Analysis of degradation observed on ancient wooden objects buried underground
2001 - IRG/WP 01-10403
Ancient wooden objects were sometimes excavated from the moat of mounded tombs in Japan. Such wooden objects were in the shape of a sunshade, bird, shield, pole, yugi(a bag that holds arrows) among others. Archaeologists discussed the usage of such shaped objects, but no one could clearly explain their use. Some objects were observed using an ordinary microscope. Deterioration by bacteria was foun...
H Sakai


The use of plastic meshes in soft rot monoculture testing
1990 - IRG/WP 2353
Plastic meshes were introduced between the wood blocks and agar medium in a miniaturised soft rot monoculture test in order to minimise transfer of the preservative from the wood and mineral salts from the agar. Although several different sizes and types of mesh were used and the blocks were wetted up to an appropriate moisture content for soft rot attack the amount of decay was substantially redu...
S M Gray


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Polyflavonoid tannins - From a cause of CCA soft-rot failure to the "missing link" between lignin and microdistribution theories
1986 - IRG/WP 3359
Polyflavonoid tannins are proven to be fast-reacting with CCA solutions and hence, to be strong competitors of the structural wood constituents for fixation of CCA preservatives. The consequence of this effect is that even relatively small amounts of tannin cause severe undertreatment of the structural wood constituents which in turn badly affects the long term durability of CCA-treated timber. Th...
A Pizzi, W E Conradie, M Bariska


Soft rot fungi as possible sources of odor in impregnated wood in buildings
1993 - IRG/WP 93-20013
Wood preservatives are frequently used inside houses. In several cases impregnated wood, particularly when used in crawlspaces or other near-ground constructions, has been found to be a source of odor. Mold fungi, soft rot fungi actinomycetes or bacteria growing on impregnated wood are possible producers of the odor. Analyses of volatile emissions from impregnated wood with odor and pure cultures ...
J Bjurman, J Kristensson


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


Ultrastructure of degraded, CCA-treated Pinus radiata wood from a marine pile
1990 - IRG/WP 1461
During an inspection of marine piles, 12 years after installation, severe degradation was noted on one of them in the vicinity of a corroded eye-bolt. The wood was dark brown in colour and tended to crumble easily. Wood fragments were examined by light microscopy and scanning and transmission electron microscopy and were also analysed for carbohydrates and lignin. Light microscopy showed numerous ...
A P Singh, M E Hedley


The evaluation of the occurrence of soft rot in creosoted wooden poles
1988 - IRG/WP 1368
The occurrence of soft rot decay in creosoted wooden poles for overhead power lines was investigated by collection of field samples, their subsequent microscopic examination and statistical analysis of the data collected. Examination of samples collected from 296 poles revealed that approximately 15% of the pole population studied (Eastern Electricity Board) showed the presence of soft rot decay. ...
A Wylde, D J Dickinson


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


High CCA retentions and the protection of eucalypt power poles
1983 - IRG/WP 3226
Tasmanian power pole material treated to high retentions, was analysed to accurately determine the amount of CCA preservative in the timber. Material from the same disc was subsequently exposed in unsterile soil in order to determine the effectiveness of treatment. Results showed that even at high retention levels, soft-rot attack was not prevented. Fourteen further poles were sampled, but this ti...
L E Leightley, J Norton


Soft rot tests
1983 - IRG/WP 2206
At the IRG meeting in Turkey it was proposed that developments in testing preservative-treated wood in unsterile soil according to techniques variously described as "fungus cellar", "soil-bed", or "accelerated field simulation" be considered along with conventional laboratory procedures as the basis for a standard test. Before formulating any co-operative test programme it is essential to examine ...
J A Butcher


The possible significance of the lignin content and lignin type on the performance of CCA-treated timber in ground contact
1988 - IRG/WP 1357
The lignin in wood samples of Alstonia scholaris, Octomeles sumatrana and a Simaruba species have been analysed. These timbers are characterised by a high lignin content and low syringyl:guaiacyl ratios. Decay tests with two soft rot fungi showed that the timbers were less susceptible than timbers with a low lignin content and higher syringyl:guaiacyl ratios. Numerous data for field performance of...
T Nilsson, J R Obst, G F Daniel


Soft-rot problems with treated hardwoods: A paper for discussion and establishment of a programme of work
1974 - IRG/WP 331
At the 5th meeting of IRG in Lahti (June 1973) it was decided that an ad hoc group should be formed to study these problems. It was decided that it's activity could be usefully directed in two main areas; a) in the encouragement and direction of existing research in this field, and b) in the organising of a collaborative field trial involving interested parties using locally important har...
D J Dickinson


Identification of terminal structures in cellulose degraded by the brown-rot fungus Postia placenta
1989 - IRG/WP 1389
To gain insight into the biochemical mechanism employed by brown-rot fungi to depolymerize cellulose, we identified the end-groups of chemically pure cellulose that had been depolymerized by the brown-rot fungus, Postia placenta. The depolymerized cellulose was acid hydrolyzed and the anion fractions isolated by ion chromatography. Sugar acids were identified by gas chromatographic and mass spectr...
T K Kirk, T L Highley, R E Ibach, M D Mozuch


