Fipronil Concentrations in Soil after Vertical Termiticide Applications Using the “Termidor®H•P High Precision Injection System”
2017 - IRG/WP 17-20630
Termidor®H•P II High Precision Termiticide concentrations in sandy-loam and sandy-clay-loam building foundation soil were measured 1.0-hour after high-pressure vertical liquid injections into the soil using the Termidor®H•P High Precision Injection System. Cylindrical, vertical 30.5-cm-deep soil cores were extracted and separated into four 7.6-cm-long sequential partitions, and fipronil res...
B M Kard


Evaluation of coating applied in treated wood: experiences in Brazil
2017 - IRG/WP 17-40814
Weathering assays study the coating degradation caused by its exposure to the action of ultraviolet radiation, winds, heat and humidity. The use of test specimens in different arrangements and exposure angles is intended to reproduce various conditions in which a product can be used. The purpose of this paper is to present the efficacy of an oil-borne varnish applied on treated wood exposed to wea...
M F Natale, J M Vidal


Preliminary Investigation into the Natural Decay Resistance of Nigerian Grown Hevea brasiliensis and Mitragyna ciliata wood to Phanerochaete chrysosporium White-Rot Fungus
2018 - IRG/WP 18-10919
Wood is an important and versatile structural building material that finds applications in numerous uses. However, wood is also a biological material vulnerable to degradation by microbial activities; this is especially true in the tropics. Following the scarcity of highly durable species from our natural forests and the introduction of so many lesser used/durable wood species into the booming tim...
J M Owoyemi, U O Emmanuel


Towards durability classification of preservative treated wood – first attempts using different European standards
2018 - RG/WP 18-20638
EN 350 (2016) gives guidance on methods for determining and classifying the durability of wood and wood-based material against biological wood destroying agents. “Wood-based materials are those derived from trees and include amongst others: untreated wood, heat treated wood, chemically modified wood, glue laminated wood, wood-based panels, wood polymer composites and wood treated with wood prese...
S Bollmus, A Gellerich, C Brischke, H Militz


Can CCA be substituted as reference preservative?
2018 - IRG/WP 18-20641
While field testing of wood protective formulations remains probably the best method to find out the effective preservative concentration, the use of chrome-copper arsenate (CCA) as reference becomes debatable due to environmental and legislative reasons. This emerges from the European standardization bodies who have discussed reference alternatives that can omit the use of CCA. The present debate...
N Terziev, M Jebrane, P Larsson Brelid, N Morsing, P-O Flaete, P Torniainen, J S Kim, G Daniel


Above-ground testing methods – review of Rotorua, New Zealand test site results after ten years
2018 - RG/WP 18-20642
A series of seven different types of above ground durability tests were initially conducted over four years to determine which type of tests would give the fastest, most consistent results. Five types of test; ground proximity, two types of decking, flat panels and double layer, were reassessed after ten years. Exposure conditions varied between tests with ground proximity producing close to groun...
D Page, T Singh


Rapid Screening test of potential antimicrobial agents for wood coatings
2018 - RG/WP 18-20644
A two-part screening test has been developed to evaluate additives for wood coatings. First, an additive is tested in the microbial laboratory and evaluated based on its inhibitory properties against selected test organisms, directly on agar plates. A microbial growth analysis is prepared and evaluated. If the additive is considered effective, it will be tested in a standard top coating (acrylic o...
J Stenbæk, E Morsing, T Østergaard Jensen


The biodegradation of creosote oil by various species of white rot fungi and bacteria isolated from the contaminated soil
2018 - IRG/WP 18-50334
The aim of the study was to determine biodegradation effectiveness of the selected polycyclic aromatic hydrocarbons (PAHs) contained in creosote oil, by two white rot fungal species (Bjerkandera adusta and Irpex lacteus) and three bacterial species (Pseudomonas putida, Pseudomonas sp. OS4 and Rahnella aquatilis). Bacteria were isolated from the soil contaminated with petroleum hydrocarbons from th...
M Sydow, J Zabielska-Matejuk, E Kaczorek, AStangierska, A Kropacz


Preserved Wood in the Story of Sustainable Forestry
2018 - IRG/WP 18-50344
Sustainable forestry, at its simplest, is about growing trees. The full story, though, is much more complex. An important chapter of that story is the role that preserved wood plays in ensuring sustainability. Too often, this part of the sustainability story is rarely mentioned. It is time for the preserved wood industry to deliver a unified message of our critical role in sustainability. By res...
D Brookes


From fungal detoxification systems to wood durability in neotropical forests
2019 - IRG/WP 19-10946
White-rot fungi are able to mineralize all the wood components due in particular to an efficient detoxification system. We hypothesised that components of this detoxification systems, glutathione transferases, could be used as tools to explore the natural durability of neotropical wood species. Analysis of the interactions between six glutathione transferases of Trametes versicolor and extracts of...
T Perrot, G Salzet, N Amusant, J Duchene, E Gelhaye


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Durability classification of preservative treated and modified wood
2019 - IRG/WP 19-20659
EN 350 (2016) allows formally to determine durability classes (DC) for wood products and wood-based materials, which was previously only possible for untreated wood in the form of natural durability. In a first study, the University of Goettingen carried out the durability classification of chemically modified (modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea, DMDHEU) and preservative-treate...
S Bollmus, L Bachle, C Brischke, H Militz


