IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1244 documents. Displaying 25 entries per page.


Which fungi should be included in the laboratory evaluation of anti-stain chemicals?
2001 - IRG/WP 01-20236
Test fungi for efficacy tests of anti-stain formulations were selected based on the assumptions that test fungi should be fungicide-tolerant antagonists and fungi resistant to both fungicides and fungicide- tolerant antagonists, and such fungi should be re-isolated from treated samples with the highest fungicidal concentration used for laboratory evaluation of fungicides. This paper discusses the ...
Hyung-Jun Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


Blue Stain Testing of Alkyd and Acrylic Stains
2003 - IRG/WP 03-20273
Resistance against blue stain of semi-transparent alkyd and acrylic stains was tested by both EN 152 and the so-called reverse exposure test methods. Comparison of the results, obtained by both methods was the most important aim of this study. As expected, performance of the water-borne acrylic paint was lower compared to protective effectiveness of the alkyd stain. This difference was even more p...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Fenton's reagent as a modification tool in brown-rot decay
1996 - IRG/WP 96-10155
A biomimetic approach was used to clarify the role and importance of the Fenton-type reaction in the carbohydrate degradation by brown-rot fungi. Spruce sawdust and microcrystalline cellulose were modified in the H2O2/Fe(II) treatment. The degree of hydrolysis of the pretreated spruce sawdust was clearly increased with the complete cellulase (Econase), purified endoglucanase from Trichoderma reese...
M Rättö, A-C Ritschkoff, J Buchert, L Viikari


The full guideline for the “double layer test method” - A field test method for determining the durability of wood out of ground
2004 - IRG/WP 04-20290
This guideline describes a test method for wood to be exposed to the weather out of ground contact. The main objective of the method is to evaluate the durability of wood in above ground exposure as shifted overlaid stakes, which form the so called double layer. The method is applicable to the testing of untreated, treated and modified wood. Initially it was developed and found to be most useful ...
A O Rapp, U Augusta


Preservative effect of cellulose insulation material against some mould fungi and brown rot fungus Coniophora puteana in pine sapwood
1991 - IRG/WP 1484
The influence of mineral wool and loose-fill cellulose wool on biodeterioration of pine sapwood was studied. The test fungi were mould fungi Aspergillus versicolor, Cladosporium sphaerospermum, Penicillium sp. and Aureobasidium pullullans and brown rot fungus Coniophora puteana. Cellulose wool inhibited the growth of mould fungi on the face of wood contacted with insulation material at RH of 97 an...
H Viitanen


On the effectiveness of fumigants against wood-destroying insects and fungi in wooden cultural property
1993 - IRG/WP 93-10030
Based on a survey of the history of the use of fumigants the actual agents are mentioned in relation to their biogenic effect on wood-destroying insects and fungi as well as their corrosive behavior on cultural property. Furthermore the conditions for the use of reactive fumigants in buildings are discussed. Trials to control wood-destroying insects and fungi by nitrogen and bromomethane are the m...
W Unger, A Unger


On-site test for indicative determination of leaching of components of preservatives from treated timber
1993 - IRG/WP 93-50001-12
In the late eighties the environmental concern about treated timber increased and it is still a hot issue in the Netherlands. From the environmental point of view three phases in the timbers life cycle can be distinguished: - the production phase - the service life - the waste phase. In the Netherlands at this moment much emphasis is laid on the production phase. In 1992 this has led to a new legi...
W J Homan, H Militz


Biochemical relationships between biodegradation of cellulose and formation of oxalic acid in brown-rot wood decay
1991 - IRG/WP 1472
Non-enzymic hydrolysis of cellulose with low concentrations of oxalic acid was examined. The incubation of pine wood pulp with 1% oxalic acid (pH 1.3) at 35°C for 4 weeks reduced the original viscosity to 60%. Reducing sugars were liberated from various cellulosic samples by the oxalic acid treatment. However, crystallinities of cellulose in those samples did not change before and after the treat...
M Shimada, Y Akamatsu, A Ohta, M Takahashi


A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman


Effect of mini-block test conditions on activity of Coniophora puteana
2000 - IRG/WP 00-20184
The influence of various factors of the mini-block test method on growth and activity of different strains of Coniophora puteana was studied. Decay rates of spruce samples in Petri dishes of different depths, at different wood fibre orientations and at various distances between growth medium and wood were compared. In deep Petri dishes, there were no significant differences between activity of the...
F Pohleven, M Petric, J Zupin


Effect of treating process on efficacy of CCA in a laboratory decay test
1990 - IRG/WP 3628
Test samples of Pinus radiata sapwood measuring 40x40x500 mm³ were treated with a range of concentrations of the copper-chrome-arsenate (CCA) formulation "Tanalith C" using Rueping (empty cell), Lowry (empty cell) and Bethell (full cell) treatment processes. Samples were then reduced to 40x40x7 mm³ test blocks and exposed to the decay fungus Coniophora puteana using an agar/block technique. Repl...
M E Hedley, K Nasheri, J G Van der Waals


The natural durability story
1997 - IRG/WP 97-20119
Wood species with superior natural durability were in use since the beginning of timber utilisation. Their importance decreased with increasing industrial timber impregnation. In recent time, however, they gained worldwide new interest due to environmental problems involved with treated timber. In Europe a special Standard (EN 350) has been published and a multinational research project on testing...
H Willeitner, R-D Peek