Practical consequences of the clarification of the chemical mechanism of CCA fixation to wood
1983 - IRG/WP 3220
Practical consequences derived from the chemical investigation of the mechanism of fixation of CCA to the wood constituents are discussed. Among these, formulas for the calculation of the time of hexavalent chrome fixation are presented. Furthermore, three parameters are shown to be important to the long-term effectiveness of CCA-treated timber: (i) the temperature of treatment, (ii) the initial p...
A Pizzi


Evaluation of substituted isothiazolone as a potential new wood preservative
1984 - IRG/WP 3306
Laboratory decay tests were carried out with isothiazolone (4,5-dichloro-2-n-octyl-4-isothiazolone-3-one) treated wood. This compound was found to be extremely effective against three common wood decaying brown-rot fungi, exhibiting toxic threshold values in the range of 0.37 to 0.50 kg/m³. For the white-rot fungus, Coriolus versicolor, the toxic threshold values for treated pine and sweetgum wer...
D D Nicholas, A F Preston, D E Greenley, S V Parikh


An illustrated comment on the soft rot problem in Australia and Papua New Guinea
1977 - IRG/WP 296
A brief survey of soft rot is presented, with particular reference to attack of preservative treated hardwood transmission poles in Australia. Possible explanations of why the preservatives are failing to protect the poles are discussed, together with current efforts to produce control measures. Examples of soft rot in variously treated eucalypt or pine specimens are shown to illustrate the morpho...
H Greaves


Fungus cellar testing as an evaluation method for performance of treated timber in ground contact
2001 - IRG/WP 01-20227
A fungus cellar method for the accelerated evaluation of performance of treated wood in ground contact is described. The test soil comprised of sandy loam, vermiculite and Japanese horticulture soil "Kanumatsuchi" in a ratio of 6:2:2 by volume. The soil was inoculated with the dominant test fungus isolated with selective medium from decayed wood samples. Pairs of treated and untreated wood specime...
Y Nagano


CCA modifications and their effect on soft rot in hardwoods. Part 2
1983 - IRG/WP 3244
The work outlined in this document is a continuation of that presented in Document No: IRG/WP/3201. The findings described in the previous paper are summarised below: a double treatment of CCB followed by arsenic (CCB+A) is more effective than a double treatment of boron followed by CCA (B+CCA) or a single treatment of CCA, CCB or CCAB in controlling soft-rot due to Chaetomium globosum in birch. C...
S M Gray, D J Dickinson


Supplementary experiment to the main trial (IRG/WP/367, 384) to determine the performance of preservative treated hardwoods with particular reference to soft rot
1977 - IRG/WP 3101
The field experiment being carried out by the IRG (described in document IRG/WP/367) is designed to obtain information on the performance of a preservative in different hardwoods in ground contact. A total of 57 timber species is being examined and 36 different field sites are involved representing a complete range of climatic conditions. IRG document WP/384 describes the treatment details of the ...
F W Brooks, C R Coggins, D J Dickinson


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 2: Laboratory fungal bioassays
2000 - IRG/WP 00-20204
Extracts from sawmill residues of the naturally durable white cypress, Callitris glaucophylla were tested for fungicidal activity in a series of laboratory bioassays. The effects of different extraction solvents, techniques and sources of material on the biocidal efficacy of the resultant extracts were evaluated. Soil jar decay tests were used initially however, contractual time constraints necess...
M A Powell, L M Stephens, L Francis, M J Kennedy


The natural durability assessment of secondary hardwood species - laboratory tests
1998 - IRG/WP 98-10295
Laboratory tests have been undertaken to assess the natural durability of 16 species of lesser known hardwoods, or hardwoods from non-traditional sources, including teak from three different plantations. Resistance to decay by both basidiomycetes and soil-inhabiting micro-fungi has been established. ´The data indicated that published information on the durability of these timbers should be treat...
J K Carey, S J Hendry


An electron spin resonance study of manganese changes in wood decayed by the brown-rot fungus, Postia placenta
1988 - IRG/WP 1359
Electron spin resonance (ESR) spectrometry was used to examine wood decay by the brown-rot fungus, Postia placenta. Wood slivers of Douglas-fir, white fir, redwood, sweetgum and yellow poplar were incubated for 4 weeks in custom-made quartz ESR tubes with or without Postia placenta. In all wood species without fungus, a weak partially resolved signal (about g=2, presumably due to manganese) was de...
B Illman, D C Meinholtz, T L Highley


Collaborative soft rot tests: Paper for discussion in Working Group II
1970 - IRG/WP II 5A
An account of the major part of the collaborative work on laboratory tests of toxicity of preservatives to soft rot fungi initiated by the European Homologation Committee at Delft in 1966 has been published in ‘Material und Organismen’ (1970) as a report of progress. The main objective of these collaborative tests, namely to establish a reliable and acceptable standard test method was not acco...
J G Savory, A F Bravery


Occurrence, prevention and repair of Dry Rot
1990 - IRG/WP 1439
Information about the frequency, detection, identification and repair of Dry Rot attacks (Serpula lacrymans) is summarized from 13 European countries. Based on 28 completed and returned questionnaires it appears that Dry Rot attacks are recognized in all countries participating, and that there is an appreciable similarity in the frequency of attacks and methods of detection and identification. How...
A P Koch