Common Decay Micromorphology “Anomalies” Challenge Current Decay Classification
2006 - IRG/WP 06-10578
Decay micromorphology was studied systematically for diversely preservative treated Pinus radiata and Fagus sylvatica 20 x 20 x 500 mm stakes across 13 in-ground field test sites, during a 6.5 year exposure. New insight into the micromorphology of the early stages of decay enabled new and more detailed interpretation of the mechanism of their formation and suggested that current decay classificati...
R Wakeling


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


Biological resistance of didecyl dimethyl ammonium tetrafluoroborate (DBF)-treated wood in soil-bed and Basidiomycetes tests
2006 - IRG/WP 06-30393
This study evaluated the decay resistance of treated wood with a new quaternary ammonia compound, didecyl dimethyl ammonium tetrafluoroborate (DBF) in laboratory soil bed and Basidiomycetes tests. Treated sugi sapwood specimens with DBF at various concentration levels were first subjected to soil bed tests using two types of soil. The specimens subjected to soil bed tests were then used for Basidi...
S N Kartal, C Brischke, A O Rapp, Y Imamura


Phenol oxidase activity and one-electron oxidation activity in wood degradation by soft-rot deuteromycetes
2007 - IRG/WP 07-10615
Wood degradation, one-electron oxidation activity as assayed by ethylene generation from 2-keto-4-thiomethylbutyric acid (KTBA), and phenol oxidase activity were measured in cultures of six deuteromyce fungi, with glucose or wood as the carbon source. The four fungi that degraded Japanese beech wood had higher one-electron oxidation activities in wood-containing cultures than in glucose-containing...
H Tanaka, M Yamakawa, S Itakura, A Enoki


Detection of Anti-Fungal Sapwood Extractives in Non-Durable Scots Pine (Pinus sylvestris), Rubberwood (Hevea brasiliensis) and Jelutong (Dyera costulata)
2007 - IRG/WP 07-10634
A general laboratory bioassay method of Woodward and Pearce (1985) was adopted to detect anti-fungal activity of sapwood or heartwood extractives of 5 Malaysian hardwoods [dark red meranti heartwood (Shorea spp.), red balau heartwood (Shorea spp.), kulim heartwood (Scorodocarpus borneensis), jelutong sapwood (Dyera costulata) and rubberwood sapwood (Hevea brasiliensis), including the temperate Pin...
A H H Wong, R B Pearce


Soft Rot Determines Service Life of L-joints with Low Borate Loading
2008 - IRG/WP 08-30470
As part of a research program on the potential use of borates by the Canadian wood products industry, Forintek set up an L-joint test of untreated and borate-diffusion treated hem-fir (western hemlock and amabilis fir) in 1990. The treated material had a low initial retention of only 0.2% boric acid equivalent and analysis after 5 years revealed no detectable borate close to the tenon. Nev...
P I Morris, J Wang, J K Ingram


Feasibility study on three furfurylated non-durable tropical wood species evaluated for resistance to brown, white and soft rot fungi
2008 - IRG/WP 08-40395
Furfurylation can protect non-durable wood species against biological degradation, but the method used today cannot fully protect the heartwood of Scots pine due to insufficient penetration. In order to test alternative wood substrates for furfurylation, three Malaysian grown wood species (Kelempayan, Rubberwood and Sena) were furfurylated and subjected to soil block decay testing. Their performan...
T Mark Venås, A H H Wong


Australian trials on the efficacy of micronized copper
2008 - IRG/WP 08-30480
Alkaline copper quat (ACQ) is an established wood preservative that is formulated with solubilised copper in amine solvent. This paper describes three separate trials in Australia that investigated whether substituting soluble copper with micronized copper affects performance. ACQ and micronized copper quat (MCQ) gave similar performance in Pinus radiata against four brown-rotting fungi in a soil-...
L J Cookson, J W Creffield, K J McCarthy, D K Scown


Effect of a biological treatment on below ground decay of Douglas-fir pole sections
2008 - IRG/WP 08-40433
The use of exogenous sugars to accelerate microbial growth and eventually limit available oxygen in soil surrounding wood in soil contact was investigated on untreated Douglas-fir poles exposed over a 3 year period in Western Oregon. Isolation frequencies differed markedly between treated and untreated poles and the treatment did appear to shift the frequency of some basidiomycetes. The treatment ...
C Freitag and J J Morrell


Effect of different ASAs (alkenyl succinic anhydrides) on the treatment of biological protection of wood in use class 4
2008 - IRG/WP 08-40440
The alkenyl suscinic anhydrides (ASAs) used in this work are adducts resulting from the maleinization reaction of fatty acid alkyl esters. Various products with different alkyl groups were synthesized from rapeseed (Brassica napus) oil esters, rich in oleic acid. The liquids obtained showed a viscosity similar to that of vegetable oils and a brown color. When applied into wood, a thermal treatment...
C Vaca-Garcia, O Pignolet


