IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1536 documents. Displaying 25 entries per page.


Decay resistance of densified ammonia-plasticized stems of oil palm (Elaeis guineensis)
1991 - IRG/WP 3673
When wafers of oil palm stems (Elaeis guineensis) were plasticized with 28% aqueous ammonia and immediately compressed mechanically, the treated material, gained 73% in basic density (average basic density, 0.695 g/cm³), and was highly resistant to decay by wood rot basidiomycetes. Compared with the control specimens (density, 0.403 g/cm³), resistance to decay of the densified specimens by Corio...
A H H Wong, M P Koh


Bacteria are important degraders of cooling tower timbers: New Zealand experience
1995 - IRG/WP 95-10128
Microscopic examinations of CCA-treated Pinus radiata timbers in industrial cooling towers in New Zealand showed bacteria and soft rot fungi to be primarily responsible for the decay of these timbers. Of these micro-organisms, erosion bacteria appeared to be most widespread, attacking wood cell walls independently as well as together with tunnelling bacteria and soft rot fungi. Tunnelling bacteria...
A P Singh, R N Wakeling


The dry rot fungus (Serpula lacrymans) in nature and its history of introduction into buildings
1999 - IRG/WP 99-10300
For many years the True dry rot fungus (Serpula lacrymans (Wulf.: Fr.)Schroet.) has exclusively been found in buildings. That is why it is called the True dry rot fungus. The origin of the fungus has always been a mystery, but a wild ancestor must have occured. In the literature there is some information about finds of Serpula lacrymans in nature, however it is difficult to distinguish it from the...
J Bech-Andersen, S A Elborne


Dimensional lumber model demonstrates the sensitivity of the particle capture immunoassay in early detection of brown-rot fungi
1995 - IRG/WP 95-20058
A dimensional lumber model was designed to test the sensitivity of the particle capture immunoassay (PCI) compared to traditional methods of culturing and microscopic examination for detection of brown-rot fungi. Southern yellow pine 2 x 4's (5.1x10.2 cm²), and 86.4 cm in length, were inoculated on one end with the brown-rot fungus, Postia placenta, and tested over the full length of the...
C A Clausen, L Ferge


Detection of brown-rot antigens in southern pine
1996 - IRG/WP 96-20090
Brown rot fungal antigens were detected by particle capture immunoassay (PCI) in southern pine 2 x 4's beyond visible or culturable hyphal growth. Further analysis of test samples revealed changes along the 2 x 4's that could be grouped into zones. Zone 1, the point of inoculation through 6 cm, showed low pH, measurable oxalic acid, high moisture, and high protein. Zone 2, throug...
C A Clausen


An evaluation of the efficacy of a chlorothalonil formulation and a chlorothalonil plus chlorpyrifos formulation in the field
1993 - IRG/WP 93-30005
Details on the treatment of Pinus radiata D. Don and Eucalyptus regnans F. Muell. sapwood specimens to three retentions of each of two preservative formulations (chlorothalonil in oil; chlorothalonil plus chlorpyrifos in oil) and their installation below ground at three field test sites in Australia are given. Specimens were treated with each formulation to achieve 3.2, 6.4 and 12.8 kg/m³ of chlo...
J W Creffield, N Chew


Lignin degradation by a non-enzymatic system supposed to be active in white rot fungi
2000 - IRG/WP 00-10340
Electron microscopic investigations have shown that ligninolytic enzymes of white-rot fungi are only able to penetrate the wood cell wall in late stages of degradation. Thus, the selective degradation of lignin of certain white-rot fungi can only be explained on the basis of a low molecular weight, highly diffusible system. A system, consisting of copper, a coordination compound and either H2O2 or...
P Lamaipis, W Gindl, T Watanabe, K Messner


Evaluation of the european standard ENV 12038 for durability testing of plywood
2001 - IRG/WP 01-20237
The latest improved version of the standard ENV 12038 drafted as document N44 by CEN Technical Committee 38 (WG 7 - WG 23) is used to evaluate the effect of wood composition and structure on plywood durability. The method described is based on the agar-block test of the EN 113 standard used for the determination of the efficacy of wood preservatives and the assessment of the natural durability of ...
J Van Acker, M Stevens, E De Clercq


Durability of surface coating systems. Mycologg - an accelerated mycological test.
2004 - IRG/WP 04-20301
Field testing and natural aging/degradation of test sample, e.g. coated wooden surfaces is a slow process. Accelerated tests focus on mechanical properties, water uptake or sometimes stain fungi. Artificially weathered coated panels are not easily compared with naturally aged panels, and show the importance of involving the biological component among the degrading facors. It is a need for acce...
L Ross Gobakken, J Mattsson, B Jacobsen, F G Evans


Hemicellulosic induction of oxalic acid in Postia placenta
1994 - IRG/WP 94-10060
Most studies suggest that enzymes produced by brown-rot fungi are too large to penetrate sound wood structures, even after decay begins. Thus, nonenzymatic agents have been proposed to initiate brown-rot decay. We have reported that the brown-rot fungus Postia placenta MAD-698 initiates a 2-fold decrease in wood pH within 7 days of colonization which is mediated by production of oxalic acid. Strai...
F Green III, M Larsen, T L Highley


Biological resistance of wood treated with waterbased resins and drying oils in a mini-block test
1998 - IRG/WP 98-40107
In recent years it was found that the resistance of wood against fungal degradation could be increased by impregnation with an etherificated melamine formaldehyde resin. Using this resin as a reference, a waterbased fatty acid modificated alkyd-resin and two drying-oils were assessed for their biological performance in a mini-block laboratory test. Although drying-oils, like linseed-oil, are often...
M Sailer, A O Rapp, R-D Peek


Comparison of methods for monitoring CCA fixation
1994 - IRG/WP 94-40023
The CCA fixation status in the outer 12.5 mm of pole sections of southern pine (Pinus sp.), red pine (Pinus resinosa) and lodgepole pine (Pinus contorta var. latifolia) were followed during fixation at 21°C under non-drying conditions by the following procedures: - Qualitative CrVI indication by the chromotropic acid spot test. - Quantitative CrVI in the expressate by the diphenylcarbazide method...
P A Cooper, Y T Ung, G Zanjani


Field trials of Sinesto B at some sawmills in Portugal
1989 - IRG/WP 3512
The efficacy of SINESTO B as antistain chemical for use in Portugal has been studied. The studies were done during the years 1987-1988 at several Portuguese sawmills in co-operation with the Instituto dos Produtos Florestais and the APCIM (Associacao Portuguesa de Comercio e Industria de Madeiras). SINESTO B was used in 5% and 8% concentrations. The storage time varied from 10 weeks to 6 months. I...
I A Linderborg


A bibliography of the dry rot fungus, Serpula lacrymans
1988 - IRG/WP 1337
For many decades the occurrence of dry rot in buildings has been the cause of serious concern in temperate regions of the world. Consequently, much effort has concentrated on determining the morphology of dry rot and on finding means of prevention and control. During early studies, observers tried to understand the phenomenon of dry rot as a whole, and in the course of the 19th century aspects cha...
G Seehann, B M Hegarty


Tolerance of Wood Decay Fungi to Commercial Copper Based Wood Preservatives
2002 - IRG/WP 02-30291
Due to the use of copper based preservatives like CCB or CCA for more than a century, copper tolerant fungi have appeared in some European countries in recent times. It is therefore important to find out whether this phenomenon is specific for only classical copper ingredients, or generally for all copper based formulation. Thus, we tested the tolerance of three commercial copper based pres...
F Pohleven, M Humar, S A Amartey, J Benedik


Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


The long road to understanding brown-rot decay. A view from the ditch
1995 - IRG/WP 95-10101
Interest in understanding how brown-rot fungi decay wood has received increasing interest in recent years because of a need to identify novel targets that can be inhibited for the next generation of antifungal wood preservatives. Brown-rot fungi are unique in that they can degrade holocellulose (cellulose and hemicellulose) in wood without first removing the lignin. Furthermore, they degrade holoc...
F Green III, T L Highley


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 18. Report of seventh inspection (72 months) in Australia
1984 - IRG/WP 4108
This report includes the results for the 72 month inspection of the IRG/COIPM International Marine Test installed in Sydney Harbour. Although, overall, attack by teredinid and limnorid borers have been most commonly encountered in test specimens at this site, slight attack, mainly by sphaeromatids, has recently been initiated on some hitherto unattacked treated Alstonia scholaris and Pinus sylvest...
L J Cookson, J E Barnacle


Evaluation of a new anti-sapstain formulation
1994 - IRG/WP 94-30035
A new anti-sapstain mixture, which consists of 2% IPBC (3-iodo-2-propynylbutyl carbamate) and 1.5% DCOI (4,5-dichloro-2-n-octylisothiazolin-3-one), was evaluated by three methods in the laboratory. A standardized test (JWPA standard 2) demonstrated that the new anti-sapstain formulation was highly effective in controlling growth of monocultures of five test fungi on wood substrate. When exposed to...
K Tsunoda, H Kumagai, M Sakurai


A shower test protocol for measuring antisapstain wash-off from small individual log billets
1996 - IRG/WP 96-50069
According to New Zealand Timber Industry Federation statistics New Zealand exported 4,835,000 m³ of logs in 1994 and it is estimated that c. 20% were anti-sapstain treated. Loss of preservative from logs as a result of rain impact after application is of considerable concern both with respect to potential loss of efficacy and environmental contamination. Whilst Environment Canada have a proposed ...
A J Pendlebury, H Pearson


Effect of test site, preservative and wood species on decay type Glenbervie pastoral and radiata pine forest sites
2000 - IRG/WP 00-30248
Pinus radiata stakes were treated with 0.8, 1.2, 1.8, 2.7 and 4.1 kg/m3 of CCA and Fagus sylvatica with 2.7, 4.1 and 6.1 kg/m3 of CCA. Both wood species were also treated with equivalent retentions of a copper plus triazole preservative (CT) (0.89, 1.3, 2 and 3 kg/m3 of copper for pine & 2.5 and 4 for beech) and chlorothalonil plus chlorpyriphos in oil (CC) (1.4, 2.1, 3.2 and 4.8 kg/m3 of chlo...
R N Wakeling


Secretion of ligninolytic enzymes by hyphal autolysis of the white rot fungus Phanerochaete chrysosporium
1991 - IRG/WP 1480
The secretion of ligninases by Phanerochaete chrysosporium was investigated with polyclonal antibodies, followed by immmunogold-silver staining and light microscopy. After growing fungal mycelium on nitrocellulose, extracellular ligninases were detected around old, plasmaless hyphae, but not at arthrospores, chlamydospores, or blastoconidia. Labeling of fungal hyphae on coverslip cultures was obse...
R Lackner, E Srebotnik, K Messner


Field evaluation determining the toxic effect and diffusion properties of Impel, Improsol and TBTO-capsules in L-joints (spruce) for pretreatment application
1991 - IRG/WP 3641
Bonded joints (L-joints and T-joints) are especially at risk from water absorption (rain, condensation) over bare, unprotected radial wood surfaces (joggle joints). It is therefore quite certain that lasting protection against fungi attack cannot be guaranteed in the long term if the surface of coating is damaged. Therefore, in a field investigation, using L-joints (spruce) over a total period of ...
R Gründlinger, K Messner, O Janotta


The performance of metal-chromium-arsenic formulations after 32 to 38 years' in-ground exposure in Australia
2000 - IRG/WP 00-30240
Two trials of metal-chromium-arsenic preservatives were exposed in-ground in Australia. In Trial 1, Pinus radiata stakes treated with Boliden K.33, Boliden S.25, Celcure A, Tanalith C and Tanalith CA were installed at Sydney and Narrandera in 1961/1962. In Trial 2, P. radiata and Eucalyptus regnans sapwood were treated with Celcure A, Celcure A21-N, Celcure A 21-O and Tanalith CA (new) and install...
G C Johnson, J D Thornton, J Beesley


Previous Page | Next Page