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown


An Australian test of wood preservatives. Part 1: Preservatives, principles and practices
1978 - IRG/WP 2123
Between November, 1963, and July, 1964, a graveyard test of some 6000 preservative-treated stakes was installed at 8 sites equally distributed between Papua New Guinea in the tropics, through Queensland and New South Wales to Victoria. More than 40 different preservatives and preservative mixtures, mostly at several different levels of retention, were used to impregnate sawn specimens of Pinus rad...
J Beesley


Oxalic acid quantification, oxaloacetase assay and ESI localization of P, C, and Fe from the brown rot fungus Postia placenta
1994 - IRG/WP 94-10063
The mechanism by which brown-rot fungi initiate depolymerization of holocellulose in wood remains unknown. Recently, oxalic acid (OA) has received considerable attention in cellulose breakdown by brown-rot fungi. The OA could serve as a proton donor for hydrolytic or an electron donor for oxidative (Fenton's reaction-H2O2/Fe2+) cleavages of cellulose. The acid may originate via oxaloaceta...
C R Jordan, W V Dashek, T L Highley


Comparative study of lignocellulolytic activities of Pleurotus spp. and white rot and brown-rot fungi
1997 - IRG/WP 97-10210
In this work, the in vitro species of Pleurotus (P.eringii, P. cornucopiae and P. ostreatus), from structures of degraded wood have been studied. This degradative activity was compared to those presented by Trametes versicolor (fungus characteristic of white rot) and Gloeophyllum trabeum (fungus representative of brown rot). The activities studied were the following: cellulase, xylanase, pectinase...
D Muñoz-Mingarro, F Llinares, M T De Troya, F Rubio, M Yuste, C Rodríguez-Borrajo, J E Garcia de los Rios, F Alvarez, P Jiménez, A Rojas, A Navarrete, P Reche


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 21: Report of eighth inspection (7 years) in Australia
1985 - IRG/WP 4119
This report tabulates the seven year (86 month) inspection results, obtained on 28 Fabruary l985, of the IRG/COIPM International Marine Test at Goat Island, Australia. This test was installed in December 1977. The results are given in Tables 1-6. Table 7 lists the number of marine borers identified from blocks (2 cm and 6 cm long respectively) cut from the ends of specimens removed at the previous...
L J Cookson, J E Barnacle


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 2: Comparison of Static and Dynamic Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20320
In routine in-ground stake tests of wood preservatives at the BAM test field Horstwalde and in the BAM fungus cellar periodical determinations of both static moduli of elasticity (MOE) on the basis of bending tests and dynamic MOE on the basis of the vibration method were performed as a possible method for the assessment of fungal attack. As expected from other publications, the absolute values of...
M Grinda, S Göller


Evidence for the participation of the osmiophilic particles in the enzymatic demethylation of lignin
1984 - IRG/WP 1239
Transmission electron microscopic observations of the white-rot fungi Trametes hirsuta and Phanerochaete chrysosporium grown on a series of wood pulp with a graded lignin content and mycelium from the clarified centre of an agar-medium containing lignin (E1-effluent from the bleaching process) showed that osmiophilic particles are only induced by native lignin. Taking into account that the osmioph...
K Messner, H Stachelberger


Proposed model for the penetration and decay of wood by the hyphal sheath of the brown-rot fungus Postia placenta
1989 - IRG/WP 1391
Scanning electron microscopy (SEM) of Pinus sp. decayed by the brown-rot fungus Postia placenta confirmed the existence of extracellular membranous structures previously described by transmission electron microscopy (TEM). These structures appear to be an integral part of the hyphal sheath and assume a variety of forms including lamellar sheets, fibrils, and vesicles. These structures were observe...
F Green III, M J Larsen, L L Murmanis, T L Highley


Production of exraxellular hydrogen peroxide and oxalic acid by brown-rot fungus Poria placenta
1995 - IRG/WP 95-10112
Hydrogen peroxide and oxalic acid have been suggested to be essential in the degradation of wood carbohydrates by brown-rot fungi. Hydrogen peroxide has been suggested to be one of the diffusible low molecular weight agents produced by brown-rot fungi for the degradation of wood carbohydrates by generating highly active radicals. The production of hydrogen peroxide and oxalic acid by Poria placent...
A-C Ritschkoff, M Rättö, J Buchert, L Viikari


Preservative treatment and field test monitoring of spruce pole stock: Pressure and diffusible chemical treatments
1990 - IRG/WP 3605
One hundred and forty four spruce (test species) and southern yellow pine (reference species) poles were variously treated by center boring, incising, or kerfing, followed by pressure treatment with CCA and/or diffusible preservatives. The diffusible preservatives included NaF/creosote, borax and ammonium bifluoride. The poles were set at a test site and evaluated for preservative distribution and...
B Goodell, A J Pendlebury


Early detection of brown-rot decay in southern yellow pine using immunodiagnostic procedures
1990 - IRG/WP 2356
Immunodiagnostic procedures have been used to detect incipient decay of southern yellow pine by six common brown-rot fungi. Rabbit polyclonal antibodies were raised to liquid culture fractions of the six fungi. The antibodies, after preadsorption to sawdust, were tested in particle agglutination assays, immuno-dot blot, and ELISA for their·ability to detect the decay organisms when they were grow...
C A Clausen, F Green III, T L Highley


Previous Page | Next Page