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


A Comparison of the Performance of Related Copper Based Preservatives against Soft Rot
2010 - IRG/WP 10-30540
The performance of pine and beech wood treated with either a soluble copper + quat (ACQ type D) preservative system or a particulate copper + quat system was evaluated in unsterile soil using the European standard ENV 807 soft rot decay test procedure. In addition, to compare soft rot performance of soluble and particulate copper directly without the influence of co-biocides, beech and pine test...
M Ray, D Dickinson, K Archer


Testing of decay resistance of sapwood and heartwood of thermally modified Scots pine and Norway spruce
2010 - IRG/WP 10-40523
Thermal modification at elevated temperatures changes the chemical, biological and physical properties of wood. One of the main targets of thermal modification is to increase the biological durability and decay resistance of wood. Although the effects of thermal modification on wood have been widely studied, the significance of sapwood and heartwood on the resistance of thermally modified wood has...
H Viitanen, S Metsä-Kortelainen


Bioresistance of Poplar Wood Compressed by Combined-Hydro-Thermo-Mechanical Wood Modification (CHTM) Process
2010 - IRG/WP 10-40532
Bioresistance of treated Poplar wood by CHTM process (Combined-Hydro-Thermo-Mechanical Wood Modification) was studied in the current research work. Resistance against brown rot fungus Gloeophyllum trabeum as well as the soft rot decay was the main concern of this work. Poplar wood blocks were hydrothermally treated at temperatures of 120,150 and 180°C for holding time of 0, 30 and 90 min. afterwa...
L Khademi-Bami, B Mohebby


Influence of soil moisture, Sarawak soil types and decay types on decay susceptibility of rubberwood and kelempayan
2012 - IRG/WP 12-10780
Wood and soils are important natural resources of the land, the former widely used as structural supports in contact with the latter. Many low durability wood species exposed to soil contact has reportedly high incidence of decay failures in poorly treated and untreated materials depending on soil types, properties and soil microbial virulence. This paper probes the relationship of the main soil t...
A H.H. Wong, P K.F. Chong, J Sabang


Evaluation of Five Novel Organotin(IV) Complexes as Wood Preservatives
2012 - IRG/WP 12-30590
Three selected non durable tropical wood species namely Alstonia scholaris (pulai), Macaranga triloba (mahang) and Hevea brasiliensis (rubber) were chemically impregnated with five novel organotin(IV) complexes using vacuum-pressure treatment method. The objectives of this study were to determine the treatability and efficacy of novel organotin(IV) complexes against white and brown rot decay fungi...
M M Rahman, I Jusoh, M A Affan, A Husaini


Classifying white rot decay resistance of some hardwoods from Sarawak and Peninsular Malaysia and correlations with their tropical in-ground durability
2012 - IRG/WP 12-10788
White rot wood decay under Malaysian (humid tropical) terrestrial conditions pose more serious threats to the in-ground service life of hardwoods than other common fungal decay types. A study is made on decay resistance variation for a total combined list of 30 Peninsular Malaysian and Sarawak timber species (plus 6 exotic reference temperate commercial woods for comparison) using the laboratory s...
A H H Wong, J M E Jem, Lai Jiew Kok


Preliminary evaluation of degradation patterns in wood samples from the Yenikapı shipwrecks
2013 - IRG/WP 13-10798
The uncovering of several shipwrecks during the excavation of the Marmaray Rail Tube Tunnel Project in Istanbul provides an important opportunity to evaluate waterlogged woods buried for centuries. Identification of these woods showed that a variety of species was used in the ships. One shipwreck (a galley) from the Yenikapı Marmaray was examined using electron microscopy. The micrographs rev...
C Köse, A M Taylor


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Incidence of soft rot attack on preservative treated Douglas-fir poles: a preliminary survey
2014 - IRG/WP 14-10818
Occurrence of soft rot decay in Douglas-fir poles treated with ammoniacal copper zinc arsenate (ACZA) or pentachlorophenol in oil was studied. Soft rot was less prevalent in poles treated with penta, but some soft rot was found in approximately 20 % of poles examined. Soft rot was more common in poles treated with ACZA, and, when present, was found in almost 20% of the cells examined. The potenti...
P Torres Andrade, J J Morrell


Identification of soft-rot fungi existed in the samples from the galley excavated at Yenikapi
2014 - IRG/WP 14-10833
The shipwrecks of the Middle Byzantine period were excavated during the construction of the Marmaray railway and metro station in Yenikapı between 2004 and 2012. This has become the largest investigations because of the size and the number of the shipwrecks and its associated artifacts. In the previous report, the electron micrographs of the samples revealed that a wide range in the degree of...
T Wada, C Köse, K Igarashi


Variability in durability of some selected South-American wood species
2014 - IRG/WP 14-10831
Within the scope of sustainable forest management one wants to encourage the proper use of lesser known wood species. Therefore the market has to shift from a demand-driven towards a supply-driven market without loss of wood quality. It is generally known that the durability from pith to bark varies thus, affecting the overall durability of wood species. Consequently, a detailed analysis is necess...
I De Windt, P ’t Hooft, J Van den Bulcke, J Van Acker


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao