
Lysimeter tests were carried out on water-soluble wood preservatives and on wood preservative components leached out of impregnated wood. The purpose of these tests was to determine the extent to which the migration behaviour of environmentally relevant ions in the soil is influenced under comparable conditions. The results clearly show that the groundwater is especially at risk when wood preserva...
E Melcher, R-D Peek


Moisture content development in lap-joints of different wood species in outside exposure trials
1998 - IRG/WP 98-20143
Lap-joint trails (following European Standard EN 12037) were set up with 11 different softwood and hardwood species. Half of the number of the lap-joint specimens were coated with an alkyd coating. The moisture development has been followed during a 19 months period. In this paper, the out comes of different moisture contents evaluations are presented. The results show, that the moisture content o...
H Militz, M Broertjes, C J Bloom