Performance of modified wood in service - multi-sensor data fusion and its multi-way analysis
2019 - IRG/WP 19-20660
Recent developments in the field of electronic sensors and analytics provide new opportunity for accurate characterization of materials often based on portable and non-destructive methods. By using several complementary techniques, the material description is precise and complete. The data provided by multiple equipment, however, are often not directly comparable due to different resolution, sensi...
A Sandak, J Sandak, M Cocchi


Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori


Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama


Knowledge exchange and transfer from academia to industry in the field of wood protection research – Activities of the IRG-WP Communications Committee
2019 - IRG/WP 19-50354
The International Research Group on Wood Protection (IRG) was founded in 1969 as a structured group of like-minded scientists and technologists focused on generating knowledge of the science of wood deterioration, and novel solutions to provide sustainably and environmentally responsible products for the protection of wood-based materials. The primary function of the IRG is to provide opportunitie...
F Latorre, B Abbott, C Brischke, M Humar, D Jones, E Larnoy, L Nunes, A Preston, T Singh


Performance of bio-based building materials – durability and moisture dynamics
2020 - IRG/WP 20-20666
When exposed to conditions favourable for decay, bio-based building materials can be susceptible to degradation. Their ability to withstand deterioration over time (performance) depends on the intrinsic or enhanced durability of the material as well as its wetting and drying behaviour. The effect of fungicidal components in wood is known since long. Other material characteristics, such as the mate...
L De Ligne, J Caes, S Omar, J Van den Bulcke, J M Baetens, B De Baets, J Van Acker


Impact of fungal decay on the bending properties of wood
2020 - IRG/WP 20-20671
Wood used outdoors is generally prone to fungal degradation, and its impact on the structural integrity of wood is an immanent factor for service life planning with timber. Wood decayed to very small mass losses can suffer from a significant reduction in mechanical strength and elastic properties. Hence, the latter are preferred indicators to detect decay in wood durability studies. Numerous previ...
S Bollmus, P B van Niekerk, C Brischke


The role of specimen format in wood durability testing
2020 - IRG/WP 20-20672
The experimental basis for testing the biological durability of wood are often incubation experiments with wood-destroying basidiomycetes. Numerous parameters can affect the mass loss by fungal decay (MLF) in laboratory durability tests and therefore being decisive for the resulting durability classification. Among others, the dimension of the wood specimen and the time of incubation impact on fun...
C Brischke, L K Grünwald, S Bollmus


Future development of durability assessment of wood, according to typical usage of preservative-treated wood and naturally durable wood in Japan
2020 - IRG/WP 20-20675
A market of preserved wood products in Japan has two unique histories. First is the market shift to residential ground sills from utility poles and sleepers; the other is the stop of CCA treatment caused by the new effluent standard. In 2018, around 85% of preserved wood products used for residential ground sills were treated with non-CCA such as Cu-based agents. Since the market of treated wood h...
T Osawa, W Ohmura, H Kurisaki


Bioremediation technology for cleaning-up of the soil contaminated with creosote oil – the overall concept of BIOREM project
2020 - IRG/WP 20-50363
The aim of the communication paper is to present the conceptual framework of the BIOREM project, which started in May 2019. The final result of the entire project will be an innovative bioremediation technology that can be used in areas contaminated with creosote oil – a commonly used wood preservative being a complex mixture of various compounds such as polycyclic aromatic hydrocarbons (PAHs). ...
M Sydow, J Zabielska-Matejuk, A Stangierska


Performance of resin-treated solid wood and laminated veneer lumber (LVL) under marine conditions
2021 - IRG/WP 21-10973
Wood is a traditional building material in the marine environment, where it is exposed to extremely harsh conditions. Most of the indigenous softwood and hardwood species in Europe are not durable against attack by marine organisms. Recently, wood modification has been considered as an alternative to protect non-durable wood species under use class (UC) 5 (EN 335, 2013) conditions. The present stu...
L Emmerich, C Brischke, S Bicke, H Militz


Experience Experience from over 20 years of field trials of resin treated wood – Marine borer resistance of MMF and DMDHEU modified wood
2021 - IRG/WP 21-10976
In 1999 a field test of Scots pine treated with MMF (Methylated Melamine Formaldehyde) resin and acetylated Scots pine post treated with MMF resin was started. Six years later a commissioned full NWPC test for BASF of Belmadur® (DMDHEU resin treated wood) was started at the same site. The testing, according to European Standard EN 275, was done in a bay by Kristineberg Marine Research Station o...
M Westin, P Larsson Brelid, A O Rapp, J Habicht


Mechanical and biological durability properties against soft-rot and subterranean termite in the field (grave-yard test) of beech wood impregnated with different derivatives of glycerol or polyglycerol and maleic anhydride followed by thermal modification in an opened or in a closed system
2021 - IRG/WP 21-40917
This paper presents mechanical and biological durability properties in soil beg test (soft-rot test) and field test (grave-yard test) against subterranean termite of the wood modified with an aqueous vinylic derivative of glycerol/polyglycerol or maleic anhydride cured in an opened or in a closed system. Wood modification was performed through impregnation of European beech (Fagus sylvatica) with ...
M Mubarok, H Militz, S Dumarcay, I W Darmawan, Y S Hadi, P Gerardin


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang